Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel
Received date: 2018-12-26
Revised date: 2019-03-22
Online published: 2019-04-08
Supported by
National Natural Science Foundation of China(No.51501056);Natural Science Foundation of Hebei Province(No.E2016209341);Educational Commission of Hebei Province(No.BJ2014031);Foundation of North China University of Science and Technology(No.JP201510)
TWIP steel as the representative of advanced high strength steel (AHSS) has a bright future in market and application owing to its excellent strength and ductility. Hydrogen embrittlement (HE) as a difficult problem of TWIP steel, researches on solving it mainly focus on alloying, few effort has been made on the mechanism of improving HE resistance by process adjustment and microstructure optimization. In this work, electrochemically combined with slow strain rate tensile test (SSRT) and OM, SEM have been used to study the effect of annealing temperature on mechanical property and deformation behavior of a Fe-18Mn-0.6C (mass fraction, %) twinning-induced plasticity (TWIP) steel, and also the influence of various microstructures on HE were discussed. The results showed that the grain size of TWIP steel increased with the increasing annealing temperature. In 700 ℃ annealed sheet, grain boundary (Fe, Mn)3C cementite was obvious. TWIP steel with uniform medium-sized grains by 900 ℃ annealing had the highest strength-ductility balance. After SSRT under ongoing hydrogen charging, strength and plasticity reduced significantly. The strength-ductility balance loss rate (R) showed a tendency of increasing with the increasing annealing temperature. Deformation twins were more likely to be produced in large-sized grains by high temperature annealing. The junctions of twin/twin and twin/grain boundary were the main sources of hydrogen induced cracks. Although relatively low temperature annealing resulted in fine grains and the change of stacking fault energy (SFE) along grain boundary, deformation twins were not easily formed. But it was very vulnerable to generate vacancies where the stress concentrated between the local coarse carbides and deformation twins, then evolved into crack sources. As a result, the plasticity of TWIP steel itself was not high when annealed at a relatively low temperature. It had no apparent effect on improving HE resistance for TWIP steel annealed below 800 ℃.
Key words: TWIP steel; hydrogen embrittlement; deformation twin; carbide
Futao DONG , Fei XUE , Yaqiang TIAN , Liansheng CHEN , Linxiu DU , Xianghua LIU . Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. Acta Metall Sin, 2019 , 55(6) : 792 -800 . DOI: 10.11900/0412.1961.2018.00566
| [1] | Chin K G, Kang C Y, Shin S Y, et al. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels [J]. Mater. Sci. Eng., 2011, A528: 2922 |
| [2] | Hong S, Shin S Y, Kim H S, et al. Effects of inclusions on delayed fracture properties of three twinning induced plasticity (TWIP) steels [J]. Metall. Mater. Trans., 2013, 44A: 776 |
| [3] | van Tol R T, Zhao L, Bracke L, et al. Investigation of the delayed fracture phenomenon in deep-drawn austenitic manganese-based twinning-induced plasticity steels [J]. Metall. Mater. Trans., 2013, 44A: 4654 |
| [4] | Koyama M, Akiyama E, Tsuzaki K. Hydrogen embrittlement in a Fe-Mn-C ternary twinning-induced plasticity steel [J]. Corros. Sci., 2012, 54: 1 |
| [5] | Koyama M, Akiyama E, Lee Y K, et al. Overview of hydrogen embrittlement in high-Mn steels [J]. Int. J. Hydrogen Energy, 2017, 42: 12706 |
| [6] | Ronevich J A, Kim S K, Speer J G, et al. Hydrogen effects on cathodically charged twinning-induced plasticity steel [J]. Scr. Mater., 2012, 66: 956 |
| [7] | Chun Y S, Park K T, Lee C S. Delayed static failure of twinning-induced plasticity steels [J]. Scr. Mater., 2012, 66: 960 |
| [8] | Koyama M, Akiyama E, Tsuzaki K. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging [J]. Acta Mater., 2013, 61: 4607 |
| [9] | Wang M Q, Akiyama E, Tsuzaki K. Hydrogen degradation of a boron-bearing steel with 1050 and 1300 MPa strength levels [J]. Scr. Mater., 2005, 52: 403 |
| [10] | Toribio J, Kharin V, Lorenzo M, et al. Role of drawing-induced residual stresses and strains in the hydrogen embrittlement susceptibility of prestressing steels [J]. Corros. Sci., 2011, 53: 3346 |
| [11] | Enos D G, Scully J R. A critical-strain criterion for hydrogen embrittlement of cold-drawn, ultrafine pearlitic steel [J]. Metall. Mater. Trans., 2002, 33A: 1151 |
| [12] | Wang M Q, Akiyama E, Tsuzaki K. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test [J]. Corros. Sci., 2007, 49: 4081 |
| [13] | Barnoush A, Vehoff H. Recent developments in the study of hydrogen embrittlement: Hydrogen effect on dislocation nucleation [J]. Acta Mater., 2010, 58: 5274 |
