Present Research Situation and Prospect of Multi-Scale Design in Novel Co-Based Superalloys: A Review
Received date: 2019-05-20
Revised date: 2019-06-19
Online published: 2019-10-24
Supported by
National Key Research and Development Program of China(2017YFB0702901);Key-Areas Research and Development Program of Guangdong Province(2019B0109430);National Natural Science Foundation of China(51831007)
In recent years, the development of material genetic methods, together with multi-scale material design theory and calculation methods has provided new ideas for the alloy design of novel Co-based superalloys. Based on the published results of multi-scale design and the research work of our laboratory, this paper systematically summarizes the present research status of multi-scale design methods in the field of novel Co-based superalloys. A review of multi-scale calculation methods including first-principle calculation, CALPHAD, phase field simulation, and machine learning is presented in this paper. The development trend of multi-scale design in novel Co-based superalloys is prospected.
LIU Xingjun , CHEN Yuechao , LU Yong , HAN Jiajia , XU Weiwei , GUO Yihui , YU Jinxin , WEI Zhenbang , WANG Cuiping . Present Research Situation and Prospect of Multi-Scale Design in Novel Co-Based Superalloys: A Review[J]. Acta Metall Sin, 2020 , 56(1) : 1 -20 . DOI: 10.11900/0412.1961.2019.00159
| [1] | Sims C T, Stoloff N S, Hagel W C. Superalloys II [M]. New York: John Wiley & Sons, 1987: 1 |
| [2] | Reed R C. The Superalloys Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 |
| [3] | Sato J, Omori T, Oikawa K, et al. Cobalt-base high-temperature alloys [J]. Science, 2006, 312: 90 |
| [4] | Suzuki A, Denolf G C, Pollock T M. Flow stress anomalies in γ/γ′ two-phase Co-Al-W-base alloys [J]. Scr. Mater., 2007, 56: 385 |
| [5] | Pollock T M, Dibbern J, Tsunekane M, et al. New Co-based γ/γ′ high-temperature alloys [J]. JOM, 2010, 62(1): 58 |
| [6] | Titus M S, Suzuki A, Pollock T M. Creep and directional coarsening in single crystals of new γ/γ′ cobalt-base alloys [J]. Scr. Mater., 2012, 66: 574 |
| [7] | Suzuki A, Inui H, Pollock T M. L12-strengthened cobalt-base superalloys [J]. Annu. Rev. Mater. Res., 2015, 45: 345 |
| [8] | Shinagawa K, Omori T, Oikawa K, et al. Ductility enhancement by boron addition in Co-Al-W high-temperature alloys [J]. Scr. Mater., 2009, 61: 612 |
| [9] | Kobayashi S, Tsukamoto Y, Takasugi T, et al. Determination of phase equilibria in the Co-rich Co-Al-W ternary system with a diffusion-couple technique [J]. Intermetallics, 2009, 17: 1085 |
| [10] | Tsukamoto Y, Kobayashi S, Takasugi T. The stability of γ'-Co3(Al, W) phase in Co-Al-W ternary system [J]. Mater. Sci. Forum, 2010, 654: 448 |
| [11] | Lass E A, Williams M E, Campbell C E, et al. γ′ Phase stability and phase equilibrium in ternary Co-Al-W at 900 ℃ [J]. J. Phase Equilib. Diffus., 2014, 35: 711 |
| [12] | Lass E A, Grist R D, Williams M E. Phase equilibria and microstructural evolution in ternary Co-Al-W between 750 and 1100 ℃ [J]. J. Phase Equilib. Diffus., 2016, 37: 387 |
| [13] | Zenk C H, Povstugar I, Li R, et al. A novel type of Co-Ti-Cr-base γ/γ′ superalloys with low mass density [J]. Acta Mater., 2017, 135: 244 |
| [14] | Bocchini P J, Sudbrack C K, Sauza D J, et al. Effect of tungsten concentration on microstructures of Co-10Ni-6Al-(0, 2, 4, 6) W-6Ti (at%) cobalt-based superalloys [J]. Mater. Sci. Eng., 2017, A700: 481 |
