Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe
Received date: 2019-03-11
Revised date: 2019-05-12
Online published: 2019-07-03
Supported by
National Key Research and Development Program of China(No.2017YFB0702302);National Natural Science Foundation of China(Nos.51671200);National Natural Science Foundation of China(51501204);National Natural Science Foundation of China(51801219)
Hydrostatic pressure was one of the critical factors affecting deep-sea corrosion. Theoretical research showed that increasing hydrostatic pressure could improve the activity of metal materials, increase the difference in activity between coupled metal materials, and aggravate the galvanic corrosion. At present, there were many researches on the corrosion behavior of metallic materials under hydrostatic pressure, but there were few researches on the influence of hydrostatic pressure on the corrosion behavior of metal materials. Due to the requirements of structure and performance in the marine environment, equipment components with different electrochemical properties must be connected. In such a harsh environment, galvanic corrosion would obviously accelerate. Therefore, it was very necessary to study the galvanic corrosion behavior of metallic materials under the condition of the deep sea. Fe-based alloys and Al-based alloys have been widely used in the marine environment, and there have been many studies on corrosion of Fe-based alloys and Al-based alloys in the deep-sea environment. As a result of single composition and structure, taking ultra-pure Al and ultra-pure Fe as the research object, the influence of phase, inclusion and other factors on corrosion behavior under hydrostatic pressure could be avoided, which was helpful to clarify the influence of hydrostatic pressure on corrosion behavior of ultrapure Al coupled with ultra-pure Fe. The influence of hydrostatic pressure on the corrosion behavior of ultrapure Al coupled with ultrapure Fe was studied in 3.5%NaCl using electrodynamic polarization and electrochemical noise. The discrete wavelet transform was utilized to remove the direct current drift of noise signal, and then the stochastic analysis based on the shot noise theory was carried out. The Hilbert-Huang transform was utilized to analyze the time-frequency characteristics of the noise signal. The surface morphology of corrosion samples was observed by SEM. The pressure distribution was simulated by finite element method. The results showed that the ultrapure Al was self-passivation in 3.5%NaCl solution under different hydrostatic pressures, pitting corrosion occurred after coupling with ultrapure Fe. With the increase of hydrostatic pressure, the galvanic potential of coupled ultrapure Al and ultrapure Fe decreased gradually, and the galvanic current increased gradually. The increase of hydrostatic pressure accelerated the pitting generation rate of ultrapure Al in galvanic corrosion, but inhibited the growth probability of pitting corrosion and reduced the tendency of local corrosion. When hydrostatic pressure was atmospheric, pitting corrosion could expand along the horizontal and vertical directions. In the presence of hydrostatic pressure, pitting corrosion was easier to expand along the horizontal direction.
MA Rongyao , MU Xin , LIU Bo , WANG Changgang , WEI Xin , ZHAO Lin , DONG Junhua , KE Wei . Effect of Hydrostatic Pressure on Corrosion Behavior of Ultra Pure Al Coupled with Ultra Pure Fe[J]. Acta Metall Sin, 2019 , 55(12) : 1593 -1605 . DOI: 10.11900/0412.1961.2019.00064
