Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature
Received date: 2019-02-26
Revised date: 2019-05-13
Online published: 2019-05-27
Supported by
National Natural Science Foundation of China((Nos.51301040 and 51601039));China Postdoctoral Science Foundation(No.2016M590591)
Mg alloy has hexagonal structure and exhibits poor workability at room temperature, which is attributed to the difficulty in activating a sufficient number of independent slips to accommodate the deformation. Twinning plays an important role in plastic deformation of Mg alloys during low and medium temperature to accommodate the imposed strain, especially the strain along the c-axis. Therefore, the microstructure and texture evolutions of AZ31 Mg alloy during multi-pass compressions at room temperature were investigated by EBSD technology. The results show that the microstructure and texture evolutions are mainly controlled by tension twinning during multi-pass compression. And the more the strain passes, the severer the texture transformation. The c-axes of the grains are almost rotated to the compression direction by tension twins. The twins generated during multi-directional compression can separate grains and then refine them. However, the de-twinning can rotate the grains back to the initial orientations, which is against the texture weakening. The Schmid law governs the characteristics of {10
Key words: Mg alloy; multi-pass deformation; twinning; texture; grain refinement
Liping DENG , Kaixuan CUI , Bingshu WANG , Hongliang XIANG , Qiang LI . Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. Acta Metall Sin, 2019 , 55(8) : 976 -986 . DOI: 10.11900/0412.1961.2019.00050
| [1] | Liu Q. Research progress on plastic deformation mechanism of Mg alloys [J]. Acta Metall. Sin., 2010, 46: 1458 |
| [1] | (刘 庆. 镁合金塑性变形机理研究进展 [J]. 金属学报, 2010, 46: 1458) |
| [2] | Chakkedath A, Boehlert C J. In situ scanning electron microscopy observations of contraction twinning and double twinning in extruded Mg-1Mn (wt. %) [J]. JOM, 2015, 67: 1748 |
| [3] | Knezevic M, Levinson A, Harris R, et al. Deformation twinning in AZ31: Influence on strain hardening and texture evolution [J]. Acta Mater., 2010, 58: 6230 |
| [4] | Barnett M R. Twinning and the ductility of magnesium alloys: Part I: "Tension" twins [J]. Mater. Sci. Eng., 2007, A464: 1 |
| [5] | Li S Q, Tang W N, Chen R S, et al. Effect of pre-induced twinning on microstructure and tensile ductility in GW92K magnesium alloy during multi-direction forging at decreasing temperature [J]. J. Magnes. Alloys, 2014, 2: 287 |
| [6] | Xu S, Liu T M, Chen H C, et al. Reducing the tension-compression yield asymmetry in a hot-rolled Mg-3Al-1Zn alloy via multidirectional pre-compression [J]. Mater. Sci. Eng., 2013, A565: 96 |
| [7] | Kuang X L, Liu T M, He J J. Evolution of texture and yielding behavior induced by {101ˉ2} twinning of magnesium alloy [J]. Chin. J. Nonferrous Met., 2014, 24: 1111 |
| [7] | (况新亮, 刘天模, 何杰军. 基于镁合金{1012}孪生的织构调整及屈服行为演变 [J]. 中国有色金属学报, 2014, 24: 1111) |
| [8] | Xin Y C, Jiang J, Chapuis A, et al. Plastic deformation behavior of AZ31 magnesium alloy under multiple passes cross compression [J]. Mater. Sci. Eng., 2012, A532: 50 |
| [9] | Song G S, Jiang J Q, Xu Y, et al. Influence of AZ31 magnesium alloy sheet compressed along various paths on mechanical properties [J]. Chin. J. Nonferrous Met., 2016, 26: 2469 |
