Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process
Received date: 2018-11-20
Revised date: 2019-02-25
Online published: 2019-04-23
Supported by
National Natural Science Foundation of China(No.51575040)
Stainless steel/carbon steel bimetallic products, which have the characteristic corrosion resistance of stainless steel as well as the characteristics of high strength and low cost of carbon steel, have been widely used in petrochemical, aviation, shipping and other industries. Roll-bonding is an efficient solid-phase joining method for industrial production of bimetallic products. Different from diffusion bonding and friction welding process, the atoms bond and diffuse at interface while the base metal undergoes severe plastic deformation in the process of roll-bonding. In present work, the micro-deformation behavior in the interfacial area of stainless steel/carbon steel during roll-bonding process is studied based on the molecular dynamics method. Firstly, the applicability of the potential function for the bimetallic composite models with different lattice structures was discussed. Then bimetallic model of FeCrNi/Fe and single metal model of FeCrNi, Fe were established. The effect of non-coherent interface on the deformation behavior was revealed by comparing the deformation process of three models. The results show that the mechanical properties and deformation processes of bimetal and single metal are different in the process of deformation bonding. Due to the existence of non-coherent interface, the dislocation in pure Fe matrix is accumulated at the interface during deformation. The local shear effect of interface atoms makes the dislocation formation in FeCrNi matrix easier, thus reducing the yield strength of FeCrNi matrix. The effect of interface on dislocation propagation during alternation makes the dislocation density change alternately in the two matrixes, which improves the ability of material to resist plastic deformation. In addition, the alternately change of the dislocation density within the two matrixes during the deformation process leads to the special phenomenon that the deformation of the two matrixes is alternately changed.
Qingdong ZHANG , Shuo LI , Boyang ZHANG , Lu XIE , Rui LI . Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process[J]. Acta Metall Sin, 2019 , 55(7) : 919 -927 . DOI: 10.11900/0412.1961.2018.00524
| [1] | Luo Z A, Wang G L, Xie G M, et al. Interfacial microstructure and properties of a vacuum hot roll-bonded titanium-stainless steel clad plate with a niobium interlayer [J]. Acta Metall. Sin. (Eng. Lett.), 2013, 26: 754 |
| [2] | Rong J H, Hong X, Xiang G Y, et al. Research on finishing rolling force model for hot rolling wide and heavy stainless steel clad sheets [J]. Appl. Mech. Mater., 2014, 488-489: 213 |
| [3] | Zhang Q D, Li S, Liu J Y, et al. Study of a bimetallic interfacial bonding process based on ultrasonic quantitative evaluation [J]. Metals, 2018, 8: 329 |
| [4] | Tzou G Y, Tieu A K, Huang M N, et al. Analytical approach to the cold-and-hot bond rolling of sandwich sheet with outer hard and inner soft layers [J]. J. Mater. Process. Technol., 2002, 125-126: 664 |
| [5] | Peng Z H, She X F. Effect of thickness ratio on the properties of stainless steel clad aluminum sheet [J]. Acta Metall. Sin., 2000, 36: 1067 |
| [5] | (彭志辉, 佘旭凡. 厚度比对不锈钢复合铝板性能的影响 [J]. 金属学报, 2000, 36: 1067) |
| [6] | Zepeda-Ruiz L A, Stukowski A, Oppelstrup T, et al. Probing the limits of metal plasticity with molecular dynamics simulations [J]. Nature, 2017, 550: 492 |
| [7] | Song J, Srolovitz D J. Molecular dynamics investigation of patterning via cold welding [J]. J. Mech. Phys. Solids, 2009, 57: 776 |
| [8] | Yuan L, Jing P, Liu Y H, et al. Molecular dynamics simulation of polycrystal silver nanowires under tensile deformation [J]. Acta Phys. Sin., 2014, 63: 016201 |
| [8] | (袁 林, 敬 鹏, 刘艳华等. 多晶银纳米线拉伸变形的分子动力学模拟研究 [J]. 物理学报, 2014, 63: 016201) |