| [15] | Bocchini P J, Sudbrack C K, Noebe R D, et al. Effects of titanium substitutions for aluminum and tungsten in Co-10Ni-9Al-9W (at%) superalloys [J]. Mater. Sci. Eng., 2017, A705: 122 |
| [16] | Shinagawa K, Omori T, Sato J, et al. Phase equilibria and microstructure on γ′ phase in Co-Ni-Al-W system [J]. Mater. Trans., 2008, 49: 1474 |
| [17] | Omori T, Oikawa K, Sato J, et al. Partition behavior of alloying elements and phase transformation temperatures in Co-Al-W-base quaternary systems [J]. Intermetallics, 2013, 32: 274 |
| [18] | Xue F, Li Z Q, Feng Q. Mo effect on the microstructure in Co-Al-W-based superalloys [J]. Mater. Sci. Forum, 2010, 654-656: 420 |
| [19] | Feng G, Li H, Li S S, et al. Effect of Mo additions on microstructure and tensile behavior of a Co-Al-W-Ta-B alloy at room temperature [J]. Scr. Mater., 2012, 67: 499 |
| [20] | Xue F, Zhou H J, Ding X F, et al. Improved high temperature γ′ stability of Co-Al-W-base alloys containing Ti and Ta [J]. Mater. Lett., 2013, 112: 215 |
| [21] | Povstugar I, Choi P P, Neumeier S, et al. Elemental partitioning and mechanical properties of Ti-and Ta-containing Co-Al-W-base superalloys studied by atom probe tomography and nanoindentation [J]. Acta Mater., 2014, 78: 78 |
| [22] | Titus M S, Eggeler Y M, Suzuki A, et al. Creep-induced planar defects in L12-containing Co-and CoNi-base single-crystal superalloys [J]. Acta Mater., 2015, 82: 530 |
| [23] | Naghavi S S, Hegde V I, Saboo A, et al. Energetics of cobalt alloys and compounds and solute-vacancy binding in fcc cobalt: A first-principles database [J]. Acta Mater., 2017, 124: 1 |
| [24] | Naghavi S S, Hegde V I, Wolverton C. Diffusion coefficients of transition metals in fcc cobalt [J]. Acta Mater., 2017, 132: 467 |
| [25] | Neumeier S, Rehman H U, Neuner J, et al. Diffusion of solutes in fcc Cobalt investigated by diffusion couples and first principles kinetic Monte Carlo [J]. Acta Mater., 2016, 106: 304 |
| [26] | Tian L Y, Lizárraga R, Larsson H, et al. A first principles study of the stacking fault energies for fcc Co-based binary alloys [J]. Acta Mater., 2017, 136: 215 |
| [27] | Breidi A, Allen J, Mottura A. First-principles calculations of thermodynamic properties and planar fault energies in Co3X and Ni3XL12 compounds [J]. Phys. Status Solidi, 2017, 254: 1600839 |
| [28] | Suzuki A, Pollock T M. High-temperature strength and deformation of γ/γ′ two-phase Co-Al-W-base alloys [J]. Acta Mater., 2008, 56: 1288 |
| [29] | Drapier J M, De Brouwer J L, Coutsouradis D. Refractory metals and intermetallic precipitates in cobalt-chromium [J]. Cobalt, 1965, 27: 59 |
| [30] | Peters E T, Tanner L E. A new high-temperature form of the intermetallic compound Co3V [J]. Metall. Trans. Soc. AIME, 1965, 233: 2126 |
| [31] | Blaise J M, Viatour P, Drapier J M. On the stability and precipitation of the Co3Ti phase in Co-Ti alloys [J]. Cobalt, 1970, 49: 192 |
| [32] | Aoki Y, Asami K, Yamamoto M. Transformation temperatures and magnetic properties of the ordered hexagonal VCo3 compound [J]. Phys. Status Solidi, 1974, 23: K167 |
| [33] | Xu W W, Han J J, Wang Z W, et al. Thermodynamic, structural and elastic properties of Co3X (X=Ti, Ta, W, V, Al) compounds from first-principles calculations [J]. Intermetallics, 2013, 32: 303 |
