Oxidation Behavior of GH984G Alloy in Steam at 700

  • Changshuai WANG ,
  • Lili GUO ,
  • Liying TANG ,
  • Rongcan ZHOU ,
  • Jianting GUO ,
  • Lanzhang ZHOU
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2. Xi’an Thermal Power Research Institute Co. , Ltd. , Xi’an 710032, China

Received date: 2018-09-14

  Revised date: 2019-01-26

  Online published: 2019-04-15

Supported by

National Key Research and Development Program of China(No.2017YFB0305204);National High Technology Research and Development Program of China(No.2012AA03A501);National Natural Science Foundation of China(No.51301171);National Energy Administration Program of China(No.NY20150102);Science and Technology Program of Sichuan Province(No.2016JZ0036)

Abstract

To produce abundant and cheap electricity in a cleaner way, the next generation of advanced ultra-supercritical (A-USC) coal-fired power plants with higher thermal efficiency will operate at service temperatures at 700 ℃ and steam pressures up to 35 MPa. However, the temperature capacity of the currently used ferritic or austenitic steels in USC plants at 600 ℃ cannot meet the requirements. GH984G is a newly developed Ni-Fe-Cr base alloy designed for A-USC, but its oxidation behavior in steam at 700 ℃ is unclear. In this work, the oxidation kinetics of GH984G alloy in steam at 700 ℃ was investigated by weighting specimens at intervals. Morphology, composition and phase constituent of the steam oxide scale were characterized using SEM, EDS and XRD. The results show that the oxidation of GH984G alloy follows a parabolic law with a rate constant of 0.00521 mg/(cm2·h1/2) and steady weight gain rate of 8×10-4 g/(m2·h). The oxide scale mainly consists of Cr2O3 and Al2O3. Meanwhile, a small amount of TiO2 was observed. The oxide scale of Cr2O3 forms on the alloy surface and then the internal oxidation of Al to be Al2O3 occurs along the grain boundaries of the matrix alloy and TiO2 forms at the surface of the external oxide scale. The morphology of Cr2O3 at the surface of the oxide scale is needle-like at the initial oxidation stage and then the agglomeration of Cr2O3 was observed and the cellular shape forms. Finally, the coalescence of the cellular Cr2O3 appears and the flat surface of the external oxide scale forms. The excellent oxidation resistant of GH984G alloy in steam at 700 ℃ can be attributed to the compact external oxide scale of Cr2O3 and the root-like internal oxide scale of Al2O3.

Cite this article

Changshuai WANG , Lili GUO , Liying TANG , Rongcan ZHOU , Jianting GUO , Lanzhang ZHOU . Oxidation Behavior of GH984G Alloy in Steam at 700 ℃[J]. Acta Metall Sin, 2019 , 55(7) : 893 -901 . DOI: 10.11900/0412.1961.2018.00440

