Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution
Received date: 2018-10-16
Revised date: 2018-12-03
Online published: 2018-12-13
Supported by
National Science and Technology Pillar Program during the Thirteenth Five-Year Plan Period(No.2016ZX05057)
Cl- and SO42- are most common aggressive ions containing in the seawater which may cause the localized corrosion of reinforcement structures. It is found that a protective passive film will form on the steel surface in the concrete pore solution. The localized breakdown of the passive film caused by the aggressive ions and the carbonation are the main reason for the localized corrosion initiation of reinforcements. In the previous studies, it is found that the performances of the SO42- on the rebar corrosion were quite different in different pH value conditions and the test results did not unify. Therefore, the influence of pH value and the SO42- on the corrosion behavior of Q235B carbon steel in the simulated pore solution was studied using anodic polarization, electrochemical impedance spectra (EIS), Mott-Schottky (M-S) and potentiostatic polarization methods. The anodic polarization curves indicate that when the pH value of the simulated pore solution was higher than 11, SO42- had no damage to the passive film. However, once the pH value of the simulated pore solution decreased to 10, a small amount of SO42- can lead to the breakdown of the passive film and induce pitting initiation. EIS and M-S measurement results suggest that the stability of the passive film would decrease with the decreasing of the solution pH. The concentration of the defect would increase in the passive film due to the pH decrease. The stability reduction and the increase of defect concentration both can lead to the passive film become fragile and more easily to be destroyed by SO42-. Through the potentiostatic polarization test in conjunction with SEM observation, it is found that SO42- can inhibit the growth of the passive film during the initial film formation period and lead to the appearance of metastable pitting corrosion under high pH value conditions. In the low pH value conditions, SO42- could accumulate at the defect of the passive film and lead to stable pitting propagate on the steel surface.
Key words: Q235B steel; passive film; SO42-; pitting corrosion
Kaiqiang LI , Lujia YANG , Yunze XU , Xiaona WANG , Yi HUANG . Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution[J]. Acta Metall Sin, 2019 , 55(4) : 457 -468 . DOI: 10.11900/0412.1961.2018.00475
| 1 | Cao Y H, Dong S G, Zheng D J, et al. Multifunctional inhibition based on layered double hydroxides to comprehensively control corrosion of carbon steel in concrete [J]. Corros. Sci., 2017, 126: 166 |
| 2 | Ales C, Kosec T, Legat A. Characterization of steel corrosion in mortar by various electrochemical and physical techniques [J]. Corros. Sci., 2013, 75: 47 |
| 3 | Valipour M, Shekarchi M, Ghods P. Comparative studies of experimental and numerical techniques in measurement of corrosion rate and time-to-corrosion-initiation of rebar in concrete in marine environments [J]. Cem. Concr. Compos., 2014, 48: 98 |
| 4 | Tan Y J. Experimental methods designed for measuring corrosion in highly resistive and inhomogeneous media [J]. Corros. Sci., 2011, 53: 1145. |
| 5 | Chakri S, Frateur I, Orazem M E, et al. Improved EIS analysis of the electrochemical behaviour of carbon steel in alkaline solution [J]. Electrochim. Acta, 2017, 246: 924. |
