Stress Relaxation Mechanism for Typical Nickel-Based Superalloys Under Service Condition
Received date: 2019-04-18
Revised date: 2019-05-11
Online published: 2019-06-14
Supported by
Supported by National Natural Science Foundation of China(51771016)
Since nickel-based superalloys are more and more used as fasteners, it is necessary to investigate the stress relaxation behavior and mechanism of nickel-based superalloy. In present work, the stress relaxation mechanism for four typical nickel-based superalloys (GH4169, GH4169D, GH4738, GH350) for fasteners under service condition was investigated. The stress relaxation tests were carried out according to GB/T 10120-2013 in the temperature range of 600~780 ℃ and initial stress range of 260~510 MPa, and the stress relaxation curves were recorded. The microstructure was studied by FESEM and TEM. The results show that the stress decreases fast in the initial stage of stress relaxation test and then trends to be steady. The stress relaxation stability decreases with increasing temperature. There is no apparent change in the microstructure after stress relaxation test. TEM observation shows that the major mechanism of stress relaxation is the movement of dislocations, and the stress relaxation properties of different alloys depend on the inhibition of dislocation movement. The species, size, shape and distribution of phases determine the ability to hinder dislocation movement and the stress relaxation property of different alloys. GH4169 alloy gets the stress relaxation property mainly by γ' phase, γ'' phase and δ phase hindering the movement of dislocations. In GH4169D alloy, both γ' phase and η phase participate in the stress relaxation process. γ' phase in GH4738 alloy can effectively impede the movement of dislocations and provide good stress relaxation property. The combined effect of γ' phase and η phase guarantees the stress relaxation stability of GH350 alloy.
Key words: superalloy; stress relaxation; microstructure evolution; mechanism
He JIANG , Jianxin DONG , Maicang ZHANG , Zhihao YAO , Jing YANG . Stress Relaxation Mechanism for Typical Nickel-Based Superalloys Under Service Condition[J]. Acta Metall Sin, 2019 , 55(9) : 1211 -1220 . DOI: 10.11900/0412.1961.2019.00121
| [1] | PiresF, ClementsR, SantosF, , et al. Evaluation of the performance of Inconel 718 fasteners subjected to cathodic protection systems in offshore and subsea applications [A]. ASME 2011 30th International Conference on Ocean, Offshore and Arctic Engineering [C]. the Netherlands: ASME, 2011: 165 |
| [2] | TechnologiesSPS. Superalloys Developed by SPS Technologies for Aerospace Fasteners [Z]. Jenkintown, PA, USA, 1998: 1 |
| [3] | NechacheA, BouzidA H. The effect of cylinder and hub creep on the load relaxation in bolted flanged joints [J]. J. Pressure Vessel Technol., 2008, 130: 031211 |
| [4] | GjestlandH, NussbaumG, RegazzoniG, , et al. Stress-relaxation and creep behaviour of some rapidly solidified magnesium alloys [J]. Mater. Sci. Eng., 1991, A134: 1197 |
| [5] | ZhouY M, ZhaoZ P, LiH L. The microstructure and stress ralaxation property of 12% Cr steel [J]. Mater. Mech. Eng., 1992, 16(1): 27 |
| [5] | 周晔明, 赵中平, 李惠琳. 12% Cr钢的组织与应力松弛性能 [J]. 机械工程材料, 1992, 16(1): 27) |
| [6] | YangX S, WangY J, WangG Y, , et al. Time, stress, and temperature-dependent deformation in nanostructured copper: Stress relaxation tests and simulations [J]. Acta Mater., 2016, 108: 252 |
