Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation

  • Xiang CHEN ,
  • Wei CHEN ,
  • Yang ZHAO ,
  • Sheng LU ,
  • Xiaoqing JIN ,
  • Xianghe PENG
Expand
  • 1. School of Advanced Manufacturing Engineering, Chongqing University of Posts and Telecommunications, Chongqing 400065, China
    2. State Key Laboratory of Mechanical Transmission, Chongqing University, Chongqing 400044, China
    3. State Key Laboratory for Strength and Vibration of Mechanical Structural, Xi'an Jiaotong University, Xi'an 710049, China

Received date: 2019-06-18

  Revised date: 2019-11-10

  Online published: 2019-11-22

Supported by

National Natural Science Foundation of China(11802047);National Natural Science Foundation of China(51807019);Foundation and Frontier Projects in Chongqing City(cstc2016jcyjA0594);Foundation and Frontier Projects in Chongqing City(cstc2016jcyjA0443);Open Fund of State Key Laboratory for Mechanical Transmission(SKLMT-KFKT-201711);Open Fund of State Key Laboratory for Strength and Vibration of Mechanical Structures(SV2018-KF-28)

Abstract

The pipe joints based on shape memory alloy (SMA) are widely used in various fields of fluid transport by virtue of their simple structure, easy assembly and high reliability. However, due to the complexity of the NiTiNb constitutive model, the plastic deformation and its effects have yet not been considered in the report of pipe joint connection system. In view of this background, this work constructs an SMA joint-steel pipe system (J-P system) and performs the finite element numerical simulation of the assembling process based on an SMA phenomenological constitutive model, where in the plastic-phase transformation coupling effect is considered. By altering the diameter expansion, wall thickness, service temperature and critical phase transformation, the change features of the von Mises stress, contact pressure and pull-out force of the J-P system are investigated. The results show that due to the coupling effect of phase transformation and plastic deformation, the evolution of Mises stress, equivalent transformation strain and equivalent plastic deformation in SMA joint show obvious regularity during assembly: in the loading stage, the phase transformation strain and plastic deformation increase with the increase of predeformation. At each subsequent loading step, the plastic strain remains unchanged. At the unloading stage, von Mises stress decreases and phase transformation strain remains unchanged. With temperature increase, the phase transformation strain decreases significantly and von Mises stress increases. At subsequent loading steps, von Mises stress and phase transformation strain remains unchanged. Within a certain size, the pull-out force decreases with the increase of diameter expansion; Among the 9 schemes with different wall thickness ratios, the pull-out force changes non-linearly with the wall thickness, and there is an optimal connection performance scheme. Within the range of room temperature (0~40 ℃), the service temperature has little impact on the performance of the J-P system; With the increase of the critical phase transformation, the stress concentration layer within the SMA joint moves from the inside to the outside, and the pull-out force increases gradually within the range of the critical phase transformation from 0.07 to 0.14. The results also show that the stress concentration at the end of contact region can significantly increase the pull-out force of the J-P system.

Cite this article

Xiang CHEN , Wei CHEN , Yang ZHAO , Sheng LU , Xiaoqing JIN , Xianghe PENG . Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation[J]. Acta Metall Sin, 2020 , 56(3) : 361 -373 . DOI: 10.11900/0412.1961.2019.00197

