High-Resolution X-Ray Diffraction Analysis of Epitaxial Films
Received date: 2019-09-29
Revised date: 2019-10-11
Online published: 2019-10-14
Epitaxy technique has been widely used for semiconductor, ferroelectric and optical materials in the development of electronic and optoelectronic devices. Epitaxial structures with strain and defects may tune the physical properties or affect the performance of devices. High-resolution X-ray diffraction (HRXRD) has significant advantages over traditional XRD with the features of small divergence, monochromatic incident beam and high resolution detection of the diffracted beam. It is a key technique for accurate characterization of epitaxial structures in non-destructive way. In this paper, the techniques of HRXRD for epitaxial film structure characterization are outlined in terms of the relationship between diffraction and reciprocal space, the difference between high-resolution diffraction and powder diffraction such as the optical system and the geometry mode of scanning etc. Based on the corresponding relationship between the epitaxial film and the matrix structure in the reciprocal space, various factors affecting the shape of the diffraction spots are analyzed, including the state of lattice match in coherence and non-coherence, super lattice and inclined growth. The other effective factors are also demonstrated, such as finite size of film, tilt and strain of epitaxial film etc. Real examples, such as Si1-xGex(x=0.1) etc., are used to explain how to obtain the structure parameters of the epitaxial films by HRXRD spectrum analysis, including lattice constant, lattice mismatch, thickness and superlattice information. To obtain more epitaxy information, reciprocal space map (RSM) analysis can be feasibly used by reconstruction of a series of HRXRD patterns. By combining HRXRD spectrum and RSM, microstructure characterizations of PbTiO3 epitaxy films, such as micro-strain, domain structure, phase transformation can be quantitatively analyzed.
Changji LI , Minjie ZOU , Lei ZHANG , Yuanming WANG , Sucheng WANG . High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. Acta Metall Sin, 2020 , 56(1) : 99 -111 . DOI: 10.11900/0412.1961.2019.00006
| [1] | Queisser H J, Haller E E. Defects in semiconductors: Some fatal, some vital [J]. Science, 1998, 281: 945 |
| [2] | Liu J F. SSMBE epitaxial growth and structure characterization of SiC thin films [D]. Hefei: University of Science and Technology of China, 2007 |
| [2] | (刘金峰. SiC薄膜的SSMBE外延生长及其结构表征 [D]. 合肥: 中国科学技术大学, 2007) |
| [3] | Spaldin N A. Multiferroics: Past, present, and future [J]. MRS Bull., 2017, 42: 385 |
| [4] | Damodaran A R, Agar J C, Pandya S, et al. New modalities of strain-control of ferroelectric thin films [J]. J. Phys. Condens. Matter, 2016, 28: 263001 |
| [5] | Shang J. Preparation and laser induced thermoelectric votalge of ferroelctric thin films [D]. Kunming: Kunming University of Science and Technology, 2010 |
| [5] | (尚 杰. 铁电氧化物薄膜的制备及其激光感生电压效应 [D]. 昆明: 昆明理工大学, 2010) |
| [6] | Birkholz M, Fewster P F, Genzel C. Thin Film Analysis by X-ray Scattering [M]. Weinheim: Wiley-VCH Verlag GmbH & Co. KGaA, 2006: 303 |
| [7] | Gao G Y. Studies on the strain states and thickness effects of epitaxial (La1-xCax)MnO3 thin films [D]. Hefei: University of Science and Technology of China, 2008 |
