Research paper

Deformation Behavior and Strengthening-Toughening Mechanism of GH4169 Alloy with Multi-Field Coupling

  • WANG Lei ,
  • AN Jinlan ,
  • LIU Yang ,
  • SONG Xiu
Expand
  • Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China

Received date: 2019-03-27

  Revised date: 2019-05-11

  Online published: 2019-06-14

Supported by

Supported by National Natural Science Foundation of China(Nos.U1708253,51571052);Scientific Research Foundation of Shenyang Aerospace University(No.18YB55)

Abstract

The superalloy is one of key metal materials, representing the level of scientific and technological development. Nickel-based superalloy is the most important which has been widely used for rotating component of aerospace. Nickel-based GH4169 alloy shows excellent combination properties including good fatigue property, excellent oxidation and corrosion resistance, as well as the microstructure stability during long-term ageing. The using amount of GH4169 alloy is about 45% of total wrought superalloys. For satisfying high performance of aero-engine, both strength and ductility of GH4169 alloy at high temperature are required to be simultaneously improved for safety servicing. It is an effective method to strengthen alloys by adding alloying elements. The alloying element addition ratio of GH4169 alloy is more than 40%, which unavoidably leads to hard deforming and plasticity declining, so that it restricts the further application of the alloy. Therefore, it is key to find methods realizing strengthening-toughening and without any losing of hot-deforming ability. In this work, the plastic deformation behavior and strengthening-toughening mechanisms of GH4169 alloy with multi-field coupling (electric-pulse current (EPC)/temperature/stress) were investigated. The results show that the deformation resistance of GH4169 alloy decreases and plastic deformation ability increases with multi-field coupling. The thermal vibration of atoms enhances and thus leads to decreasing of Peierls force with multi-field coupling, which is the essential factor on decreasing of deformation resistance and increasing of plastic deformation coordinate ability. When the alloy aged with electric-pulse treatment (EPT)/temperature coupling, the ultimate strength, yield strength and fracture elongation increase simultaneously at elevated temperatures. The vacancy concentration increases of the alloy aged with EPT/temperature coupling. Vacancy induces ultrafine nm-sized γ" phase to precipitate during tensile deformation at high temperature, which is the key factor on strength and ductility improvement. At the same time, because of the EPT/temperature coupling ageing, part of γ" phases precipitate around dislocation, while, due to the increasing of γ" phase size, the ductility of the alloy will be improved. With the multi-field coupling treatment, the strengthening-toughening of GH4169 alloy can be realized depended on an appropriate distribution of two kind sizes of γ" phase.

Cite this article

WANG Lei , AN Jinlan , LIU Yang , SONG Xiu . Deformation Behavior and Strengthening-Toughening Mechanism of GH4169 Alloy with Multi-Field Coupling[J]. Acta Metall Sin, 2019 , 55(9) : 1185 -1194 . DOI: 10.11900/0412.1961.2019.00085