References

[1] Quan D, Hai X. Shape memory alloy in various aviation field [J]. Proc. Eng., 2015, 99: 1241
[2] Dordoni E, Meoli A, Wu W, et al. Fatigue behaviour of nitinol peripheral stents: The role of plaque shape studied with computational structural analyses [J]. Med. Eng. Phys., 2014, 36: 842
[3] Hartl D J, Lagoudas D C, Calkins F T. Advanced methods for the analysis, design, and optimization of SMA-based aerostructures [J]. Smart Mater. Struct., 2011, 20: 094006
[4] Ochoński W. Application of shape memory materials in fluid sealing technology [J]. Ind. Lubr. Tribol., 2010, 62: 99
[5] Chen X, Peng X H, Chen B, et al. Experimental investigation to thermal-mechanical behavior of Ni47Ti44Nb9 SMA under pure tension and pure torsion [J]. J. Alloys Compd., 2014, 610: 151
[6] Zhang C S, Wang Y Q, Chai W, et al. The study of constitutional phases in a Ni47Ti44Nb9 shape memory alloy [J]. Mater. Chem. Phys., 1991, 28: 43
[7] Zhao L Z, Duerig T W, Wayman C M. Transformation and mechanical behavior of Ni47Ti44Nb9 shape memory alloy [A]. MRS International Meeting on Advanced Materials [C]. Tokyo, Japan, 1989: 171
[8] Shu X Y, Lu S Q, Li G F, et al. Nb solution influencing on phase transformation temperature of Ni47Ti44Nb9 alloy [J]. J. Alloys Compd., 2014, 609: 156
[9] Piotrowski B, Ben Zineb T, Patoor E, et al. Modeling of niobium precipitates effect on the Ni47Ti44Nb9 shape memory alloy behavior [J]. Int. J. Plast., 2012, 36: 130
[10] Arghavani J, Auricchio F, Naghdabadi R. A finite strain kinematic hardening constitutive model based on hencky strain: General framework, solution algorithm and application to shape memory alloys [J]. Int. J. Plast., 2011, 27: 940
[11] Hartl D J, Chatzigeorgiou G, Lagoudas D C. Three-dimensional modeling and numerical analysis of rate-dependent irrecoverable deformation in shape memory alloys [J]. Int. J. Plast., 2010, 26: 1485
[12] Yu C, Kang G Z, Song D, et al. Micromechanical constitutive model considering plasticity for super-elastic NiTi shape memory alloy [J]. Comput. Mater. Sci., 2012, 56: 1
[13] Zhou B, Zhao S C. A constitutive model of shape memory alloy with temperature memory effect [J]. Sci. Sin.(Phys. Mech. Astronom., 2013, 43: 1084
[13] 周 博, 赵士成. 考虑温度记忆效应的形状记忆合金本构模型 [J]. 中国科学: 物理学 力学 天文学, 2013, 43: 1084
[14] Peng X, Yang Y, Huang S. A comprehensive description for shape memory alloys with a two-phase constitutive model [J]. Int. J. Solids Struct., 2001, 38: 6925
[15] Brinson L C. One-dimensional constitutive behavior of shape memory alloys: Thermomechanical derivation with non-constant material functions and redefined martensite internal variable [J]. J. Intell. Mater. Syst. Struct., 1993, 4: 229
[16] Jiang S Y, Liang Y L, Zhang Y Q, et al.Influence of addition of Nb on phase transformation, microstructure and mechanical properties of equiatomic NiTi SMA [J]. J. Mater. Eng. Perform., 2016, 25: 4341
[17] Uchida K, Shigenaka N, Sakuma T, et al. Effects of pre-strain and heat treatment temperature on phase transformation temperature and shape recovery stress of Ti-Ni-Nb shape memory alloys for pipe joint applications [J]. Mater. Trans., 2008, 49: 1650
[18] Chen B. Research of micro and macro mechanical behavior of Ni47Ti44Nb9 shape memory alloy [D]. Chongqing: Chongqing University, 2013
[18] 陈 斌. 镍钛铌形状记忆合金宏细观力学行为研究 [D]. 重庆: 重庆大学, 2013
