Generation and Interaction Mechanism of Tension Kink Band in AZ31 Magnesium Alloy
Received date: 2019-05-07
Revised date: 2019-08-02
Online published: 2019-08-23
Supported by
National Natural Science Foundation of China(Nos.11374028);National Natural Science Foundation of China(U1330112);National Natural Science Foundation of China(51621003);Scientific Research Key Program of Beijing Municipal Commission of Education(No.KZ201310005002);Beijing Municipal Found for Scientific Innovation(No.PXM2019_014204_500031)
The deformation structures, such as deformation twins, dislocations and kink bands, play an important role in the plasticity of magnesium alloys during the deformation process. However, due to the complexity of hcp structure, the deformation structures of the magnesium alloys, especially the interactions between deformation structures are still not well understood. Thus, it is of great scientific significance to study the microstructure of magnesium alloys, especially to characterize their structural characteristics of the interaction areas, which plays a significant role in understanding the structure and performance relationships of magnesium alloys. In this work, a combination of TEM and SAED pattern was applied to study the interaction mechanism associated with different kinds of deformation structures in Mg-Al-Zn (AZ31) alloy. When the applied external force is not beneficial for deformation twins and dislocations, kink bands act as a supplementary deformation mode to coordinate the asymmetry of hcp structure. According to crystallographic analysis, it is found that under the action of tensile stress nearly lie on basal plane in hcp structures, the basal dislocation pairs form and move to the opposite directions, forming tension kink band with the interface of {10
Key words: Mg alloy; kink band; deformation twins; TEM
ZHOU Bo , SUI Manling . Generation and Interaction Mechanism of Tension Kink Band in AZ31 Magnesium Alloy[J]. Acta Metall Sin, 2019 , 55(12) : 1512 -1518 . DOI: 10.11900/0412.1961.2019.00149
| [1] | Aghion E, Bronfin B. Magnesium alloys development towards the 21st century [A]. Materials Science Forum [C]. Switzerland: Trans. Tech. Publications, 2000: 19 |
| [2] | Barnett M R. Twinning and the ductility of magnesium alloys [J]. Mater. Sci. Eng., 2007, A464: 8 |
| [3] | Cizek P, Barnett M R. Characteristics of the contraction twins formed close to the fracture surface in Mg-3Al-1Zn alloy deformed in tension [J]. Scr. Mater., 2008, 59: 959 |
| [4] | Suh B C, Shim M S, Shin K S, et al. Current issues in magnesium sheet alloys: Where do we go from here? [J]. Scr. Mater., 2014, 84-85: 1 |
| [5] | Pollock T M. Weight loss with magnesium alloys [J]. Science, 2010, 328: 986 |
| [6] | Frankel G S. Magnesium alloys: Ready for the road [J]. Nat. Mater., 2015, 14: 1189 |
| [7] | Joost W J, Krajewski P E. Towards magnesium alloys for high-volume automotive applications [J]. Scr. Mater., 2017, 128: 107 |
| [8] | Yoo M H, Lee J K. Deformation twinning in h.c.p. metals and alloys [J]. Philos. Mag., 1991, 63A: 987 |
| [9] | Yoo M H. Slip, twinning, and fracture in hexagonal close-packed metals [J]. Metall. Trans., 1981, 12A: 409 |
| [10] | Mu S J, Tang F, Gottstein G. A cluster-type grain interaction deformation texture model accounting for twinning-induced texture and strain-hardening evolution: Application to magnesium alloys [J]. Acta Mater., 2014, 68: 310 |
| [11] | Orowan E. A type of plastic deformation new in metals [J]. Nature, 1942, 149: 643 |
| [12] | Hess J B, Barrett C S. Structure and nature of kink bands in zinc [J]. JOM, 1949, 1(9): 599 |
| [13] | Shao X H, Yang Z Q, Ma X L. Strengthening and toughening mechanisms in Mg-Zn-Y alloy with a long period stacking ordered structure [J]. Acta Mater., 2010, 58: 4760 |
| [14] | Shao X H, Peng Z Z, Jin Q Q, et al. Atomic-scale segregations at the deformation-induced symmetrical boundary in an Mg-Zn-Y alloy [J]. Acta Mater., 2016, 118: 177 |
| [15] | Matsumoto T, Yamasaki M, Hagihara K, et al. Configuration of dislocations in low-angle kink boundaries formed in a single crystalline long-period stacking ordered Mg-Zn-Y alloy [J]. Acta Mater., 2018, 151: 112 |
| [16] | Hagihara K, Mayama T, Honnami M, et al. Orientation dependence of the deformation kink band formation behavior in Zn single crystal [J]. Int. J. Plast., 2016, 77: 174 |
| [17] | Yang X Y, Jiang Y P. Morphology and crystallographic characteristics of deformation bands in Mg alloy under hot deformation [J]. Acta Metall. Sin., 2010, 46: 451 |
| [17] | (杨续跃, 姜育培. 镁合金热变形下变形带的形貌和晶体学特征 [J]. 金属学报, 2010, 46: 451) |
| [18] | Wang J, Beyerlein I J, Tomé C N. Reactions of lattice dislocations with grain boundaries in Mg: Implications on the micro scale from atomic-scale calculations [J]. Int. J. Plast., 2014, 56: 156 |
| [19] | Zhou N, Zhang Z Y, Jin L, et al. Ductility improvement by twinning and twin-slip interaction in a Mg-Y alloy [J]. Mater. Des., 2014, 56: 966 |
| [20] | Wang F L, Agnew S. Magnesium Technology 2015 [M]. New Jersey: Springer, 2015: 139 |
| [21] | Beyerlein I J, Wang J, Barnett M R, et al. Double twinning mechanisms in magnesium alloys via dissociation of lattice dislocations [J]. Proc. Roy. Soc., 2012, 468A: 1496 |
| [22] | Zhou B, Tai J, Lu Y, et al. Dislocation-modified high index twinning mechanisms in deformed magnesium alloy [J]. J. Alloys Compd., 2019, 787: 423 |
| [23] | Anderson T B. Kink Bands [M]. Berlin: Springer, 1987: 373 |
| [24] | Li X C, Li J W, Zhou B, et al. Interaction of {1122} twin variants in hexagonal close-packed titanium [J]. J. Mater. Sci. Technol., 2019, 35: 660 |
/
| 〈 |
|
〉 |