Solidification of Al-Bi Alloy and Influence of Microalloying Element Sn

  • Wang LI ,
  • Qian SUN ,
  • Hongxiang JIANG ,
  • Jiuzhou ZHAO
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2. School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China

Received date: 2018-09-25

  Revised date: 2019-01-21

  Online published: 2019-02-26

Supported by

National Natural Science Foundation of China(Nos.51471173);National Natural Science Foundation of China(51771210);National Natural Science Foundation of China(51501207);National Natural Science Foundation of China(China Manned Space Engineering Project)

Abstract

Al-Bi alloy has a low friction coefficient and high wear-resistant properties and is a good self-lubricating material for advanced bearings in automotive applications if the soft Bi-rich phase is dispersedly distributed in the comparatively harder Al-based matrix. However, Al-Bi alloy is a typical immiscible alloy. When cooling a homogeneous single phase liquid of Al-Bi alloy in the miscibility gap, it transforms into two liquids. The liquid-liquid phase transformation generally leads to the formation of a phase segregated microstructure. In the last decades, considerable efforts have been made to study the solidification behavior of Al-Bi alloy. It is demonstrated that the microstructure evolution during the liquid-liquid decomposition is a result of concurrent actions of the nucleation, growth, Ostwald ripening and motions of the Bi-rich droplets. The nucleation and the immigration of the Bi-rich droplets show a dominant influence on the solidification microstructure of Al-Bi alloy. Enhancing the nucleation rate and reducing the Marangoni migration velocity of the Bi-rich droplets promote the formation of a well dispersed microstructure. Considering that addition of surface active element to the alloy may result in a reduction in the liquid-liquid interface energy, and thus reduce the nucleation energy barrier and Marangoni migration velocity of the Bi-rich droplets, the possibility to control the solidification process and microstructure of Al-Bi alloys by adding micro-alloying element Sn was investigated. The experimental results show that microalloying element Sn can cause an effective refinement of the Bi-rich particles. The refining effect increases with the increase of Bi content up to 0.10%Sn (mass fraciton). A model was developed to calculate the microstructure formation. The numerical results demonstrate that Sn can act as an effective surface active element for Al-Bi alloys and promote the formation of a well dispersed microstructure.

Cite this article

Wang LI , Qian SUN , Hongxiang JIANG , Jiuzhou ZHAO . Solidification of Al-Bi Alloy and Influence of Microalloying Element Sn[J]. Acta Metall Sin, 2019 , 55(7) : 831 -839 . DOI: 10.11900/0412.1961.2018.00450

