Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet
Received date: 2018-11-16
Revised date: 2019-03-13
Online published: 2019-04-24
Supported by
National Natural Science Foundation of China (No.51741107)(No.51741107);Major Innovation Projects for Building First-Class Universities in China's Western Region(No.ZKZD17003);National First-Class Discipline Construction Project of Ningxia(No.NXYLXK2017A04)
The microstructures and open circuit potential (OCP) of 2A97 Al-Li alloy sheets with different ageing and their corrosion features in intergranular corrosion (IGC) medium were investigated. As the extension of ageing time, T1 (Al2CuLi) phases are precipitated, the alloy potential is decreased, which is accompanied with the following corrosion mode evolution: pitting, IGC (including local IGC and general IGC) and pitting again. Meanwhile, with ageing progress, the IGC depth is increased firstly and then decreased. Compared to T6 ageing, T8 ageing accelerates the precipitation of T1 phases, the potential therefore decreases more quickly. After a certain ageing, the lower the potential, the smaller the IGC degree, and the greater the pitting degree. A correlation between OCP and corrosion mode was proposed, which may be used to compare the IGC sensitivity of Al-Li alloy with different tempers.
Key words: Al-Li alloy; ageing precipitation; intergranular corrosion; potential
Chao CAI , Yang LI , Jinfeng LI , Zhao ZHANG , Jianqing ZHANG . Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet[J]. Acta Metall Sin, 2019 , 55(8) : 958 -966 . DOI: 10.11900/0412.1961.2018.00519
| [1] | Rioja R J, Liu J. The evolution of Al-Li base products for aerospace and space applications [J]. Metall. Mater. Trans., 2012, 43A: 3325 |
| [2] | Zhang X F, Li G A, Lu Z, et al. Effect of preaged stretch after quenched on the properties and microstructure of a naturally aged Al-Li alloy [J]. Acta Metall. Sin., 2016, 52: 1497 |
| [2] | (张显峰, 李国爱, 陆 政等. 淬火后预拉伸对自然时效状态Al-Li合金组织和性能的影响 [J]. 金属学报, 2016, 52: 1497) |
| [3] | Zhang X L, Zhang L, Wu G H, et al. Influences of Mg content on the microstructures and mechanical properties of cast Al-2Li-2Cu-0.2Zr alloy [J]. J. Mater. Sci., 2019, 54: 791 |
| [4] | Yang Y, Zhou K, Li G J. Surface gradient microstructural characteristics and evolution mechanism of 2195 aluminum lithium alloy induced by laser shock peening [J]. Opt. Laser. Technol., 2019, 109: 1 |
| [5] | Wei X Y, Zheng Z Q, She L J, et al. Microalloying roles of Mg and Zn additions in 2099 Al-Li alloy [J]. Rare Met. Mater. Eng., 2010, 39: 1583 |
| [5] | (魏修宇, 郑子樵, 佘玲娟等. Mg、Zn在2099铝锂合金中的微合金化作用 [J]. 稀有金属材料与工程, 2010, 39: 1583) |
| [6] | Luo X F, Zheng Z Q, Zhong J F, et al. Effects of Mg, Ag and Zn multi-alloying on aging behavior of new Al-Cu-lialloy [J]. Chin. J. Nonferrous Met., 2013, 23: 1833 |
| [6] | (罗先甫, 郑子樵, 钟继发等. Mg、Ag、Zn多元微合金化对新型Al-Cu-Li合金时效行为的影响 [J]. 中国有色金属学报, 2013, 23: 1833) |
| [7] | Li J F, Birbilis N, Liu D Y, et al. Intergranular corrosion of Zn-free and Zn-microalloyed Al-xCu-y Lialloys [J]. Corros. Sci., 2016, 105: 44 |
| [8] | Liu D Y, Li J F, Ma Y L, et al. A closer look at the role of Zn in the microstructure and corrosion of an Al-Cu-Li alloy [J]. Corros. Sci., 145: 220 |
| [9] | Liu F J, Fu L, Zhang W Y. Interface structure and mechanical pro-perties of friction stir welding joint of 2099-T83/2060-T8 dissimilar Al-Li alloys [J]. Acta Metall. Sin., 2015, 51: 281 |