| [1] | Ma R Y, Zhao L, Wang C G, et al. Influence of hydrostatic pressure on the thermodynamics and kinetics of metal corrosion [J]. Acta Metall. Sin., 2019, 55: 281 |
| [1] | (马荣耀, 赵 林, 王长罡等. 静水压力对金属腐蚀热力学及动力学的影响 [J]. 金属学报, 2019, 55: 281) |
| [2] | Xing S H, Li Y, Wharton J A, et al. Effect of dissolved oxygen and coupled resistance on the galvanic corrosion of Cr-Ni low-alloy steel/90-10 cupronickel under simulated deep sea condition [J]. Mater. Corros., 2017, 68: 1123 |
| [3] | Li Q C, Yang J, Wu L, et al. Influence of pressure on galvanic corrosion of 907/921/B10 couples in simulated deep-sea environment [J]. Int. J. Electrochem. Sci., 2016, 11: 6443 |
| [4] | Mansfeld F, Chen C, Lee C C, et al. The effect of asymmetric electrodes on the analysis of electrochemical impedance and noise data [J]. Corros. Sci., 1996, 38: 497 |
| [5] | Lowe A M, Eren H, Bailey S I. Electrochemical noise analysis: Detection of electrode asymmetry [J]. Corros. Sci., 2003, 45: 941 |
| [6] | Chen J F, Bogaerts W F. Electrochemical emission spectroscopy for monitoring uniform and localized corrosion [J]. Corrosion, 1996, 52: 753 |
| [7] | Bertocci U, Gabrielli C, Huet F, et al. Noise resistance applied to corrosion measurements: I. Theoretical analysis [J]. J. Electrochem. Soc., 1997, 144: 31 |
| [8] | Bertocci U, Huet F. Noise resistance applied to corrosion measurements: III. Influence of the instrumental noise on the measurements [J]. J. Electrochem. Soc., 1997, 144: 2786 |
| [9] | Bautista A, Huet F. Noise resistance applied to corrosion measurements: IV. Asymmetric coated electrodes [J]. J. Electrochem. Soc., 1999, 146: 1730 |
| [10] | Bautista A, Bertocci U, Huet F. Noise resistance applied to corrosion measurements: V. Influence of electrode asymmetry [J]. J. Electrochem. Soc., 2001, 148: B412 |
| [11] | Cottis R A. The significance of electrochemical noise measurements on asymmetric electrodes [J]. Electrochim. Acta, 2007, 52: 7585 |
| [12] | Curioni M, Cottis R A, Di Natale M, et al. Corrosion of dissimilar alloys: Electrochemical noise [J]. Electrochim. Acta, 2011, 56: 6318 |
| [13] | Curioni M, Cottis R A, Di Natale M, et al. Electrochemical noise analysis on multiple dissimilar electrodes: Theoretical analysis [J]. Electrochim. Acta, 2011, 56: 10270 |
| [14] | Curioni M, Balaskas A C, Thompson G E. An alternative to the use of a zero resistance ammeter for electrochemical noise measurement: Theoretical analysis, experimental validation and evaluation of electrode asymmetry [J]. Corros. Sci., 2013, 77: 281 |
| [15] | Curioni M, Cottis R A, Thompson G E. Interpretation of electrochemical noise generated by multiple electrodes [J]. Corrosion, 2013, 69: 158 |
| [16] | Curioni M, Skeldon P, Thompson G E. Reliability of the estimation of polarization resistance of corroding electrodes by electrochemical noise analysis: Effects of electrode asymmetry [J]. Electrochim. Acta, 2013, 105: 642 |
| [17] | Astarita A, Curioni M, Squillace A, et al. Corrosion behaviour of stainless steel-titanium alloy linear friction welded joints: Galvanic coupling [J]. Mater. Corros., 2015, 66: 111 |
| [18] | Blasco-Tamarit E, Igual-Mu?oz A, García Antón J, et al. Corrosion behaviour and galvanic coupling of titanium and welded titanium in LiBr solutions [J]. Corros. Sci., 2007, 49: 1000 |
| [19] | Sakairi M, Shimoyama Y, Takahashi H. Electrochemical noise analysis of galvanic corrosion of anodized aluminum in chloride environments [J]. Electrochemistry, 2006, 74: 458 |
