Microstructure and Electric Conductance of Mg2(Sn, Si) Thin Films by Sputtering
Received date: 2019-04-12
Revised date: 2019-08-12
Online published: 2019-09-02
Supported by
National Natural Science Foundation of China(51772193)
The Mg content in Mg2(Sn, Si) films obtained by PVD method often deviates its stoichiometric composition due to the easy evaporation of Mg in low pressure. In order to control the Mg content in Mg2(Sn, Si) lattice and achieve enhancements in thermoelectric efficiency, The Mg-Sn-Si-Bi thin films were deposited on single Si(111) substrate using a Mg-Sn-Si-Bi alloy target and a high pure Mg target by magnetron sputtering alternately. The results show that the Mg content greatly increases, while contents of both Sn and Si decrease in the films with the increasing sputtering time of the Mg target. The thin films possess single cubic Mg2(Sn, Si) solution phase as the Mg content (atomic fraction) is in the range from 71.437% to 64.497%, the Mg2(Sn, Si) solution phase disappear and both of Mg2Sn and Mg2Si phases occur as the Mg content decreases below 59.813% in the films. Furthermore, the Mg2Sn phase decomposes and metal Sn occurs as the Mg content in the films decreases to 54.006%. The metal Sn content increases and the Mg2Sn phase content decreases with the decreasing Mg content in the films, accompanying the near invariable Mg2Sn phase content. XPS spectrum data show that Mg exhibits the tendency to lose electrons. However, the Sn, Si and Bi exhibit the tendency to obtain electrons in deposited films. It is indicated that the Mg-Sn-Si-Bi thin film with single cubic solution phase possesses higher conductivity due to its higher carrier concentration and higher mobility. The mobility greatly decreases due to the occurrence of metal Sn in the films, thus the conductivity of the films greatly decreases.
Key words: Mg2(Sn; Si) film; Mg content; conductivity; mobility; XPS
Guihong SONG , Guipeng LI , Qiannan LIU , Hao DU , Fang HU . Microstructure and Electric Conductance of Mg2(Sn, Si) Thin Films by Sputtering[J]. Acta Metall Sin, 2019 , 55(11) : 1469 -1476 . DOI: 10.11900/0412.1961.2019.00115
| [1] | ZhangX, LiuH L, LuQ M, et al. Enhanced thermoelectric performance of Mg2Si0.4Sn0.6 solid solutions by in nanostructures and minute Bi-doping [J]. Appl. Phys. Lett., 2013, 103: 063901 |
| [2] | Pshenai-SeverinD A, FedorovM I, SamuninA Y. The influence of grain boundary scattering on thermoelectric properties of Mg2Si and Mg2Si0.8Sn0.2 [J]. J. Electron. Mater., 2013, 42: 1707 |
| [3] | ZhangB, ZhengT, SunC, et al. Electrical transport characterization of Al and Sn doped Mg2Si thin films [J]. J. Alloys Compd., 2017, 720: 156 |
| [4] | JangJ, RyuB, JaeJ S, et al. Antimony-induced heterogeneous microstructure of Mg2Si0.6Sn0.4 thermoelectric materials and their thermoelectric properties [J]. J. Alloys Compd., 2018, 739: 129 |
| [5] | VlachosN, PolymerisG S, ManoliM, et al. Effect of antimony-doping and germanium on the highly efficient thermoelectric Si-rich-Mg2(Si, Sn, Ge) materials [J]. J. Alloys Compd., 2017, 714: 502 |
| [6] | IoannouM, PolymerisG S, HatzikraniotisE, et al. Effect of Bi-doping and Mg-excess on the thermoelectric properties of Mg2Si materials [J]. J. Phys. Chem. Solids, 2014, 75: 984 |