| [14] | Takagi S, Toji Y, Yoshino M, et al. Hydrogen embrittlement resistance evaluation of ultra high strength steel sheets for automobiles [J]. ISIJ Int., 2012, 52: 316 |
| [15] | Song E J, Bhadeshia H K D H, Suh D W. Interaction of aluminium with hydrogen in twinning-induced plasticity steel [J]. Scr. Mater., 2014, 87: 9 |
| [16] | Dieudonné T, Marchetti L, Wery M, et al. Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe-Mn-C TWIP steels [J]. Corros. Sci., 2014, 82: 218 |
| [17] | Malard B, Remy B, Scott C, et al. Hydrogen trapping by VC precipitates and structural defects in a high strength Fe-Mn-C steel studied by small-angle neutron scattering [J]. Mater. Sci. Eng., 2012, A536: 110 |
| [18] | Zhao Y Y, Wang J F, Zhou S, et al. Effects of rare earth addition on microstructure and mechanical properties of a Fe-15Mn-1.5Al-0.6C TWIP steel [J]. Mater. Sci. Eng., 2014, A608: 106 |
| [19] | Dini G, Najafizadeh A, Ueji R, et al. Tensile deformation behavior of high manganese austenitic steel: The role of grain size [J]. Mater. Des., 2010, 31: 3395 |
| [20] | Chen L, Kim H S, Kim S K, et al. Localized deformation due to Portevin-LeChatelier effect in 18Mn-0.6C TWIP austenitic steel [J]. ISIJ Int., 2007, 47: 1804 |
| [21] | Guo P C, Qian L H, Meng J Y, et al. Monotonic tension and tension-compres-sion cyclic deformation behaviors of high manganese austenitic TWIP steel [J]. Acta Metall. Sin., 2014, 50: 415 |
| [21] | (郭鹏程, 钱立和, 孟江英等. 高锰奥氏体TWIP钢的单向拉伸与拉压循环变形行为 [J]. 金属学报, 2014, 50: 415) |
| [22] | El-Danaf E, Kalidindi S R, Doherty R D. Influence of deformation path on the strain hardening behavior and microstructure evolution in low SFE FCC metals [J]. Int. J. Plast., 2001, 17: 1245 |
| [23] | Ueji R, Tsuchida N, Terada D, et al. Tensile properties and twinning behavior of high manganese austenitic steel with fine-grained structure [J]. Scr. Mater., 2008, 59: 963 |
| [24] | Park I J, Lee S M, Jeon H H, et al. The advantage of grain refinement in the hydrogen embrittlement of Fe-18Mn-0.6C twinning-induced plasticity steel [J]. Corros. Sci., 2015, 93: 63 |
| [25] | Oudriss A, Creus J, Bouhattate J, et al. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel [J]. Acta Mater., 2012, 60: 6814 |
| [26] | Oudriss A, Creus J, Bouhattate J, et al. The diffusion and trapping of hydrogen along the grain boundaries in polycrystalline nickel [J]. Scr. Mater., 2012, 66: 37 |
| [27] | Du Y A, Ismer L, Rogal J, et al. First-principles study on the interaction of H interstitials with grain boundaries in α- and γ-Fe [J]. Phys. Rev., 2011, 84B: 144121 |
| [28] | Hutchinson B, Ridley N. On dislocation accumulation and work hardening in Hadfield steel [J]. Scr. Mater., 2006, 55: 299 |
| [29] | Idrissi H, Renard K, Ryelandt L, et al. On the mechanism of twin formation in Fe-Mn-C TWIP steels [J]. Acta Mater., 2010, 58: 2464 |
| [30] | Hermida J D, Roviglione A. Stacking fault energy decrease in austenitic stainless steels induced by hydrogen pairs formation [J]. Scr. Mater., 1998, 39: 1145 |
| [31] | Steinmetz D R, Japel T, Wietbrock B, et al. Revealing the strain-hardening behavior of twinning-induced plasticity steels: Theory, simulations, experiments [J]. Acta Mater., 2013, 61: 494 |
| [32] | Saeed-Akbari A, Mosecker L, Schwedt A, et al. Characterization and prediction of flow behavior in high-manganese twinning induced plasticity steels: Part I. Mechanism maps and work-hardening behavior [J]. Metall. Mater. Trans., 2012, 43A: 1688 |
| [33] | Idrissi H, Renard K, Schryvers D, et al. On the relationship between the twin internal structure and the work-hardening rate of TWIP steels [J]. Scr Mater., 2010, 63: 961 |
| [34] | Sevillano J G. Geometrically necessary twins and their associated size effects [J]. Scr. Mater., 2008, 59: 135 |
| [35] | Hong S, Lee J, Lee B J, et al. Effects of intergranular carbide precipitation on delayed fracture behavior in three twinning induced plasticity (TWIP) steels [J]. Mater. Sci. Eng., 2013, A587: 85 |
| [36] | Herbig M, Kuzmina M, Haase C, et al. Grain boundary segregation in Fe-Mn-C twinning-induced plasticity steels studied by correlative electron backscatter diffraction and atom probe tomography [J]. Acta Mater., 2015, 83: 37 |
| [37] | Hickel T, Sandl?bes S, Marceau R K W, et al. Impact of nanodiffusion on the stacking fault energy in high-strength steels [J]. Acta Mater., 2014, 75: 147 |
| [38] | Mahajan S, Chin G Y. Formation of deformation twins in f.c.c. crystals [J]. Acta Metall., 1973, 21: 1353 |
| [39] | Gutierrez-Urrutia I, Raabe D. Influence of Al content and precipitation state on the mechanical behavior of austenitic high-Mn low-density steels [J]. Scr. Mater., 2013, 68: 343 |
/
| 〈 |
|
〉 |