| 6 | Mundra S, Criado M, Bernal S A, et al. Chloride-induced corrosion of steel rebars in simulated pore solutions of alkali-activated concretes [J]. Cem. Concr. Res., 2017, 100: 385 |
| 7 | Qiao B, Du R G, Chen W, et al. Effect of NO2- and Cl- on the corrosion behavior of reinforcing steel in simulated concrete pore solutions [J]. Acta Metall. Sin., 2010, 46: 245 |
| 7 | 乔 冰, 杜荣归, 陈 雯等. NO2-和Cl-对模拟混凝土孔隙液中钢筋腐蚀行为的影响 [J]. 金属学报, 2010, 46: 245 |
| 8 | Kumar M P, Mini K M, Rangarajan M. Ultrafine GGBS and calcium nitrate as concrete admixtures for improved mechanical properties and corrosion resistance [J]. Constr. Build. Mater., 2018, 182: 249 |
| 9 | Angst U, Elsener B, Larsen C K, et al. Critical chloride content in reinforced concrete—A review [J]. Cem. Concr. Res., 2009, 39: 1122 |
| 10 | Ann K Y, Song H W. Chloride threshold level for corrosion of steel in concrete [J]. Corros. Sci., 2007, 49: 4113 |
| 11 | Jin Z Q, Zhao X, Zhao T J, et al. Effect of Ca(OH)2, NaCl, and Na2SO4 on the corrosion and electrochemical behavior of rebar [J]. Chin. J. Oceanol. Limnol., 2017, 35: 681 |
| 12 | Ghods P, Isgor O B, McRae G, et al. The effect of concrete pore solution composition on the quality of passive oxide films on black steel reinforcement [J]. Cem. Concr. Compos., 2009, 31: 2 |
| 13 | El Aal E E A, El Wanees S A, Diab A, et al. Environmental factors affecting the corrosion behavior of reinforcing steel III. Measurement of pitting corrosion currents of steel in Ca(OH)2 solutions under natural corrosion conditions [J]. Corros. Sci., 2009, 51: 1611 |
| 14 | El Haleem S M A, El Wanees S A, El Aal E E A, et al. Environmental factors affecting the corrosion behavior of reinforcing steel II. Role of some anions in the initiation and inhibition of pitting corrosion of steel in Ca(OH)2 solutions [J]. Corros. Sci., 2010, 52: 292 |
| 15 | El Haleem S M A, El Wanees S A, Bahgat A. Environmental factors affecting the corrosion behaviour of reinforcing steel. V. Role of chloride and sulphate ions in the corrosion of reinforcing steel in saturated Ca(OH)2 solutions [J]. Corros. Sci., 2013, 75: 1 |
| 16 | Liu G J, Zhang Y S, Ni Z W, et al. Corrosion behavior of steel submitted to chloride and sulphate ions in simulated concrete pore solution [J]. Constr. Build. Mater., 2016, 115: 1 |
| 17 | Al-Amoudi O S B, Maslehuddin M. The effect of chloride and sulfate ions on reinforcement corrosion [J]. Cem. Concr. Res., 1993, 23: 139 |
| 18 | Al-Amoudi O S B, Rasheeduzzafar A A, Maslehuddin M, et al. Influence of sulfate ions on chloride-induced reinforcement corrosion in Portland and blended cement concretes [J]. Cem. Concr. Aggreg., 1994, 16(1): 3 |
| 19 | Shaheen F, Pradhan B. Effect of chloride and conjoint chloride-sulfate ions on corrosion of reinforcing steel in electrolytic concrete powder solution (ECPS) [J]. Constr. Build. Mater., 2015, 101: 99 |
| 20 | Shaheen F, Pradhan B. Influence of sulfate ion and associated cation type on steel reinforcement corrosion in concrete powder aqueous solution in the presence of chloride ions [J]. Cem. Concr. Res., 2017, 91: 73 |
| 21 | Williamson J, Isgor O B. The effect of simulated concrete pore solution composition and chlorides on the electronic properties of passive films on carbon steel rebar [J]. Corros. Sci., 2016, 106: 82 |
| 22 | Yang L J, Xu Y Z, Zhu Y S, et al. Evaluation of interaction effect of sulfate and chloride ions on reinforcements in simulated marine environment using electrochemical methods [J]. Int. J. Electrochem. Sci., 2016, 52: 6943 |
