Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel

  • Miao JIN ,
  • Wenquan LI ,
  • Shuo HAO ,
  • Ruixue MEI ,
  • Na LI ,
  • Lei CHEN
Expand
  • 1. College of Mechanical Engineering, Yanshan University, Qinhuangdao 066004, China
    2. National Engineering Research Center for Equipment and Technology of Cold Strip Rolling, Qinhuangdao 066004, China

Received date: 2018-06-27

  Revised date: 2018-07-29

  Online published: 2019-04-11

Supported by

National Natural Science Foundation of China(Nos.51675467);National Natural Science Foundation of China(Nos.51675465);Natural Science Foundation of Hebei Province(No.E2016203284);China Post Doctoral Science Foundation(Nos.2016-M600194);China Post Doctoral Science Foundation(Nos.2017T100712)

Abstract

Advanced duplex stainless steels (DSSs) in which Ni is mostly or completely replaced by Mn and N have been developed in recent years. Such Mn-N bearing DSSs can readily achieve exceptional room-temperature tensile properties through the transformation-induced plasticity (TRIP) effect of metastable austenite. During the processing of DSSs, solution treatment is a critical step that tailors the phase fraction and the overall properties. In particular, the phase chemistry can change due to different element partitioning between two constituents, resulting in a different TRIP kinetics, when DSS is solution treated at different temperature. In this work, the effect of solution temperature on tensile deformation behavior of a new Mn-N bearing DSS was studied. The mechanical properties and work-hardening characteristic of the steels solution treated at different solution temperature (1000~1200 ℃) were investigated by thermal modeling test, and the effects of solution temperature on the deformation substructure and fracture characteristics were analyzed by OM, SEM and EBSD. The results show that as the solution temperature increases, the yield strength and tensile strength of the steels decrease, while the elongation (uniform elongation and total elongation) increases firstly and then decreases. The steel solution treated at 1100 ℃ shows the optimum uniform elongation of 46.7%, and a better combination of ultimate tensile strength and ductility of approximately 44.6 GPa·%. The work-hardening rate of the steel shows a three-stage characteristic, namely it declines firstly and then increases and subsequently declines again as the strain increases. However, the increasing extent of the work-hardening rate decreases as the solution temperature increases. The strain-induced martensitic transformation (SIMT) of metastable austenite which causes the TRIP effect has two evolution mechanisms of γεα' and γα'. But SIMT can be suppressed when the solution temperature increases. The fracture surfaces of specimens solution treated at different temperatures show a quasi-cleavage mode, in which both ferrite and strain-induced martensite exhibit cleavage fracture while the residual austenite displays a dimple-mode fracture. Furthermore, the Md30 which can characterize the stability of metastable austenite was calculated, which decreases from 81 ℃ to 38 ℃ as the solution temperature increases from 1000 ℃ to 1200 ℃, indicating that the TRIP effect gets weakening at a higher solution temperature, and the work-hardening and plasticity therefore decrease.

Cite this article

Miao JIN , Wenquan LI , Shuo HAO , Ruixue MEI , Na LI , Lei CHEN . Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel[J]. Acta Metall Sin, 2019 , 55(4) : 436 -444 . DOI: 10.11900/0412.1961.2018.00276

