Effects of Zn Addition on the Natural Ageing Behavior and Bake Hardening Response of a Pre-Aged Al-Mg-Si-Cu Alloy

  • Shang ZHU ,
  • Zhihui LI ,
  • Lizhen YAN ,
  • Xiwu LI ,
  • Yongan ZHANG ,
  • Baiqing XIONG
Expand
  • 1. State Key Laboratory of Nonferrous Metals and Processes, GRINMAT Engineering Institute Co. , Ltd. , Beijing 101407, China
    2. GRINM Group Co. , Ltd. , Beijing 100088, China

Received date: 2018-12-19

  Revised date: 2019-03-28

  Online published: 2019-05-24

Supported by

National Key Research and Development Program of China(2016YFB0300802)

Abstract

Al-Mg-Si(-Cu) alloys are widely used in automotive body panels because of their excellent combined performance of high strength-to-weight ratio, good formability and corrosion resistance. Zn additions to Al-Mg-Si(-Cu) alloys have been tested and shown to effectively affect the precipitation microstructure and enhance the age-hardening response. The present study investigates the natural ageing (NA) behavior and bake hardening response in the pre-aged Al-0.9Mg-0.8Si-0.2Cu (mass fraction, %) and Al-0.9Mg-0.8Si-0.2Cu-0.6Zn (mass fraction, %) alloys. The results are compared to clarify the effect of Zn addition. During NA after pre-ageing at 80 ℃ for 15 min (PA), cluster growth is the dominant process in the Zn-free and Zn-added alloys. Some Zn atoms are partitioned into the clusters under PA+NA condition. Partitioning of Zn may change the stability of clusters, increasing the growth rate of clusters. The yield strength of the two alloys increases with the increasing NA time. The smaller cluster spacing and larger cluster shear modulus lead to the higher yield strength in the Zn-added alloy during NA after PA. The prolonged NA inhibits the transformation of clusters to GP zones and β″ phases during bake hardening (BH) treatment at 170 ℃ for 30 min in the Zn-free and Zn-added alloys, resulting in the lower BH response. The Zn does not significantly partition into clusters or precipitates, and the majority of Zn remains in the Al matrix during BH treatment, prompting the transformation from solute clusters to GP zones and β″ phases. As a result, the yield strength of the Zn-added alloy after PA+NA+BH treatment is higher than that of the Zn-free alloy.

Cite this article

Shang ZHU , Zhihui LI , Lizhen YAN , Xiwu LI , Yongan ZHANG , Baiqing XIONG . Effects of Zn Addition on the Natural Ageing Behavior and Bake Hardening Response of a Pre-Aged Al-Mg-Si-Cu Alloy[J]. Acta Metall Sin, 2019 , 55(11) : 1395 -1406 . DOI: 10.11900/0412.1961.2018.00555