| [34] | Xu W W, Shang S L, Wang C P, et al. Accelerating exploitation of Co-Al-based superalloys from theoretical study [J]. Mater. Des., 2018, 142: 139 |
| [35] | Wang C P, Yan L H, Han J J, et al. Effects of alloying elements on the structural, elastic and thermodynamic properties of Co3Ta compounds from first-principles calculations [J]. J. Alloys Compd., 2017, 726: 490 |
| [36] | Wang C P, Deng B, Xu W W, et al. Effects of alloying elements on relative phase stability and elastic properties of L12 Co3V from first-principles calculations [J]. J. Mater. Sci., 2018, 53: 1204 |
| [37] | Jin M, Miao N H, Zhao W Y, et al. Structural stability and mechanical properties of Co3(Al, M) (M=Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, W) compounds [J]. Comp. Mater. Sci., 2018, 148: 27 |
| [38] | Wang W Y, Xue F, Zhang Y, et al. Atomic and electronic basis for solutes strengthened (010) anti-phase boundary of L12 Co3(Al, TM): A comprehensive first-principles study [J]. Acta Mater., 2018, 145: 30 |
| [39] | Chen M, Wang C Y. First-principles investigation of the site preference and alloying effect of Mo, Ta and platinum group metals in γ′-Co3(Al, W) [J]. Scr. Mater., 2009, 60: 659 |
| [40] | Chen M, Wang C Y. First-principle investigation of 3d transition metal elements in γ′-Co3(Al, W) [J]. J. Appl. Phys., 2010, 107: 093705 |
| [41] | Jiang C. First-principles study of Co3(Al, W) alloys using special quasi-random structures [J]. Scr. Mater., 2008, 59: 1075 |
| [42] | Xu W W, Han J J, Wang Y, et al. First-principles investigation of electronic, mechanical and thermodynamic properties of L12 ordered Co3(M, W)(M= Al, Ge, Ga) phases [J]. Acta Mater., 2013, 61: 5437 |
| [43] | Xu W W, Wang Y, Wang C P, et al. Alloying effects of Ta on the mechanical properties of γ' Co3(Al, W): A first-principles study [J]. Scr. Mater., 2015, 100: 5 |
| [44] | Mottura A, Janotti A, Pollock T M. A first-principles study of the effect of Ta on the superlattice intrinsic stacking fault energy of L12-Co3(Al, W) [J]. Intermetallics, 2012, 28: 138 |
| [45] | Saal J E, Wolverton C. Energetics of antiphase boundaries in γ′ Co3(Al, W)-based superalloys [J]. Acta Mater., 2016, 103: 57 |
| [46] | Chen M, Wang C Y. First-principles study of the partitioning and site preference of Re or Ru in Co-based superalloys with γ/γ′ interface [J]. Phys. Lett., 2010, 374A: 3238 |
| [47] | Lu X G, Wang Z, Cui Y W, et al. Computational thermodynamics, computational kinetics and materials design [J]. Chin. Sci. Bull., 2013, 58: 3656 |
| [47] | (鲁晓刚, 王 卓, Cui Y W等. 计算热力学、计算动力学与材料设计 [J]. 科学通报, 2013, 58: 3656) |
| [48] | Feng W F, Wang Q C, Zhang L. Calculation during material design, A new tendency in material design [J]. Mater. Sci. Technol., 2000, 8(4): 57 |
| [48] | (冯武锋, 王春青, 张 磊. 材料设计的发展新趋势—材料设计计算方法 [J]. 材料科学与工艺, 2000, 8(4): 57) |
| [49] | Wang X, Zhu L L, Fang J, et al. Applications of "Materials Genome Engineering" based methods in nickel-based superalloys [J]. Sci. Technol. Rev., 2015, 33(10): 79 |
| [49] | (王 薪, 朱礼龙, 方 姣等. 基于“材料基因组工程”的3种方法在镍基高温合金中的应用 [J]. 科技导报, 2015, 33(10): 79) |
| [50] | Dupin N, Sundman B. A thermodynamic database for Ni-base superalloys [J]. Scand. J. Metall., 2001, 30: 184 |
| [51] | Jiang L, Zhao J C, Feng G J, et al. Nickel-containing alloys, method of manufacture thereof and articles derived thereform [P]. US Pat, 006945OA1, 2005 |