| [7] | LiuW J, JonasJ J. A stress relaxation method for following carbonitride precipitation in austenite at hot working temperatures [J]. Metall. Trans., 1988, 19A: 1403 |
| [8] | LiuW J. A review of the stress-relaxation method for following the kinetics of precipitation, recovery and recrystallization [J]. Mater. Sci. Forum, 2012, 706-709: 2758 |
| [9] | MonajatiH, ZarandiF, JahaziM, , et al. Strain induced γ' precipitation in nickel base superalloy Udimet 720 using a stress relaxation based technique [J]. Scr. Mater., 2005, 52: 771 |
| [10] | RolphJ, EvansA, ParadowskaA, , et al. Stress relaxation through ageing heat treatment—A comparison between in situ and ex situ neutron diffraction techniques [J]. CR Phys., 2012, 13: 307 |
| [11] | D'souzaN, KelleherJ, QiuC L, , et al. The role of stress relaxation and creep during high temperature deformation in Ni-base single crystal superalloys—Implications to strain build-up during directional solidification [J]. Acta Mater., 2016, 106: 322 |
| [12] | WoodfordD A. Advances in the use of stress relaxation data for design and life assessment in combustion turbines [J]. JSME Int. J., 2002, 45A: 98 |
| [13] | CalvoJ, ShuS Y, CabreraJ M. Characterization of precipitation kinetics of Inconel 718 superalloy by the stress relaxation technique [J]. Mater. Sci. Forum, 2012, 706-709: 2393 |
| [14] | FossB J, GrayS, HardyM C, , et al. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR1000 [J]. Acta Mater., 2013, 61: 2548 |
| [15] | ZhuZ, ZhangL W, SongG Y, , et al. Study on stress relaxation behavior of Hastelloy C-276 alloy [J]. Rare Met. Mater. Eng., 2012, 41: 697 |
| [15] | 朱 智, 张立文, 宋冠宇等. Hastelloy C-276合金应力松弛行为的研究 [J]. 稀有金属材料与工程, 2012, 41: 697 |
| [16] | CollinsD M, D'SouzaN, PanwisawasC. In-situ neutron diffraction during stress relaxation of a single crystal nickel-base superalloy [J]. Scr. Mater., 2017, 131: 103 |
| [17] | NathalM V, BiererJ, EvansL, , et al. Stress relaxation behavior in single crystal superalloys [J]. Mater. Sci. Eng., 2015, A640: 295 |
| [18] | NiT W, DongJ X. Creep behaviors and mechanisms of Inconel 718 and Allvac 718 plus [J]. Mater. Sci. Eng., 2017, A700: 406 |
| [19] | ChenK, DongJ X, YaoZ H, , et al. Creep performance and damage mechanism for Allvac 718Plus superalloy [J]. Mater. Sci. Eng., 2018, A738: 308 |
| [20] | ZhangX M, MaoX P, DengZ Q, , et al. Stress relaxation characteristics in bending of Cu-Be alloys [J]. Chin. J. Nonferrous Met., 2001, 11: 988 |
| [20] | 张新明, 毛新平, 邓至谦等. 铍铜带材弯曲应力松弛的力学行为 [J]. 中国有色金属学报, 2001, 11: 988 |
| [21] | ChaturvediM C, HanY F. Strengthening mechanisms in Inconel 718 superalloy [J]. Met. Sci., 1983, 17: 145 |
| [22] | LinY C, ChenM S, ZhongJ. Prediction of 42CrMo steel flow stress at high temperature and strain rate [J]. Mech. Res. Commun., 2008, 35: 142 |
| [23] | LinY C, WenD X, DengJ, , et al. Constitutive models for high-temperature flow behaviors of a Ni-based superalloy [J]. Mater. Des., 2014, 59: 115 |
| [24] | WangY, ShaoW Z, ZhenL, , et al. Flow behavior and microstructures of superalloy 718 during high temperature deformation [J]. Mater. Sci. Eng., 2008, A497: 479 |
| [25] | LinY C, ChenX M, WenD X, , et al. A physically-based constitutive model for a typical nickel-based superalloy [J]. Comput. Mater. Sci., 2014, 83: 282 |
/
| 〈 |
|
〉 |