Effect of Boron Content on Microstructure Evolution During Solidification and Mechanical Properties of K417G Alloy
Received date: 2018-11-01
Revised date: 2018-12-27
Online published: 2019-04-29
Boron is a key element in superalloys and many other metallic materials for strengthening the grain boundaries. However, it also has harmful effect on aggravating the solidification segregation of the alloys. Although the mechanism for the influences of B on the alloys has been studied extensively, it is still required to study in some alloys currently because the compositive effects of boron in different alloys are sometimes distinct. K417G, a cast superalloy with good comprehensive properties, has been applied in aero engines of China. In the present work, the effects of boron content on the microstructure evolution during the solidification and the mechanical properties of the as cast K417G alloy have been investigated, providing some fundamental information for the control of boron addition in the alloy. It has been found that boron aggravated the elemental segregation and promoted the eutectic (γ+γ') precipitation at the final stage of the solidification of K417G alloy. In addition, boron decreased the precipitation temperature, and hence reduced the nucleation rate of the γ matrix. When the boron content was below 0.036%, the grain size was increased with the increment of B content, which is caused by the decreased nucleation of the γ phase. When the B addition was increased up to 0.060%, the grain was refined at some local places, because the growth of the dendrites was inhibited and the γ phase could nucleate at the inner part of the subcooled liquids. The mechanical properties of K417G alloy were significantly influenced by the precipitation of the boride at the grain boundaries. The borides were precipitated as fine particles at the grain boundaries when the B addition was below 0.036%, and the tensile properties at 900 ℃ and the stress rupture properties at 900 ℃ and 315 MPa were markedly improved with the increasing B content in this addition range. When the B content was increased to 0.060%, the boride was precipitated as eutectic form in front of the eutectic (γ+γ'). The tensile and stress rupture properties were decreased due to the weak cohesion between the eutectic (γ+γ') and the eutectic form borides.
Key words: K417G alloy; B; solidification process; microstructure; mechanical property
Qiaomu LIU , Shunzhou HUANG , Fang LIU , Yan YANG , Hongqiang NAN , Dong ZHANG , Wenru SUN . Effect of Boron Content on Microstructure Evolution During Solidification and Mechanical Properties of K417G Alloy[J]. Acta Metall Sin, 2019 , 55(6) : 720 -728 . DOI: 10.11900/0412.1961.2018.00491
| [1] | Garosshen T J, Tillman T D, McCarthy G P. Effects of B, C, and Zr on the structure and properties of a P/M nickel base superalloy [J]. Metall. Mater. Trans., 1987, 18A: 69 |
| [2] | Yan B C, Zhang J, Lou L H. Effect of boron additions on the microstructure and transverse properties of a directionally solidified superalloy [J]. Mater. Sci. Eng., 2008, A474: 39 |
| [3] | Shulga A V. Boron and carbon behavior in the cast Ni-base superalloy EP962 [J]. J. Alloys Compd., 2007, 436: 155 |
| [4] | Zhao G D, Yu L X, Yang G L, et al. The role of boron in modifying the solidification and microstructure of nickel-base alloy U720Li [J]. J. Alloys Compd., 2016, 686: 194 |
| [5] | Hu Q, Liu L, Zhao X B, et al. Effect of carbon and boron additions on segregation behavior of directionally solidified nickel-base superalloys with rhenium [J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 3257 |
