Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel
Received date: 2018-12-07
Revised date: 2019-01-17
Online published: 2019-03-04
Supported by
National Natural Science Foundation of China and Baowu Steel Group Co., Ltd.(U1660205)
Low-cost ferritic stainless steels with excellent oxidation resistance and anti-corrosion ability are widely used in the fields of household appliances, hardware decoration, architectural structures, fuel cells and automobile exhaust systems. In order to achieve good formability of the ferritic stainless steel, the annealing process of hot-rolled sheet is crucial. As a newly developed 444-type heat-resistant ferritic stainless steel containing W and Ce, however, the influence of hot band annealing process of 19Cr2Mo1W ferritic stainless steel on its formability is not clear and need to have a deep understanding. In this work, the effect of annealing temperature of hot band on the microstructure, texture and formability of this steel was studied by means of XRD, EBSD, roughness measurement and formability test. The results indicated that although annealing processes were carried out at different temperatures after hot rolling, the characteristic of texture in the hot-rolled and annealed sheet was inherited to the cold-rolled sheet to some extent. The increased intensities of {223}<1
Houlong LIU , Mingyu MA , Lingling LIU , Liangliang WEI , Liqing CHEN . Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. Acta Metall Sin, 2019 , 55(5) : 566 -574 . DOI: 10.11900/0412.1961.2018.00540
| [1] | WeiX, DongJ H, TongJ, et al. Influence of temperature on pitting corrosion resistance of Cr26Mo1 ultra pure high chromium ferrite stainless steel in 3.5% NaCl solution[J]. Acta Metall. Sin., 2012, 48: 502 |
| [1] | (魏 欣, 董俊华, 佟 健等. 温度对Cr26Mo1超纯高铬铁素体不锈钢在3.5%NaCl溶液中耐点蚀性能的影响 [J]. 金属学报, 2012, 48: 502) |
| [2] | MalitckiiE, YagodzinskyyY, LehtoP, et al. Hydrogen effects on mechanical properties of 18%Cr ferritic stainless steel[J]. Mater. Sci. Eng., 2017, A700: 331 |
| [3] | GaoF, LiuZ Y, ZhangW N, et al. Textures and precipitates in a 17Cr% ferritic stainless steel[J]. Acta Metall. Sin., 2012, 48: 1166 |
| [3] | (高 飞, 刘振宇, 张维娜等. 17Cr%铁素体不锈钢中的第二相与织构 [J]. 金属学报, 2012, 48: 1166) |
| [4] | LiuJ, LuoX H, HuX Q, et al. Effect of Ti and Nb micro-alloying on the microstructure of the ultra-purified 11%Cr ferrite stainless steels[J]. Acta Metall. Sin., 2011, 47: 688 |
| [4] | (刘 静, 罗兴宏, 胡小强等. Ti和Nb微合金化对超纯11%Cr铁素体不锈钢组织的影响 [J]. 金属学报, 2011, 47: 688) |
| [5] | WeiL L, ChenL Q, MaM Y, et al. Oxidation behavior of ferritic stainless steels in simulated automotive exhaust gas containing 5 vol. % water vapor[J]. Mater. Chem. Phys., 2018, 205: 508 |
| [6] | WeiL L, ZhengJ H, ChenL Q, et al. High temperature oxidation behavior of ferritic stainless steel containing W and Ce[J]. Corros. Sci., 2018, 142: 79 |
| [7] | MaM Y, HeC L, ChenL Q, et al. Effect of W and Ce additions on the electrochemical corrosion behaviour of 444-type ferritic stainless steel[J]. Corros. Eng. Sci. Technol., 2018, 53: 199 |
| [8] | LiuH T, LiuZ Y, WangG D. Effect of annealing after hot rolling on formability of ultra-purified Cr17 steel[J]. Mater. Sci. Technol., 2011, 19(3): 19 |
| [8] | (刘海涛, 刘振宇, 王国栋. 热轧后退火对超纯Cr17钢成形性能的影响 [J]. 材料科学与工艺, 2011, 19(3): 19) |
| [9] | MaX G, ZhaoJ W, DuW, et al. Effects of rolling processes on ridging generation of ferritic stainless steel[J]. Mater. Charact., 2018, 137: 201 |
| [10] | De AbreuH F G, BrunoA D S, TavaresS S M, et al. Effect of high temperature annealing on texture and microstructure on an AISI-444 ferritic stainless steel[J]. Mater. Charact., 2006, 57: 342 |
| [11] | HuhM Y, EnglerO. Effect of intermediate annealing on texture, formability and ridging of 17%Cr ferritic stainless steel sheet[J]. Mater. Sci. Eng., 2001, A308: 74 |
| [12] | HongS H, LeeD N. Recrystallization textures in cold-rolled Ti bearing IF steel sheet[J]. ISIJ Int., 2002, 42: 1278 |
| [13] | RayR K, JonasJ J, HookR E. Cold rolling and annealing textures in low carbon and extra low carbon steels[J]. Int. Mater. Rev., 1994, 39: 129 |
| [14] | CaiG J, LiC S, WangD G, et al. Investigation of annealing temperature on microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel[J]. Mater. Charact., 2018, 141: 169 |
| [15] | ZhangC, ZhaoA M, DingR, et al. Effect of annealing temperature on formability of Cr17 ferritic stainless steel[J].Heat Treat. Metal., 2015, 40(4): 113 |
| [15] | (张 聪, 赵爱民, 丁 然等. 退火温度对Cr17铁素体不锈钢成形性能的影响 [J]. 金属热处理, 2015, 40(4): 113) |
| [16] | GhoshP, ChromikR R, VasheghiB, et al. Effect of crystallographic texture on the bulk magnetic properties of non-oriented electrical steels[J]. J. Magn. Magn. Mater., 2014, 365: 14 |
| [17] | GaoF, LiuZ Y, LiuH T, et al. Texture evolution and formability under different hot rolling conditions in ultra purified 17%Cr ferritic stainless steels[J]. Mater. Charact., 2013, 75: 93 |
| [18] | InagakiH. Fundamental aspect of texture format ion in low carbon steel[J]. ISIJ Int., 1994, 34: 313 |
| [19] | DuW, JiangL Z, SunQ S, et al. Effect of hot band annealing processes on microstructure, texture and r-value of ferritic stainless steel[J]. J. Iron Steel Res. Int., 2010, 17: 58 |
| [20] | GaoF, LiuZ Y, LiuH T, et al. Evolution of through-thickness texture in ultra purified 17% Cr ferritic stainless steels[J]. J. Iron Steel Res. Int., 2013, 20: 31 |
| [21] | DanielD, JonasJ J. Measurement and prediction of plastic anisotropy in deep-drawing steels[J]. Metall. Mater. Trans., 1990, 21A: 331 |
| [22] | LiuH T, LiuZ Y, WangG D. Texture development and formability of strip cast 17% Cr ferritic stainless steel[J]. ISIJ Int., 2009, 49: 890 |
| [23] | DuW, Y, JiangL Z, SunQ S, et al. Microstructure, texture, and formability of Nb+Ti stabilized high purity ferritic stainless steel[J]. J. Iron Steel Res. Int., 2010, 17: 47 |
| [24] | ShinH J, AnJ K, ParkS H, et al. The effect of texture on ridging of ferritic stainless steel[J]. Acta Mater., 2003, 51: 4693 |
| [25] | MaX G, ZhaoJ W, DuW, et al. An analysis of ridging of ferritic stainless steel 430[J]. Mater. Sci. Eng., 2017, A685: 358 |
/
| 〈 |
|
〉 |