References

[1] Freitas E S, Silva A P, Spinelli J E, et al. Inter-relation of microstructural features and dry sliding wear behavior of monotectic Al-Bi and Al-Pb alloys [J]. Tribol. Lett., 2014, 55: 111
[2] Ratke L, Diefenbach S. Liquid immiscible alloys [J]. Mater. Sci. Eng., 1995, R15: 263
[3] Zhao J Z, Jiang H X, Sun Q, et al. Progress of research on solidification process and microstructure control of immiscible alloys [J]. Mater. China, 2017, 36: 252
[3] (赵九洲, 江鸿翔, 孙 倩等. 偏晶合金凝固过程及凝固组织控制方法研究进展 [J]. 中国材料进展, 2017, 36: 252)
[4] Zhao J Z, Jiang H X. Progress in the solidification of monotectic alloys [J]. Acta Metall. Sin., 2018, 54: 682
[4] (赵九洲, 江鸿翔. 偏晶合金凝固过程研究进展 [J]. 金属学报, 2018, 54: 682)
[5] Lu W Q, Zhang S G, Zhang W, et al. A full view of the segregation evolution in Al-Bi immiscible alloy [J]. Metall. Mater. Trans., 2017, 48A: 2701
[6] Lu W Q, Zhang S G, Zhang W, et al. Direct observation of the segregation driven by bubble evolution and liquid phase separation in Al-10 wt.% Bi immiscible alloy [J]. Scr. Mater., 2015, 102: 19
[7] Lu W Q, Zhang S G, Li J G. Segregation driven by collision and coagulation of minor droplets in Al-Bi immiscible alloys under aerodynamic levitation condition [J]. Mater. Lett., 2013, 107: 340
[8] Silva A P, Spinelli J E, Mangelinck-No?l N, et al. Microstructural development during transient directional solidification of hypermonotectic Al-Bi alloys [J]. Mater. Des., 2010, 31: 4584
[9] Jia P, Zhang J Y, Geng H R, et al. High-efficiency inhibition of gravity segregation in Al-Bi immiscible alloys by adding Lanthanum [J]. Met. Mater. Int., 2018, 24: 1262
[10] Man T N, Zhang L, Xu N K, et al. Effect of rare-earth Ce on macrosegregation in Al-Bi immiscible alloys [J]. Metals, 2016, 6: 177
[11] Silva A P, Spinelli J E, Garcia A. Microstructural evolution during upward and downward transient directional solidification of hypomonotectic and monotectic Al-Bi alloys [J]. J. Alloys Compd., 2009, 480: 485
[12] Zha M, Li Y J, Mathiesen R H, et al. Dispersion of soft Bi particles and grain refinement of matrix in an Al-Bi alloy by equal channel angular pressing [J]. J. Alloys Compd., 2014, 605: 131
[13] Kang Z Q, Zhang Y B, Yang X, et al. Distribution law of rich Bi phase in Al-Bi monotectic alloy during the solidification process [J]. Mater. Rev., 2018, 32: 598
[13] (康智强, 张煜博, 杨 雪等. Al-Bi过偏晶合金凝固过程中富Bi相分布规律研究 [J]. 材料导报, 2018, 32: 598)
[14] Wu Y Q, Li C J. Investigation of the phase separation of Al-Bi immiscible alloy melts by viscosity measurements [J]. J. Appl. Phys., 2012, 111: 073521
[15] Zhang H W, Xian A P. Study of Al-Bi immiscible alloy controlcasting technique [J]. Acta Metall. Sin., 1999, 35: 1187
[15] (张宏闻, 冼爱平. Al-Bi偏晶合金的控制铸造技术探索 [J]. 金属学报, 1999, 35: 1187)
[16] He J, Zhao J Z, Wang X F, et al. An experimental study of the rapid continuous solidification of Al-Bi immiscible alloy [J]. Acta Metall. Sin., 2006, 42: 67
[16] (何 杰, 赵九洲, 王晓峰等. Al-Bi难混溶合金快速连续凝固的实验研究 [J]. 金属学报, 2006, 42: 67)
[17] Phanikumar G, Dutta P, Galun R, et al. Microstructural evolution during remelting of laser surface alloyed hyper-monotectic Al-Bi alloy [J]. Mater. Sci. Eng., 2004, A371: 91
[18] Zhang H W, Xian A P. Effect of the third element on the structure of casting Al-Bi immiscible alloys [J]. Acta Metall. Sin., 2000, 36: 347
[18] (张宏闻, 冼爱平. 第三组元对Al-Bi偏晶合金凝固组织的影响 [J]. 金属学报, 2000, 36: 347)
[19] Silva A P, Spinelli J E, Garcia A. Thermal parameters and microstructure during transient directional solidification of a monotectic Al-Bi alloy [J]. J. Alloys Compd., 2009, 475: 347
[20] He J, Zhao J Z, Wang X F, et al. Investigation of rapid directional solidification of Al-based immiscible alloys Ⅲ. Effect of the third element [J]. Acta Metall. Sin., 2007, 43: 573