| [6] | Whitesell H S, Overfelt R A. Influence of solidification variables on the microstructure, macrosegregation, and porosity of directionally solidified Mar-M247 [J]. Mater. Sci. Eng., 2001, A318: 264 |
| [7] | Hong H U, Kim I S, Choi B G, et al. On the mechanism of serrated grain boundary formation in Ni-based superalloys with low γ′ volume fraction [A]. Superalloys 2012 [C]. Hoboken, NJ: John Wiley & Sons, Inc., 2012: 53 |
| [8] | Alam T, Felfer P J, Chaturvedi M, et al. Segregation of B, P, and C in the Ni-based superalloy, Inconel 718 [J]. Metall. Mater. Trans., 2012, 43A: 2183 |
| [9] | Zhang H R, Ojo O A. TEM analysis of Cr-Mo-W-B phase in a DS nickel based superalloy [J]. J. Mater. Sci., 2008, 43: 6024 |
| [10] | Zhang H R, Ojo O A, Chaturvedi M C. Nanosize boride particles in heat-treated nickel base superalloys [J]. Scr. Mater., 2008, 58: 167 |
| [11] | Blavette D, Duval P, Letellier L, et al. Atomic-scale APFIM and TEM investigation of grain boundary microchemistry in Astroloy nickel base superalloys [J]. Acta Mater., 1996, 44: 4995 |
| [12] | Yang F, Hou J S, Gao S, et al. The effects of boron addition on the microstructure stability and mechanical properties of a Ni-Cr based superalloy [J]. Mater. Sci. Eng., 2018, A715: 126 |
| [13] | Hosseini S A, Abbasi S M, Madar K Z, et al. The effect of boron and zirconium on wrought structure and γ-γ' lattice misfit characterization in nickel-based superalloy ATI 718Plus [J]. Mater. Chem. Phys., 2018, 211: 302 |
| [14] | Kontis P, Alabort E, Barba D, et al. On the role of boron on improving ductility in a new polycrystalline superalloy [J]. Acta Mater., 2017, 124: 489 |
| [15] | Wang C S, Guo Y A, Guo J T, et al. Microstructural stability and mechanical properties of a boron modified Ni-Fe based superalloy for steam boiler applications [J]. Mater. Sci. Eng., 2015, A639: 380 |
| [16] | Du B N, Sheng L Y, Lai C, et al. Evolution and structure characterization of the carbide and boride during creep in a Ni-based superalloy [J]. Rare Met. Mater. Eng., 2017, 46: 2123 |
| [16] | (都贝宁, 盛立远, 赖 琛等. 一种镍基高温合金蠕变过程中碳、硼化物的演变行为及结构表征 [J]. 稀有金属材料与工程, 2017, 46: 2123) |
| [17] | Yu Z H, Zhang Y, Zhai Y N, et al. The research progress of the role of C, B and Hf in nickel-based superalloy [J]. Foundry, 2017, 66: 1076 |
| [17] | (余竹焕, 张 洋, 翟娅楠等. C、B、Hf在镍基高温合金中作用的研究进展 [J]. 铸造, 2017, 66: 1076) |
| [18] | Zhang H W, Qin X Z, Li X W, et al. Incipient melting behavior and its influences on the mechanical properties of a directionally solidified Ni-based superalloy with high boron content [J]. Acta Metall. Sin., 2017, 53: 684 |
| [18] | (张洪伟, 秦学智, 李小武等. 一种高硼定向凝固合金的初熔行为及其对力学性能的影响 [J]. 金属学报, 2017, 53: 684) |
| [19] | Du B N, Shi Z W, Yang J X, et al. M5B3 boride at the grain boundary of a nickel-based superalloy [J]. J. Mater. Sci. Technol., 2016, 32: 265 |
| [20] | Wu B P, Li L H, Wu J T, et al. Effect of boron addition on the microstructure and stress-rupture properties of directionally solidified superalloys [J]. Int. J. Miner. Metall. Mater., 2014, 21: 1120 |
| [21] | Hu Z Q, Sun W R, Song H W. A new method for strengthening wrought superalloys-micro-alloying with phosphorus and boron [J]. Eng. Sci., 2005, 3(4): 1 |
| [22] | Zhu Y X, Zhang S N, Zhang T X, et al. A new way to improve the superalloys [A]. Superalloys 1992 [C]. Warrendale, PA: TMS, 1992: 145) |
| [23] | High Temperature Material Branch of the Chinese Society for Metals. China Superalloys Handbook (Volume Two) [M]. Beijing: Standards Press of China, 2012: 93 |
| [23] | (中国金属学会高温材料分会. 中国高温合金手册, 下卷 [M]. 北京: 中国标准出版社, 2012: 93) |
/
| 〈 |
|
〉 |