Mechanical Properties and Strengthening Mechanism of Graphene Nanoplatelets Reinforced Magnesium Matrix Composites
Received date: 2019-05-20
Revised date: 2019-09-18
Online published: 2019-10-23
Supported by
National Natural Science Foundation of China(11672055);National Natural Science Foundation of China(11272072)
To improve the mechanical properties of Mg alloys and broaden their application fields, high performance Mg matrix nanocomposites have received more and more attention nowadays. Therefore, the research on the basic mechanical properties and strengthening mechanism of new Mg matrix composites at nanoscale has important theoretical and practical significance. The mechanical properties of pristine single-layer graphene nanoplatelets (GNPs) and single-side and double-side nickel-coated GNP (Ni-GNP, Ni-GNP-Ni) reinforced Mg composites (GNP/Mg, Ni-GNP/Mg, Ni-GNP-Ni/Mg) are studied under uniaxial tension by molecular dynamics (MD) simulations. Meanwhile, their tensile properties are also compared with those of double-side nickel-coated GNP with vacancy defects (Ni-defected GNP-Ni) and double-side nickel-coated multilayer GNPs (Ni-nGNPs-Ni) reinforced Mg-based composites. The simulated results show that the mechanical properties of Mg matrix composites are improved significantly by the addition of GNPs. Compared with single crystal Mg, the tensile strength and elastic modulus of GNP/Mg nanocomposites at 300 K and 1×109 s-1 are increased by 32.60% and 37.91%, respectively; while the tensile strength and elastic modulus of Ni-GNP-Ni/Mg composites are increased by 46.79% and 54.53%, separately. In addition, there is a larger increase in the elastic modulus and tensile strength but a smaller increase in the fracture strain for Ni-defected GNP-Ni/Mg composites, while there is a larger increase in the tensile strength and fracture strain but a smaller increase in the elastic modulus for Ni-GNP/Mg composites as compared with those of GNP/Mg composites. The elastic modulus, tensile strength and fracture strain of Ni-GNP-Ni/Mg composites decreases with increase in temperature, showing a temperature softening effect, but the variation in the elastic modulus of the composites is insensitive to temperature. With increasing of the layers or volume fractions of GNPs in Ni-nGNPs-Ni, the elastic modulus, tensile strength and fracture strain of the composites are all increased significantly, and the composites show excellent comprehensive mechanical properties. It is concluded that the main strengthening mechanisms for Ni-GNP-Ni/Mg nanocomposites are strong interface bonding, effective load transfer from the Mg matrix to the Ni-GNP-Ni and dislocation strengthening by analysis of the evolution of atomic structure.
Xia ZHOU , Xiaoxia LIU . Mechanical Properties and Strengthening Mechanism of Graphene Nanoplatelets Reinforced Magnesium Matrix Composites[J]. Acta Metall Sin, 2020 , 56(2) : 240 -248 . DOI: 10.11900/0412.1961.2019.00158
| [1] | Lu L, Lai M O, Froyen L. Structure and properties of Mg metal-metal composite [J]. Key Eng. Mater., 2002, 230-232: 287 |
| [2] | Dieringa H. Properties of magnesium alloys reinforced with nanoparticles and carbon nanotubes: A review [J]. J. Mater. Sci., 2011, 46: 289 |
| [3] | Zhou X, Su D P, Wu C W, et al. Tensile mechanical properties and strengthening mechanism of hybrid carbon nanotube and silicon carbide nanoparticle-reinforced magnesium alloy composites [J]. J. Nanomater., 2012, 2012: 851862 |
| [4] | Novoselov K S, Geim A K, Morozov S V, et al. Electric field effect in atomically thin carbon films [J]. Science, 2004, 306: 666 |
| [5] | Balandin A A, Ghosh S, Bao W Z, et al. Superior thermal conductivity of single layer graphene [J]. Nano Lett., 2008, 8: 902 |
