Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching
Received date: 2018-09-28
Online published: 2018-11-26
Supported by
Supported by National Natural Science Foundation of China (No.51231008)
Freestanding nanowires have ultrahigh elastic strain limits (4%~7%) and yield strengths, it is expected that composites reinforced by nanowires will have exceptional mechanical properties. However, the results obtained so far have been disappointing, primarily because the intrinsic mechanical properties of nanowires have not been successfully exploited in bulk composites. This is thought to be due to the inelastic strain incompatibilities at typical dislocation-piled-up interfaces. Therefore, we proposed a concept of elastic and transformation strain matching to realize the intrinsic mechanical properties of the nanowires. By creating a nanostructured composite consisting of nano Nb embedded in a NiTi matrix, the intrinsic mechanical properties of Nb nanowires, nano ribbons and nano particles are realized. Besides, this breakthrough triggers a new mechanism of stress coupling that induces the nanocomposite showing excellent mechanical properties. Based on the design strategy, we developed an in situ composite that possesses a large quasi-linear elastic strain of over 6%, a low Young's modulus of less than 28 GPa, and a high yield strength of 1.65 GPa.
Lishan CUI , Daqiang JIANG . Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching[J]. Acta Metall Sin, 2019 , 55(1) : 45 -58 . DOI: 10.11900/0412.1961.2018.00457
| [1] | Wong E W, Sheehan P E, Lieber C M.Nanobeam mechanics: Elasticity, strength, and toughness of nanorods and nanotubes[J]. Science, 1997, 277: 1971 |
| [2] | Zhu T, Li J.Ultra-strength materials[J]. Prog. Mater. Sci., 2010, 55: 710 |
| [3] | Yue Y H, Liu P, Zhang Z, et al.Approaching the theoretical elastic strain limit in copper nanowires[J]. Nano Lett., 2011, 11: 3151 |
| [4] | Koziol K, Vilatela J, Moisala A, et al.High-performance carbon nanotube fiber[J]. Science, 2007, 318: 1892 |
| [5] | Dzenis Y.Materials science: Structural nanocomposites[J]. Science, 2008, 319: 419 |
| [6] | Podsiadlo P, Kaushik A K, Arruda E M, et al.Ultrastrong and stiff layered polymer nanocomposites[J]. Science, 2007, 318: 80 |
| [7] | Coleman J N, Khan U, Gun'ko Y K. Mechanical reinforcement of polymers using carbon nanotubes[J]. Adv. Mater., 2006, 18: 689 |
| [8] | Thilly L, van Petegem S, Renault P O, et al. A new criterion for elasto-plastic transition in nanomaterials: Application to size and composite effects on Cu-Nb nanocomposite wires[J]. Acta Mater., 2009, 57: 3157 |
| [9] | Vidal V, Thilly L, van Petegem S, et al. Plasticity of nanostructured Cu-Nb-based wires: Strengthening mechanisms revealed by in situ deformation under neutrons[J]. Scr. Mater., 2009, 60: 171 |
| [10] | Ayd?ner C C, Brown D W, Mara N A, et al.In situ x-ray investigation of freestanding nanoscale Cu-Nb multilayers under tensile load[J]. Appl. Phys. Lett., 2009, 94: 031906 |
| [11] | Thilly L, Renault P O, Vidal V, et al.Plasticity of multiscale nanofilamentary Cu/Nb composite wires during in situ neutron diffraction: Codeformation and size effect[J]. Appl. Phys. Lett., 2006, 88: 191906 |
| [12] | Hao S J, Cui L S, Jiang D Q, et al.A transforming metal nanocomposite with large elastic strain, low modulus, and high strength[J]. Science, 2013, 339: 1191 |
| [13] | Wang S, Cui L, Hao S, et al.Locality and rapidity of the ultra-large elastic deformation of Nb nanowires in a NiTi phase-transforming matrix[J]. Sci. Rep., 2014, 4: 6753 |
| [14] | Liu Z Y.Study of structure and functional property of Nb/NiTi composite [D]. Beijing: China University of Petroleum, 2014(刘镇洋. Nb纳米线/NiTi记忆合金复合材料结构与功能特性研究 [D]. 北京: 中国石油大学(北京), 2014) |
