Molecular Dynamics Simulation of the Structure and Deformation Behavior of γ/α2 Interface in TiAl Alloys
Received date: 2018-05-07
Online published: 2018-11-20
Supported by
Supported by National Key Research and Development Program of China (No.2016YFB0701304), National Natural Science Foundation of China (No.51671195), Aeronautical Science Foundation of China (No.20160292002), Youth Innovation Promotion Association of Chinese Academy of Sciences (No.2015151) and Special Project on Information Technology of Chinese Academy of Sciences (No.XXH13506-304)
TiAl alloys with γ-TiAl and α2-Ti3Al dual-phase lamellar structure possess not only excellent high temperature performance but also density only about half of traditional superalloys. Such lamellar structure largely determines the mechanical properties of TiAl alloys. However, there is still a lack of understanding on the atomic structure of lamella, as well as their influence on the mechanical behaviors. For this reason, molecular dynamics with an embedded-atom potential is employed to investigate the energies of both the coherent and semi-coherent γ/α2 interfaces. The interface coherency is found to depend on the thickness ratio of γ lamellae to α2 lamellae, and there exists a critical lamella thickness, below/above which the interface is coherent/semi-coherent. Tensile loading perpendicular to the lamella interface indicates that the yield strength of coherent interface is higher than that of semi-coherent interface and the crack nucleation behavior varies with the thickness ratio of γ lamellae to α2 lamellae. The plastic deformation occurs first in the γ region, forming Shockley partial dislocations and then crosses the γ/α2 interface via slip transfer, activating stacking faults on the pyramidal plane in the α2 region. In this process, the γ/α2 interface provides nucleation sites for subsequent dislocations and cracks.
Key words: TiAl; interface; plastic deformation; mechanical behavior; molecular dynamics
Aidong TU , Chunyu TENG , Hao WANG , Dongsheng XU , Yun FU , Zhanyong REN , Rui YANG . Molecular Dynamics Simulation of the Structure and Deformation Behavior of γ/α2 Interface in TiAl Alloys[J]. Acta Metall Sin, 2019 , 55(2) : 291 -298 . DOI: 10.11900/0412.1961.2018.00182
| [1] | Yang R.Advances and challenges of TiAl base alloys[J]. Acta Metall. Sin., 2015, 51: 129(杨锐. 钛铝金属间化合物的进展与挑战[J]. 金属学报, 2015, 51: 129) |
| [2] | Froes F H, Suryanarayana C, Eliezer D.Synthesis, properties and applications of titanium aluminides[J]. J. Mater. Sci., 1992, 27: 5113 |
| [3] | Clemens H, Kestler H.Processing and applications of intermetallic γ-TiAl-based alloys[J]. Adv. Eng. Mater., 2000, 2: 551 |
| [4] | Yamaguchi M, Inui H, Ito K.High-temperature structural intermetallics[J]. Acta Mater., 2000, 48: 307 |
| [5] | Appel F, Clemens H, Fischer F D.Modeling concepts for intermetallic titanium aluminides[J]. Prog. Mater. Sci., 2016, 81: 55 |
| [6] | Fujiwara T, Nakamura A, Hosomi M, et al.Deformation of polysynthetically twinned crystals of TiAl with a nearly stoichiometric composition[J]. Philos. Mag., 1990, 61A: 591 |
| [7] | Appel F, Beaven P A, Wagner R.Deformation processes related to interfacial boundaries in two-phase γ-titanium aluminides[J]. Acta Metall. Mater., 1993, 41: 1721 |
| [8] | Lu Y H, Zhang Y G, Qiao L J, et al.In-situ TEM study of fracture mechanisms of polysynthetically twinned (PST) crystals of TiAl alloys[J]. Mater. Sci. Eng., 2000, A289: 91 |
| [9] | Pyo S G, Kim N J.Role of interface boundaries in the deformation behavior of TiAl polysynthetically twinned crystal: In situ transmission electron microscopy deformation study[J]. J. Mater. Res., 2005, 20: 1888 |
| [10] | Ji Z W, Lu S, Hu Q M, et al.Mapping deformation mechanisms in lamellar titanium aluminide[J]. Acta Mater., 2018, 144: 835 |
| [11] | Liu R C, Wang Z, Liu D, et al.Microstructure and tensile properties of Ti-45.5Al-2Cr-2Nb-0.15B alloy processed by hot extrusion[J]. Acta Metall. Sin., 2013, 49: 641(刘仁慈, 王震, 刘冬等. Ti-45.5Al-2Cr-2Nb-0.15B合金热挤压组织与拉伸性能研究[J]. 金属学报, 2013, 49: 641) |
| [12] | Dimiduk D M, Hazzledine P M, Parthasarathy T A, et al.The role of grain size and selected microstructural parameters in strengthening fully lamellar TiAl alloys[J]. Metall. Mater. Trans., 1998, 29A: 37 |
