Effect of Annealing on Microstructure of Thermally Aged 308L Stainless Steel Weld Metal
Received date: 2018-08-11
Revised date: 2018-12-04
Online published: 2018-12-17
Supported by
National Natural Science Foundation of China(51571204)
Austenitic stainless steel weld metal has been widely used as nozzle/safe-end joint and inner surface cladding of reactor pressure vessel, due to its good mechanical property and corrosion resistance. However, long-term thermal ageing at the service temperature (280~330 ℃) could induce hardening and embrittlement of the weld metal. To recover the thermal ageing embrittlement, the annealing treatment has been proposed since the annealing could affect the ageing-induced microstructural changes such as spinodal decomposition and G-phase precipitation in ferrite. However, there is still an incomplete understanding as well as a lack of nanoscale investigation about the annealing effect on the microstructural change of the weld metal. In this work, 308L stainless steel weld metal was thermally aged at 410 ℃ for 7000 h, followed by an annealing treatment at 550 ℃ for 1 h. Since the weld metal has a dual-phase structure of austenite and δ-ferrite, the phase transformation of austenite and δ-ferrite as well as the element segregation at the δ-ferrite/austenite phase boundary were investigated by TEM and atom probe tomography. The results revealed that austenite was unaffected by annealing while the ageing-induced spinodal decomposition of δ-ferrite was completely recovered. In addition, the number density of G phase in δ-ferrite was significantly reduced following annealing. This indicates that austenite has a higher stability compared with δ-ferrite. As for the δ-ferrite/austenite phase boundary, thermal ageing induced the segregation of Ni, Mn and C at the phase boundary, while the contents of Cr, Si and P remained almost unchanged. Following the annealing treatment, the segregation of all elements was eliminated. Further, only a small quantity of Ni and Mn was enriched in austenite near the phase boundary. The results suggested that the microstructure of the annealed specimen was similar to that of the unaged specimen, indicating a good recovery of the microstructure by annealing.
Xiaodong LIN , Qunjia PENG , En-Hou HAN , Wei KE . Effect of Annealing on Microstructure of Thermally Aged 308L Stainless Steel Weld Metal[J]. Acta Metall Sin, 2019 , 55(5) : 555 -565 . DOI: 10.11900/0412.1961.2018.00365
| [1] | MaC, HanE H, PengQ J, et al. Effect of polishing process on corrosion behavior of 308L stainless steel in high temperature water[J]. Appl. Surf. Sci., 2018, 442: 423 |
| [2] | DeLongW T. Ferrite in austenitic stainless steel weld metal[J]. Weld. J., 1974, 53: 273s |
| [3] | RaoK P, KumarS P. Corrosion behavior of austenitic weld and clad metals in accelerated boiling acid tests simulating passive conditions[J]. Corrosion, 1986, 42: 1 |
| [4] | DongL J, HanE H, PengQ J, et al. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water[J]. Corros. Sci., 2017, 117: 1 |
| [5] | LeeJ S, KimI S, KasadaR, et al. Microstructural characteristics and embrittlement phenomena in neutron irradiated 309L stainless steel RPV clad[J]. J. Nucl. Mater., 2004, 326: 38 |
| [6] | ChungH M, LeaxT R. Embrittlement of laboratory and reactor aged CF3,CF8, and CF8M duplex stainless steels[J]. Mater. Sci. Technol., 1990, 6: 249 |
| [7] | LiS L, WangY L, WangX T, et al. G-phase precipitation in duplex stainless steels after long-term thermal aging: A high-resolution transmission electron microscopy study[J]. J. Nucl. Mater., 2014, 452: 382 |
| [8] | TakeuchiT, KamedaJ, NagaiY, et al. Study on microstructural changes in thermally-aged stainless steel weld-overlay cladding of nuclear reactor pressure vessels by atom probe tomography[J]. J. Nucl. Mater., 2011, 415: 198 |
| [9] | AlexanderK B, MillerM K, AlexanderD J, et al. Microscopical evaluation of low temperature aging of type 308 stainless steel weldments[J]. Mater. Sci. Technol., 1990, 6: 314 |
