Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy
Received date: 2019-04-30
Revised date: 2019-08-22
Online published: 2019-09-29
Supported by
National Natural Science Foundation of China(No.51701209)
Button ingots were prepared by arc melting and feed bars for directional solidification were prepared by optimized drop casting technique. The Ti-43Al-3Si directionally solidified bars with lamellar boundaries perpendicular to the growth direction were prepared at the growth rate of 180 mm/h in an optical floating zone furnace. Cylindrical sections were cut from these perpendicular lamellae with appropriate direction and then fixed on polycrystalline TiAl bars by mechanical setting method to serve as the initial seeds. The ultimate Ti-43Al-3Si seeds with parallel lamellar microstructure were successfully prepared from these initial seeds at the growth rate of 5 mm/h. To avoid the nucleation of stray grains, drop-cast bars with the shape of frustum of a cone were used for the preparation of ultimate seeds. At the growth rates of 5 and 180 mm/h, the primary phase of Ti-43Al-3Si alloy was always the α phase. Polysynthetically twinned (PST) crystals of Ti-47Al alloy were obtained from the Ti-43Al-3Si ultimate seeds and the seeding process was studied by microscopic analysis. Lamellar microstructure of the seed kept stable and recrystallization of the seed was not found. Lamellar orientation of Ti-47Al PST crystals was successfully controlled by the ultimate Ti-43Al-3Si seed.
JIN Hao , JIA Qing , LIU Ronghua , XIAN Quangang , CUI Yuyou , XU Dongsheng , YANG Rui . Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. Acta Metall Sin, 2019 , 55(12) : 1519 -1526 . DOI: 10.11900/0412.1961.2019.00138
| [1] | Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129 |
| [1] | (杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129) |
| [2] | Wu X H. Review of alloy and process development of TiAl alloys [J]. Intermetallics, 2006, 14: 1114 |
| [3] | Kim Y W, Dimiduk D M. Progress in the understanding of gamma titanium aluminides [J]. JOM, 1991, 43(8): 40 |
| [4] | Lin J P, Zhao L L, Li G Y, et al. Effect of Nb on oxidation behavior of high Nb containing TiAl alloys [J]. Intermetallics, 2011, 19: 131 |
| [5] | Liu Z C, Lin J P, Li S J, et al. Effects of Nb and Al on the microstructures and mechanical properties of high Nb containing TiAl base alloys [J]. Intermetallics, 2002, 10: 653 |
| [6] | Inui H, Oh M H, Nakamura A, et al. Room-temperature tensile deformation of polysynthetically twinned (PST) crystals of TiAl [J]. Acta Metall. Mater., 1992, 40: 3095 |
| [7] | Oh M H, Inui H, Misaki M, et al. Environmental-effects on the room-temperature ductility of polysynthetically twinned (PST) crystals of binary and some ternary TiAl compounds [A]. Proceeding of the 5th High-Temperature Ordered Intermetallic Alloys V [C]. Boston, MA: Mater. Res. Soc. Symp. Proc., 1993, 288: 1001 |
| [8] | Johnson D R, Inui H, Yamaguchi M. Directional solidification and microstructural control of the TiAl/Ti3Al lamellar microstructure in TiAl-Si alloys [J]. Acta Mater., 1996, 44: 2523 |
| [9] | Johnson D R, Masuda Y, Inui H, et al. Alignment of the TiAl/Ti3Al lamellar microstructure in TiAl alloys by growth from a seed material [J]. Acta Mater., 1997, 45: 2523 |
| [10] | Umeda H, Kishida K, Inui H, et al. Effects of Al-concentration and lamellar spacing on the room-temperature strength and ductility of PST crystals of TiAl [J]. Mater. Sci. Eng., 1997, A239-240: 336 |
| [11] | Yamanaka T, Johnson D R, Inui H, et al. Directional solidification of TiAl-Re-Si alloys with aligned γ/α2 lamellar microstructures [J]. Intermetallics, 1999, 7: 779 |
