Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings
Received date: 2019-04-01
Revised date: 2019-05-09
Online published: 2019-07-03
Supported by
Supported by National Natural Science Foundation of China(U1708253);National Key Research and Deve-lopment Program of China(2017YFB0702901);Shenzhen Municipal Science and Technology Inovation Council(JCYJ20160608161000821)
Significant interior residual stresses, which were generated during the manufacture process, could affect the machining dimension precision and structural stability during the subsequent machining process and service operation in the superalloys component, such as turbine disk. In this paper, the neutron diffraction method and contour method are described for measuring the distribution of interior residual stresses. The distribution, evolution of interior residual stress, and its mechanism are analyzed during quenching, ageing heat treatment and machining process in superalloys disk forging. The residual stresses are mainly generated by the temperature gradient formed during rapid cooling after solution heat treatment. After quenching, the residual stresses in hoop direction and radial direction of disc forging are significant, and its distribution along the profile is characterized by "internal tension and external pressure". The magnitudes of the residual stresses are equivalent to the yield strength of as-quenched alloys at room temperature. Quenching-induced residual stresses are partially relieved during the ageing process due to plastic strain and creep-controlled dislocation rearrangement. The precipitation behavior of γ″ or γ′ phase during heat treatment has a significant interaction with the distribution and magnitude of residual stress. During the machining process, part of the residual stresses contributing to the equilibrium of the internal forces are removed along with the material. Additional moment caused by re-balance of residual stresses results in the serious consequences of distortion in the remaining body.
Key words: superalloy; residual stress; neutron diffraction; contour method; turbine disk
Zhongnan BI , Hailong QIN , Zhiguo DONG , Xiangping WANG , Ming WANG , Yongquan LIU , Jinhui DU , Ji ZHANG . Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings[J]. Acta Metall Sin, 2019 , 55(9) : 1160 -1174 . DOI: 10.11900/0412.1961.2019.00089
| [1] | GuY F, CuiC Y, YuanY, , et al. Research progress in a high performance cast & wrought superalloy for turbine disc applications [J]. Acta Metall. Sin., 2015, 51: 1191 |
| [1] | 谷月峰, 崔传勇, 袁 勇等. 一种高性能航空涡轮盘用铸锻合金的研究进展 [J]. 金属学报, 2015, 51: 1191 |
| [2] | ZhangB J, ZhaoG P, ZhangW Y, , et al. Investigation of high performance disc alloy GH4065 and associated advanced processing techniques [J]. Acta Metall. Sin., 2015, 51: 1227 |
| [2] | 张北江, 赵光普, 张文云等. 高性能涡轮盘材料GH4065及其先进制备技术研究 [J]. 金属学报, 2015, 51: 1227 |
| [3] | LuX D, DuJ H, DengQ. High temperature structure stability of GH4169 superalloy [J]. Mater. Sci. Eng., 2013, A559: 623 |
| [4] | DuJ H, LuX D, DengQ, , et al. High-temperature structure stability and mechanical properties of novel 718 superalloy [J]. Mater. Sci. Eng., 2007, A452-453: 584 |
| [5] | ZhuangJ Y, DuJ H, DengQ, , et al. Wrought Superalloy GH4169 [M]. Beijing: Metallurgical Industry Press, 2006: 1 |
| [5] | 庄景云, 杜金辉, 邓 群等. 变形高温合金GH4169 [M]. 北京: 冶金工业出版社, 2006: 1) |
| [6] | GengL, NaY S, ParkN K. Continuous cooling transformation behavior of Alloy 718 [J]. Mater. Lett., 1997, 30: 401 |
| [7] | DyeD, ConlonK T, ReedR C. Characterization and modeling of quenching-induced residual stresses in the nickel-based superalloy IN718 [J]. Metall. Mater. Trans., 2004, 35A: 1703 |
| [8] | RistM A, JamesJ A, TinS, , et al. Residual stresses in a quenched superalloy turbine disc: Measurements and modeling [J]. Metall. Mater. Trans., 2006, 37A: 459 |
| [9] | KaradgeM, GrantB, WithersP J, , et al. Thermal relaxation of residual stresses in nickel-based superalloy inertia friction welds [J]. Metall. Mater. Trans., 2011, 42A: 2301 |
| [10] | FossB J, GrayS, HardyM C, , et al. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR1000 [J]. Acta Mater., 2013, 61: 2548 |
| [11] | WithersP J, BhadeshiaH K D K. Residual stress. Part 1 Measurement techniques [J]. Mater. Sci. Technol., 2001, 17: 355 |
| [12] | Aba-PereaP E, PirlingT, PreussM. In-situ residual stress analysis during annealing treatments using neutron diffraction in combination with a novel furnace design [J]. Mater. Des., 2016, 110: 925 |
| [13] | RolphJ, EvansA, ParadowskaA, , et al. Stress relaxation through ageing heat treatment—A comparison between in situ and ex situ neutron diffraction techniques [J]. C. R.Phys., 2012, 13: 307 |
| [14] | Ghasri-KhouzaniM, PengH, RoggeR, , et al. Experimental measurement of residual stress and distortion in additively manufactured stainless steel components with various dimensions [J]. Mater. Sci. Eng., 2017, A707: 689 |