References

[1] PogatscherS, AntrekowitschH, LeitnerH, et al. Mechanisms controlling the artificial aging of Al-Mg-Si alloys [J]. Acta Mater., 2011, 59: 3352
[2] EdwardsG A, StillerK, DunlopG L, et al. The precipitation sequence in Al-Mg-Si alloys [J]. Acta Mater., 1998, 46: 3893
[3] WengY Y, JiaZ H, DingL P, et al. Clustering behavior during natural aging and artificial aging in Al-Mg-Si alloys with different Ag and Cu addition [J]. Mater. Sci. Eng., 2018, A732: 273
[4] MartinsenF A, EhlersF J H, Tors?terM, et al. Reversal of the negative natural aging effect in Al-Mg-Si alloys [J]. Acta Mater., 2012, 60: 6091
[5] FallahV, KorinekA, Ofori-OpokuN, et al. Atomic-scale pathway of early-stage precipitation in Al-Mg-Si alloys [J]. Acta Mater., 2015, 82: 457
[6] MurayamaM, HonoK, MiaoW F, et al. The effect of Cu additions on the precipitation kinetics in an Al-Mg-Si alloy with excess Si [J]. Metall. Mater. Trans., 2001, 32A: 239
[7] NiniveP H, StrandlieA, Gulbrandsen-DahlS, et al. Detailed atomistic insight into the β″ phase in Al-Mg-Si alloys [J]. Acta Mater., 2014, 69: 126
[8] YangW C, WangM P, ZhangR R, et al. The diffraction patterns from β″ precipitates in 12 orientations in Al-Mg-Si alloy [J]. Scr. Mater., 2010, 62: 705
[9] DingL P, HeY, WenZ, et al. Optimization of the pre-aging treatment for an AA6022 alloy at various temperatures and holding times [J]. J. Alloys Compd., 2015, 647: 238
[10] SerizawaA, HirosawaS, SatoT. Three-dimensional atom probe characterization of nanoclusters responsible for multistep aging behavior of an Al-Mg-Si alloy [J]. Metall. Mater. Trans., 2008, 39A: 243
[11] ArugaY, KozukaM, TakakiY, et al. Evaluation of solute clusters associated with bake-hardening response in isothermal aged Al-Mg-Si alloys using a three-dimensional atom probe [J]. Metall. Mater. Trans., 2014, 45A: 5906
[12] Tors?terM, HastingH S, LefebvreW, et al. The influence of composition and natural aging on clustering during preaging in Al-Mg-Si alloys [J]. J. Appl. Phys., 2010, 108: 0735527
[13] ZandbergenM W, XuQ, CerezoA, et al. Study of precipitation in Al-Mg-Si alloys by atom probe tomography I. Microstructural changes as a function of ageing temperature [J]. Acta Mater., 2015, 101: 136
[14] TakakiY, MasudaT, KobayashiE, et al. Effects of natural aging on bake hardening behavior of Al-Mg-Si alloys with multi-step aging process [J]. Mater. Trans., 2014, 55: 1257
[15] ArugaY, KozukaM, TakakiY, et al. Effects of natural aging after pre-aging on clustering and bake-hardening behavior in an Al-Mg-Si alloy [J]. Scr. Mater., 2016, 116: 82
[16] DingX P, CuiH, ZhangJ X, et al. The effect of Zn on the age hardening response in an Al-Mg-Si alloy [J]. Mater. Des., 2015, 65: 1229
[17] YanL Z, ZhangY A, LiX W, et al. Effect of Zn addition on microstructure and mechanical properties of an Al-Mg-Si alloy [J]. Prog. Nat. Sci.Mater. Int., 2014, 24: 97
[18] SaitoT, WennerS, OsmundsenE, et al. The effect of Zn on precipitation in Al-Mg-Si alloys [J]. Philos. Mag., 2014, 94: 2410
[19] GuoM X, ZhangY, ZhangX K, et al. Non-isothermal precipitation behaviors of Al-Mg-Si-Cu alloys with different Zn contents [J]. Mater. Sci. Eng., 2016, A669: 20
[20] HonoK. Atom probe microanalysis and nanoscale microstructures in metallic materials [J]. Acta Mater., 1999, 47: 3127
[21] WangB, WangX J, SongH, et al. Strengthening effects of microstructure evolution during early ageing process in Al-Mg-Si alloy [J]. Acta Metall. Sin., 2014, 50: 685
[21] 汪 波, 王晓姣, 宋 辉等. Al-Mg-Si合金时效早期显微组织演变及其对强化的影响 [J]. 金属学报, 2014, 50: 685
[22] ShaG, M?llerH, StumpfW E, et al. Solute nanostructures and their strengthening effects in Al-7Si-0.6Mg alloy F357 [J]. Acta Mater., 2012, 60: 692
[23] BuhaJ, LumleyR N, CroskyA G, et al. Secondary precipitation in an Al-Mg-Si-Cu alloy [J]. Acta Mater., 2007, 55: 3015
[24] LiH, LiuW Q. Nanoprecipitates and their strengthening behavior in Al-Mg-Si alloy during the aging process [J]. Metall. Mater. Trans., 2017, 48A: 1990
[25] KarneskyR A, SudbrackC K, SeidmanD N. Best-fit ellipsoids of atom-probe tomographic data to study coalescence of γ′ (L12) precipitates in Ni-Al-Cr [J]. Scr. Mater., 2007, 57: 353
[26] GaultB, MoodyM P, CairneyJ M, et al. Atom Probe Microscopy [M]. New York: Springer, 2012: 270
[27] EsmaeiliS, LloydD J, PooleW J. Modeling of precipitation hardening for the naturally aged Al-Mg-Si-Cu alloy AA6111 [J]. Acta Mater., 2003, 51: 3467
[28] StarinkM J, CaoL F, RometschP A. A model for the thermodynamics of and strengthening due to co-clusters in Al-Mg-Si-based alloys [J]. Acta Mater., 2012, 60: 4194
[29] MarceauR K W, de VaucorbeilA, ShaG, et al. Analysis of strengthening in AA6111 during the early stages of aging: Atom probe tomography and yield stress modelling [J]. Acta Mater., 2013, 61: 7285
[30] BrandesE A, BrookG B. Smithells Metals Reference Book [M]. 7th Ed., London: Butterworth-Heinemann, 1992: 15
[31] LiuG, ZhangG J, DingX D, et al. Modeling the strengthening response to aging process of heat-treatable aluminum alloys containing plate/disc- or rod/needle-shaped precipitates [J]. Mater. Sci. Eng., 2003, A344: 113
[32] SeidmanD N, MarquisE A, DunandD C. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys [J]. Acta Mater., 2002, 50: 4021
[33] KingH W. Quantitative size-factors for metallic solid solutions [J]. J. Mater. Sci., 1966, 1: 79
[34] ZandbergenM W, CerezoA, SmithG D W. Study of precipitation in Al-Mg-Si alloys by atom probe tomography II. Influence of Cu additions [J]. Acta Mater., 2015, 101: 149
[35] ArugaY, KozukaM, TakakiY, et al. Formation and reversion of clusters during natural aging and subsequent artificial aging in an Al-Mg-Si alloy [J]. Mater. Sci. Eng., 2015, A631: 86
[36] AdachiH, NakanishiH, AsanoM. Soft X-ray XAFS studies on Al-Mg-Si alloys with different aging conditions [J]. J. Jpn.Inst.Light Met., 2015, 65: 411(足立 大樹, 中西 英貴, 浅野 峰生. 時効条件が異なるAl-Mg-Si合金における軟X線XAFS測定 [J]. 軽金属, 2015, 65: 411
[37] ZhuS, LiZ H, YanL Z, et al. Effects of Zn addition on the age hardening behavior and precipitation evolution of an Al-Mg-Si-Cu alloy [J]. Mater. Charact., 2018, 145: 258
Outlines

/