Anomalous Thermal Expansion Behavior of Cold-RolledTi-35Nb-2Zr-0.3O Alloy
Received date: 2018-07-25
Revised date: 2018-10-23
Online published: 2019-03-27
Supported by
Guangxi Natural Science Foundation(Nos.2018GXNSFAA138057);Guangxi Natural Science Foundation(2018JJA110055);Open Foundation of Guangxi Key Laboratory of Processing for Non-Ferrous Metals and Featured Materials, Guangxi University(Nos.GXYSOF1802);Open Foundation of Guangxi Key Laboratory of Processing for Non-Ferrous Metals and Featured Materials, Guangxi University(GXYSOF1810)
Thermal expansion behavior is one of the intrinsic properties of most materials, which is very difficult to control their thermal expansion behavior. Metallic material with ultra-low coefficient of thermal expansion named Invar effect was first found in Fe-Ni alloys. Recently, a multifunctional titanium alloy termed Gum metal (the typical composition is Ti-36Nb-2Ta-3Zr-0.3O, mass fraction, %; three electronic parameters: electron per atom ratio e/a≈4.24, bond order Bo≈2.87 and d electron orbital energy level Md≈2.45 eV) has been developed, and the alloy exhibits Invar effect after severe cold working. It is well known that the Invar effect of Fe-Ni alloys is related to the magnetic transition. However, titanium and its alloys are paramagnetic, and thus this mechanism cannot be used to explain Invar effect of Gum metal. In addition, the Invar effect of Gum metal is related to a dislocation-free plastic deformation mechanism. So far, there is still some controversy about this mechanism. In this study, a new β-type Ti-Nb base alloy Ti-35Nb-2Zr-0.3O (mass fraction, %) was developed whose three electronic parameters are different from those of the above mentioned Gum metal. The alloy was melted under high-purity argon atmosphere in an electric arc furnace, and the effects of cold rolling on microstructures and thermal expansion behaviors were characterized by OM, XRD, SEM, TEM and thermal mechanical analyzer (TMA). Results showed that the stress-induced martensitic α" (SIM α") phase transformation occurs after cold rolling, and the dominant <110> texture forms after severe plastic deformation. The equiaxed grains of Ti-35Nb-2Zr-0.3O alloy exhibit ordinary positive thermal expansion behavior and the thermal expansion rate increases with the increase of temperature. After cold deformation, negative thermal expansion occurs along rolling direction, and normal thermal expansion higher than solution treated sample occurs along transverse direction. The abnormal thermal expansion extent of the alloy increases with the increase of deformation reduction. The 30% cold deformed alloy along rolling direction possesses Invar effect between room temperature to 250 ℃, which is possibly related to SIM α" phase transformation, lattice distortion and <110> texture formation. The anomalous thermal expansion of the cold deformed samples in a temperature range from 25 ℃ to 110 ℃ is attributed to the lattice transition of SIM α" to β phase, while above 110 ℃ is attributed to the precipitation of ω and α phases.
Chunbo LAN , Jianeng LIANG , Yuanxia LAO , Dengfeng TAN , Chunyan HUANG , Xianzhong MO , Jinying PANG . Anomalous Thermal Expansion Behavior of Cold-RolledTi-35Nb-2Zr-0.3O Alloy[J]. Acta Metall Sin, 2019 , 55(6) : 701 -708 . DOI: 10.11900/0412.1961.2018.00347
| [1] | Kainuma R, Wang J J, Omori T, et al. Invar-type effect induced by cold-rolling deformation in shape memory alloys [J]. Appl. Phys. Lett., 2002, 80: 4348 |
| [2] | Nakai M, Niinomi M, Akahori T, et al. Anomalous thermal expansion of cold-rolled Ti-Nb-Ta-Zr alloy [J]. Mater. Trans., 2009, 50: 423 |
| [3] | Guillaume C E. The anomaly of the nickel-steels [J]. Proc. Phys. Soc. London, 1920, 32: 374 |
| [4] | Li X F, Chen N N, Li J J, et al. Effect of temperature and strain rate on deformation behavior of Invar 36 alloy [J]. Acta. Metall. Sin., 2017, 53: 968 |
| [4] | (李细锋, 陈楠楠, 李佼佼等. 温度与应变速率对Invar 36合金变形行为的影响 [J]. 金属学报, 2017, 53: 968) |
| [5] | Abdel-Hady M, Morinaga M. Controlling the thermal expansion of Ti alloys [J]. Scr. Mater., 2009, 61: 825 |
| [6] | Chen J, Hu L, Deng J X, et al. Negative thermal expansion in functional materials: Controllable thermal expansion by chemical modifications [J]. Chem. Soc. Rev., 2015, 44: 3522 |
| [7] | Liu X N, Lin K, Gao Q L, et al. Structure and phase transformation in the giant magnetostriction laves-phase SmFe2 [J]. Inorg. Chem., 2017, 57: 689 |
| [8] | Song Y Z, Chen J, Liu X Z, et al. Zero thermal expansion in magnetic and metallic Tb(Co,Fe)2 intermetallic compounds [J]. J. Am. Chem. Soc., 2018, 140: 602 |