| [12] | Johnson D R, Inui H, Muto S, et al. Microstructural development during directional solidification of α-seeded TiAl alloys [J]. Acta Mater., 2006, 54: 1077 |
| [13] | Fu H Z, Su Y Q, Guo J J, et al. The solidification behavior of high temperature intermetallics [J]. Acta Metall. Sin., 2002, 38: 1127 |
| [13] | (傅恒志, 苏彦庆, 郭景杰等. 高温金属间化合物的定向凝固特性 [J]. 金属学报, 2002, 38: 1127) |
| [14] | Yamaguchi M, Inui H, Yokoshima S, et al. Recent progress in our understanding of deformation and fracture of two-phase and single-phase TiAl alloys [J]. Mater. Sci. Eng., 1996, A213: 25 |
| [15] | Lee H N, Johnson D R, Inui H, et al. Microstructural control through seeding and directional solidification of TiAl alloys containing Mo and C [J]. Acta Mater., 2000, 48: 3221 |
| [16] | Lee H N, Johnson D R, Inui H, et al. Directional solidification and creep deformation of a Ti-46Al-1.5Mo-0.2C (at. %) alloy [J]. Intermetallics, 2002, 10: 841 |
| [17] | Lee H N, Johnson D R, Inui H, et al. A composition window in the TiAl-Mo-Si system suitable for lamellar structure control through seeding and directional solidification [J]. Mater. Sci. Eng., 2002, A329-331: 19 |
| [18] | Kim J H, Kim S W, Lee H N, et al. Effects of Si and C additions on the thermal stability of directionally solidified TiAl-Nb alloys [J]. Intermetallics, 2005, 13: 1038 |
| [19] | Luo W Z, Shen J, Li Q L, et al. Microstructural evolution of Ti-47Al alloy during directional solidification by seeding method [J]. Acta Metall. Sin., 2007, 43: 897 |
| [19] | (罗文忠, 沈 军, 李庆林等. Ti-47Al合金籽晶法定向凝固过程中的组织演化 [J]. 金属学报, 2007, 43: 897) |
| [20] | Zheng X Q, Shen J, Ding H S, et al. Preparation of fully lamellar microstructure Ti-43Al-3Si alloy with alignment perpendicular to the growth direction in steel mould [J]. Mater. Rep., 2005, 19(3): 118 |
| [20] | (郑循强, 沈 军, 丁宏升等. 单一取向的Ti-43Al-3Si全片层组织制备 [J]. 材料导报, 2005, 19(3): 118) |
| [21] | Luo W Z, Shen J, Li Q L, et al. Effects of growth rate on microstructure of directionally solidified Ti-43Al-3Si alloy with a seed technique [J]. Acta Metall. Sin., 2006, 42: 1238 |
| [21] | (罗文忠, 沈 军, 李庆林等. 抽拉速率对Ti-43Al-3Si合金籽晶法定向凝固组织的影响 [J]. 金属学报, 2006, 42: 1238) |
| [22] | Fan J L, Li X Z, Guo J J, et al. Structure evolution of directionally solidified Ti-43Al-3Si alloy I. Microstructure evolution in the transition region [J]. Acta Metall. Sin., 2009, 45: 302 |
| [22] | (樊江磊, 李新中, 郭景杰等. 定向凝固Ti-43Al-3Si合金的组织演化规律 Ⅰ. 初始过渡区组织演化规律 [J]. 金属学报, 2009, 45: 302) |
| [23] | Li X Z, Fan J L, Guo J J, et al. Structure evolution of directionally solidified Ti-43Al-3Si alloy II. Microstructure evolution in the steady-state growth region [J]. Acta Metall. Sin., 2009, 45: 308 |
| [23] | (李新中, 樊江磊, 郭景杰等. 定向凝固Ti-43Al-3Si合金的组织演化规律 Ⅱ. 稳态生长区组织演化规律 [J]. 金属学报, 2009, 45: 308) |
| [24] | Liu R H, Cui Y Y, Yang R. Effect of seed shape and size on the seeding of TiAl directional solidification [J]. Rare Met. Mater. Eng., 2008, 37(suppl.3): 141 |
| [24] | (刘荣华, 崔玉友, 杨 锐. 籽晶形状和尺寸对TiAl合金引晶生长的影响 [J]. 稀有金属材料与工程, 2008, 37(增刊3): 141) |
| [25] | Luo W Z, Shen J, Li Q L, et al. Preparation of aligned lamellar microstructure in TiAl alloys by directional solidification with a seed technique [J]. Acta Metall. Sin., 2007, 43: 1287 |
| [25] | (罗文忠, 沈 军, 李庆林等. TiAl合金定向全片层组织的籽晶法制备 [J]. 金属学报, 2007, 43: 1287) |
| [26] | Koohpayeh S M, Fort D, Abell J S. The optical floating zone technique: A review of experimental procedures with special reference to oxides [J]. Prog. Cryst. Growth Charact. Mater., 2008, 54: 121 |
| [27] | Koohpayeh S M, Fort D, Bradshaw A, et al. Thermal characterization of an optical floating zone furnace: A direct link with controllable growth parameters [J]. J. Cryst. Growth, 2009, 311: 2513 |
/
| 〈 |
|
〉 |