References

1 He J, Han G, Fukuyama S, et al. Tensile behaviour of duplex stainless steel at low temperatures [J]. Metal. Sci. J., 1999, 15: 909
2 Badji R, Bacroix B, Bouabdallah M.Texture, microstructure and anisotropic properties in annealed 2205 duplex stainless steel welds[J]. Mater. Charact.,2011, 62: 833
3 Jiang L Z, Zhang W, Wang Z Y. Research and development of lean duplex stainless steels [J]. J. Iron Steel Res., 2013, 25(4): 1
3 江来珠, 张 伟, 王治宇. 经济型双相不锈钢的研发进展 [J]. 钢铁研究学报, 2013, 25(4): 1)
4 Du C F, Zhan F, Yang Y H, et al. Research progress in nickel-saving duplex stainless steel [J]. Met. Funct. Mater., 2010: 17(5): 63
4 杜春风, 詹 凤, 杨银辉等. 节镍型双相不锈钢的研究进展 [J]. 金属功能材料, 2010: 17(5): 63)
5 Herrera C, Ponge D, Raabe D. Design of a novel Mn-based 1 GPa duplex stainless TRIP Steel with 60% ductility by a reduction of austenite stability [J]. Acta Mater., 2011, 59: 4653
6 Wang J, Uggowitzer P J, Magdowski R, et al. Nickel-free duplex stainless steels [J]. Scr. Mater., 1998, 40: 123
7 Ran Q X, Xu Y L, Li J, et al. Effect of heat treatment on transformation-induced plasticity of economical Cr19 duplex stainless steel [J]. Mater. Des., 2014, 56: 959
8 Choi J Y, Ji J H, Hwang S W, et al. TRIP aided deformation of a near-Ni-free, Mn-N bearing duplex stainless steel [J]. Mater. Sci. Eng., 2012, A535: 32
9 Kang J Y, Kim H, Kim K I, et al. Effect of austenitic texture on tensile behavior of lean duplex stainless steel with transformation induced plasticity (TRIP) [J]. Mater. Sci. Eng., 2017, A681: 114
10 Zhang W N, Liu Z Y, Wang G D. Martensitic transformation induced by deformation and work-hardening behavior of high manganese TRIP steels [J]. Acta Metall. Sin., 2010, 46: 1230
10 张维娜, 刘振宇, 王国栋. 高锰TRIP钢的形变诱导马氏体相变及加工硬化行为 [J]. 金属学报, 2010, 46: 1230
11 Chen L, Li F, Zhang Y J, et al. Calculation for the phase diagram and stability of metastable austenite in a TRIP/TWIP duplex stainless steel [J]. J. Yanshan Univ., 2016, 40: 35
11 陈 雷, 李 飞, 张英杰等. 一种TRIP/TWIP型双相不锈钢的相图及其亚稳奥氏体组织稳定性计算 [J]. 燕山大学学报, 2016, 40: 35
12 Li X F, Li Z B, Guo H S, et al. Influence of solution temperature on structure and properties of Ni-free type dual stainless steel 00Cr21 Mn5Ni1N [J]. J. Iron Steel Res., 2007, 19(10): 44
12 李学锋, 李正邦, 郭海生等. 固溶温度对00Cr21Mn5Ni1N节镍型双相不锈钢组织和性能的影响 [J]. 钢铁研究学报, 2007, 19(10): 44)
13 Chen L, Zhang Y J, Li F, et al. Effect of solution temperature on TRIP/TWIP behavior of a lean duplex stainless steel [J]. Iron Steel, 2017, 52(4): 55
13 陈 雷, 张英杰, 李 飞等. 固溶温度对节约型双相不锈钢TRIP/TWIP行为的影响 [J]. 钢铁, 2017, 52(4): 55)
14 Guo B F, Zhang Q F, Chen L, et al. Influence of annealing temperature on the strain-hardening behavior of a lean duplex stainless steel [J]. Mater. Sci. Eng., 2018, A722: 216
15 Tang Z Y, Wu Z Q, Zan N, et al. Microstructure evolution and deformation behavior of high manganese TRIP/TWIP symbiotic effect steels under high-speed deformation [J]. Acta Metall. Sin., 2011, 47: 1426
15 唐正友, 吴志强, 昝 娜等. 高锰TRIP/TWIP效应共生钢高速变形过程中的组织演变及变形行为 [J]. 金属学报, 2011, 47: 1426
16 Choi J Y, Ji J H, Hwang S W, et al. Effects of nitrogen content on TRIP of Fe-20Cr-5Mn-xN duplex stainless steel [J]. Mater. Sci. Eng., 2012, A534: 673
17 Choi J Y, Ji J H, Hwang S W, et al. Strain induced martensitic transformation of Fe-20Cr-5Mn-0.2Ni duplex stainless steel during cold rolling: Effects of nitrogen addition [J]. Mater. Sci. Eng., 2011, A528: 6012
18 Wang M M, Tasan C C, Ponge D, et al. Spectral TRIP enables ductile 1.1 GPa martensite [J]. Acta Mater., 2016, 111: 262
19 Masumura T, Nakada N, Tsuchiyama T, et al. The difference in thermal and mechanical stabilities of austenite between carbon- and nitrogen-added metastable austenitic stainless steels [J]. Acta Mater., 2015, 84: 330
20 Kim E Y, Woo W C, Heo Y U, et al. Effect of kinematic stability of the austenite phase on phase transformation behavior and deformation heterogeneity in duplex stainless steel using the crystal plasticity finite element method [J]. Int. J. Plast., 2016, 79: 48
21 Lin Y C, Chen M S, Zhong J. Static recrystallization behaviors of deformed 42CrMo steel [J]. J. Cent. South Univ. (Sci. Technol.), 2009, 40: 411
21 蔺永诚, 陈明松, 钟 掘. 42CrMo钢形变奥氏体的静态再结晶 [J]. 中南大学学报(自然科学版), 2009, 40: 411
22 Gutierrez-Urrutia I, Raabe D. Multistage strain hardening through dislocation substructure and twinning in a high strength and ductile weight-reduced Fe-Mn-Al-C steel [J]. Acta Mater. 2012, 60: 5791
23 Lu F Y, Yang P, Meng L, et al. Microstructure, mechanical properties and crystallography analysis of Fe-22Mn TRIP/TWIP steel after tensile deformation [J]. Acta Metall. Sin., 2013, 49: 1
23 鲁法云, 杨 平, 孟 利等. Fe-22Mn TRIP/TWIP钢拉伸过程组织、性能及晶体学行为分析 [J]. 金属学报, 2013, 49: 1
24 Yen H W, Ooi S W, Eizadjou M, et al. Role of stress-assisted martensite in the design of strong ultrafine-grained duplex steels [J]. Acta Mater., 2015, 82: 100
25 Bian H X. The research of plastic instability on austenitic stainless steel during hot deformation [D]. Lanzhou: Lanzhou University of Technology, 2014
25 边红霞. 奥氏体不锈钢热变形过程中的塑性失稳研究 [D]. 兰州: 兰州理工大学, 2014
26 Sun P L, Cerreta E K, Bingert J F, et al. Enhanced tensile ductility through boundary structure engineering in ultrafine-grained aluminum [J]. Mater. Sci. Eng., 2007, A464: 343
27 Chen J H, Cao R. Micromechanism of cleavage fracture of weld metals [J]. Acta Metall. Sin., 2017, 53: 1427
27 陈剑虹, 曹 睿. 焊缝金属解理断裂微观机理 [J]. 金属学报, 2017, 53: 1427
28 Moallemi M, Zarei-Hanzaki A, Baghbadorani H S. Evolution of microstructure and mechanical properties in a cold deformed nitrogen bearing TRIP-assisted duplex stainless steel after reversion annealing [J]. Mater. Sci. Eng., 2017, A683: 83
29 Zhang W, Hu J C. Effect of annealing temperature on transformation induced plasticity effect of a lean duplex stainless steel [J]. Mater. Charact., 2013, 79: 37
Outlines

/