| [10] | DanoixF, AugerP, BlavetteD. Hardening of aged duplex stainless steels by spinodal decomposition[J]. Microsc. Microanal., 2004, 10: 349 |
| [11] | CaoX Y, ZhuP, DingX F, et al. An investigation on microstructure and mechanical property of thermally aged stainless steel weld overlay cladding[J]. J. Nucl. Mater., 2017, 486: 172 |
| [12] | TakeuchiT, KakuboY, MatsukawaY, et al. Effects of thermal aging on microstructure and hardness of stainless steel weld-overlay claddings of nuclear reactor pressure vessels[J]. J. Nucl. Mater., 2014, 452: 235 |
| [13] | JangH, HongS H, JangC, et al. The effects of reversion heat treatment on the recovery of thermal aging embrittlement of CF8M cast stainless steels[J]. Mater. Des., 2014, 56: 517 |
| [14] | LiS L, ZhangH L, WangY L, et al. Annealing induced recovery of long-term thermal aging embrittlement in a duplex stainless steel[J]. Mater. Sci. Eng., 2013, A564: 85 |
| [15] | MateoA, PalominoJ L, SalanN, et al. Mechanical evaluation of a reversion heat treatment for a duplex stainless steel thermally embrittled[A]. Proceedings of the 11th Biennial European Conference on Fracture[C]. Warley: Engineering Materials Advisory Services Ltd., 1996: 779 |
| [16] | BrooksJ A, ThompsonA W. Microstructural development and solidification cracking susceptibility of austenitic stainless steel welds[J]. Int. Mater. Rev., 1991, 36: 16 |
| [17] | LongC J, De LongW T. The ferrite content of austenitic stainless steel weld metal[J]. Weld. J., 1973, 52: 281S |
| [18] | NateshM, ShamanthV, RavishankarK S. Effect of reversion heat treatment on the mechanical properties of thermally embrittled UNS S32760 duplex stainless steel[J]. Mater. Sci. Forum, 2015, 830-831: 127 |
| [19] | ShamanthV, RavishankarK S. Dissolution of alpha-prime precipitates in thermally embrittled S2205-duplex steels during reversion-heat treatment[J]. Results Phys., 2015, 5: 297 |
| [20] | ChungH M. Aging and life prediction of cast duplex stainless steel components[J]. Int. J. Pres, Ves. Pip., 1992, 50: 179 |
| [21] | VitekJ M, DavidS A, AlexanderD J, et al. Low temperature aging behavior of type 308 stainless steel weld metal[J]. Acta Metall. Mater., 1991, 39: 503 |
| [22] | TakeuchiT, KamedaJ, NagaiY, et al. Microstructural changes of a thermally aged stainless steel submerged arc weld overlay cladding of nuclear reactor pressure vessels[J]. J. Nucl. Mater., 2012, 425: 60 |
| [23] | LachT G, ByunT S, LeonardK J, Mechanical property degradation and microstructural evolution of cast austenitic stainless steels under short-term thermal aging [J]. J. Nucl. Mater., 2017, 497: 139 |
| [24] | ZhangB, XueF, LiS L, et al. Non-uniform phase separation in ferrite of a duplex stainless steel[J]. Acta Mater., 2017, 140: 388 |
| [25] | BruemmerS M. Grain boundary composition and effects on environmental degradation[A]. 9th International Conference on Intergranular and Interphase Boundaries in Materials[C]. Zurich-Uetikon: Transtec Publications Ltd., 1999: 75 |
| [26] | JiaoZ J, WasG S. Novel features of radiation-induced segregation and radiation-induced precipitation in austenitic stainless steels[J]. Acta Mater., 2011, 59: 1220 |
| [27] | HallR N. Variation of the distribution coefficient and solid solubility with temperature[J]. J. Phys. Chem. Solids, 1957, 3: 63 |
| [28] | AugerP, DanoixF, MenandA, et al. Atom probe and transmission electron microscopy study of aging of cast duplex stainless steels[J]. Mater. Sci. Technol., 1990, 6: 301 |
| [29] | StrangwoodM, DruceS G. Aging effects in welded cast CF3 stainless steel[J]. Mater. Sci. Technol., 1990, 6: 237 |
| [30] | PumphreyP H, AkhurstK N. Aging kinetics of CF3 cast stainless steel in temperature range 300-400 ℃[J]. Mater. Sci. Technol., 2013, 6: 211 |
| [31] | YamadaT, OkanoS, KuwanoH. Mechanical property and microstructural change by thermal aging of SCS14A cast duplex stainless steel[J]. J. Nucl. Mater., 2006, 350: 47 |
