Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels

  • Xingpin CHEN ,
  • Wenjia LI ,
  • Ping REN ,
  • Wenquan CAO ,
  • Qing LIU
Expand
  • 1. College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China
    2. Special Steel Department of Central Iron & Steel Research Institute, Beijing 100081, China

Received date: 2019-01-17

  Revised date: 2019-03-24

  Online published: 2019-04-24

Supported by

National Natural Science Foundation of China((Nos.51871062 and 51421001));and Fundamental Research Funds for the Central Universities(No.2018CDJDCL0019)

Abstract

The lightweight Fe-Mn-Al-C steels (so-called low-density steels) have received great attentions as promising candidate for automobile structure applications due to their excellent combination of density reduction, mechanical properties and corrosion resistance. In previous studies, most examinations of the Fe-Mn-Al-C alloys focused on the deformation mechanisms and the relationship between the microstructure and mechanical properties. It is well known that chemical composition, especially C content, which enhances strength as the interstitial element and reduces the density of steels, plays an important role in the control of microstructure and performance. However, the influence of C element in the alloy with high Mn content is barely studied. In this work, the effects of C content on microstructure and mechanical properties of four Fe-30Mn-10Al-xC (x=0.53, 0.72, 1.21, 1.68, mass fraction, %) alloys were studied by EBSD, TEM, XRD and universal testing machine. The results show that with the increase of C content, the amount of austenite gradually increases and the ferrite/austenite dual-phase microstructure transforms into single phase austenite. In addition, the strength increases monotonously, while the elongation increases and then decreases ultimately with increasing C content. Statistical analysis reveals that the strain coordination capacity of austenite is higher than that of ferrite. Therefore, with the increase of austenite content, the ductility of the dual-phase steel remarkably increases, while the strength increases slightly. For single austenite steels, the yield strength increases but the elongation and work hardening ability decrease with increasing C content, which is related to the precipitation of κ′ carbides.

Cite this article

Xingpin CHEN , Wenjia LI , Ping REN , Wenquan CAO , Qing LIU . Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels[J]. Acta Metall Sin, 2019 , 55(8) : 951 -957 . DOI: 10.11900/0412.1961.2019.00014

