Effect of Surface Roughness by Shot Peening on Stress Corrosion Cracking Behavior of Pure Titanium Welded Joints in HCl Solution
Received date: 2019-03-01
Revised date: 2019-04-16
Online published: 2019-05-21
Supported by
National Natural Science Foundation of China(51274160)
Pure titanium is often used in the manufacture of pressure vessels due to its excellent corrosion resistance. Pressure vessels are generally operated in various corrosive media and subjected to varying degrees of corrosion. Stress corrosion cracking is one of the most dangerous forms of damage to pressure vessels used in various fields. Welded joints become the weak link of the pressure vessels because of the uneven microstructure and welding residual stress, which could cause stress corrosion and directly affect the overall performance and service life of pressure vessels. At present, as a method to improve the mechanical and corrosion properties of materials, shot peening has been widely studied. However, shot peening often leads to the increase of surface roughness and even causes defects such as cracks and surface damage, which will affect the effect of improving the corrosion resistance of materials. It remains to be further studied that the specific influence of surface roughness on the stress corrosion resistance of metal materials. In this work, the stress corrosion behavior of the original samples, ultrasonic shot peening (USSP) samples and USSP with surface polished samples of TA2 titanium welded joints in 10%HCl solution were studied by slow strain rate tension (SSRT) experiment. OM, TEM and SEM were used to observe the microstructure and corrosion fracture morphology of the welded joints. The surface roughness and residual stress of different processed samples were measured, and the corrosion mechanisms were analyzed. The results showed that both stress corrosion and hydrogen embrittlement occurred in pure titanium welded joints in this system, and weld metal (WM) was the weakest link in the welded joint. The stress corrosion cracking susceptibility index (ISCC) of the original sample in this system was 25.61%, indicating a tendency of stress corrosion. The ISCC of the USSP sample was reduced by 28.78%, and that of the USSP with surface polished (1500#) sample was reduced by 53.3%; both of them had no obvious tendency of stress corrosion in the system. The roughness of the USSP surface could cause stress concentration to form a crack source, which was similar to the pitting propagation. USSP with surface polished treatment reduced the surface roughness, achieving the homogenization of the stress distribution and increasing the elongation and the plasticity of the samples, which could further improve the stress corrosion cracking resistance.
Key words: USSP; pure titanium; stress corrosion; SSRT; roughness
Conghui ZHANG , Hua RONG , Guodong SONG , Kun HU . Effect of Surface Roughness by Shot Peening on Stress Corrosion Cracking Behavior of Pure Titanium Welded Joints in HCl Solution[J]. Acta Metall Sin, 2019 , 55(10) : 1282 -1290 . DOI: 10.11900/0412.1961.2019.00056
| [1] | Chen S, Sun T, Jiang X, et al. Online monitoring and evaluation of the weld quality of resistance spot welded titanium alloy [J]. J. Manuf. Processes, 2016, 23: 183 |
| [2] | Qi Y L, Deng J, Hong Q ,et al. Electron beam welding, laser beam welding and gas tungsten arc welding of titanium sheet [J]. Mater. Sci. Eng., 2000, A280: 177 |
| [3] | Shih D S, Robertson I M, Birnbaum H K. Hydrogen embrittlement of α titanium: In situTEM studies [J]. Acta Metall., 1988, 36: 111 |
| [4] | Nishimura R, Shirono J, Jonokuchi A. Hydrogen-induced cracking of pure titanium in sulphuric acid and hydrochloric acid solutions using constant load method [J]. Corros. Sci., 2008, 50: 2691 |
| [5] | Raja V S, Shoji T. Stress Corrosion Cracking [M]. Cambridge: Woodhead Publishing, 2011: 381 |
| [6] | Lalik S, Cebulski J, Michalik R. Corrosion resistance of welding joint from titanium in water solution of hydrochloric acid [J]. J.Achieve. Mater. Manuf. Eng., 2007, 20: 147 |
| [7] | Hollis A C, Scully J C. The stress corrosion cracking and hydrogen embrittlement of titanium in methanol-hydrochloric acid solutions [J]. Corros. Sci., 1993, 34: 821 |