| [7] | LiuW, ZhangQ, YinK, et al. High figure of merit and thermoelectric properties of Bi-doped Mg2Si0.4Sn0.6 solid solutions [J]. J. Solid State Chem., 2013, 203: 333 |
| [8] | GaoH L, LiuX X, ZhuT J, et al. Effect of Sb doping on the thermoelectric properties of Mg2Si0.7Sn0.3 solid solutions [J]. J. Electron. Mater., 2011, 40: 830 |
| [9] | TangX D, ZhangY M, ZhengY, et al. Improving thermoelectric performance of p-type Ag-doped Mg2Si0.4Sn0.6 prepared by unique melt spinning method [J]. Appl. Thermal Eng., 2017, 111: 1396 |
| [10] | KimS, WiendlochaB, JinH, et al. Electronic structure and thermoelectric properties of p-type Ag-doped Mg2Sn and Mg2Sn1-xSix (x=0.05, 0.1) [J]. J. Appl. Phys., 2014, 116: 153706 |
| [11] | ChenZ J, ZhouB Y, LiJ X, et al. Thermoelectric properties of Al-doped Mg2Si thin films deposited by magnetron sputtering [J]. Appl. Surf. Sci., 2016, 386: 389 |
| [12] | PrahoveanuC, LacosteA, BéchuS, et al. Investigation of Mg2(Si, Sn) thin films for integrated thermoelectric devices [J]. J. Alloys Compd., 2015, 649: 573 |
| [13] | SongG H, LiuQ N, DuH, et al. The thermoelectric properties of the Mg2(Sn, Si) films by magnetron sputtering with different microstructure [J]. Surf. Coat. Technol., 2019, 359: 252 |
| [14] | JiangY H, ChiuI C, KaoP K, et al. Influence of rapid-thermal-annealing temperature on properties of rf-sputtered SnOx thin films [J]. Appl. Surf. Sci., 2015, 327: 358 |
| [15] | LiangL Y, LiuZ M, CaoH T, et al. Microstructural, optical, and electrical properties of SnO thin films prepared on quartz via a two-step method [J]. ACS Appl. Mater. Interface, 2010, 2: 1060 |
| [16] | KhanA U, VlachosN V, HatzikraniotisE, et al. Thermoelectric properties of highly efficient Bi-doped Mg2Si1-x-ySnxGey materials [J]. Acta Mater., 2014, 77: 43 |
| [17] | OgawaS, KatagiriA, ShimizuT, et al. Electrical properties of (110)-oriented nondoped Mg2Si films with p-type conduction prepared by RF magnetron sputtering method [J]. J. Electron. Mater., 2014, 43: 2269 |
| [18] | ImaiY, SohmaM, SuemasuT. Effect of oxygen incorporation in the Mg2Si lattice on its conductivity type—A possible reason of the p-type conductivity of postannealed Mg2Si thin film [J]. J. Alloys Compd., 2016, 676: 91 |
| [19] | MaoJ, ZhuH T, DingZ W, et al. High thermoelectric cooling performance of n-type Mg3Bi2-based materials [J]. Science, 2019, 365: 495 |
| [20] | ZhangY, WangX L, YeohW K, et al. Electrical and thermoelectric properties of single-wall carbon nanotube doped Bi2Te3 [J]. Appl. Phys. Lett., 2012, 101: 031909 |
| [21] | TanM, DengY, WangY. Ordered structure and high thermoelectric properties of Bi2(Te, Se)3 nanowire array [J]. Nano Energy, 2014, 3: 144 |
| [22] | LinZ Y, YinA X, MaoJ, et al. Scalable solution-phase epitaxial growth of symmetry-mismatched heterostructures on two-dimensional crystal soft template [J]. Sci. Adv., 2016, 2: e1600993 |
| [23] | AoW Q, PengM, LiuF S, et al. High thermoelectric properties in Mg2Ge0.25Sn0.75-xSbx solid solution [J]. J. Electron. Mater., 2019, 48: 5959 |
| [24] | GaoH L, ZhuT J, ZhaoX B, et al. Influence of Sb doping on thermoelectric properties of Mg2Ge materials [J]. Intermetallics, 2015, 56: 33 |
| [25] | LiuW, TanX J, YinK, et al. Convergence of conduction bands as a means of enhancing thermoelectric performance of n-type Mg2Si1-xSnx solid solutions [J]. Phys. Rev. Lett., 2012, 108: 166601 |
/
| 〈 |
|
〉 |