Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy
Received date: 2019-01-31
Revised date: 2019-03-16
Online published: 2019-04-24
Supported by
Supported by National Natural Science Foundation of China(U1708253);National Science and Technology Major Project(2017-VI-0002)
In 2006, stable γ' phase was found in Co-Al-W alloy, which provides a new way for developing Co-based superalloys. In order to meet the requirements for applications, the Co-Al-W-based superalloys need to have good oxidation and corrosion resistance. But the oxidation and corrosion resistance of the Co-Al-W-based superalloys is relatively low. In this work, pre-oxidation treatments were used to improve the oxidation and corrosion resistance. Three types of pre-oxidation treatments were carried out at 900 ℃ (in air), 950 ℃ (in air) and 1000 ℃ (in 1%O2+99%Ar), which were marked as 900-PreO, 950-PreO and 1000-LPreO, respectively. High temperature oxidation tests of both the pre-oxidation treated and untreated superalloys were carried out at 1000 ℃. And hot corrosion behaviors were also investigated at both 800 and 850 ℃. XRD, SEM and EDS were used to examine the characteristics of the oxidation and corrosion behaviors. The results show that the pre-oxide layers of the superalloys after different pre-oxidation treatments are compact. During oxidation at 1000 ℃, the Cr2O3 scale in 900-PreO treated superalloy is oxidized to form volatile products, and the diffusion resistance of both oxygen and the metal elements through the oxide layer is poor. In 1000-LPreO treated superalloy, serious spallation of the oxides occurs and leads to poor oxidation resistance. In 950-PreO treated superalloy, since the continuous CoCr2O4 and Al2O3 scales help to reduce the diffusion of oxygen and the metal elements, the mass gain of 950-PreO treated superalloy is consequently decreased. During the hot corrosion process, the pre-oxide layer of 950-PreO treated superalloy can hinder the diffusion of corrosive medium. Therefore, the corrosion resistance can be significantly improved by 950-PreO treatment, and the mass gain is decreased by over 80%.
Bo GAO , Lei WANG , Xiu SONG , Yang LIU , Shuyu YANG , Akihiko CHIBA . Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. Acta Metall Sin, 2019 , 55(10) : 1273 -1281 . DOI: 10.11900/0412.1961.2019.00032
| [1] | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 1 |
| [2] | Sato J, Omori T, Oikawa K ,et al. Cobalt-base high-temperature alloys [J]. Science, 2006, 312: 90 |
| [3] | Saal J E, Wolverton C. Thermodynamic stability of Co-Al-W L12γ' [J]. Acta Mater., 2013, 61: 2330 |
| [4] | Guo J T. Materials Science and Engineering for Superalloys (Book 3) [M]. Beijing: Science Press, 2010: 123 |
| [4] | (郭建亭. 高温合金材料学(下册) [M]. 北京: 科学出版社, 2010: 123) |
| [5] | Shinagawa K, Omori T, Sato J ,et al. Phase equilibria and microstructure on γ' phase in Co-Ni-Al-W system [J]. Mater. Trans., 2008, 49: 1474 |
| [6] | Xue F, Zhou H J, Ding X F, et al. Improved high temperature γ' stability of Co-Al-W-base alloys containing Ti and Ta [J]. Mater. Lett., 2013, 112: 215 |
| [7] | Bauer A, Neumeier S, Pyczak F, et al. Microstructure and creep strength of different γ/γ'-strengthened Co-base superalloy variants [J]. Scr. Mater., 2010, 63: 1197 |
| [8] | Yan H Y, Vorontsov V A, Dye D. Alloying effects in polycrystalline γ' strengthened Co-Al-W base alloys [J]. Intermetallics, 2014, 48: 44 |