| 23 | Xu Y Z, He L M, Yang L J, et al. Electrochemical study of steel corrosion in saturated calcium hydroxide solution with chloride ions and sulfate ions [J]. Corrosion, 2018, 74: 1063 |
| 24 | Vigneshwaran K K K, Permeh S, Echeverría M, et al. Corrosion of post-tensioned tendons with deficient grout, part 1: Electrochemical behavior of steel in alkaline sulfate solutions [J]. Corrosion, 2018, 74: 362 |
| 25 | Ai Z Y, Jiang J Y, Sun W, et al. Enhanced passivation of alloy corrosion-resistant steel Cr10Mo1 under carbonation—Passive film formation, the kinetics and mechanism analysis [J]. Cem. Concr. Compos., 2018, 92: 178 |
| 26 | Ai Z Y, Jiang J Y, Sun W, et al. Passive behaviour of alloy corrosion-resistant steel Cr10Mo1 in simulating concrete pore solutions with different pH [J]. Appl. Surf. Sci., 2016, 389: 1126 |
| 27 | Sánchez M, Gregori J, Alonso C, et al. Electrochemical impedance spectroscopy for studying passive layers on steel rebars immersed in alkaline solutions simulating concrete pores [J]. Electrochim. Acta, 2007, 52: 7634 |
| 28 | Chakri S, Frateur I, Orazem M E, et al. Improved EIS analysis of the electrochemical behaviour of carbon steel in alkaline solution [J]. Electrochim. Acta, 2017, 246: 924 |
| 29 | Saremi M, Mahallati E. A study on chloride-induced depassivation of mild steel in simulated concrete pore solution [J]. Cem. Concr. Res., 2002, 32: 1915 |
| 30 | Li Y, Cheng Y F. Passive film growth on carbon steel and its nanoscale features at various passivating potentials [J]. Appl. Surf. Sci., 2017, 396: 144 |
| 31 | Chen W, Du R G, Ye C Q, et al. Study on the corrosion behavior of reinforcing steel in simulated concrete pore solutions using in situ Raman spectroscopy assisted by electrochemical techniques [J]. Electrochim. Acta, 2010, 55: 5677 |
| 32 | Sato N. Anodic breakdown of passive films on metals [J]. J. Electrochem. Soc., 1982, 129: 255 |
| 33 | El Haleem S M A, El Aal E E A, El Wanees S A, et al. Environmental factors affecting the corrosion behaviour of reinforcing steel: I. The early stage of passive film formation in Ca(OH)2 solutions [J]. Corros. Sci., 2010, 52: 3875 |
| 34 | Freire L, Nóvoa X R, Montemor M F, et al. Study of passive films formed on mild steel in alkaline media by the application of anodic potentials [J]. Mater. Chem. Phys., 2009, 114: 962 |
| 35 | Morrison S R. Electrochemistry at semiconductor and oxidized metal electrodes [M]. New York: Plenum Press, 1980: 416 |
| 36 | MacDonald D D. The history of the point defect model for the passive state: A brief review of film growth aspects [J]. Electrochim. Acta, 2011, 56: 1761 |
| 37 | Dong Z H, Shi W, Guo X P. Initiation and repassivation of pitting corrosion of carbon steel in carbonated concrete pore solution [J]. Corros. Sci., 2011, 56: 5890 |
| 38 | Lu Y F, Dong J H, Ke W. Effects of SO42- on the corrosion behavior of NiCu Low alloy steel in deaerated bicarbonate solutions [J]. Acta Metall. Sin., 2015, 51: 1067 |
| 38 | 卢云飞, 董俊华, 柯 伟. SO42-对NiCu低合金钢在除氧NaHCO3溶液中腐蚀行为的影响 [J]. 金属学报, 2015, 51: 1067 |
| 39 | Niu L B, Nakada K. Effect of chloride and sulfate ions in simulated boiler water on pitting corrosion behavior of 13Cr steel [J]. Corros. Sci., 2015, 96: 171 |
| 40 | Kolics A, Polkinghorne J C, Wieckowski A. Adsorption of sulfate and chloride ions on aluminum [J]. Electrochim. Acta, 1998, 43: 2605 |
/
| 〈 |
|
〉 |