| [7] | (高关胤. (La1-xCax)MnO3外延膜的应力与厚度效应研究 [D]. 合肥: 中国科学技术大学, 2008) |
| [8] | Liu Y. Aberration corrected transmission electron microscopy investigation of domains and interfaces in ferroelectric thin films [D]. Beijing: University of Chinese Academy of Sciences, 2017 |
| [8] | (刘 颖. 铁电薄膜畴结构及界面结构的像差校正透射电子显微学研究 [D]. 北京: 中国科学院大学, 2017) |
| [9] | Moram M A, Vickers M E. X-ray diffraction of III-nitrides [J]. Rep. Prog. Phys., 2009, 72: 036502 |
| [10] | Fewster P F. X-ray analysis of thin films and multilayers [J]. Rep. Prog. Phys., 1996, 59: 1339 |
| [11] | Li C R, Wu L J, Chen W C. Studies of the impurity effects on crystalline quality by high-resolution X-ray diffraction [J]. Acta Phys. Sin., 2001, 50: 2185 |
| [11] | (李超荣, 吴立军, 陈万春. 高分辨X射线衍射研究杂质对晶体结构完整性的影响 [J]. 物理学报, 2001, 50: 2185) |
| [12] | Moram M A, Vickers M E, Kappers M J, et al. The effect of wafer curvature on X-ray rocking curves from gallium nitride films [J]. J. Appl. Phys., 2008, 103: 093528 |
| [13] | Mzoughi T, Fitouri H, Moussa I, et al. High resolution X-ray diffraction study of InAs layers grown with and without bismuth flow on GaAs substrates by metalorganic vapor phase epitaxy [J]. J. Alloys Compd., 2012, 524: 26 |
| [14] | Li X F, Zhang J W, Gao H K, et al. The analysis on the reciprocal space mapping of the AlGaAs/GaAs epitaxial layer in the transparent GaAs photocathode [J]. Acta Photon. Sin., 2002, 31: 312 |
| [14] | (李晓峰, 张景文, 高鸿楷等. 透射式GaAs光电阴极AlGaAs/GaAs外延层倒易点二维图分析 [J]. 光子学报, 2002, 31: 312) |
| [15] | Fulthorpe B D, Ryan P A, Hase T P A, et al. High-resolution X-ray diffraction studies of roughness and mosaic defects in epitaxial Fe/Au multilayers [J]. J. Phys., 2001, 34D: A203 |
| [16] | Kopp V S, Kaganer V M, Jenichen B, et al. Analysis of reciprocal space maps of GaN(0001) films grown by molecular beam epitaxy [J]. J. Appl. Cryst., 2014, 47: 256 |
| [17] | Chen Y, Deng H, Ji H. Characterization of structure of GaN films by high resolution X-ray diffraction analysis [J]. Anal. Test. Technol. Inst., 2009, 15: 21 |
| [17] | (陈 勇, 邓 宏, 姬 洪. 利用高分辨X射线衍射仪表征GaN薄膜的结构特性 [J]. 分析测试技术与仪器, 2009, 15: 21) |
| [18] | Yu G J, Xu M S, Hu X B, et al. High resolution X-ray diffraction analysis of GaN epitaxial layer grown on SiC substrate [J]. J. Synth. Cryst., 2014, 43: 1017 |
| [18] | (于国建, 徐明升, 胡小波等. SiC衬底上生长的GaN外延层的高分辨X射线衍射分析 [J]. 人工晶体学报, 2014, 43: 1017) |
| [19] | Cui Y X, Xu M S, Xu X G, et al. High resolution X-ray diffraction analysis of defect density of gallium nitride epitaxial layer [J]. J. Inorg. Mater., 2015, 30: 1904 |
| [19] | (崔潆心, 徐明升, 徐现刚等. 高分辨X射线衍射表征氮化镓外延层缺陷密度 [J]. 无机材料学报, 2015, 30: 1904) |
| [20] | Ayers J E. The measurement of threading dislocation densities in semiconductor crystals by X-ray diffraction [J]. J. Cryst. Growth, 1994, 135: 71 |
| [21] | Christen H M, Nam J H, Kim A J, et al. Stress-induced R-MA-MC-T symmetry changes in BiFeO3 films [J]. Phys. Rev., 2011, 83B: 144107 |
| [22] | Chen Z H, Luo Z L, Huang C W, et al. Low-symmetry monoclinic phases and polarization rotation path mediated by epitaxial strain in multiferroic BiFeO3 thin films [J]. Adv. Funct. Mater., 2011, 21: 133 |
| [23] | Mai Z H. Thin Film Structure Characterization by X-Ray [M]. Beijing: Science Press, 2007: 1, 11 |
| [23] | (麦振洪. 薄膜结构X射线表征 [M]. 北京: 科学出版社, 2007: 1, 11) |
| [24] | Birkholz F C, Fewster P F, Genzel C. Thin Film Analysis by X-Ray Scattering [M]. Weinheim: Wiley-VCH Verlag GmbH & Co. KGaA, 2006: 297 |