References

[1] DengG J, TuS T, ZhangX C, , et al. Small fatigue crack initiation and growth mechanisms of nickel-based superalloy GH4169 at 650 ℃ in air [J]. Eng. Fract. Mech., 2016, 153: 35
[2] LiY J, TengY F, FengX H, , et al. Effects of pulsed magnetic field on microsegregation of solute elements in a Ni-based single crystal superalloy [J]. J. Mater. Sci. Technol., 2017, 33: 105
[3] ZhangJ, LouL H. Basic research in development and application of cast superalloy [J]. Acta Metall. Sin., 2018, 11: 1637
[3] 张 健, 楼琅洪. 铸造高温合金研发中的应用基础研究 [J]. 金属学报, 2018, 11: 1637
[4] GongL, ChenB, DuZ H, , et al. Investigation of solidification and segregation characteristics of cast Ni-base superalloy K417G [J]. J. Mater. Sci. Technol., 2018, 34: 541
[5] LiuG, CantóJ S, WinwoodS, , et al. The effects of microstructure and microtexture generated during solidification on deformation micromechanism in IN713C nickel-based superalloy [J]. Acta Mater., 2018, 148: 391
[6] ZhouX, SongJ. Effects of alloying elements on vacancies and vacancy-hydrogen clusters at coherent twin boundaries in nickel alloys [J]. Acta Mater., 2018, 148: 9
[7] RaoY, SmithT M, MillsM J, , et al. Segregation of alloying elements to planar faults in γ'-Ni3Al [J]. Acta Mater., 2018, 148: 173
[8] XiM Z, ZhouW, ShangJ Y, , et al. Effect of heat treatment on microstructure and mechanical properties of consecutive point-mode forging and laser rapid forming GH4169 alloy [J]. Acta Metall. Sin., 2017, 53: 239
[8] 席明哲, 周 玮, 尚俊英等. 热处理对连续点式锻压激光快速成形GH4169合金组织与拉伸性能的影响 [J]. 金属学报, 2017, 53: 239
[9] MedeirosS C, PrasadY V R K, FrazierW G, , et al. Microstructural modeling of metadynamic recrystallization in hot working of IN 718 superalloy [J]. Mater. Sci. Eng., 2000, A293: 198
[10] WangJ G, LiuD, YangY H. Mechanisms of non-uniform microstruc-ture evolution in GH4169 alloy during heating process [J]. Acta Metall. Sin., 2016, 52: 707
[10] 王建国, 刘 东, 杨艳慧. GH4169合金非均匀组织在加热过程中的演化机理 [J]. 金属学报, 2016, 52: 707
[11] LiuY, WangL, DingY, , et al. Effects of electric field treatment on microstructure and deformation behavior of GH4199 superalloy [J]. Chin. J. Nonferrous Met., 2006, 16: 1749
[11] 刘 杨, 王 磊, 丁 扬等. 电场处理对GH4199合金组织与变形行为的影响 [J]. 中国有色金属学报, 2006, 16: 1749
[12] WangL, LiuY, CuiT, , et al. Effects of electric-field treatment on a Ni-base superalloy [J]. Rare Met., 2007, 26: 210
[13] LiuY, WangL, FengF, , et al. Effects of electropulsing treatment on coarsening behavior of γ' phase in a nikel base superalloy [J]. J. Mater. Metall., 2011, 10: 288
[13] 刘 杨, 王 磊, 冯 飞等. 脉冲电流对一种镍基高温合金γ'相粗化行为的影响 [J]. 材料与冶金学报, 2011, 10: 288
[14] WangL, AnJ L, LiuY, , et al. Influence of electric field treatment on precipitation behavior of δ phase in GH4169 superalloy [J]. Acta Metall. Sin., 2015, 51: 1235
[14] 王 磊, 安金岚, 刘 杨等. 静电场处理对GH4169合金中δ相析出行为的影响 [J]. 金属学报, 2015, 51: 1235
[15] WangL, WangY, LiuY, , et al. Coarsening behavior of γ′ and γ" phases in GH4169 superalloy by electric field treatment [J]. Int.J.Miner.Metall. Mater., 2013, 20: 861
[16] BulsaraA R, GammaitoniL. Tuning in to noise [J]. Phys. Today, 1996, 49: 39
[17] TroitskiiO A, SpitsynV I, SokolovN V, , et al. Electroplastic drawing of stainless steel [J]. Soviet Phys. Dokl., 1977, 22: 769
[18] AntolovichS D, ConradH. The effects of electric currents and fields on deformation in metals, ceramics, and ionic materials: An interpretive survey [J]. Mater. Manuf. Processes, 2004, 19: 587
[19] XuX F, ZhaoY G, MaB D, , et al. Rapid grain refinement of 2024 Al alloy through recrystallization induced by electropulsing [J]. Mater. Sci. Eng., 2014, A612: 223
[20] WangL, LiuM C, HuangJ C, , et al. Effect of temperature on the yield strength of a binary CuZr metallic glass: Stress-induced glass transition [J]. Intermetallics, 2012, 26: 162
[21] YadavS K, RamprasadR, MisraA, , et al. Core structure and Peierls stress of edge and screw dislocations in TiN: A density functional theory study [J]. Acta Mater., 2014, 74: 268
[22] WuR H, SandfeldS. A dislocation dynamics-assisted phase field model for Nickel-based superalloys: the role of initial dislocation density and external stress during creep [J]. J. Alloys Compd., 2017, 703: 389
[23] YangD Z. Dislocations and Strengthening Mechanisms of Metals [M]. Harbin: Harbin Institute of Technology Press, 1991: 107
[23] 杨德庄. 位错与金属强化机制 [M]. 哈尔滨: 哈尔滨工业大学出版社, 1991: 107)
[24] NabarroF R N. Dislocations in a simple cubic lattice [J]. Proc. Phys. Soc., 1947, 59: 256
[25] PeierlsR. The size of a dislocation [J]. Proc. Phys. Soc., 1940, 52: 34
[26] TroitskiiO A. Pressure shaping by the application of a high energy [J]. Mater. Sci. Eng., 1985, 75: 37
[27] AnJ L, WangL, SongX, , et al. New approach for plastic deformation behavior of GH4169 superalloy with in-situ electric-pulse current at 800 ℃, Mater. Sci. Eng., 2017, A707: 356
[28] AnJ L, WangL, SongX, , et al. Improving mechanism of both strength and ductility of GH4169 alloy induced by electric-pulse treatment [J]. Mater. Sci. Eng., 2018, A724: 439
Outlines

/