| [9] | Omori T, Oikawa K, Sato J, et al. Partition behavior of alloying elements and phase transformation temperatures in Co-Al-W-base quaternary systems [J]. Intermetallics, 2013, 32: 274 |
| [10] | Birks N, Meier G H, Pettit F S. Introduction to the High-Temperature Oxidation of Metals [M]. 2nd Ed., Cambridge: Cambridge University Press, 2006: 1 |
| [11] | Li M S. High Temperature Hot Corrosion of Metals [M]. Beijing: Metallurgical Industry Press, 2001: 239 |
| [11] | (李美栓. 金属的高温腐蚀 [M]. 北京: 冶金工业出版社, 2001: 239) |
| [12] | Zhang Y. Cyclic oxidation behavior of two novel Co-base superalloys [D]. Shenyang: Northeastern University, 2018 |
| [12] | (张 莹. 两种新型钴基高温合金的循环氧化行为 [D]. 沈阳: 东北大学, 2018) |
| [13] | Gao B, Wang L, Liu Y, et al. Corrosion behavior of new type Co-based superalloys with different Ni contents [J]. Corros. Rev., 2017, 35: 455 |
| [14] | Xu Y T, Xia T D, Yan J Q. Effect of alloying element tungsten on hot corrosion behavior of novel Co-Al-W superalloys [J]. Chin. J. Nonferrous Met., 2011, 21: 110 |
| [14] | (徐仰涛, 夏天东, 闫健强. 合金元素钨对新型Co-Al-W合金热腐蚀行为的影响 [J]. 中国有色金属学报, 2011, 21: 110) |
| [15] | Xu Y T, Xia T D, Yan J Q. Effect of alloying elements to hot corrosion behavior of novel Co-Al-W superalloy [J]. J.Chin. Soc. orros. Prot., 2010, 30: 457 |
| [15] | (徐仰涛, 夏天东, 闫健强. 合金元素对新型Co-Al-W合金热腐蚀行为的影响 [J]. 中国腐蚀与防护学报, 2010, 30: 457) |
| [16] | Klein L, Shen Y, Killian M S ,et al. Effect of B and Cr on the high temperature oxidation behaviour of novel γ/γ′-strengthened Co-base superalloys [J]. Corros. Sci., 2011, 53: 2713 |
| [17] | Guo J T. Materials Science and Engineering for Superalloys (Book 1) [M]. Beijing: Science Press, 2008: 664 |
| [17] | (郭建亭. 高温合金材料学(上册) [M]. 北京: 科学出版社, 2008: 664) |
| [18] | Huang L, Sun X F, Guan H R ,et al. Dgradation behavior of aluminide coatings on directionally solidified nickel base superalloy M951 [J]. Corros. Sci. Prot. Technol., 2005, 17: 34 |
| [18] | (黄 粮, 孙晓峰, 管恒荣等. 定向凝固高温合金M951低压渗铝涂层的高温氧化及相变过程 [J]. 腐蚀科学与防护技术, 2005, 17: 34) |
| [19] | Talic B, Molin S, Hendriksen P V, et al. Effect of pre-oxidation on the oxidation resistance of Crofer 22 APU [J]. Corros. Sci., 2018, 138: 189 |
| [20] | Ou D R, Cheng M J. Effect of pre-oxidation on the oxidation resistance of spinel-coated Fe-Cr ferritic alloy for solid oxide fuel cell applications [J]. J. Power Sources., 2014, 247: 84 |
| [21] | Li Z M, Qian S Q, Wang W, et al. Effect of preoxidation temperature on high temperature cyclic oxidation resistance of GH3128 superalloy [J]. Rare Met. Mater. Eng., 2012, 41: 1980 |
| [21] | (李志明, 钱士强, 王 伟等. 预氧化温度对GH3128合金抗高温循环氧化性能的影响 [J]. 稀有金属材料与工程, 2012, 41: 1980) |
| [22] | Young D J. High Temperature Oxidation and Corrosion of Metals [M]. Amsterdam: Elsevier, 2008: 193 |
| [23] | Zheng L, Zhang M C, Dong J X. Oxidation behavior and mechanism of powder metallurgy Rene95 nickel based superalloy between 800 and 1000 ℃ [J]. Appl. Surf. Sci., 2010, 256: 7510 |
| [24] | Sun D J, Liang C Y, Shang J L ,et al. Effect of Y2O3 contents on oxidation resistance at 1150 ℃ and mechanical properties at room temperature of ODS Ni-20Cr-5Al alloy [J]. Appl. Surf. Sci., 2016, 385: 587 |
| [25] | Li T F. High Temperature Oxidation and Hot Corrosion of Metals [M]. Beijing: Chemical Industry Press, 2003: 30 |
| [25] | (李铁蕃. 金属高温氧化和热腐蚀 [M]. 北京: 化学工业出版社, 2003: 30) |
| [26] | Li X, Peng X Y, Duan Y L ,et al. Thermal oxidation behavior of commercial purity titanium at high temperature [J]. Chin. J. Nonferrous Met., 2013, 23: 2190 |
| [26] | (李 旭, 彭小燕, 段雨露等. 工业纯钛的高温热氧化行为 [J]. 中国有色金属学报. 2013, 23: 2190) |
/
| 〈 |
|
〉 |