Fabrication and Properties of Novel Multi-LayeredMetal Composites

  • Le ZHANG ,
  • Wei WANG ,
  • Shahzad M. Babar ,
  • Yiyin SHAN ,
  • Ke YANG
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2. School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    3. Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2019-07-24

  Revised date: 2019-08-26

  Online published: 2019-11-13

Supported by

National Natural Science Foundation of China(51472249);National Natural Science Foundation of China Research Fund for International Young Scientists(51750110515);Youth Innovation Promotion Association of Chinese Academy of Sciences(2017233);Innovation Project of Institute of Metal Research(2015-ZD04);Shenyang Science and Technology Project(Z18-0-026)

Abstract

With the development of science and technology, more and more products with excellent quanlity and abundant functionalities have been exploited and provided. Inspired by the concept of "brick wall" structure or layer structure with alternated distribution of hard and soft phases discovered in nature creatures such as mother pearl shellfish, a entirely novel steel composite which not only can minimize the shortcomings of the original materials at the maximum extent, but also possess excellent mechanical performance as well as new physical properties, has been developed. Taking ultra-high strength maraging steel and 316L austenitic stainless steel as the original materials, the influence of deformation reduction under high vacuum on interfacial bonding strength and interface characteristics of heterogeneous multi-layered metal composites was studied, and the fabrication feasibility of heterogeneous multi-layered metal composites was explored. The results showed that in the vacuum hot-pressing process, the interfaces under different deformations were clear and straight. Slight mutual diffusion phenomenon occurred in the hot-pressing process. Due to the difference of rheological properties of the original materials at high temperature, dynamic recovery and dynamic recrystallization occurred in the 316L layer, while deformed microstructure was dominant in the maraging steel layer. Combined with rolling process and heat treatment, bulk metal composites with 9 layers and 11 layers were prepared, respectively. The results of the three-point bending experiment showed that the crack occurred firstly at the outermost side of the multi-layer composites which withstood the tensile stress. Due to the passivation, delamination and bridging of heterogeneous interface in the multi-layer metal composites, the propagation path of crack was greatly extended and more energy was consumed, which showed excellent ability to block the crack propagation.

Cite this article

Le ZHANG , Wei WANG , Shahzad M. Babar , Yiyin SHAN , Ke YANG . Fabrication and Properties of Novel Multi-LayeredMetal Composites[J]. Acta Metall Sin, 2020 , 56(3) : 351 -360 . DOI: 10.11900/0412.1961.2019.00245