| [9] | He A M, Shao J L, Wang P, et al. Plastic deformation of single-crystalline copper films with surface orientation [001]: Molecular dynamics simulations [J]. Acta Phys. Sin., 2010, 59: 8836 |
| [9] | (何安民, 邵建立, 王 裴等. 单晶Cu(001)薄膜塑性变形的分子动力学模拟 [J]. 物理学报, 2010, 59: 8836) |
| [10] | Zhang H W, Fu Y F, Zheng Y G, et al. Molecular dynamics investigation of plastic deformation mechanism in bulk nanotwinned copper with embedded cracks [J]. Phys. Lett., 2014, 378A: 736 |
| [11] | Mendelev M I, Srolovitz D J, Ackland G J, et al. Effect of Fe segregation on the migration of a non-symmetric Σ5 tilt grain boundary in Al [J]. J. Mater. Res., 2005, 20: 208 |
| [12] | Bonny G, Pasianot R C, Castin N, et al. Ternary Fe-Cu-Ni many-body potential to model reactor pressure vessel steels: First validation by simulated thermal annealing [J]. Philos. Mag., 2009, 89: 3531 |
| [13] | Stukowski A, Sadigh B, Erhart P, et al. Efficient implementation of the concentration-dependent embedded atom method for molecular-dynamics and Monte-Carlo simulations [J]. Modell. Simul. Mater. Sci. Eng., 2009, 17: 075005 |
| [14] | Zheng D L, Chen S D, Soh A K, et al. Molecular dynamics simulations of glide dislocations induced by misfit dislocations at the Ni/Al interface [J]. Comput. Mater. Sci., 2010, 48: 551 |
| [15] | Hoagland R G, Hirth J P, Misra A. On the role of weak interfaces in blocking slip in nanoscale layered composites [J]. Philos. Mag., 2006, 86: 3537 |
| [16] | Wang J, Misra A. An overview of interface-dominated deformation mechanisms in metallic multilayers [J]. Curr. Opin. Solid State Mater. Sci., 2011, 15: 20 |
| [17] | Shao S, Medyanik S N. Interaction of dislocations with incoherent interfaces in nanoscale FCC-BCC metallic bi-layers [J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 055010 |
| [18] | Wang J, Hoagland R G, Hirth J P, et al. Atomistic simulations of the shear strength and sliding mechanisms of copper-niobium interfaces [J]. Acta Mater., 2008, 56: 3109 |
| [19] | Misra A, Hirth J P, Hoagland R G. Length-scale-dependent deformation mechanisms in incoherent metallic multilayered composites [J]. Acta Mater., 2005, 53: 4817 |
| [20] | Weng S Y, Ning H M, Hu N, et al. Strengthening effects of twin interface in Cu/Ni multilayer thin films—A molecular dynamics study [J]. Mater. Des., 2016, 111: 1 |
| [21] | Luo X, Qian G F, Wang Y M. Computer simulation of metal interfaces [J]. Acta Phys. Sin., 1994, 43: 1957 |
| [21] | (罗 旋, 钱革非, 王煜明. Ag/Ni和Cu/Ni界面的分子动力学模拟 [J]. 物理学报, 1994, 43: 1957) |
| [22] | Cheng D, Yan Z J, Yan L. Molecular dynamics simulation of strengthening mechanism of Cu/Ni multilayers [J]. Acta Metall. Sin., 2008, 44: 1461 |
| [22] | (程 东, 严志军, 严 立. Cu/Ni多层膜强化机理的分子动力学模拟 [J]. 金属学报, 2008, 44: 1461) |
| [23] | Cheng C, Chen S D, Wu Y Z, et al. Molecular dynamics simulations of deformation behaviors for nanocrystalline Cu/Ni films under different strain rates [J]. J. Mater. Eng., 2015, 43(3): 60 |
| [23] | (成 聪, 陈尚达, 吴勇芝, 等. 不同应变率下纳米多晶Cu/Ni薄膜变形行为的分子动力学模拟 [J]. 材料工程, 2015, 43(3): 60) |
| [24] | Bonny G, Castin N, Terentyev D. Interatomic potential for studying ageing under irradiation in stainless steels: The FeNiCr model alloy [J]. Modell. Simul. Mater. Sci. Eng., 2013, 21: 085004 |
| [25] | Eich S M, Beinke D, Schmitz G. Embedded-atom potential for an accurate thermodynamic description of the iron-chromium system [J]. Comput. Mater. Sci., 2015, 104: 185 |
| [26] | Kelchner C L, Plimpton S J, Hamilton J C. Dislocation nucleation and defect structure during surface indentation [J]. Phys. Rev., 1998, 58B: 11085 |
| [27] | Yu J, Xin L, Wang J J, et al. First-principles study of the relaxation and energy of bcc-Fe, fcc-Fe and AISI-304 stainless steel surfaces [J]. Appl. Surf. Sci., 2009, 255: 9032 |
| [28] | Stukowski A, Albe K. Extracting dislocations and non-dislocation crystal defects from atomistic simulation data [J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 085001 |
/
| 〈 |
|
〉 |