| [25] | Darakchieva V, Paskova T, Paskov P P, et al. Structural characteristics and lattice parameters of hydride vapor phase epitaxial GaN free-standing quasisubstrates [J]. J. Appl. Phys., 2005, 97: 013517 |
| [26] | Lee S R, West A M, Allerman A A, et al. Effect of threading dislocations on the Bragg peakwidths of GaN, AlGaN, and AlN heterolayers [J]. Appl. Phys. Lett., 2005, 86: 241904 |
| [27] | Macrander A T, Schwartz G P, Gualtieri G J. X-ray and Raman characterization of AlSb/GaSb strained layer superlattices and quasiperiodic Fibonacci lattices [J]. J. Appl. Phys., 1988, 64: 6733 |
| [28] | Paduano Q S, Weyburne D W, Drehman A J. An X-ray diffraction technique for analyzing structural defects including microstrain in nitride materials [J]. J. Cryst. Growth, 2011, 318: 418 |
| [29] | Paduano Q S, Weyburne D W, Drehman A J. An X-ray diffraction technique for analyzing basal-plane stacking faults in GaN [J]. Phys. Status Solidi, 2010, 207A: 2446 |
| [30] | Mariager S O, Lauridsen S L, Dohn A, et al. High-resolution three-dimensional reciprocal-space mapping of InAs nanowires [J]. J. Appl. Cryst., 2009, 42: 369 |
| [31] | Mariager S O, Schlepütz C M, Aagesen M, et al. High-resolution three-dimensional reciprocal space mapping of semiconductor nanostructures [J]. Phys. Status Solidi, 2009, 206A: 1771 |
| [32] | Cornelius T W, Davydok A, Jacques V L R, et al. In situ three-dimensional reciprocal-space mapping during mechanical deformation [J]. J. Synchrotron Rad., 2012, 19: 688 |
| [33] | Takahasi M, Nakata Y, Suzuki H, et al. In situ three-dimensional X-ray reciprocal-space mapping of GaAs epitaxial films on Si(001) [J]. J. Cryst. Growth, 2013, 378: 34 |
| [34] | Bauer S, Lazarev S, Bauer M, et al. Three-dimensional reciprocal space mapping with a two-dimensional detector as a low-latency tool for investigating the influence of growth parameters on defects in semipolar GaN [J]. J. Appl. Cryst., 2015, 48: 1000 |
| [35] | Sasaki T, Takahasi M, Suzuki H, et al. In situ three-dimensional X-ray reciprocal-space mapping of InGaAs multilayer structures grown on GaAs(001) by MBE [J]. J. Cryst. Growth, 2015, 425: 13 |
| [36] | Diffracplus Leptos (User Manual). Version 7. Karlsruhe: Bruker AXS GmbH., 2009 |
| [37] | Catalan G, Seidel J, Ramesh R, et al. Domain wall nanoelectronics [J]. Rev. Mod. Phys., 2012, 84: 119 |
| [38] | Luo Z L, Chen Z H, Yang Y J, et al. Periodic elastic nanodomains in ultrathin tetragonal-like BiFeO3 films [J]. Phys. Rev., 2013, 88B: 064103 |
| [39] | Catalan G, Janssens A, Rispens G, et al. Polar domains in lead titanate films under tensile strain [J]. Phys. Rev. Lett., 2006, 96: 127602 |
| [40] | Chen Z H, Liu J, Qi Y J, et al. 180° ferroelectric stripe nanodomains in BiFeO3 thin films [J]. Nano Lett., 2015, 15: 6506 |
| [41] | Barchuk M, Holy V, Kriegner D, et al. Diffuse x-ray scattering from stacking faults in a-plane GaN epitaxial layers [J]. Phys. Rev., 2011, 84B: 094113 |
| [42] | Moram M A, Johnston C F, Kappers M J, et al. Investigating stacking faults in nonpolar gallium nitride films using X-ray diffraction [J]. Physica, 2009, 404B: 2189 |
| [43] | Moram M A, Johnston C F, Hollander J L, et al. Understanding X-ray diffraction of nonpolar gallium nitride films [J]. J. Appl. Phys., 2009, 105: 113501 |
/
| 〈 |
|
〉 |