| [9] | Kuramoto S, Furuta T, Hwang J H, et al. Plastic deformation in a multifunctional Ti-Nb-Ta-Zr-O alloy [J]. Metall. Mater. Trans., 2006, 37A: 657 |
| [10] | Furuta T, Kuramoto S, Chen R, et al. Effect of oxygen on phase stability and elastic deformation behavior in Gum metal [J]. J. Jpn. Inst. Met., 2006, 70: 579 |
| [11] | Wang W, Huang R, Zhao Y, et al. Adjustable zero thermal expansion in Ti alloys at cryogenic temperature [J]. J. Alloys Compd., 2018, 740: 47 |
| [12] | Saito T, Furuta T, Hwang J H, et al. Multifunctional alloys obtained via a dislocation-free plastic deformation mechanism [J]. Science, 2003, 300: 464 |
| [13] | Xing H, Guo W Y, Sun J. Substructure of recovered Ti-23Nb-0.7Ta-22r-O alloy [J]. Trans. Nonferrous Met. Soc. China, 2007, 17: 1456 |
| [14] | Talling R J, Dashwood R J, Jackson M, et al. On the mechanism of superelasticity in Gum metal [J]. Acta Mater., 2009, 57: 1188 |
| [15] | Talling R J, Dashwood R J, Jackson M, et al. Compositional variability in Gum metal [J]. Scr. Mater., 2009, 60: 1000 |
| [16] | Besse M, Castany P, Gloriant T. Mechanisms of deformation in Gum metal TNTZ-O and TNTZ titanium alloys: A comparative study on the oxygen influence [J]. Acta Mater., 2011, 59: 5982 |
| [17] | Yang Y, Li G P, Cheng G M, et al. Multiple deformation mechanisms of Ti-22.4Nb-0.73Ta-2.0Zr-1.34O alloy [J]. Appl. Phys. Lett., 2009, 94: 061901 |
| [18] | Kim H Y, Wei L S, Kobayashi S, et al. Nanodomain structure and its effect on abnormal thermal expansion behavior of a Ti-23Nb-2Zr-0.7Ta-1.2O alloy [J]. Acta Mater., 2013, 61: 4874 |
| [19] | Gutkin M Y, Ishizaki T, Kuramoto S, et al. Nanodisturbances in deformed Gum metal [J]. Acta Mater., 2006, 54: 2489 |
| [20] | Wei L S, Kim H Y, Miyazaki S. Effects of oxygen concentration and phase stability on nano-domain structure and thermal expansion behavior of Ti-Nb-Zr-Ta-O alloys [J]. Acta Mater., 2015, 100: 313 |
| [21] | Lan C B, Li G, Wu Y, et al. Effects of cold deformation on microstructure and mechanical properties of Ti-35Nb-2Zr-0.3O alloy for biomedical applications [J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 1537 |
| [22] | Lan C B, Wu Y, Chen F. Effects of cold rolling on microstructure and anomalous thermal expansion behaviors of Ti-35Nb-2Zr-0.3O alloy [J]. Key Eng. Mater., 2017, 729: 46 |
| [23] | Guo W, Quadir M Z, Ferry M. The mode of deformation in a cold-swaged multifunctional Ti-Nb-Ta-Zr-O alloy [J]. Metall. Mater. Trans., 2013, 44A: 2307 |
| [24] | J W Jr Morris, Hanlumyuang Y, Sherburne M, et al. Anomalous transformation-induced deformation in <110> textured Gum metal [J]. Acta Mater., 2010, 58: 3271 |
| [25] | Lan C B, Wu Y, Guo L L, et al. Microstructure, texture evolution and mechanical properties of cold rolled Ti-32.5Nb-6.8Zr-2.7Sn biomedical beta titanium alloy [J]. J. Mater. Sci. Technol., 2018, 34: 788 |
| [26] | Lan C B, Wu Y, Guo L L, et al. Effects of cold rolling on microstructure, texture evolution and mechanical properties of Ti-32.5Nb-6.8Zr-2.7Sn-0.3O alloy for biomedical applications [J]. Mater. Sci. Eng., 2017, A690: 170 |
| [27] | Hwang J, Kuramoto S, Furuta T, et al. Phase-stability dependence of plastic deformation behavior in Ti-Nb-Ta-Zr-O alloys [J]. J. Mater. Eng. Perform., 2005, 14: 747 |
| [28] | Wei Q Q, Wang L Q, Fu Y F, et al. Influence of oxygen content on microstructure and mechanical properties of Ti-Nb-Ta-Zr alloy [J]. Mater. Des., 2011, 32: 2934 |
| [29] | Wang Y, Gao J H, Wu H J, et al. Strain glass transition in a multifunctional β-type Ti alloy [J]. Sci. Rep., 2015, 4: 3995 |
| [30] | Kim H Y, Sasaki T, Okutsu K, et al. Texture and shape memory behavior of Ti-22Nb-6Ta alloy [J]. Acta Mater., 2006, 54: 423 |
| [31] | Afonso C R M, Ferrandini P L, Ramirez A J, et al. High resolution transmission electron microscopy study of the hardening mechanism through phase separation in a β-Ti-35Nb-7Zr-5Ta alloy for implant applications [J]. Acta Biomater., 2010, 6: 1625 |
| [32] | Málek J, Hnilica F, Vesely J, et al. The influence of chemical composition and thermo-mechanical treatment on Ti-Nb-Ta-Zr alloys [J]. Mater. Des., 2012, 35: 731 |
| [33] | Guo Q H, Zhan Y Z, Mo H L, et al. Aging response of the Ti-Nb system biomaterials with β-stabilizing elements [J]. Mater. Des., 2010, 31: 4842 |
| [34] | Ferrandini P L, Cardoso F F, Souza S A, et al. Aging response of the Ti-35Nb-7Zr-5Ta and Ti-35Nb-7Ta alloys [J]. J. Alloys Compd., 2007, 433: 207 |
| [35] | Guo W Y, Li J, Sun J. Thermal expansion behavior of Ti-23Nb-0.7Ta-2Zr-O alloy [J]. Mater Res. Appl., 2010, 4: 169 |
| [35] | (郭文渊, 李 俊, 孙 坚. Ti-23Nb-0.7Ta-2Zr-O合金的热膨胀行为 [J]. 材料研究与应用, 2010, 4: 169) |
/
| 〈 |
|
〉 |