References

[1] Bugge J, Kj?r S, Blum R. High-efficiency coal-fired power plants development and perspectives [J]. Energy, 2006, 31: 1437
[2] Zhou L Z. Recent development and material selection for 700 ℃ ultra-supercritical coal-fired power plants [A]. First Symposia on Heat Resistant Materials Used for 700 ℃ Ultra-supercritical Coal-fired Power Plants [C]. Beijing: The Secretariat of China USC Coal-fired Power Generation Technology Innovation Consortium, 2011: 13
[2] (周兰章. 700 ℃超超临界机组耐热材料的研制现状及选材思考 [A]. 国家700 ℃计划耐热材料第一次专题研讨会论文集 [C]. 北京: 国家700 ℃超超临界燃煤发电技术创新联盟秘书处, 2011: 13)
[3] Abe F. Research and development of heat-resistant materials for advanced USC power plants with steam temperatures of 700 ℃ and above [J]. Engineering, 2015, 1: 211
[4] Kl?wer J, Husemann R U, Bader M. Development of nickel alloys based on alloy 617 for components in 700 ℃ power plants [J]. Procedia Eng., 2013, 55: 226
[5] Zhao S Q, Xie X S, Smith G D, Patel S J. Research and improvement on structure stability and corrosion resistance of nickel-base superalloy INCONEL alloy 740 [J]. Mater. Des., 2006, 27: 1120
[6] Liu Z D, Chong Y, Bao H S, et al. Boiler tube for 700 ℃ steam parameter thermal power generating unit and preparation method thereof [P]. Chin Pat, 103276251, 2013
[6] (刘正东, 崇 严, 包汉生等. 一种700 ℃蒸汽参数火电机组用锅炉管及其制备方法 [P]. 中国专利, 103276251, 2013)
[7] Wei K, Zhang M C, Xie X S. Recrystallization mechanisms in hot working processes of a nickel-based alloy for ultra-supercritical power plant application [J]. Acta Metall. Sin., 2017, 53: 1611
[7] (韦 康, 张麦仓, 谢锡善. 超超临界电站用镍基合金热加工过程的再结晶机理 [J]. 金属学报, 2017, 53: 1611)
[8] Shingledecker J P, Evans N D. Creep-rupture performance of 0.07C-23Cr-45Ni-6W-Ti,Nb austenitic alloy (HR6W) tubes [J]. Int. J. Press. Vessels Pip., 2010, 87: 345
[9] Tan M L, Wang C S, Guo Y A, et al. Influence of Ti/Al ratios on γ′ coarsening behavior and tensile properties of GH984G alloy during long-term thermal exposure [J]. Acta Metall. Sin., 2014, 50: 1260
[9] (谭梅林, 王常帅, 郭永安等. Ti/Al比对GH984G合金长期时效过程中γ′沉淀相粗化行为及拉伸性能的影响 [J]. 金属学报, 2014, 50: 1260)
[10] Wang C S, Guo Y A, Guo J T, et al. Investigation and improvement on structural stability and stress rupture properties of a Ni-Fe based alloy [J]. Mater. Des., 2015, 88: 790
[11] Wang C S, Guo Y A, Guo J T, et al. Microstructural changes and their effect on tensile properties of a Ni-Fe based alloy during long-term thermal exposure [J]. Mater. Sci. Eng., 2016, A670: 178
[12] Wang C S, Guo Y A, Guo J T, et al. Microstructural characteristics and mechanical properties of a Mo modified Ni-Fe-Cr based alloy [J]. Mater. Sci. Eng., 2016, A675: 314
[13] Wang C S, Su H J, Guo Y A, et al. Solidification characteristics and segregation behavior of a P-containing Ni-Fe-Cr-based alloy [J]. Appl. Phys., 2017, 123A: 587
[14] Guo Y, Jia J M, Hou S F, et al. Steam oxidation behavior of domestic TP347H FG steel [J]. Corros. Sci. Prot. Technol., 2011, 23: 505
[14] (郭 岩, 贾建民, 侯淑芳等. 国产TP347H FG钢的水蒸汽氧化行为研究 [J]. 腐蚀科学与防护技术, 2011, 23: 505)
[15] Yuan J T, Wu X M, Wang W, et al. Effect of grain size on oxidation of heat-resistant steels in high temperature water steam [J]. J. Chin. Soc. Corros. Prot., 2013, 33: 257
[15] (袁军涛, 吴细毛, 王 文等. 晶粒尺寸对耐热钢在高温水蒸汽中的氧化行为的影响 [J]. 中国腐蚀与防护学报, 2013, 33: 257)
[16] Bai Y, Liu Z D, Xie J X, et al. Effect of pre-oxidation treatment on the behavior of high temperature oxidation in steam of G115 steel [J]. Acta Metall. Sin., 2018, 54: 895
[16] (白 银, 刘正东, 谢建新等. 预氧化处理对G115钢高温蒸气氧化行为的影响 [J]. 金属学报, 2018, 54: 895)
[17] Otsuka N, Fujikawa H. Scaling of austenitic stainless steels and nickel-base alloys in high-temperature steam at 973 K [J]. Corrosion, 1991, 47: 240
[18] Quadakkers W J, Zurek J, H?nsel. Effect of water vapor on high-temperature oxidation of FeCr alloys [J]. JOM, 2009, 61(7): 44
[19] Garcia-Fresnillo L, Chyrkin A, B?hme C, et al. Oxidation behaviour and microstructural stability of alloy 625 during long-term exposure in steam [J]. J. Mater. Sci., 2014, 49: 6127
[20] Intiso L, Johansson L G, Svensson J E, et al. Oxidation of Sanicro 25 (42Fe22Cr25NiWCuNbN) in O2 and O2+H2O environments at 600-750 ℃ [J]. Oxid. Met., 2015, 83: 367
[21] Yang Z, Lu J T, Yuan Y, et al. Oxidation behavior of a new Fe-Ni-Cr-based alloy in pure steam at 750 ℃ [J]. Mater. High Temp., 2016, 33: 164
[22] Liu G M, Wang C F, Yu F, et al. Evolution of oxide film of T91 steel in water vapor atmosphere at 750 ℃ [J]. Oxid. Met., 2014, 81: 383
[23] Dudziak T, ?ukaszewicz M, Simms N, et al. Analysis of high temperature steam oxidation of superheater steels used in coal fired boilers [J]. Oxid. Met., 2016, 85: 171
[24] Peng X, Shen J N, Hu W S, et al. A comparative investigation of oxidation performance of superalloys M17 and M17F at high temperatures [J]. J. Chin. Soc. Corros. Prot., 1996, 16: 20
[24] (彭 晓, 沈嘉年, 胡武生等. 高温合金M17和M17F抗氧化性能的比较研究 [J]. 中国腐蚀与防护学报, 1996, 16: 20)
[25] Li Y, Shang H B, Guo J T, et al. Isothermal oxidation behavior of a cast Ni-base superalloy K35 [J]. Acta Metall. Sin., 2003, 39: 749
[25] (李 云, 尚海波, 郭建亭等. 铸造镍基高温合金K35的高温氧化行为 [J]. 金属学报, 2003, 39: 749)
[26] Cao J D, Zhang J S, Chen R F, et al. High temperature oxidation behavior of Ni-based superalloy GH202 [J]. Mater. Charact., 2016, 118: 122
[27] Ren X, Sridharan K, Allen T R. Corrosion behavior of alloys 625 and 718 in supercritical water [J]. Corrosion, 2007, 63: 603
[28] Wang C S, Wang T T, Guo J T, et al. Ni-Fe based alloy GH984G used for 700 ℃ coal-fired power plants [A]. Energy Materials 2017 [C]. Cham: Springer, 2017: 143
[29] Rothman S J, Nowicki L J, Murch G E. Self-diffusion in austenitic Fe-Cr-Ni alloys [J]. J. Phys., 1980, 10F: 383
[30] Pérez-González F A, Garza-Montes-de Oca N F, Colás R. High temperature oxidation of the Haynes 282? nickel-based superalloy [J]. Oxid. Met., 2014, 82: 145
[31] Abe F, Araki H, Yoshida H, et al. The role of aluminum and titanium on the oxidation process of a nickel-base superalloy in steam at 800 ℃ [J]. Oxid. Met., 1987, 27: 21
Outlines

/