| [15] | Zang K T, Mao S C, Cai J X, et al.Revealing ultralarge and localized elastic lattice strains in Nb nanowires embedded in NiTi matrix[J]. Sci. Rep., 2015, 5: 17530 |
| [16] | Hao S J, Cui L S, Wang H, et al.Retaining large and adjustable elastic strains of kilogram-scale Nb nanowires[J]. ACS Appl. Mater. Interfaces, 2016, 8: 2917 |
| [17] | Hao S J, Cui L S, Guo F M, et al.Achieving large linear elasticity and high strength in bulk nanocompsite via synergistic effect[J]. Sci. Rep., 2015, 5: 8892 |
| [18] | Hao S J, Cui L S, Jiang D Q, et al.Nanostructured Nb reinforced NiTi shape memory alloy composite with high strength and narrow hysteresis[J]. Appl. Phys. Lett., 2013, 102: 231905 |
| [19] | Zhang J S, Cui L S, Jiang D Q, et al.A biopolymer-like metal enabled hybrid material with exceptional mechanical prowess[J]. Sci. Rep., 2015, 5: 8357 |
| [20] | Hao S J, Liu Y N, Ren Y, et al.Achieving superior two-way actuation by the stress-coupling of nanoribbons and nanocrystalline shape memory alloy[J]. ACS Appl. Mater. Interfaces, 2016, 8: 16310 |
| [21] | Hao S J, Cui L S, Wang Y D, et al.The ultrahigh mechanical energy-absorption capability evidenced in a high-strength NbTi-NiTi nanocomposite[J]. Appl. Phys. Lett., 2011, 99: 024102 |
| [22] | Zhang J S, Liu Y N, Ren Y, et al.In situ synchrotron X-ray diffraction study of deformation behavior and load transfer in a Ti2Ni-NiTi composite[J]. Appl. Phys. Lett., 2014, 105: 041910 |
| [23] | Jiang D Q, Hao S J, Zhang J S, et al. In situ synchrotron investigation of the deformation behavior of nanolamellar Ti5Si3-TiNi composite [J]. Scr. Mater., 2014, 78-79: 53 |
| [24] | Zhang J S, Liu Y N, Huan Y, et al.High damping NiTi-Ti3Sn in situ composite with transformation-mediated plasticity[J]. Mater. Des., 2014, 63: 460 |
| [25] | Shao Y, Guo F M, Huan Y, et al.Fabrication, microstructure and mechanical properties of W-NiTi composites[J]. J Alloys Compd., 2017, 695: 1976 |
| [26] | Shao Y, Guo F M, Ren Y, et al.Tensile properties of a novel W-NiTi heavy alloy with transforming matrix[J]. Mater. Sci. Eng., 2017, A683: 103 |
| [27] | Shao Y, Yu K Y, Jiang D Q, et al.High strength W/TiNi micro-laminated composite with transformation-mediated ductility[J]. Mater. Des., 2016, 106: 415 |
| [28] | Du M S, Cui L S, Cao Y, et al.Mechanoelectrochemical catalysis of the effect of elastic strain on a platinum nanofilm for the ORR exerted by a shape memory alloy substrate[J]. J. Am. Chem. Soc., 2015, 137: 7397 |
| [29] | Feng C, Zhao J C, Yang F, et al.Nonvolatile modulation of electronic structure and correlative magnetism of L10-FePt films using significant strain induced by shape memory substrates[J]. Sci. Rep., 2016, 6: 20199 |
| [30] | Feng C, Zhao J C, Yang F, et al.Reversible and nonvolatile modulations of magnetization switching characteristic and domain configuration in L10-FePt films via nonelectrically controlled strain engineering[J]. ACS Appl. Mater. Interfaces, 2016, 8: 7545 |
| [31] | Du M S, Wan Q, Wang Z Q, et al.Elastic strain induced improvement in the photocatalytic activity of semiconducting film exerted by the surface relief of Fe-Ni-Co-Ti alloy substrate[J]. Mater. Lett., 2016, 168: 192 |
| [32] | Du M S, Cui L S, Wan Q.Tensile strain induced narrowed bandgap of TiO2 films: Utilizing the two-way shape memory effect of TiNiNb substrate and in-situ mechanical bending[J]. Mater. Sci. Eng., 2016, B207: 7 |
| [33] | Du M S, Wan Q, Wang Z Q, et al.Elastic strain effects on the photocatalytic TiO2 nanofilm: Utilizing the martensitic surface relief of FeNiCoTi alloy substrate[J]. Chem. Phys. Lett., 2016, 658: 130 |
/
| 〈 |
|
〉 |