| [9] | (刘奋军, 傅 莉, 张纹源等. 2099-T83/2060-T8异质Al-Li合金搅拌摩擦焊搭接界面结构与力学性能 [J]. 金属学报, 2015, 51: 281) |
| [10] | Liu W C, Feng S, Li Z Q, et al. Effect of rolling strain on microstructure and tensile properties of dual-phase Mg-8Li-3Al-2Zn-0.5Y alloy [J]. J. Mater. Sci. Technol., 2018, 34: 2256 |
| [11] | Zhou X, Liu Q, Liu R R, et al. Characterization of microstructure and mechanical properties of Mg-8Li-3Al-1Y alloy subjected to different rolling processes [J]. Met. Mater. Int., 2018, 24: 1359 |
| [12] | Donatus U, Berbel L O, Costa I. Qualitative use of potentiodynamic polarization and anodic hydrogen evolution in the assessment of corrosion susceptibility in AA2198-T851 Al-Cu-Li alloy [J]. Mater. Corros., 2018, 69: 1375 |
| [13] | Liu Q, Zhu R H, Liu D Y, et al. Correlation between artificial aging and intergranular corrosion sensitivity of a new Al-Cu-Li alloy sheet [J]. Mater. Corros., 2017, 68: 65 |
| [14] | Huang J L, Li J F, Liu D Y, et al. Correlation of intergranular corrosion behaviour with microstructure in Al-Cu-Li alloy [J]. Corros. Sci., 2018, 139: 215 |
| [15] | Proton V, Alexis J, Andrieu E, et al. The influence of artificial ageing on the corrosion behaviour of a 2050 aluminium-copper-lithium alloy [J]. Corros. Sci., 2014, 80: 494 |
| [16] | Cai C, Li J F, Wang H, et al. Dependence of intergranular corrosion sensitivity of Al-Li alloys on aging stage [J]. Rare Met. Mater. Eng., 2015, 44: 2523 |
| [16] | (蔡 超, 李劲风, 王 恒等. 铝锂合金晶间腐蚀敏感性与时效阶段的相关性 [J]. 稀有金属材料与工程, 2015, 44: 2523) |
| [17] | Ning A L, Liu Z Y, Feng C, et al. Study of microstructure, electrical conductivity and stress corrosion resistance of Al-Zn-Mg-Cu alloys [J]. Trans. Mater. Heat Treat., 2008, 29(2): 108 |
| [17] | (宁爱林, 刘志义, 冯 春等. Al-Zn-Mg-Cu合金组织和电导率及抗应力腐蚀性能研究 [J]. 材料热处理学报, 2008, 29(2): 108) |
| [18] | Guyot P, Cottignies L. Precipitation kinetics, mechanical strength and electrical conductivity of Al-Zn-Mg-Cu alloys [J]. Acta Mater., 1996, 44: 4161 |
| [19] | Zhang F, Shen J, Yan X D, et al. Dynamic softening mechanism of 2099 alloy during hot deformation process [J]. Acta Metall. Sin., 2014, 50: 691 |
| [19] | (张飞, 沈健, 闫晓东等. 2099合金热变形过程中的动态软化机制 [J]. 金属学报, 2014, 50: 691) |
| [20] | Xia L, Zhan X H, Yu H S. Morphology and formation mechanism of equiaxed grains along the fusion boundary in Al-Li alloy weld seam [J]. Mater. Res. Exp., 2018, 5: 116523 |
| [21] | Li J F, Ye Z H, Liu D Y, et al. Influence of pre-deformation on aging precipitation behavior of three Al-Cu-Li alloys [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 133 |
| [22] | Gable B M, Zhu A W, Csontos A A, et al. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al-Li-Cu-X alloy [J]. J. Light Met., 2001, 1: 1 |
| [23] | Sun J, Wang C, Song J L, et al. Multi-functional application of oil-infused slippery Al surface: From anti-icing to corrosion resistance [J]. J. Mater. Sci., 2018, 53: 16099 |
| [24] | Li J F, Zheng Z Q, Li S C, et al. Simulation study on function mechanism of some precipitates in localized corrosion of Al alloy [J]. Corros. Sci., 2007, 49: 2436 |
| [25] | Li J F, Li C X, Peng Z W, et al. Corrosion mechanism associated with T1 and T2 precipitates of Al-Cu-Li alloys in NaCl solution [J]. J. Alloys Compd., 2008, 460: 688 |
/
| 〈 |
|
〉 |