| [52] | Yang S Y, Jiang M, Wang L. Applications of thermodynamic calculations of phase diagrams to new-type Co-based superalloy design [J]. J. Mater. Metall., 2011, 10: 278 |
| [52] | (杨舒宇, 蒋 敏, 王 磊. 相图热力学计算在新型钴基高温合金设计中的应用 [J]. 材料与冶金学报, 2011, 10: 278) |
| [53] | Du Z M, Lü D X. Thermodynamic modeling of the Co-Ni-Y system [J]. Intermetallics, 2005, 13: 586 |
| [54] | Zhang Y B, Li C R, Du Z M, et al. The thermodynamic assessment of the ternary Co-Ni-Sb system [J]. Calphad, 2009, 33: 405 |
| [55] | Li C G, Zhu D M, Zhang Y B, et al. Thermodynamic assessment of the Co-Fe-Sb system [J]. Calphad, 2014, 47: 23 |
| [56] | Ruan J J, Liu X J, Yang S Y, et al. Novel Co-Ti-V-base superalloys reinforced by L12-ordered γ′ phase [J]. Intermetallics, 2018, 92: 126 |
| [57] | Liu X J, Yu Y, Liu Y H, et al. Experimental investigation and thermodynamic calculation of the phase equilibria in the Co-Cu-V ternary system [J]. J. Phase Equilib. Diffus., 2017, 38: 733 |
| [58] | Liu X J, Huang L S, Jiang H X, et al. Experimental investigation of the phase equilibria in the Co-V-Sn ternary system [J]. J. Phase Equilib. Diffus., 2017, 38: 723 |
| [59] | Liu X J, Yang S Y, Xiong H P, et al. Experimental investigation of phase equilibria in the Co-Ni-Zr ternary system [J]. Int. J. Mater. Res., 2016, 107: 887 |
| [60] | Ruan J J, Wang C P, Yang S Y, et al. Experimental investigations of microstructures and phase equilibria in the Co-V-Ta ternary system [J]. J. Alloys Compd., 2016, 664: 141 |
| [61] | Wang C P, Zhao C C, Lu Y, et al. Experimental observation of magnetically induced phase separation and thermodynamic assessment in the Co-V binary system [J]. Mater. Chem. Phys. Lett., 2015, 162A: 555 |
| [62] | Wang C P, Yang S, Yang S Y, et al. Experimental investigation of the phase Equilibria in the Co-Nb-V ternary system [J]. J. Phase Equilib. Diffus., 2015, 36: 592 |
| [63] | Ruan J J, Wang C P, Zhao C C, et al. Experimental investigation of phase equilibria and microstructure in the Co-Ti-V ternary system [J]. Intermetallics, 2014, 49: 121 |
| [64] | Wang C P, Zhao C C, Lin Z, et al. Experimental determination and thermodynamic calculation of the phase equilibria in the Co-Mn-Ta system [J]. Int. J. Mater. Res., 2014, 105: 1179 |
| [65] | Zhao C C, Yang S Y, Liu X J, et al. Experimental determination of the phase equilibria in the Co-Cr-Ta ternary system [J]. J. Alloys Compd., 2014, 608: 118 |
| [66] | Liu X J, Yu Y, Lu Y, et al. Interdiffusion and atomic mobilities in fcc Co-Ga and Co-V Alloys [J]. J. Phase Equilib. Diffus., 2018, 39: 2 |
| [67] | Sundman B, Jansson B, Andersson J O. The thermo-calc databank system [J]. Calphad, 1985, 9: 153 |
| [68] | Gómez-Acebo T, Navarcorena B, Castro F. Interdiffusion in multiphase, Al-Co-Cr-Ni-Ti diffusion couples [J]. J. Phase Equilib. Diffus., 2004, 25: 237 |
| [69] | Chen J, Liu Y J, Sheng G, et al. Atomic mobilities, interdiffusivities and their related diffusional behaviors in fcc Co-Cr-Ni alloys [J]. J. Alloys Compd., 2015, 621: 428 |
| [70] | Chen W M, Zhang L J, Li W, et al. Experimental measurements of the interdiffusivities in fcc Co-rich Co-Ti, Co-W and Co-Ti-W systems [J]. Int. J. Refract. Met. Hard. Mater., 2018, 71: 153 |