| [9] | (宋广胜, 姜敬前, 徐 勇等. AZ31镁合金板材变路径压缩对力学性能影响 [J]. 中国有色金属学报, 2016, 26: 2469) |
| [10] | Hou D W, Liu T M, Luo L J, et al. Twinning behaviors of a rolled AZ31 magnesium alloy under multidirectional loading [J]. Mater. Charact., 2017, 124: 122 |
| [11] | Yang X Y, Miura H, Sakai T. Structural development at severely high strain in AZ31 magnesium alloy processed by cold forging and subsequent annealing [J]. Mater. Des., 2013, 44: 573 |
| [12] | Xia X S, Chen Q, Zhao Z D, et al. Microstructure, texture and mechanical properties of coarse-grained Mg-Gd-Y-Nd-Zr alloy processed by multidirectional forging [J]. J. Alloys Compd., 2015, 623: 62 |
| [13] | Jiang M G, Yan H, Chen R S. Twinning, recrystallization and texture development during multi-directional impact forging in an AZ61 Mg alloy [J]. J. Alloys Compd., 2015, 650: 399 |
| [14] | Ulacia I, Dudamell N V, Gálvez F, et al. Mechanical behavior and microstructural evolution of a Mg AZ31 sheet at dynamic strain rates [J]. Acta Mater., 2010, 58: 2988 |
| [15] | Chun Y B, Davies C H J. Twinning-induced negative strain rate sensitivity in wrought Mg alloy AZ31 [J]. Mater. Sci. Eng., 2011, A528: 5713 |
| [16] | Yang X Y, Sun Z Y, Zhang L. Preparation of submicro and nanosized magnesium alloys by multiply compressed deformation [J]. Acta Metall. Sin., 2010, 46: 607 |
| [16] | (杨续跃, 孙争艳, 张 雷. 室温多向多道次压缩变形制备亚微米和纳米级镁合金 [J]. 金属学报, 2010, 46: 607) |
| [17] | Wang B S, Shi J J, Ye P, et al. In-situ investigation on nucleation and propagation of {101ˉ2} twins during uniaxial multi-pass compression in an extruded AZ31 Mg alloy [J]. Mater. Sci. Eng., 2018, A731: 71 |
| [18] | Li J Q, Liu J, Cui Z S. Microstructures and mechanical properties of AZ61 magnesium alloy after isothermal multidirectional forging with increasing strain rate [J]. Mater. Sci. Eng., 2015, A643: 32 |
| [19] | Wang L F, Huang G S, Quan Q, et al. The effect of twinning and detwinning on the mechanical property of AZ31 extruded magnesium alloy during strain-path changes [J]. Mater. Des., 2014, 63: 177 |
| [20] | Guo C F, Xin R L, Ding C H, et al. Understanding of variant selection and twin patterns in compressed Mg alloy sheets via combined analysis of Schmid factor and strain compatibility factor [J]. Mater. Sci. Eng., 2014, A609: 92 |
| [21] | Wang B S, Deng L P, Guo N, et al. EBSD analysis of {101ˉ2} twinning activity in Mg-3Al-1Zn alloy during compression [J]. Mater. Charact., 2014, 98: 180 |
| [22] | Xin R L, Liang Y C, Ding C H, et al. Geometrical compatibility factor analysis of paired extension twins in extruded Mg-3Al-1Zn alloys [J]. Mater. Des., 2015, 86: 656 |
| [23] | Xin Y C, Zhou X J, Wu Y, et al. Deformation behavior and mechanical properties of composite twin structures under different loading paths [J]. Mater. Sci. Eng., 2015, A640: 118 |
| [24] | Wang C, Ding H, Wang B S, et al. Effects of deformation texture and twins on the corrosion resistance of rolled AZ31 Mg alloy under 5% uniaxial compression [J]. Acta. Metall. Sin. (Engl. Lett.), 2017, 30: 921 |
| [25] | Park S H, Hong S G, Lee J H, et al. Texture evolution of rolled Mg-3Al-1Zn alloy undergoing a {101ˉ2} twinning dominant strain path change [J]. J. Alloys Compd., 2015, 646: 573 |
/
| 〈 |
|
〉 |