| [32] | KawaguchiS, SakamotoN, TakanoG, et al. Microstructural changes and fracture behavior of CF8M duplex stainless steels after long-term aging[J]. Nucl. Eng. Des., 1997, 174: 273 |
| [33] | XuX, WestraadtJ E, OdqvistJ, et al. Effect of heat treatment above the miscibility gap on nanostructure formation due to spinodal decomposition in Fe-52.85at.%Cr[J]. Acta Mater., 2018, 145: 347 |
| [34] | DengP, PengQ J, HanE-H, et al. Study of irradiation damage in domestically fabricated nuclear grade stainless steel[J].Acta Metall. Sin., 2017, 53: 1588 |
| [34] | (邓 平, 彭群家, 韩恩厚等. 国产核用不锈钢辐照损伤研究 [J]. 金属学报, 2017, 53: 1588) |
| [35] | ThompsonK, LawrenceD, LarsonD J, et al. In situ site-specific specimen preparation for atom probe tomography[J]. Ultramicroscopy, 2007, 107: 131 |
| [36] | MillerM K, KenikE A. Atom probe tomography: A technique for nanoscale characterization[J]. Microsc. Microanal., 2004, 10: 336 |
| [37] | LiuW Q, LiuQ D, GuJ F. Development and application of atom probe tomography[J].Acta Metall. Sin., 2013, 49: 1025 |
| [37] | (刘文庆, 刘庆冬, 顾剑锋. 原子探针层析技术(APT)最新进展及应用 [J]. 金属学报, 2013, 49: 1025) |
| [38] | ChandraK, KainV, RajaV S, et al. Low temperature thermal ageing embrittlement of austenitic stainless steel welds and its electrochemical assessment[J]. Corros. Sci., 2012, 54: 278 |
| [39] | LiS L, WangY L, LiS X, et al. Microstructures and mechanical properties of cast austenite stainless steels after long-term thermal aging at low temperature[J]. Mater. Des., 2013, 50: 886 |
| [40] | DanoixF, AugerP. Atom probe studies of the Fe-Cr system and stainless steels aged at intermediate temperature: A review[J]. Mater. Charact., 2000, 44: 177 |
| [41] | LiS L, WangY L, ZhangH L, et al. Microstructure evolution and impact fracture behaviors of Z3CN20-09M stainless steels after long-term thermal aging[J]. J. Nucl. Mater., 2013, 433: 41 |
| [42] | ChandraD, SchwartzL H. M?ssbauer effect study of the 475 ℃ decomposition of Fe-Cr[J]. Metall. Trans., 1971, 2: 511 |
| [43] | MatsukawaY, TakeuchiT, KakuboY, et al. The two-step nucleation of G-phase in ferrite[J]. Acta Mater., 2016, 116: 104 |
| [44] | PareigeC, EmoJ, SailletS, et al. Kinetics of G-phase precipitation and spinodal decomposition in very long aged ferrite of a Mo-free duplex stainless steel[J]. J. Nucl. Mater., 2015, 465: 383 |
| [45] | DanoixF, AugerP, BlavetteD. An atom-probe investigation of some correlated phase transformations in Cr, Ni, Mo containing supersaturated ferrites[J]. Surf. Sci., 1992, 266: 364 |
| [46] | MateoA, LlanesL, AngladaM, et al. Characterization of the intermetallic G-phase in an AISI 329 duplex stainless steel[J]. J. Mater. Sci., 1997, 32: 4533 |
| [47] | HamaokaT, KonnoT J, SawabeT, et al. Effects of molybdenum on precipitation behaviours in aged cast stainless steels[J]. Philos. Mag., 2016, 96: 2518 |
| [48] | BabuS S, DavidS A, VitekJ M, et al. Atom probe field ion microscopy of type 308 CRE stainless steel welds[J]. Appl. Surf. Sci., 1995, 87-88: 207 |
| [49] | LiH, XiaS, LiuW Q, et al. Atomic scale study of grain boundary segregation before carbide nucleation in Ni-Cr-Fe alloys[J]. J. Nucl. Mater., 2013, 439: 57 |
| [50] | LiH, XiaS, ZhouB X, et al. C-Cr segregation at grain boundary before the carbide nucleation in alloy 690[J]. Mater. Charact., 2012, 66: 68 |
| [51] | JiaoZ J, HesterbergJ, WasG S. Effect of post-irradiation annealing on the irradiated microstructure of neutron-irradiated 304L stainless steel[J]. J. Nucl. Mater., 2018, 500: 220 |
| [52] | Bar'yakhtarV G, TimoshevskiiA N, SoolshenkoV K, et al. Influence of substitutional (Cr, Mn, Ni) and interstitial (C, N, O) impurities on the electronic structure and magnetic properties of α-Fe based alloys[J]. J. Magn. Magn. Mater., 1995, 140-144: 115 |
| [53] | BlanterM S, MagalasL B. Carbon-substitutional interaction in austenite[J]. Scr. Mater., 2000, 43: 435 |
| [54] | ChenQ, JeppssonJ, ?grenJ. Analytical treatment of diffusion during precipitate growth in multicomponent systems[J]. Acta Mater., 2008, 56: 1890 |
/
| 〈 |
|
〉 |