Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass

  • YANG Gaolin ,
  • LIN Xin ,
  • LU Xiangang
Expand
  • 1. Institute of Laser Advanced Manufacturing, Zhejiang University of Technology, Hangzhou 310014, China
    2. State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China

Received date: 2019-05-05

  Revised date: 2019-06-06

  Online published: 2019-09-11

Supported by

Supported by the Fund of the State Key Laboratory of Solidification Processing in NWPU(No.SKLSP201745);Zhejiang Provincial Natural Science Foundation of China(No.LY16E050014)

Abstract

Laser additive manufacturing technology is a feasible technology for the fabrication of bulk metallic glass with complex geometry. It has the characteristics of small molten pool and high cooling rate. However, crystallization often occurs in heat affected zone (HAZ). In this work, laser multiple remelting of Zr55Cu30Al10Ni5 metallic glass by pulsed laser was carried out and the morphological evolution of the HAZ crystalline phase in the multiple remelting process was studied. The results show that with the increase of the remelting times, the crystalline grains number and size are both improved. With the growth of the grains, the crystallization caused by the growth of the crystalline grains in the molten pool also becomes more and more remarkable. Both the size and number of the grains in the HAZ increase linearly with the increase of the remelting times. The nucleation rate and growth rate of different metallic glass plates are close, whereas the initial crystalline grains number and size are different, which are attributed to the different cooling process in the copper casting of the metallic glass plates.

Cite this article

YANG Gaolin , LIN Xin , LU Xiangang . Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass[J]. Acta Metall Sin, 2019 , 55(12) : 1544 -1550 . DOI: 10.11900/0412.1961.2019.00140

