Low alloy high strength steel, owing to its good mechanical properties and low cost, is widely used in bridge, building, pressure vessel and other engineering structures. Steel structures will inevitably produce residual stress and deformation after welding with the characteristics of concentrated heat source and local heating. Heat treatment is recognized as an effective method to eliminate the residual stress after welding. However, there is no quantitative and systematic study on the mechanism of heat treatment to eliminate residual stress when numerical simulation method is used to study post weld heat treatment (PWHT). Meanwhile, creep is an important factor in the process of PWHT on low alloy high strength steel. It is necessary to study the influence of creep on residual stress prediction so as to develop a simplified creep model used in practice more efficiently. Based on MSC. Marc software platform, a thermal-elastic-plastic finite element method (T-E-P FEM) considering creep effect is developed. The stress field during welding and PWHT of Q345 remelting joint was simulated by the integrated calculation method. The effect of creep on welding residual stress during PWHT was emphatically studied. Based on the results of numerical simulation, the mechanism of eliminating residual stress by PWHT was explored. At the same time, the residual stresses of welded and heat treated joints were measured by blind-hole method, and the results were compared with those of numerical simulation. In addition, the effect of two different creep models on the calculation accuracy of residual stress in PWHT is also discussed. A simple and efficient creep model suitable for engineering application is proposed for Q345 low alloy high strength steel. The results show that the residual stresses obtained by numerical simulation agree well with the experimental values, which verifies the validity of the integrated calculation method developed. It is necessary to consider creep effect in the process of PWHT, otherwise the residual stress after heat treatment will be seriously overestimated. By using the simple creep model proposed, the calculation efficiency could be increased by about 10 times with less loss of calculation accuracy.
LU Shijie , WANG Hu , DAI Peiyuan , DENG Dean . Effect of Creep on Prediction Accuracy and Calculating Efficiency of Residual Stress in Post Weld Heat Treatment[J]. Acta Metall Sin, 2019 , 55(12) : 1581 -1592 . DOI: 10.11900/0412.1961.2019.00208
| [1] | Zou Z D, Li Y J, Yin S K, et al. Welding and Engineering Application of Low Alloy Modulated High Strength Steel [M]. Beijing: Chemical Industry Press, 2000: 26 |
| [1] | (邹增大, 李亚江, 尹士科等. 低合金调质高强度钢焊接及工程应用 [M]. 北京: 化学工业出版社, 2000: 26) |
| [2] | Chen X Z, Huang Y M. Hot deformation behavior of HSLA steel Q690 and phase transformation during compression [J]. J. Alloys Compd., 2015, 619: 564 |
| [3] | Ji G L, Li F G, Li Q H, et al. Research on the dynamic recrystallization kinetics of Aermet100 steel [J]. Mater. Sci. Eng., 2010, A527: 2350 |
| [4] | Dai W Z, Liu J F, Gao L. Application Technology and Case of Welding Engineering for Building Steel Structures [M]. Beijing: Chemical Industry Press, 2016: 38 |
| [4] | (戴为志, 刘景凤, 高 良. 建筑钢结构焊接工程应用技术及案例 [M]. 北京: 化学工业出版社, 2016: 38) |
| [5] | Yan H. The experiment study of residual stress in welded steel structure and FEM analysis [D]. Wuhan: Wuhan University of Technology, 2006 |
| [5] | (严 浩. 钢结构厚板焊接残余应力实验研究与有限元分析 [D]. 武汉: 武汉理工大学, 2006) |
| [6] | An J W. The effect of welding residual stress to the performance of resistance to earthquake of beam-column connection [D]. Tianjin: Tianjin University, 2005 |
| [6] | (安俊伟. 焊接残余应力对梁柱节点抗震性能的影响 [D]. 天津: 天津大学, 2005) |
| [7] | Shi G, Shi Y J, Ban H Y. High Strength Steel Structures [M]. Beijing: China Construction Industry Press, 2014: 30 |
| [7] | (施 刚, 石永久, 班慧勇. 高强度钢材钢结构 [M]. 北京: 中国建筑工业出版社, 2014: 30) |
| [8] | Jia L. Finite element analysis on residual stress of welding assembly for I-beam and end-plate [D]. Ji'nan: Shandong University, 2013 |