| [6] | Lee C, Wei X D, Kysar J W, et al. Measurement of the elastic properties and intrinsic strength of monolayer graphene [J]. Science, 2008, 321: 385 |
| [7] | Lee C, Wei X D, Li Q Y, et al. Elastic and frictional properties of graphene [J]. Phys. Status Solidi, 2009, 246B: 2562 |
| [8] | Rafiee M A, Rafiee J, Wang Z, et al. Enhanced mechanical properties of nanocomposites at low graphene content [J]. ACS Nano, 2009, 3: 3884 |
| [9] | Du X M, Zhen K F, Liu F G. Graphene reinforced magnesium matrix composites by hot pressed sintering [J]. Dig. J. Nanomater. Bios., 2018, 13: 827 |
| [10] | Yuan Q H, Zhou G H, Liao L, et al. Interfacial structure in AZ91 alloy composites reinforced by graphene nanosheets [J]. Carbon, 2018, 127: 177 |
| [11] | Xiang S L, Gupta M, Wang X J, et al. Enhanced overall strength and ductility of magnesium matrix composites by low content of graphene nanoplatelets [J]. Composites, 2017, 100A: 183 |
| [12] | Rong Y, He H P, Zhang L, et al. Molecular dynamics studies on the strengthening mechanism of Al matrix composites reinforced by grapnene nanoplatelets [J]. Comp. Mater. Sci., 2018, 153: 48 |
| [13] | Rezaei R. Tensile mechanical characteristics and deformation mechanism of metal-graphene nanolayered composites [J]. Comp. Mater. Sci., 2018, 151: 181 |
| [14] | Barfmal M, Montazeri A. MD-based design of SiC/graphene nanocomposites towards better mechanical performance [J]. Ceram. Int., 2017, 43: 17167 |
| [15] | Zhou X, Liu X X, Sansoz F, et al. Molecular dynamics simulation on temperature and stain rate-dependent tensile response and failure behavior of Ni-coated CNT/Mg composites [J]. Appl. Phys., 2018, 124A: 506 |
| [16] | Zhou X, Song S Y, Li L, et al. Molecular dynamics simulation for mechanical properties of magnesium matrix composites reinforced with nickel-coated single-walled carbon nanotubes [J]. J. Compos. Mater., 2016, 50: 191 |
| [17] | LAMMPS simulation software program. LAMMPS Users Manual. 2003. 11 May 2018 version. URL: |
| [18] | Li C Y, Browning A R, Christensen S, et al. Atomistic simulations on multilayer graphene reinforced epoxy composites [J]. Composites, 2012, 43A: 1293 |
| [19] | Stukowski A. Visualization and analysis of atomistic simulation data with OVITO—The open visualization tool [J]. Model. Simul. Mater. Sci. Eng., 2010, 18: 015012 |
| [20] | Chen W, Fish J. A mathematical homogenization perspective of virial stress [J]. Int. J. Numer. Meth. Eng., 2006, 67: 189 |
| [21] | Sun D Y, Mendelev M I, Becker C A, et al. Crystal-melt interfacial free energies in hcp metals: A molecular dynamics study of Mg [J]. Phys. Rev., 2006, 73B: 024116 |
| [22] | Stuart S J, Tutein A B, Harrison J A. A reactive potential for hydrocarbons with intermolecular interactions [J]. J. Chem. Phys., 2000, 112: 6472 |
| [23] | Sammalkorpi M, Krasheninnikov A, Kuronen A, et al. Mechanical properties of carbon nanotubes with vacancies and related defects [J]. Phys. Rev., 2004, 70B: 245416 |
| [24] | Shibuta Y, Maruyama S. Bond-order potential for transition metal carbide cluster for the growth simulation of a single-walled carbon nanotube [J]. Comp. Mater. Sci., 2007, 39: 842 |
| [25] | He L C, Guo S S, Lei J C, et al. The effect of stone-thrower-wales defects on mechanical properties of graphene sheets—A molecular dynamics study [J]. Carbon, 2014, 75: 124 |
| [26] | Liang J H, Li H J, Qi L H, et al. Influence of Ni-CNTs additions on the microstructure and mechanical properties of extruded Mg-9Al alloy [J]. Mater. Sci. Eng., 2016, A678: 101 |
| [27] | Juneja A, Rajasekaran G. Effect of temperature and strain-rate on mechanical properties of defected graphene sheet: A molecular dynamics study [J]. IOP Conf. Ser. Mater. Sci. Eng., 2018, 402: 012020 |
/
| 〈 |
|
〉 |