| [20] | Sakairi M, Shimoyama Y. Electrochemical random signal analysis during galvanic corrosion of anodized aluminum alloy [J]. J. JSEM, 2007, 7(Spec. issue):114 |
| [21] | Monta?és M T, Sánchez-Tovar R, García-Antón J, et al. Influence of the flowing conditions on the galvanic corrosion of the copper/AISI 304 pair in lithium bromide using a zero-resistance ammeter [J]. Int. J. Electrochem. Sci., 2010, 5: 1934 |
| [22] | Sun H J, Liu L, Li Y, et al. The performance of Al-Zn-In-Mg-Ti sacrificial anode in simulated deep water environment [J]. Corros. Sci., 2013, 77: 77 |
| [23] | Gusmano G, Montesperelli G, Pacetti S, et al. Electrochemical noise resistance as a tool for corrosion rate prediction [J]. Corrosion, 1997, 53: 860 |
| [24] | Cottis R A. Interpretation of electrochemical noise data [J]. Corrosion, 2001, 57: 265 |
| [25] | Ma R Y, Wang C G, Mu X, et al. Influence of hydrostatic pressure on corrosion behavior of ultrapure Fe [J]. Acta Metall. Sin., 2019, 55: 859 |
| [25] | (马荣耀, 王长罡, 穆 鑫等. 静水压力对超纯Fe腐蚀行为的影响 [J]. 金属学报, 2019, 55: 859) |
| [26] | Rilling G, Flandrin P, Goncalves P. On empirical mode decomposition and its algorithms [A]. Proceedings of the IEEE-EURASIP Workshop on Nonlinear Signal and Image Processing [C]. Grado, Italy: IEEE, 2003: 8 |
| [27] | Flandrin P, Rilling G, Goncalves P. Empirical mode decomposition as a filter bank [J]. IEEE Signal Process. Lett., 2004, 11: 112 |
| [28] | Cao C N. Principles of Electrochemistry of Corrosion [M]. Beijing: Chemical Industry Press, 2008: 105 |
| [28] | (曹楚南. 腐蚀电化学原理 [M]. 北京: 化学工业出版社, 2008: 105) |
| [29] | Shao Y W, Huang H, Zhang T, et al. Corrosion protection of Mg-5Li alloy with epoxy coatings containing polyaniline [J]. Corros. Sci., 2009, 51: 2906 |
| [30] | Cao F H, Zhang Z, Su J X, et al. Electrochemical noise analysis of LY12-T3 in EXCO solution by discrete wavelet transform technique [J]. Electrochim. Acta, 2006, 51: 1359 |
| [31] | Aballe A, Bethencourt M, Botana F J, et al. Wavelet transform-based analysis for electrochemical noise [J]. Electrochem. Commun., 1999, 1: 266 |
| [32] | Dong Z H, Guo X P, Zheng J S, et al. Calculation of noise resistance by use of the discrete wavelets transform [J]. Electrochem. Commun., 2001, 3: 561 |
| [33] | Moshrefi R, Mahjani M G, Jafarian M. Application of wavelet entropy in analysis of electrochemical noise for corrosion type identification [J]. Electrochem. Commun., 2014, 48: 49 |
| [34] | Aballe A, Bethencourt M, Botana F J, et al. Using wavelets transform in the analysis of electrochemical noise data [J]. Electrochim. Acta, 1999, 44: 4805 |
| [35] | Cai C, Zhang Z, Cao F H, et al. Analysis of pitting corrosion behavior of pure Al in sodium chloride solution with the wavelet technique [J]. J. Electroanal. Chem., 2005, 578: 143 |
| [36] | Homborg A M, van Westing E P M, Tinga T, et al. Novel time-frequency characterization of electrochemical noise data in corrosion studies using Hilbert spectra [J]. Corros. Sci., 2013, 66: 97 |
| [37] | Homborg A M, Tinga T, Zhang X, et al. Transient analysis through Hilbert spectra of electrochemical noise signals for the identification of localized corrosion of stainless steel [J]. Electrochim. Acta, 2013, 104: 84 |
| [38] | Zhao B, Li J H, Hu R G, et al. Study on the corrosion behavior of reinforcing steel in cement mortar by electrochemical noise measurements [J]. Electrochim. Acta, 2007, 52: 3976 |
/
| 〈 |
|
〉 |