| [8] | Alkhaldi H S, Zaid A I O, Alkhaldi S M. Shot peening as a process for improving fatigue life, strength and enhancing the resistance to stress corrosion cracking [J]. Int. J. Sci. Eng. Res., 2017, 8: 584 |
| [9] | Xian N, Liu D X, Ren C Q ,et al. Improvement of SCC behavior of pipeline steel X80 weld joint by shot peening [J]. Corros. Sci. Prot. Technol., 2008, 20: 466 |
| [9] | (鲜 宁, 刘道新, 任呈强等. 喷丸强化改善管线钢X80焊接接头SCC行为研究 [J]. 腐蚀科学与防护技术, 2008, 20: 466) |
| [10] | Ling X, Ma G. Effect of ultrasonic impact treatment on the stress corrosion cracking of 304 stainless steel welded joints [J]. J. Pressure Vessel Technol., 2009, 131: 051502 |
| [11] | Yu J, Gou G, Zhang L, et al. Ultrasonic impact treatment to improve stress corrosion cracking resistance of welded joints of aluminum alloy [J]. J. Mater. Eng. Perform., 2016, 25: 3046 |
| [12] | Hatamleh O, Singh P M, Garmestani H. Corrosion susceptibility of peened friction stir welded 7075 aluminum alloy joints [J]. Corros. Sci., 2009, 51: 135 |
| [13] | Lu Z M, Shi L M, Zhu S J ,et al. Effect of high energy shot peening pressure on the stress corrosion cracking of the weld joint of 304 austenitic stainless steel [J]. Mater. Sci. Eng., 2015, A637: 170 |
| [14] | Kong D J, Ye C D, Wang W C ,et al. Effects of surface qualities on corrosion performances of X80 pipeline steel welded joints by laser shock processing [J]. Trans. China Weld. Inst., 2014, 35(5): 63 |
| [14] | (孔德军, 叶存冬, 王文昌等. 激光冲击处理后X80焊接接头表面质量对腐蚀性能的影响 [J]. 焊接学报, 2014, 35(5): 63) |
| [15] | Peyre P, Scherpereel X, Berthe L ,et al. Surface modifications induced in 316L steel by laser peening and shot-peening. Influence on pitting corrosion resistance [J]. Mater. Sci. Eng., 2000, A280: 294 |
| [16] | Lee H S, Kim D S, Jung J S ,et al. Influence of peening on the corrosion properties of AISI 304 stainless steel [J]. Corros. Sci., 2009, 51: 2826 |
| [17] | Azar V, Hashemi B, Yazdi M. The effect of shot peening on fatigue and corrosion behavior of 316L stainless steel in Ringer's solution [J]. Surf. Coat. Technol., 2010, 204: 3546 |
| [18] | Wang T B, Li B L, Li Y C ,et al. High-speed deformation response of dislocation boundaries in commercially pure titanium [J]. Rare Met. Mater. Eng., 2017, 46: 1380 |
| [18] | (王同波, 李伯龙, 李颖超等. 工业纯钛位错界面的高速形变响应 [J]. 稀有金属材料与工程, 2017, 46: 1380) |
| [19] | Zhang C H, Song W, Li F B, et al. Microstructure and corrosion properties of Ti-6Al-4V alloy by ultrasonic shot peening [J]. Int. J. Electrochem. Sci., 2015, 10: 9167 |
| [20] | Nie X F, He W F, Wang X D, et al. Effects of laser shock peening on microstructure and mechanical properties of TC17 titanium alloy [J]. Rare Met. Mater. Eng., 2014, 43: 1691 |
| [20] | (聂祥樊, 何卫锋, 王学德等. 激光冲击强化对TC17钛合金微观组织和力学性能的影响 [J]. 稀有金属材料与工程, 2014, 43: 1691) |
| [21] | Zhang C H, Wang J, Song W ,et al. An analyses of high energy shot-peening (HESP) industrial pure titanium welded joints' corrosion behavior in 10%HCl solution [J]. Mater. Rev., 2018, 32: 1564 |
| [21] | (张聪惠, 王 婧, 宋 薇等. 高能喷丸处理工业纯钛焊接接头在10%HCl溶液中的腐蚀行为 [J]. 材料导报, 2018, 32: 1564) |
| [22] | Pereira H B, Panossian Z, Baptista I P ,et al. Investigation of stress corrosion cracking of austenitic, duplex and super duplex stainless steels under drop evaporation test using synthetic seawater [J]. Mater. Res., 2019, 22: e20180211 |
| [23] | Burnett T L, Holroyd N J H, Scamans G M, et al. The role of crack branching in stress corrosion cracking of aluminium alloys [J]. Corros. Rev., 2015, 33: 443 |
| [24] | Cao S, Zhu S M, Samuel Lim C V ,et al. The mechanism of aqueous stress-corrosion cracking of α+β titanium alloys [J]. Corros. Sci., 2017, 125: 29 |
| [25] | Li Z J, Liu H, Gao K W, et al. Molecular dynamics simulation of adsorption-enhanced dislocation emission, motion and crack propagation [J]. Acta Metall. Sin., 2001, 37: 1013 |
| [25] | (李忠吉, 刘 辉, 高克玮等. 吸附促进位错发射、运动以及裂纹扩展的分子动力学模拟 [J]. 金属学报, 2001, 37: 1013) |
| [26] | Yao C F, Ma L F, Du Y X ,et al. Surface integrity and fatigue behavior in shot-peening for high-speed milled 7055 aluminum alloy [J]. Proc.Inst. Mech. Eng. Part B: J. Eng. Manuf., 2017, 231: 243 |
| [27] | Kentish P. Stress corrosion cracking of gas pipelines—Effect of surface roughness, orientations and flattening [J]. Corros. Sci., 2007, 49: 2521 |
/
| 〈 |
|
〉 |