References

[1] Mazínová I, Florian P. Modern Methods of Construction Design [M]. Cham: Springer, 2014: 145
[2] Jackson A P, Vincent J F V, Turner R M. The mechanical design of nacre [J]. Proc. Roy. Soc., 1988, 234B: 415
[3] Xu L P, Peng J T, Liu Y B, et al. Nacre-inspired design of mechanical stable coating with underwater superoleophobicity [J]. ACS Nano, 2013, 7: 5077
[4] Rodrigues J R, Alves N M, Mano J F. Nacre-inspired nanocomposites produced using layer-by-layer assembly: Design strategies and biomedical applications [J]. Mater. Sci. Eng., 2017, C76: 1263
[5] Gerhard E M, Wang W, Li C Y, et al. Design strategies and applications of nacre-based biomaterials [J]. Acta Biomater., 2017, 54: 21
[6] Chen C T, Martin-Martinez F J, Ling S J, et al. Nacre-inspired design of graphene oxide-polydopamine nanocomposites for enhanced mechanical properties and multi-functionalities [J]. Nano Futures, 2017, 1: 011003
[7] She J H, Inoue T, Ueno K. Fabrication and characterization of multilayer alumina-based composites with improved fracture behavior [J]. Mater. Lett., 2000, 42: 155
[8] Bouaziz O, Masse J P, Petitgand G, et al. A novel strong and ductile TWIP/martensite steel composite [J]. Adv. Eng. Mater., 2016, 18: 56
[9] Daneshvar F, Reihanian M, Gheisari K. Al-based magnetic composites produced by accumulative roll bonding (ARB) [J]. Mater. Sci. Eng., 2016, B206: 45
[10] Liu B X, Huang L J, Geng L, et al. Microstructure and tensile behavior of novel laminated Ti-TiBw/Ti composites by reaction hot pressing [J]. Mater. Sci. Eng., 2013, A583: 182
[11] Naseri M, Reihanian M, Borhani E. Bonding behavior during cold roll-cladding of tri-layered Al/brass/Al composite [J]. J. Manuf. Processes, 2016, 24: 125
[12] Leedy K D, Stubbins J F. Copper alloy-stainless steel bonded laminates for fusion reactor applications: Tensile strength and microstructure [J]. Mater. Sci. Eng., 2001, A297: 10
[13] Zu G Y, Wang N, Yu J M, et al. Research on bonding mechanism of composite cold rolling plate of stainless steel/steel [J]. Res. Iron Steel, 2004, 32(4): 32
[13] 祖国胤, 王 宁, 于九明等. 不锈钢/碳钢冷轧复合机理的研究 [J]. 钢铁研究, 2004, 32(4): 32
[14] Xie Z X, Liu Q Y, Yang J H, et al. Effect of microalloying element Mo on dynamic recrystallization of microalloyed steels [J]. J. Iron Steel Res., 2009, 21(1): 33
[14] 谢志翔, 刘清友, 杨景红等. 微量钼对微合金钢动态再结晶的影响 [J]. 钢铁研究学报, 2009, 21(1): 33
[15] Song R B, Xiang J Y, Hou D P, et al. Behavior and mechanism of hot work-hardening for 316L stainless steel [J]. Acta Metall. Sin., 2010, 46: 57
[15] 宋仁伯, 项建英, 侯东坡等. 316L不锈钢热加工硬化行为及机制 [J]. 金属学报, 2010, 46: 57
[16] Zu G Y. Theories and Technologies of Preparation Layered Metal Composite [M]. Shenyang: Northeastern University Press, 2013: 15
[16] 祖国胤. 层状金属复合材料制备理论与技术 [M]. 沈阳: 东北大学出版社, 2013: 15
[17] Mozaffari A, Hosseini M, Manesh H D. Al/Ni metal intermetallic composite produced by accumulative roll bonding and reaction annealing [J]. J. Alloys Compd., 2011, 509: 9938
[18] Kümmel F, Haus?l T, H?ppel H W, et al. Enhanced fatigue lives in AA1050A/AA5005 laminated metal composites produced by accumulative roll bonding [J]. Acta Mater., 2016, 120: 150
[19] Kum D W, Oyama T, Wadsworth J, et al. The impact properties of laminated composites containing ultrahigh carbon (UHC) steels [J]. J. Mech. Phys. Solids, 1983, 31: 173
[20] Wadsworth J, Lesuer D R. Ancient and modern laminated composites——From the great pyramid of gizeh to Y2K [J]. Mater. Charact., 2000, 45: 289
[21] Roy S, Nataraj B R, Suwas S, et al. Accumulative roll bonding of aluminum alloys 2219/5086 laminates: Microstructural evolution and tensile properties [J]. Mater. Des., 2012, 36: 529
[22] Yu H L, Lu C, Tieu A K, et al. Annealing effect on microstructure and mechanical properties of Al/Ti/Al laminate sheets [J]. Mater. Sci. Eng., 2016, A660: 195
[23] Jha S C, Delagi R G, Forster J A, et al. High-strength high-conductivity Cu-Nb microcomposite sheet fabricatedvia multiple roll bonding [J]. Metall. Trans., 1993, 24A: 15
[24] Zhang X P, Yang T H, Castagne S, et al. Microstructure; bonding strength and thickness ratio of Al/Mg/Al alloy laminated composites prepared by hot rolling [J]. Mater. Sci. Eng., 2011, A528: 1954
[25] Pardal J M, Tavares S S M, Fonseca M P C, et al. Influence of temperature and aging time on hardness and magnetic properties of the maraging steel grade 300 [J]. J. Mater. Sci., 2007, 42: 2276
[26] Tanhaei S, Gheisari K, Zaree S R A. Effect of cold rolling on the microstructural, magnetic, mechanical, and corrosion properties of AISI 316L austenitic stainless steel [J]. Int. J. Miner. Metall. Mater., 2018, 25: 630
Outlines

/