[19] Chen B, Peng X, Chen X, et al. A three-dimensional model of shape memory alloys under coupled transformation and plastic deformation [J]. CMC, 2012, 30: 145
[20] Piotrowski B, Ben Zineb T, Patoor E, et al. A finite element-based numerical tool for Ni47Ti44Nb9 SMA structures design: Application to tightening rings [J]. J. Intell. Mater. Syst. Struct., 2012, 23: 141
[21] Xu X, Kan Q H, Kang G Z. Finite element analysis of NiTi shape memory alloy pipe coupling [J]. J. Sichuan Univ. Sci. Eng. (Nat. Sci. Ed.), 2016, 29(4: 26
[21] 徐 祥, 阚前华, 康国政. 镍钛形状记忆合金管接头有限元分析 [J]. 四川理工学院学报(自然科学版), 2016, 29(4): 26
[22] Kang Z T, Zhou B, Xue S F. Finite element numerical simulation on thermo-mechanical coupling behavior in shape memory alloy pipe connection [J]. J. Mech. Eng., 2018, 54(18): 68
[22] 康泽天, 周 博, 薛世峰. 形状记忆合金管接头热机耦合行为的有限元数值模拟 [J]. 机械工程学报, 2018, 54(18): 68
[23] Ma Y, Li W. Structure optimization and finite element analysis of shape memory alloy coupling [J]. J. Northeastern Univ. (Nat. Sci)., 2013, 34: 1166
[23] 马 彦, 李 威. 形状记忆合金管接头结构优化与有限元分析 [J]. 东北大学学报(自然科学版), 2013, 34: 1166
[24] Zhi Y H, Liu Y S, Yue Z F. Finite element analysis of shape memory alloy joint under different loads [J]. Mach. Des. Manuf., 2009, (2): 4
[24] 智友海, 刘永寿, 岳珠峰. 不同载荷下形状记忆合金管接头性能的有限元分析 [J]. 机械设计与制造, 2009, (2): 4
[25] Zhang H B, Wang J, Jin W, et al. Coupling force simulation of TiNiFe shape memory alloy pipe-coupling [J]. Chin. J. Nonferrous Met., 2010, 20(Spec.1): 510
[25] 张慧博, 王 健, 金 伟等. TiNiFe形状记忆合金管接头应力场模拟 [J]. 中国有色金属学报, 2010, 20(专辑1): 510
[26] Yin X Q, Gao B D, Mi X J. Numerical simulation of radial pressures for TiNiNb pipe-couplings [J]. Chin. J. Rare Met., 2008, 32: 579
[26] 尹向前, 高宝东, 米绪军. TiNiNb形状记忆合金管接头径向压应力的模拟计算 [J]. 稀有金属, 2008, 32: 579
[27] Zhang H B, Jin W, Yang R. 3D finite element simulation of pull-out force of TiNiFe shape memory pipe coupling with inner convex [J]. Acta Metall. Sin., 2012, 48: 1520
[27] 张慧博, 金 伟, 杨 锐. 内脊型TiNiFe记忆合金管接头拉脱力的三维有限元模拟 [J]. 金属学报, 2012, 48: 1520
[28] Chen Q, Wang K L, Lu S Q, et al. Numerical simulation analysis on Φ10 mm NiTiNb shape memory alloy pipe-coupling [J]. Hot Work. Technol., 2017, 46(2): 81
[28] 陈 强, 王克鲁, 鲁世强等. Φ10 mm NiTiNb形状记忆合金管接头数值模拟分析 [J]. 热加工工艺, 2017, 46(2): 81
[29] Chen X, Chen W, Lu S, et al. Thermodynamic performance test and phenomenological constitutive model construction of NiTiNb shape memory alloy [J]. J. Mech. Eng., accepted
[29] 陈 翔, 陈 伟, 禄 盛等. NiTiNb记忆合金热力学性能试验及其唯象学本构模型研究 [J]. 机械工程学报, (已录用)
[30] Lemaitre J, Chaboche J L, Maji A K. Mechanics of solid materials [J]. J. Eng. Mech., 1993, 119: 642
[31] Souza A C, Mamiya E N, Zouain N. Three-dimensional model for solids undergoing stress-induced phase transformations [J]. Eur. J. Mech., 1998, 17A: 789
[32] Yan J L, Shen Y P, Chen R. The finite element analysis of the shape memory alloy pipe connector [J]. Chin. J. Theor. Appl. Mech., 1998, 30: 370
[32] 严金良, 沈亚鹏, 陈 儒. 形状记忆合金管接头空间轴对称有限元分析 [J]. 力学学报, 1998, 30: 370
[33] Zhang C S, Zhao L C, Duerig T W, et al. Effects of deformation on the transformation hysteresis and shape memory effect in a Ni47Ti44Nb9 alloy [J]. Scr. Metall. Mater., 1990, 24: 1807
[34] Chen X, Peng X H, Chen B, et al. Experimental investigation on transformation, reorientation and plasticity of Ni47Ti44Nb9 SMA under biaxial thermal-mechanical loading [J]. Smart Mater. Struct., 2015, 24: 075025
Outlines

/