Effect of Alternating Current Magnetic Field on the Primary Phase of Hypereutectic Al-Fe Alloy
Received date: 2018-12-21
Revised date: 2019-07-21
Online published: 2019-09-11
Supported by
China Postdoctoral Science Foundation Funded Project No(2015M571320);and Fundamental Research Funds for the Central Universities(N150504002)
The type, morphology and distribution of the Fe-phase in the Al-Fe alloy are some of the key factors affecting the mechanical properties of the Al-Fe alloy. The alternating current (AC) magnetic field can significantly affect the solidification structure of the Al-Fe alloy. However, the mechanism of the Fe-phase in the Al-Fe alloy influenced by the AC magnetic field has not been fully revealed. Therefore, the effect of AC magnetic field on the primary phase of hypereutectic Al-2.55%Fe alloy is studied by means of XRD and OM in this work. The results show that the AC magnetic field cannot change the type of primary phase of the hypereutectic Al-2.55%Fe alloy, which means that the primary phase remains to be Al3Fe phase regardless of the treatment of the AC magnetic field, but the AC magnetic field can obviously influence the distribution and the morphology of the primary Al3Fe phase. Without treatment of AC magnetic field, the primary Al3Fe phase is fine and granular, and uniformly distributed at the bottom of the sample under the effect of gravity. However, under the influence of the AC magnetic field, most of the primary Al3Fe phase is located at the top edge of the sample and is distributed in the shape of a triangle along the radial direction, with only a small part of the fine, granular primary Al3Fe phase distributed in the shape of a pyramid at the bottom of the sample. At the same time, the primary Al3Fe phase morphology in the top of the sample transforms from the original fine particles to large blocks and rods. With the increase of the magnetic induction intensity, the influence of the AC magnetic field on the distribution and morphology of the primary Al3Fe phase grows stronger, and the content of the primary Al3Fe phase in the top of the sample also increases. The influence of AC magnetic field on the primary phase distribution and morphology of the hypereutectic Al-2.55%Fe alloy is the result of the combined action of the Lorentz force and the magnetic force generated by the AC magnetic field.
Jianfeng ZHANG , Qing LAN , Ruizhen GUO , Qichi LE . Effect of Alternating Current Magnetic Field on the Primary Phase of Hypereutectic Al-Fe Alloy[J]. Acta Metall Sin, 2019 , 55(11) : 1388 -1394 . DOI: 10.11900/0412.1961.2018.00560
| [1] | LuL, DahleA K. Iron-rich intermetallic phases and their role in casting defect formation in hypoeutectic Al-Si alloys [J]. Metall. Mater. Trans., 2005, 36A: 819 |
| [2] | KhalifaW, SamuelF H, GruzleskiJ E. Iron intermetallic phases in the Al corner of the Al-Si-Fe system [J]. Metall. Mater. Trans., 2003, 34A: 807 |
| [3] | PengS, ChenL P, ZhouQ. Research progress on microstructure refinement of Al-Fe alloy [J]. Found. Technol., 2013, 34: 523 |
| [3] | 彭 帅, 陈乐平, 周 全. Al-Fe合金凝固组织细化研究新进展 [J]. 铸造技术, 2013, 34: 523 |
| [4] | WangX, GuanR G, WangY. Formation mechanism of nanoscale Al3Fe phase in Al-Fe alloy during semisolid forming process [J]. Metall. Mater. Trans., 2018, 49B: 2225 |
