Effect of Cooling Rate on Boride and Room Temperature Tensile Properties of β-Solidifying γ-TiAl Alloys
Received date: 2019-04-03
Revised date: 2019-04-26
Online published: 2019-05-31
Supported by
National Natural Science Foundation of China(51701209);National Key Research and Development Program of China(2016YFB0701304);National Key Research and Development Program of China(2016YFB0701305)
β-solidifying γ-TiAl alloys have attracted much attention for their higher specific strength and better mechanical properties at elevated temperature. They usually need some boron addition to refine the lamellar grain size, which is believed to improve their poor room temperature ductility. However, the boron addition may cause some side effects on mechanical properties for the formation of borides with unfavorable morphology and crystal structure, which is severely influenced by the alloy composition and cooling rate during casting. The components of γ-TiAl applied usually have complex structure, such as different thicknesses, which leads to different cooling rates and therefore different microstructures and mechanical properties. To evaluate the influence of cooling rate on the microstructure and mechanical properties of γ-TiAl investment casting, plate with step thicknesses was designed to achieve different cooling rates. Step plates of β-solidifying boron-containing TiAl alloy were fabricated by centrifugal casting in Y2O3 facing coating ceramic moulds. It was found that boride mainly distributed on grain boundary, and its aspect ratio increased with increasing cooling rate, with its morphology varying from short, flat plate to long, curvy ribbon. The short plate and curvy ribbon borides were TiB with B27 and Bf structure, respectively. Both types of boride exhibit anisotropic growth characteristics (especially for Bf structure), with the slowest growth rate along [100] and [010] for B27 structure and Bf structure, respectively. This is attributed to the difficulty of atomic rearrangement along corresponding directions during solidification. The cooling rate increase caused the increase of yield strength but the decrease of room temperature ductility, the former results from the decreasing of grain size and lamellar spacing, while the latter results from the easy cracking nucleation and propagation of the long curvy boride, leaving smooth curvy surfaces on the fracture surface. Samples containing short flat plate boride showed better ductility, and no smooth curvy surface was observed.
Key words: γ-TiAl alloy; β-solidifying; investment casting; cooling rate; boride; tensile property
Xi WANG , Renci LIU , Ruxin CAO , Qing JIA , Yuyou CUI , Rui YANG . Effect of Cooling Rate on Boride and Room Temperature Tensile Properties of β-Solidifying γ-TiAl Alloys[J]. Acta Metall Sin, 2020 , 56(2) : 203 -211 . DOI: 10.11900/0412.1961.2019.00100
| [1] | Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129 |
| [1] | (杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129) |
| [2] | Kim Y W, Dimiduk D M. Progress in the understanding of gamma titanium aluminides [J]. JOM, 1991, 43(8): 40 |
| [3] | Kim Y W. Ordered intermetallic alloys, part III: Gamma titanium aluminides [J]. JOM, 1994, 46(7): 30 |
| [4] | Hu D W. Role of boron in TiAl alloy development: A review [J]. Rare Met., 2016, 35: 1 |
| [5] | Larsen D E, Kampe S, Christodoulou L. Effect of XD? TiB2 volume fraction on the microstructure of a cast near-gamma titanium aluminide alloy [J]. MRS Proc., 1990, 194: 285 |
| [6] | Cheng T T. The mechanism of grain refinement in TiAl alloys by boron addition—An alternative hypothesis [J]. Intermetallics, 2000, 8: 29 |
| [7] | Inkson B J, Boothroyd C B, Humphreys C J. Boride morphology in a (Fe, V, B)Ti-alloy containing B2-phase [J]. Acta Metall. Mater., 1995, 43: 1429 |