| [71] | Cui Y W, Jiang M, Ohnuma I, et al. Computational study of atomic mobility in Co-Fe-Ni ternary fcc alloys [J]. J. Phase Equilib. Diffus., 2008, 29: 312 |
| [72] | Moon K W, Campbell C E, Williams M E, et al. Diffusion in fcc Co-rich Co-Al-W alloys at 900 and 1000 ℃ [J]. J. Phase Equilib. Diffus., 2016, 37: 402 |
| [73] | Wang J F, Wang Y, Zhu N Q, et al. Experimental and computational study of interdiffusion for fcc Ni-Co-W alloys [J]. J. Phase Equilib. Diffus., 2017, 38: 37 |
| [74] | Wang Y, Lu X G. Interdiffusion and diffusion mobility for fcc Ni-Co-Mo alloys [J]. J. Phase Equilib. Diffus., 2017, 38: 656 |
| [75] | Wang Y, Zhu N Q, Wang H, et al. Interdiffusion and diffusion mobility for fcc Ni-Co-Al alloys [J]. Metall. Mater. Trans., 2017, 48A: 943 |
| [76] | Zhang W B, Liu D D, Zhang L J, et al. Experimental investigation and computational study of atomic mobility in fcc ternary Co-Cr-W alloys [J]. Calphad, 2014, 45: 118 |
| [77] | Zhou Z, Liu Y J. Atomic mobilities and diffusivities in fcc Co-Cr-Ti alloys [J]. J. Phase Equilib. Diffus., 2016, 37: 155 |
| [78] | Moelans N, Blanpain B, Wollants P. An introduction to phase-field modeling of microstructure evolution [J]. Calphad, 2008, 32: 268 |
| [79] | Kundin J, Mushongera L, Emmerich H. Phase-field modeling of microstructure formation during rapid solidification in Inconel 718 superalloy [J]. Acta Mater., 2015, 95: 343 |
| [80] | Lopez-Galilea I, Huth S, Fries S G, et al. Microsegregation and secondary phase formation during directional solidification of the single-crystal Ni-based superalloy LEK94 [J]. Metall. Mater. Trans., 2012, 43A: 5153 |
| [81] | Ta N, Zhang L J, Du Y. Design of the precipitation process for Ni-Al alloys with optimal mechanical properties: A phase-field study [J]. Metall. Mater. Trans., 2014, 45A: 1787 |
| [82] | Zhu J Z, Wang T, Ardell A J, et al. Three-dimensional phase-field simulations of coarsening kinetics of γ′ particles in binary Ni-Al alloys [J]. Acta Mater., 2004, 52: 2837 |
| [83] | Wu X C, Li Y S, Liu W, et al. Dynamics evolution of γ′ precipitates size and composition interface between γ/γ′ phases in Ni-Al alloy at different aging temperatures [J]. Rare Met., 2016, 1 |
| [84] | Takahashi A, Kobayashi Y, Kikuchi M. Phase field simulation of rafting behavior of γ' phase in nickel base superalloy [J]. Adv. Mater. Res., 2008, 33-37: 471 |
| [85] | Mushongera L T, Fleck M, Kundin J, et al. Effect of Re on directional γ′-coarsening in commercial single crystal Ni-base superalloys: A phase field study [J]. Acta Mater., 2015, 93: 60 |
| [86] | Yang M, Zhang J, Wei H, et al. Study of γ′ rafting under different stress states—A phase-field simulation considering viscoplasticity [J]. J. Alloys Compd., 2018, 769: 453 |
| [87] | Gao Y P, Ding H, Jin X J. γ' precipitation during ageing of a CoAlW alloy by phase field simulation [J]. J. Jilin Univ. (Eng. Technol. Ed.), 2011, 41: 84 |
| [87] | (高一鹏, 丁 洪, 金学军. CoAlW合金时效过程中γ'相析出的相场模拟 [J]. 吉林大学学报(工学版), 2011, 41: 84) |
| [88] | Koyama T. Simulation of microstructural evolution based on the phase-field method and its applications to material development [J]. J. Jpn. Inst. Met., 2009, 73: 891 |
| [88] | (小山敏幸. フェーズフィールド法に基づく 組織形成シミュレーションとその材料開発への応用 [J]. 日本金属学会誌, 2009, 73: 891) |
| [89] | Jokisaari A M, Naghavi S S, Wolverton C, et al. Predicting the morphologies of γ' precipitates in cobalt-based superalloys [J]. Acta Mater., 2017, 141: 273 |