[20] (何 杰, 赵九洲, 王晓峰等. Al基难混溶合金快速定向凝固研究Ⅲ. 第三组元的影响 [J]. 金属学报, 2007, 43: 573)
[21] Zhu J, Wang T M, Cao F, et al. Real-time observation on evolution of droplets morphology affected by electric current pulse in Al-Bi immiscible alloy [J]. J. Mater. Eng. Perform., 2013, 22: 1319
[22] He J, Zhao J Z, Wang X F, et al. Investigation of rapid directional solidification of Al-based immiscible alloys Ⅱ. Effect of static magnetic field [J]. Acta Metall. Sin., 2007, 43: 567
[22] (何 杰, 赵九洲, 王晓峰等. Al基难混溶合金快速定向凝固研究Ⅱ. 恒定磁场的影响 [J]. 金属学报, 2007, 43: 567)
[23] Huang Q, Luo X H, Li Y Y. An alloy solidification experiment conducted on Shenzhou spacecraft [J]. Adv. Space Res., 2005, 36: 86
[24] Yang Z Z, Sun Q, Zhao J Z. Directional solidification of monotectic composition Al-Bi alloy [J]. Acta Metall. Sin., 2014, 50: 25
[24] (杨志增, 孙 倩, 赵九洲. Al-Bi偏晶点成分合金定向凝固过程研究 [J]. 金属学报, 2014, 50: 25)
[25] Lu W Q, Zhang S G, Hu Q D, et al. Interaction between L2 droplets and L1/L interface in solidifying Al-Bi immiscible alloy [J]. Mater. Lett., 2016, 182: 351
[26] Sun Q, Jiang H X, Zhao J Z, et al. Microstructure evolution during the liquid-liquid phase transformation of Al-Bi alloys under the effect of TiC particles [J]. Acta Mater., 2017, 129: 321
[27] Zhao J Z, Ratke L. A model describing the microstructure evolution during a cooling of immiscible alloys in the miscibility gap [J]. Scr. Mater., 2004, 50: 543
[28] Zhao J Z, Li H L, Zhang X F, et al. Nucleation determined microstructure formation in immiscible alloys [J]. Mater. Lett., 2008, 62: 3779
[29] Wu M H, Ludwig A, Ratke L. Modeling of marangoni-induced droplet motion and melt convection during solidification of hypermonotectic alloys [J]. Metall. Mater. Trans., 2003, 34A: 3009
[30] Sun Q, Jiang H X, Zhao J Z. Effect of micro-alloying element Bi on solidification and microstructure of Al-Pb alloy [J]. Acta Metall. Sin., 2016, 52: 497
[30] (孙 倩, 江鸿翔, 赵九洲. 微量元素Bi对Al-Pb合金凝固过程及显微组织的影响 [J]. 金属学报, 2016, 52: 497)
[31] Wang C P, Liu X J, Ohnuma I, et al. Formation of immiscible alloy powders with egg-type microstructure [J]. Science, 2002, 297: 990
[32] Li H L, Zhao J Z, Zhang Q X, et al. Microstructure formation in a directionally solidified immiscible alloy [J]. Metall. Mater. Trans., 2008, 39A: 3308
[33] Zhao L, Zhao J Z. Microstructure formation in a gas-atomized drop of Al-Pb-Sn immiscible alloy [J]. Metall. Mater. Trans., 2012, 43A: 5019
[34] Christian J W. The Theory of Transformations in Metals and Alloys [M]. Amsterdam: Pergamon Press Ltd, 2002: 546
[35] Budai I, Benk? M Z, Kaptay G. Comparison of different theoretical models to experimental data on viscosity of binary liquid alloys [J]. Mater. Sci. Forum, 2007, 537-538: 489
[36] Kaptay G. A new theoretical equation for temperature dependent self-diffusion coefficients of pure liquid metals [J]. Int. J. Mat. Res., 2008, 99: 14
[37] Kaban I, K?hler M, Ratke L, et al. Interfacial tension, wetting and nucleation in Al-Bi and Al-Pb monotectic alloys [J]. Acta Mater., 2011, 59: 6880
[38] He J. Formation mechanism of microstructure in rapidly solidified immiscible alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2006
[38] (何 杰. 快速冷却条件下难混溶合金凝固组织形成机理 [D]. 沈阳: 中国科学院金属研究所, 2006)
[39] Yang S, Liu W J, Jia J. Directional solidification of Al-3.4wt%Bi monotectic alloy [J]. Prog. Nat. Sci., 2001, 11: 729
[39] (杨 森, 刘文今, 贾 均. Al-3.4wt%Bi偏晶合金定向凝固组织演变规律研究 [J]. 自然科学进展, 2001, 11: 729)
[40] Jin G. Surfactant Chemistry [M]. Hefei: University of Science and Technology of China Press, 2008: 59
[40] (金 谷. 表面活性剂化学 [M]. 合肥: 中国科学技术大学出版社, 2008: 59)
Outlines

/