| [5] | WangX J, ZhaoZ H, ZuoY B, et al. Effects of low frequency electromagnetic field on solidification of 7050 aluminium alloy during hot top casting [J]. Mater. Sci. Technol., 2009, 25: 1207 |
| [6] | PathakB N, KumarA, SahooK L, et al. Effect of Ni-Mg on the microstructure and properties of Al-(4-5)Fe-1V-1Si alloys [J]. Mater. Sci. Eng., 2006, A433: 310 |
| [7] | ZhaoY H, WangX B, LiuY L, et al. Influence of Si content and heat treatment on microstructure of Al-Fe-Si alloys [J]. China Found., 2014, 11: 418 |
| [8] | WangX, GuanR G, MisraR D K, et al. The mechanistic contribution of nanosized Al3Fe phase on the mechanical properties of Al-Fe alloy [J]. Mater. Sci. Eng., 2018, A724: 452 |
| [9] | LiuB, YuanX G, HuangH J. Microstructure and mechanical properties of hypereutectic Al-Fe alloys prepared by semi-solid formation [J]. China Found., 2011, 8: 424 |
| [10] | GillonP. Uses of intense d.c. magnetic fields in materials processing [J]. Mater. Sci. Eng., 2000, A287: 146 |
| [11] | JiaP, WangE G, LuH, et al. Effect of electromagnetic field on microstructure and mechanical property for Inconel 625 superalloy [J]. Acta Metall. Sin., 2013, 49: 1573 |
| [11] | 贾 鹏, 王恩刚, 鲁 辉等. 电磁场对Inconel 625合金凝固组织及力学性能的影响 [J]. 金属学报, 2013, 49: 1573 |
| [12] | LiX, RenZ M, FautrelleY. Phase distribution and phase structure control through a high gradient magnetic field during the solidification process [J]. Mater. Des., 2008, 29: 1796 |
| [13] | ChenD D, ZhangH T, WangX J, et al. Investigation on Microsegregation of Al-4.5%Cu alloy produced by low frequency electromagnetic casting [J]. Acta Metall. Sin., 2011, 47: 185 |
| [13] | 陈丹丹, 张海涛, 王向杰等. 低频电磁铸造Al-4.5%Cu合金微观偏析研究 [J]. 金属学报, 2011, 47: 185 |
| [14] | XuX J, DengA Y, WangE G, et al. Evolvement mechanism of surface oscillation marks on round billet during soft-contact electromagnetic continuous casting [J]. Acta Metall. Sin., 2009, 45: 464 |
| [14] | 许秀杰, 邓安元, 王恩刚等. 电磁软接触连铸圆坯表面振痕演变机理 [J]. 金属学报, 2009, 45: 464 |
| [15] | HanY, BanC Y, GuoS J, et al. Alignment behavior of primary Al3Fe phase in Al-Fe alloy under a high magnetic field [J]. Mater. Lett., 2007, 61: 983 |
| [16] | Huhemandula, YangH T, JiW H, et al. Effect of alternating magnetic field on microstructure and property of Al-5%Fe alloy [J]. Found. Technol., 2016, 37: 285 |
| [16] | 呼和满都拉, 杨洪涛, 冀文慧等. 电磁物理场对Al-5%Fe合金组织与性能的影响[J]. 铸造科技, 2016, 37: 285 |
| [17] | ZhangH T, NagaumiH, ZuoY B, et al. Coupled modeling of electromagnetic field, fluid flow, heat transfer and solidification during low frequency electromagnetic casting of 7XXX aluminum alloys: Part 1: Development of a mathematical model and comparison with experimental results [J]. Mater. Sci. Eng., 2007, A448: 189 |
| [18] | LiM J, TamuraT, MiwaK. Controlling microstructures of AZ31 magnesium alloys by an electromagnetic vibration technique during solidification: From experimental observation to theoretical understanding [J]. Acta Mater., 2007, 55: 4635 |
| [19] | ZhangT, RenW L, DongJ W, et al. Effect of high magnetic field on the primary dendrite arm spacing and segregation of directionally solidified superalloy DZ417G [J]. J. Alloys Compd., 2009, 487: 612 |
| [20] | GuoS H. Electrodynamics [M]. 2nd Ed., Beijing: Higher Education Press, 1997: 118 |
| [20] | 郭硕鸿. 电动力学 [M]. 第2版,北京: 高等教育出版社, 1997: 118 |
/
| 〈 |
|
〉 |