| [8] | (贾 栗. 工字钢-端板组焊结构焊接残余应力有限元分析 [D]. 济南: 山东大学, 2013) |
| [9] | Li X Y, Wu C S, Li W S. Study on the progress of welding science and technology in China [J]. Chin. J. Mech. Eng., 2012, 48(6): 19 |
| [9] | (李晓延, 武传松, 李午申. 中国焊接制造领域学科发展研究 [J]. 机械工程学报, 2012, 48(6): 19) |
| [10] | Deng D A, Ren S D, Li S, et al. Influence of multi-thermal cycle and constraint condition on residual stress in P92 steel weldment [J]. Acta Metall. Sin., 2017, 53: 1532 |
| [10] | (邓德安, 任森栋, 李 索等. 多重热循环和约束条件对P92钢焊接残余应力的影响 [J]. 金属学报, 2017, 53: 1532) |
| [11] | Fang H Y. Welding Structures [M]. 2nd Ed., Beijing: Machinery Industry Press, 2017: 109 |
| [11] | (方洪渊. 焊接结构学 [M]. 第2版,北京: 机械工业出版社, 2017: 109) |
| [12] | Zhao R. Study of welding residual stress's numerical simulation and relieving [D]. Dalian: Dalian University of Technology, 2006 |
| [12] | (赵 锐. 焊接残余应力的数值模拟及控制消除研究 [D]. 大连: 大连理工大学, 2006) |
| [13] | Zhao X C, Zhang Y D, Zhang H W, et al. Simulation of vibration stress relief after welding based on FEM [J]. Acta Metall. Sin. (Engl. Lett.), 2008, 21: 289 |
| [14] | Yu L. Welding residual stress analysis and optimization of post weld heat treatment of narrow gap submerged arc welding [D]. Shanghai: East China University of Science and Technology, 2017 |
| [14] | (余 磊. 窄间隙埋弧焊焊接残余应力及其热处理消除的模拟和优化研究 [D]. 上海: 华东理工大学, 2017) |
| [15] | Venkata K A, Kumar S, Dey H C, et al. Study on the effect of post weld heat treatment parameters on the relaxation of welding residual stresses in electron beam welded P91 steel plates [J]. Procedia Eng., 2014, 86: 223 |
| [16] | Dong P S, Song S P, Zhang J M. Analysis of residual stress relief mechanisms in post-weld heat treatment [J]. Int. J. Press. Vessels Pip., 2014, 122: 6 |
| [17] | Deng D A, Ogawa K, Kiyoshima S, et al. Prediction of residual stresses in a dissimilar metal welded pipe with considering cladding, buttering and post weld heat treatment [J]. Comput. Mater. Sci., 2009, 47: 398 |
| [18] | Sun J M, Zhu J Y, Xia L Y, et al. Numerical simulation of welding residual stress and deformation induced by electro slag welding [J]. Trans. China Weld. Inst., 2016, 37(5): 23 |
| [18] | (孙加民, 朱家勇, 夏林印, 等. 电渣焊接头焊接残余应力与变形的数值模拟 [J]. 焊接学报, 2016, 37(5): 23) |
| [19] | Deng D A, Kiyoshima S. Numerical simulation of welding residual stresses in a multi-pass butt-welded joint of austenitic stainless steel using variable length heat source [J]. Acta Metall. Sin., 2010, 46: 195 |
| [19] | (邓德安, 清岛祥一. 用可变长度热源模拟奥氏体不锈钢多层焊对接接头的焊接残余应力 [J]. 金属学报, 2010, 46: 195) |
| [20] | Tan Z, Guo G W. Thermophysical Properties of Engineering Alloys [M]. Beijing: Metallurgical Industry Press, 1994: 42 |
| [20] | (谭 真, 郭广文. 工程合金热物性 [M]. 北京: 冶金工业出版社, 1994: 42) |
| [21] | Yuan G L, Shu Q J, Huang Z H, et al. An experimental investigation of properties of Q345 steel pipe at elevated temperatures [J]. J. Constr. Steel Res., 2016, 118: 41 |
| [22] | Kasuya T, Ichikawa K, Fuji M. Derivation of carbon equivalent to assess hardenability of steel [J]. Sci. Technol. Weld. Join., 1998, 3(6): 317 |
| [23] | Deng D A, Kiyoshima S. Numerical simulation of welding temperature field, residual stress and deformation induced by electro slag welding [J]. Comput. Mater. Sci., 2012, 62: 23 |
| [24] | MARC. Analysis Research Corporation. Theory and user information. Palo Alto, 2007 |
| [25] | Goldak J, Chakravarti A, Bibby M. A new finite element model for welding heat sources [J]. Metall. Trans., 1984, 15B: 299 |
| [26] | Deng D A, Zhang C H, Pu X W, et al. Influence of material model on prediction accuracy of welding residual stress in an austenitic stainless steel multi-pass butt-welded joint [J]. J. Mater. Eng. Perform., 2017, 26: 1494 |
| [27] | Fields B A, Fields R J. The prediction of elevated temperature deformation of structural steel under anisothermal conditions [R]. Gaithersburg: Department of Commerce National Institute of Standards and Technology, 1991 |
| [28] | Yan S H. Experimental study on creep behavior in steel at elevated temperature [D]. Chongqing: Chongqing University, 2015 |
| [28] | (闫守海. 钢材高温蠕变性能试验研究 [D]. 重庆: 重庆大学, 2015) |
/
| 〈 |
|
〉 |