| [15] | MasoudiS, AmirianG, SaeediE, , et al. The effect of quench-induced residual stresses on the distortion of machined thin-walled parts [J]. J. Mater. Eng. Perform., 2015, 24: 3933 |
| [16] | KrempaszkyC, WernerE A, StockingerM. Measurement of marcoscopic residual stress and resulting distortion during machining [A]. Proc.MS&T 2005 Iron & Steel Society and TMS [C]. Pittsburgh, PA, USA: TMS, 2005: 109 |
| [17] | WithersP J, BhadeshiaH K D K. Residual stress. Part 2 Nature and origins [J]. Mater. Sci. Technol., 2001, 17: 366 |
| [18] | ShenG S, CooperN, OttowN, , et al. Integration and automation of residual stress and service stress modeling for superalloy component design [A].Superalloy 2012 [C]. Hoboken, NJ: Wiley, 2012: 129 |
| [19] | RolphJ, PreussM, IqbalN, , et al. Residual stress evolution during manufacture of aerospace forgings [A].Superalloy 2012 [C]. Hoboken, NJ: Wiley, 2012: 881 |
| [20] | DahanY, NouveauS, GeorgesE, , et al. Residual stresses in Inconel 718 engine disks [J]. MATEC Web Conf., 2014, 14: 10003 |
| [21] | XuP G, TomotaY. Progress in materials characterization technique based on in situ neutron diffraction [J]. Acta Metall. Sin., 2006, 42: 681 |
| [21] | 徐平光, 友田阳. 原位中子衍射材料表征技术的进展 [J]. 金属学报, 2006, 42: 681 |
| [22] | DongP, WangH, LiJ, , et al. Residual stress in welded Beryllium ring by neutron diffraction and finite element modeling [J]. At. Energ. Sci. Technol., 2015, 49: 2255 |
| [22] | 董 平, 王 虹, 李 建等. 铍环焊接残余应力的中子衍射测试与有限元分析 [J]. 原子能科学技术, 2015, 49: 2255 |
| [23] | CollinsD M, D'SouzaN, PanwisawasC. In-situ neutron diffraction during stress relaxation of a single crystal nickel-base superalloy [J]. Scr. Mater., 2017, 131: 103 |
| [24] | AllenA J, HutchingsM T, WindsorC G, , et al. Neutron diffraction methods for the study of residual stress fields [J]. Adv. Phys., 1985, 34: 445 |
| [25] | SantistebanJ R, DaymondM R, JamesJ A, , et al. ENGIN-X: A third-generation neutron strain scanner [J]. J. Appl. Cryst., 2006, 39: 812 |
| [26] | WagnerJ N, HofmannM, WimporyR, , et al. Microstructure and temperature dependence of intergranular strains on diffractometric macroscopic residual stress analysis [J]. Mater. Sci. Eng., 2014, A618: 271 |
| [27] | PrimeM B. Cross-sectional mapping of residual stresses by measuring the surface contour after a cut [J]. J. Eng. Mater. Technol., 2001, 123: 162 |
| [28] | Oradei-BasileA, RadavichJ F. A current T-T-T Diagram for wrought alloy 718 [A]. Superalloys 718, 625 and Various Derivatives [C]. Pittsburgh, PA,USA: The Minerals, Metals & Materials Society, 1991: 325 |
| [29] | JianM, ChangK M, YangW H, , et al. Cooling precipitation and strengthening study in powder metallurgy superalloy U720LI [J]. Metall. Mater. Trans., 2001, 32A: 2441 |
| [30] | YaoZ H, DongJ X, ZhangM C, , et al. Influence of solution and stabilization heat treatment on carbide and gamma prime for super alloy GH738 [J]. Trans. Mater. Heat Treat., 2013, 34(10): 43 |
| [30] | 姚志浩, 董建新, 张麦仓等. 固溶及稳定化工艺对GH738合金碳化物和γ'相析出规律的影响 [J]. 材料热处理学报, 2013, 34(10): 43) |
| [31] | QinH L, BiZ N, YuH Y, , et al. Assessment of the stress-oriented precipitation hardening designed by interior residual stress during ageing in IN718 superalloy [J]. Mater. Sci. Eng., 2018, A728: 183 |
| [32] | QinH L, ZhangR Y, BiZ N, , et al. Study on the evolution of residual stress during the ageing treatment in a GH4169 alloy disk [J]. Acta Metall. Sin., 2019, 55: 997 |
| [32] | 秦海龙, 张瑞尧, 毕中南等. GH4169合金圆盘时效过程残余应力的演化规律研究 [J]. 金属学报, 2019, 55: 997 |
| [33] | ChaturvediM C, HanY F. Effect of particle size on the creep rate of superalloy Inconel 718 [J]. Mater. Sci. Eng., 1987, 89: L7 |
| [34] | KuoC M, YangY T, BorH Y, , et al. Aging effects on the microstructure and creep behavior of Inconel 718 superalloy [J]. Mater. Sci. Eng., 2009, A510-511: 289 |
| [35] | RaoA, BouchardP J, NorthoverS M, , et al. Anelasticity in austenitic stainless steel [J]. Acta Mater., 2012, 60: 6851 |
| [36] | FiskM, IonJ C, LindgrenL E. Flow stress model for IN718 accounting for evolution of strengthening precipitates during thermal treatment [J]. Comput. Mater. Sci., 2104, 82: 531 |
| [37] | CoakleyJ, MaD, FrostM, , et al. Lattice strain evolution and load partitioning during creep of a Ni-based superalloy single crystal with rafted γ′ microstructure [J]. Acta Mater., 2017, 135: 77 |
| [38] | QinH L, BiZ N, LiD F, , et al. Study of precipitation-assisted stress relaxation and creep behavior during the ageing of a nickel-iron superalloy [J]. Mater. Sci. Eng., 2019, A742: 493 |
| [39] | QinH L, BiZ N, YuH Y, , et al. Influence of stress on γ″ precipitation behavior in Inconel 718 during Aging [J]. J. Alloys Compd., 2018, 740: 997 |
| [40] | MaK, GoetzR, SrivatsaS K. Modeling of residual stress and machining distortion in aerospace components [A]. ASM Handbook [M]. Volume22B, Ohio, United States: ASM, 2010: 386 |
/
| 〈 |
|
〉 |