References

[1] Inoue A. Bulk glassy alloys: Historical development and current research [J]. Engineering, 2015, 1: 185
[2] Hu Z Q, Zhang H F. Recent progress in the area of bulk amorphous alloys and composites [J]. Acta Metall. Sin., 2010, 46: 1391
[2] (胡壮麒, 张海峰. 块状非晶合金及其复合材料研究进展 [J]. 金属学报, 2010, 46: 1391)
[3] Trexler M M, Thadhani N N. Mechanical properties of bulk metallic glasses [J]. Prog. Mater. Sci., 2010, 55: 759
[4] Li H X, Lu Z C, Wang S L, et al. Fe-based bulk metallic glasses: Glass formation, fabrication, properties and applications [J]. Prog. Mater. Sci., 2019, 103: 235
[5] Wang Y S, Linghu R K, Liu Y Y, et al. Superplasticity and constitutive relationship in a Ti-based metallic glassy composite [J]. J. Alloys Compd., 2018, 751: 391
[6] Gong P, Kou H C, Wang S B, et al. Research on thermoplastic formability and nanomoulding mechanism of lightweight Ti-based bulk metallic glasses [J]. J. Alloys Compd., 2019, 801: 267
[7] Hui X D, Chen G L. Bulk Amorphous Alloys [M]. Beijing: Chemical Industry Press., 2007: 1
[7] (惠希东, 陈国良. 块体非晶合金 [M]. 北京: 化学工业出版社, 2007: 1)
[8] Wang W H. The Nature and properties of amorphous matter [J]. Prog. Phys., 2013, 33: 177
[8] (汪卫华. 非晶态物质的本质和特性 [J]. 物理学进展, 2013, 33: 177)
[9] Chen H S. Glassy metals [J]. Rep. Prog. Phys., 1980, 43: 353
[10] Wen X L, Wang Q Z, Mu Q, et al. Laser solid forming additive manufacturing TiB2 reinforced 2024Al composite: Microstructure and mechanical properties [J]. Mater. Sci. Eng., 2019, A745: 319
[11] Zhang Y Y, Lin X, Wang L L, et al. Microstructural analysis of Zr55Cu30Al10Ni5 bulk metallic glasses by laser surface remelting and laser solid forming [J]. Intermetallics, 2015, 66: 22
[12] Zhang Y Y, Lin X, Wei L, et al. Influence of powder size on the crystallization behavior during laser solid forming Zr55Cu30Al10Ni5 bulk amorphous alloy [J]. Intermetallics, 2016, 76: 1
[13] Mahbooba Z, Thorsson L, Unosson M, et al. Additive manufacturing of an iron-based bulk metallic glass larger than the critical casting thickness [J]. Appl. Mater. Today, 2018, 11: 264
[14] Lu Y Z, Huang Y J, Wu J. Laser additive manufacturing of structural-graded bulk metallic glass [J]. J. Alloys Compd., 2018, 766: 506
[15] Shen Y Y, Li Y Q, Chen C, et al. 3D printing of large, complex metallic glass structures [J]. Mater. Des., 2017, 117: 213
[16] Li Y Q, Shen Y Y, Chen C, et al. Building metallic glass structures on crystalline metal substrates by laser-foil-printing additive manufacturing [J]. J. Mater. Process. Technol., 2017, 248: 249
[17] Li Y Q, Shen Y Y, Hung C H, et al. Additive manufacturing of Zr-based metallic glass structures on 304 stainless steel substrates via V/Ti/Zr intermediate layers [J]. Mater. Sci. Eng., 2018, A729: 185
[18] Li Y Q, Shen Y Y, Leu M C, et al. Building Zr-based metallic glass part on Ti-6Al-4V substrate by laser-foil-printing additive manufacturing [J]. Acta Mater., 2018, 144: 810
[19] Yang G L, Lin X, Liu F C, et al. Laser solid forming Zr-based bulk metallic glass [J]. Intermetallics, 2012, 22: 110
[20] Yang G L, Lin X, Hu Q, et al. Crystallization behavior of annealed Zr55Cu30Al10Ni5 bulk metallic glass during pulsed laser remelting [J]. Acta Metall. Sin., 2013, 49: 649
[20] (杨高林, 林 鑫, 胡 桥等. Zr55Cu30Al10Ni5块体非晶合金退火处理后脉冲激光重熔晶化行为 [J]. 金属学报, 2013, 49: 649)
[21] Liu W W, Lin X, Yang G L, et al. Crystallization behavior of heat-affected zone by laser remelting bulk metallic glass Zr55Al10Ni5Cu30 [J]. Chin. J. Lasers, 2010, 37: 2104
[21] (刘伟伟, 林 鑫, 杨高林等. 脉冲激光重熔Zr55Al10Ni5Cu30合金非晶的热影响区晶化行为 [J]. 中国激光, 2010, 37: 2104)
[22] Kurz W, Fisher D J, translated by Li J G, Hu Q D. Fundamentals of Solidification [M]. 4th Ed., Beijing: Higher Education Press, 2010: 116
[22] (Kurz W, Fisher D J著, 李建国, 胡侨丹译. 凝固原理 [M]. 第四版, 北京: 高等教育出版社, 2010: 116)
[23] Chen J X, Wang Q, Dong C. Cluster rule in alloy phase and its application in Zr-Al-Ni system [J]. Rare Met. Mater. Eng., 2011, 40: 69
[23] (陈季香, 王 清, 董 闯. 合金相团簇规律及其在Zr-Al-Ni非晶体系中的应用 [J]. 稀有金属材料与工程, 2011, 40: 69)
[24] Hao S M, Jiang M, Li H X. Thermodynamics of Materials [M]. Beijing: Chemical Industry Press, 2004: 240
[24] (郝士明, 蒋 敏, 李洪晓. 材料热力学 [M]. 北京: 化学工业出版社, 2004: 240)
[25] Schroers J, Johnson W L. History dependent crystallization of Zr41Ti14Cu12Ni10Be23 melts [J]. J. Appl. Phys., 2000, 88: 44
[26] Yang G L, Lin X, Hu Q, et al. Effect of specimen temperature on crystallization during laser remeltitng Zr55Cu30Al10Ni5 bulk metallic glass [J]. Acta Metall. Sin., 2013, 49: 925
[26] (杨高林, 林 鑫, 胡 桥等. 试样温度对激光重熔Zr55Cu30Al10Ni5块体非晶合金晶化的影响 [J]. 金属学报, 2013, 49: 925)
Outlines

/