| [90] | Shang S L, Zhou B C, Wang W Y, et al. A comprehensive first-principles study of pure elements: Vacancy formation and migration energies and self-diffusion coefficients [J]. Acta Mater., 2016, 109: 128 |
| [91] | Han J J, Wang C P, Liu X J. A modified model to predict self-diffusion coefficients in metastable fcc, bcc and hcp structures [J]. J. Phase Equilib. Diffus., 2013, 34: 17 |
| [92] | Neumann G. A model for the calculation of monovacancy and divacancy contributions to the impurity diffusion in noble metals [J]. Phys. Status Solidi, 1987, 144B: 329 |
| [93] | Mantina M, Wang Y, Chen L Q, et al. First principles impurity diffusion coefficients [J]. Acta Mater., 2009, 57: 4102 |
| [94] | Hargather C Z, Shang S L, Liu Z K. A comprehensive first-principles study of solute elements in dilute Ni alloys: Diffusion coefficients and their implications to tailor creep rate [J]. Acta Mater., 2018, 157: 126 |
| [95] | Zeng Y Z, Bai K W. High-throughput prediction of activation energy for impurity diffusion in fcc metals of Group I and VIII [J]. J. Alloys Compd., 2015, 624: 201 |
| [96] | Wu H, Lorenson A, Anderson B, et al. Robust FCC solute diffusion predictions from ab-initio machine learning methods [J]. Comp. Mater. Sci., 2017, 134: 160 |
| [97] | Wang C P, Qin S Y, Lu Y, et al. Interdiffusion and atomic mobilities in fcc Co-Cr-Mo alloys [J]. J. Phase Equilib. Diffus., 2018, 39: 437 |
| [98] | Yang Y L, Shi Z, Luo Y S, et al. Interdiffusion and atomic mobility studies in Ni-rich fcc Ni-Co-Al alloys [J]. J. Phase Equilib. Diffus., 2016, 37: 269 |
| [99] | Shi L, Yu J J, Cui C Y, et al. Effect of Ta additions on microstructure and mechanical properties of a single-crystal Co-Al-W-base alloy [J]. Mater. Lett., 2015, 149: 58 |
| [100] | Morinaga M, Yukawa N, Adachi H, et al. New PHACOMP and its application to alloy design [J]. Superalloys, 1984, 1984: 523 |
| [101] | Fischer C C, Tibbetts K J, Morgan D, et al. Predicting crystal structure by merging data mining with quantum mechanics [J]. Nat. Mater., 2006, 5: 641 |
| [102] | Ren F, Ward L, Williams T, et al. Accelerated discovery of metallic glasses through iteration of machine learning and high-throughput experiments [J]. Sci. Adv., 2018, 4: eaaq1566 |
| [103] | Nosengo N. Can artificial intelligence create the next wonder material? [J]. Nature, 2016, 533: 22 |
| [104] | Raccuglia P, Elbert K C, Adler P D F, et al. Machine-learning-assisted materials discovery using failed experiments [J]. Nature, 2016, 533: 73 |
| [105] | Guo J T, Hou J S, Zhou L Z, et al. Prediction and improvement of mechanical properties of corrosion resistant superalloy K44 with adjusting minor additions C, B and Hf [J]. Mater. Trans., 2006, 47: 198 |
| [106] | Yu J X, Guo S, Chen Y C, et al. A two-stage predicting model for γ′ solvus temperature of L12-strengthened Co-base superalloys based on machine learning [J]. Intermetallics, 2019, 110: 106466 |
| [107] | Burges C J C. A tutorial on support vector machines for pattern recognition [J]. Data Min. Knowl. Dis., 1998, 2: 121 |
| [108] | Belhumeur P N, Hespanha J P, Kriegman D J. Eigenfaces vs. fisherfaces: Recognition using class specific linear projection [J]. IEEE Trans. Pattern Anal. Mach. Intell., 1997, 19: 711 |
| [109] | Breiman L. Random forests [J]. Mach. Learn., 2001, 45: 5 |
/
| 〈 |
|
〉 |