| [8] | Godfrey A B. Grain refinement of a gamma-based titanium aluminide using microalloy additions [D]. Birmingham: The University of Birmingham, 1996 |
| [9] | Hecht U, Witusiewicz V, Drevermann A, et al. Grain refinement by low boron additions in niobium-rich TiAl-based alloys [J]. Intermetallics, 2008, 16: 969 |
| [10] | De Graef M, L?fvander J P A, McCullough C, et al. The evolution of metastable Bf borides in a Ti-Al-B alloy [J]. Acta Metall. Mater., 1992, 40: 3395 |
| [11] | Hu D. Effect of composition on grain refinement in TiAl-based alloys [J]. Intermetallics, 2001, 9: 1037 |
| [12] | Kitkamthorn U, Zhang L C, Aindow M. The structure of ribbon borides in a Ti-44Al-4Nb-4Zr-1B alloy [J]. Intermetallics, 2006, 14: 759 |
| [13] | Hyman M E, McCullough C, Levi C G, et al. Evolution of boride morphologies in TiAl-B alloys [J]. Metall. Mater. Trans., 1991, 22A: 1647 |
| [14] | Yang L L, Zheng L J, Xiao Z X, et al. Effect of withdrawal rate on the microstructure of directional solidified Ti-47Al-2Cr-2Nb-0.8B alloys [J]. Acta Metall. Sin., 2010, 46: 879 |
| [14] | (杨莉莉, 郑立静, 肖志霞等. 抽拉速率对定向凝固Ti-47Al-2Cr-2Nb-0.8B合金组织的影响 [J]. 金属学报, 2010, 46: 879) |
| [15] | Imayev R M, Imayev V M, Oehring M, et al. Alloy design concepts for refined gamma titanium aluminide based alloys [J]. Intermetallics, 2007, 15: 451 |
| [16] | Hu D, Mei J F, Wickins M, et al. Microstructure and tensile properties of investment cast Ti-46Al-8Nb-1B alloy [J]. Scr. Mater., 2002, 47: 273 |
| [17] | Hu D. Effect of boron addition on tensile ductility in lamellar TiAl alloys [J]. Intermetallics, 2002, 10: 851 |
| [18] | Lin B C, Liu R C, Jia Q, et al. Effect of surface topography on room temperature tensile ductility of TiAl [J]. JOM, 2017, 69: 2583 |
| [19] | Lin B C. Study on effect of surface condition and casting defects on mechanical properties of TiAl [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2017 |
| [19] | (林博超. 表面状态和铸造缺陷对TiAl力学性能影响研究 [D]. 沈阳: 中国科学院金属研究所, 2017) |
| [20] | Liu R C. Microstructure evolution and mechanical properties of Ti-47Al-2Cr-2Nb-0.15B alloy processed by hot extrusion [D]. Beijing: University of Chinese Academy of Sciences, 2013 |
| [20] | (刘仁慈. Ti-47Al-2Cr-2Nb-0.15B合金挤压变形组织演变及其力学性能研究 [D]. 北京: 中国科学院大学, 2013) |
| [21] | Hyman M E, McCullough C, Valencia J J, et al. Microstructure evolution in TiAl alloys with B additions: Conventional solidification [J]. Metall. Mater. Trans., 1989, 20A: 1847 |
| [22] | Witusiewicz V T, Bondar A A, Hecht U, et al. The Al-B-Nb-Ti system: V. Thermodynamic description of the ternary system Al-B-Ti [J]. J. Alloys Compd., 2009, 474: 86 |
| [23] | Maziasz P J, Liu C T. Development of ultrafine lamellar structures in two-phase γ-TiAl alloys [J]. Metall. Mater. Trans., 1998, 29A: 105 |
| [24] | Lin B C, Liu R C, Jia Q, et al. Effect of yttria inclusion on room temperature tensile properties of investment cast TiAl [J]. Mater. Sci. Eng., 2018, A712: 73 |
| [25] | Liu R C, Liu D, Tan J, et al. Textures of rectangular extrusions and their effects on the mechanical properties of thermo-mechanically treated, lamellar microstructure, Ti-47Al-2Cr-2Nb-0.15B [J]. Intermetallics, 2014, 52: 110 |
| [26] | Huang X X. Size effects on the strength of metals [J]. Acta Metall. Sin., 2014, 50: 137 |
| [26] | (黄晓旭. 金属强度的尺寸效应 [J]. 金属学报, 2014, 50: 137) |
| [27] | Yang C, Jiang H, Hu D, et al. Effect of boron concentration on phase transformation texture in as-solidified Ti44Al8NbxB [J]. Scr. Mater., 2012, 67: 85 |
| [28] | Liu R C, Wang Z, Liu D, et al. Microstructure and tensile properties of Ti-45.5Al-2Cr-2Nb-0.15B alloy processed by hot extrusion [J]. Acta Metall. Sin., 2013, 49: 641 |
| [28] | (刘仁慈, 王 震, 刘 冬等. Ti-45.5A1-2Cr-2Nb-0.15B合金热挤压组织与拉伸性能研究 [J]. 金属学报, 2013, 49: 641) |
| [29] | Hu D, Jiang H, Wu X. Microstructure and tensile properties of cast Ti-44Al-4Nb-4Hf-0.1Si-0.1B alloy with refined lamellar microstructures [J]. Intermetallics, 2009, 17: 744 |
/
| 〈 |
|
〉 |