References

[1] Ha M C, Koo J M, Lee J K, et al. Tensile deformation of a low density Fe-27Mn-12Al-0.8C duplex steel in association with ordered phases at ambient temperature [J]. Mater. Sci. Eng., 2013, A586: 276
[2] Welsch E, Ponge D, Haghighat S M H, et al. Strain hardening by dynamic slip band refinement in a high-Mn lightweight steel [J]. Acta Mater., 2016, 116: 188
[3] Gutierrez-Urrutia I, Raabe D. Multistage strain hardening through dislocation substructure and twinning in a high strength and ductile weight-reduced Fe-Mn-Al-C steel [J]. Acta Mater., 2012, 60: 5791
[4] Yao M J, Welsch E, Ponge D, et al. Strengthening and strain hardening mechanisms in a precipitation-hardened high-Mn lightweight steel [J]. Acta Mater., 2017, 140: 258
[5] Yanushkevich Z, Belyakov A, Kaibyshev R, et al. Effect of cold rolling on recrystallization and tensile behavior of a high-Mn steel [J]. Mater. Charact., 2016, 112: 180
[6] Chen X P, Xu Y P, Ren P, et al. Aging hardening response and β-Mn transformation behavior of high carbon high manganese austenitic low-density Fe-30Mn-10Al-2C steel [J]. Mater. Sci. Eng., 2017, A703: 167
[7] Scott C, Allain S, Faral M, et al. The development of a new Fe-Mn-C austenitic steel for automotive applications [J]. Rev. Met. Paris, 2006, 103: 293
[8] Choi K, Seo C H, Lee H, et al. Effect of aging on the microstructure and deformation behavior of austenite base lightweight Fe-28Mn-9Al-0.8C steel [J]. Scr. Mater., 2010, 63: 1028
[9] Ren P, Chen X P, Cao Z X, et al. Synergistic strengthening effect induced ultrahigh yield strength in lightweight Fe-30Mn-11Al-1.2C steel [J]. Mater. Sci. Eng., 2019, A752: 160
[10] Rana R. Low-density steels [J]. JOM, 2014, 66: 1730
[11] Kim Y G, Han J M, Lee J S. Composition and temperature dependence of tensile properties of austenitic Fe-Mn-Al-C alloys [J]. Mater. Sci. Eng., 1989, A114: 51
[12] Kalashnikov I, Shalkevich A, Acselrad O, et al. Chemical composition optimization for austenitic steels of the Fe-Mn-Al-C system [J]. J. Mater. Eng. Perform., 2000, 9: 597
[13] Hwang C N, Chao C Y, Liu T F. Grain boundary precipitation in an Fe-8.0Al-31.5Mn-1.05C alloy [J]. Scr. Metall. Mater., 1993, 28: 263
[14] Gutierrez-Urrutia I, Raabe D. High strength and ductile low density austenitic FeMnAlC steels: Simplex and alloys strengthened by nanoscale ordered carbides [J]. Mater. Sci. Technol., 2014, 30: 1099
[15] Chen S P, Rana R, Haldar A, et al. Current state of Fe-Mn-Al-C low density steels [J]. Prog. Mater. Sci., 2017, 89: 345
[16] Lin C L, Chao C G, Juang J Y, et al. Deformation mechanisms in ultrahigh-strength and high-ductility nanostructured FeMnAlC alloy [J]. J. Alloys Compd., 2014, 586: 616
[17] Sato K, Tagawa K, Inoue Y. Spinodal decomposition and mechanical properties of an austenitic Fe-30wt.%Mn-9wt.%Al-0.9wt.%C alloy [J]. Mater. Sci. Eng., 1989, A111: 45
[18] Chang K M, Chao C G, Liu T F. Excellent combination of strength and ductility in an Fe-9Al-28Mn-1.8C alloy [J]. Scr. Mater., 2010, 63: 162
[19] Chen P C, Chao C G, Liu T F. A novel high-strength, high-ductility and high-corrosion-resistance FeAlMnC low-density alloy [J]. Scr. Mater., 2013, 68: 380
[20] Wang C S, Hwang C N, Chao C G, et al. Phase transitions in an Fe-9Al-30Mn-2.0C alloy [J]. Scr. Mater., 2007, 57: 809
[21] Chu C M, Huang H, Kao P W, et al. Effect of alloying chemistry on the lattice constant of austenitic Fe-Mn-Al-C alloys [J]. Scr. Metall. Mater., 1994, 30: 505
[22] Seol J B, Jung J E, Jang Y W, et al. Influence of carbon content on the microstructure, martensitic transformation and mechanical properties in austenite/ε-martensite dual-phase Fe-Mn-C steels [J]. Acta Mater., 2013, 61: 558
[23] Sutou Y, Kamiya N, Umino R, et al. High-strength Fe-20Mn-Al-C-based alloys with low density [J]. ISIJ Int., 2010, 50: 893
[24] Ding H, Han D, Zhang J, et al. Tensile deformation behavior analysis of low density Fe-18Mn-10Al-xC steels [J]. Mater. Sci. Eng., 2016, A652: 69
[25] Wu X L, Yang M X, Yuan F P, et al. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility [J]. Proc. Natl. Acad. Sci. USA, 2015, 112: 14501
[26] Fan Z, Tsakiropoulos P, Miodownik A P. A generalized law of mixtures [J]. J. Mater. Sci., 1994, 29: 141
[27] Hwang S W, Ji J H, Lee E G, et al. Tensile deformation of a duplex Fe-20Mn-9Al-0.6C steel having the reduced specific weight [J]. Mater. Sci. Eng., 2011, A528: 5196
Outlines

/