| [13] | Liu C T, Maziasz P J.Microstructural control and mechanical properties of dual-phase TiAl alloys[J]. Intermetallics, 1998, 6: 653 |
| [14] | Maziasz P J, Liu C T.Development of ultrafine lamellar structures in two-phase γ-TiAl alloys[J]. Metall. Mater. Trans., 1998, 29A: 105 |
| [15] | Parthasarathy T A, Mendiratta M G, Dimiduk D M.Flow behavior of PST and fully lamellar polycrystals of Ti-48Al in the microstrain regime[J]. Acta Mater., 1998, 46: 4005 |
| [16] | Maruyama K, Suzuki G, Kim H Y, et al. Saturation of yield stress and embrittlement in fine lamellar TiAl alloy [J]. Mater. Sci. Eng., 2002, A329-331: 190 |
| [17] | Maruyama K, Yamaguchi M, Suzuki G, et al.Effects of lamellar boundary structural change on lamellar size hardening in TiAl alloy[J]. Acta Mater., 2004, 52: 5185 |
| [18] | Misra A, Hirth J P, Hoagland R G.Length-scale-dependent deformation mechanisms in incoherent metallic multilayered composites[J]. Acta Mater., 2005, 53: 4817 |
| [19] | Shen T D, Schwarz R B, Feng S, et al.Effect of solute segregation on the strength of nanocrystalline alloys: Inverse Hall-Petch relation[J]. Acta Mater., 2007, 55: 5007 |
| [20] | Hazzledine P M.Coherency and loss of coherency in lamellar Ti-Al[J]. Intermetallics, 1998, 6: 673 |
| [21] | Maruyama K, Tabata A, Toriyama Y, et al.Effects of lamellar thickness on misfit dislocation introduction and mechanical properties of γ/α2 nano-lamellar TiAl alloys[J]. J. Phys. Conf. Ser., 2010, 240: 012101 |
| [22] | Chen Y L, Pope D P, Vitek V.Dislocation/twin/interface interactions during deformation of PST TiAl single crystals, an AFM study[J]. MRS Proc., 2002, 753: 456 |
| [23] | Katzarov I H, Paxton A T.Atomistic studies of interactions between the dominant lattice dislocations and γ/γ-lamellar boundaries in lamellar γ-TiAl[J]. Acta Mater., 2009, 57: 3349 |
| [24] | Kanani M, Hartmaier A, Janisch R.Interface properties in lamellar TiAl microstructures from density functional theory[J]. Intermetallics, 2014, 54: 154 |
| [25] | Chen G, Peng Y B, Zheng G, et al.Polysynthetic twinned TiAl single crystals for high-temperature applications[J]. Nat. Mater., 2016, 15: 876 |
| [26] | Appel F, Christoph U, Wagner R.An electron microscope study of deformation and crack propagation in (α2+γ) titanium aluminides[J]. Philos. Mag., 1995, 72A: 341 |
| [27] | Zope R R, Mishin Y.Interatomic potentials for atomistic simulations of the Ti-Al system[J]. Phys. Rev., 2003, 68B: 024102 |
| [28] | Nosé S.A unified formulation of the constant temperature molecular dynamics methods[J]. J. Chem. Phys., 1984, 81: 511 |
| [29] | Parrinello M, Rahman A.Polymorphic transitions in single crystals: A new molecular dynamics method[J]. J. Appl. Phys., 1981, 52: 7182 |
| [30] | Li J.AtomEye: An efficient atomistic configuration viewer[J]. Model. Simul. Mater. Sci. Eng., 2003, 11: 173 |
| [31] | Wang Q, Ding H S, Zhang H L, et al.Growth rates dependence of macro/microstructures and mechanical properties of Ti-47Al-2Nb-2Cr-0.2Er alloy directionally solidified by cold crucible[J]. Mater. Des., 2017, 125: 146 |
| [32] | Wang Q, Ding H S, Zhang H L, et al.An investigation on the compressive strength enhancing mechanism of directionally solidified Ti-47Al-2Nb-2Cr-0.2Er alloy in case of cyclic loading[J]. Mater. Sci. Eng., 2017, A692: 102 |
| [33] | Appel F, Paul J D H, Oehring M. Gamma Titanium Aluminide Alloys: Science and Technology[M]. Weinheim: Wiley-VCH, 2011: 140 |
| [34] | Appel F, Christoph U.Coherency stresses and interface-related deformation phenomena in two-phase titanium aluminides[J]. Intermetallics, 1999, 7: 1173 |
| [35] | Appel F, Wagner R.Microstructure and deformation of two-phase γ-titanium aluminides[J]. Mater. Sci. Eng., 1998, R22: 187 |
| [36] | Legros M, Minonishi Y, Caillard D.An in-situ transmission electron microscopy study of pyramidal slip in Ti3Al: I. Geometry and kinetics of glide[J]. Philos. Mag., 1997, 76A: 995 |
| [37] | Legros M, Minonishi Y, Caillard D.An in-situ transmission electron microscopy study of pyramidal slip in Ti3Al: II. Fine structure of dislocations and dislocation loops[J]. Philos. Mag., 1997, 76A: 1013 |
| [38] | Wiezorek J M K, Kulovits A, Zhang X D, et al. Slip transfer across hetero-interfaces in two-phase titanium aluminum intermetallics[J]. Metall. Mater. Trans., 2011, 42A: 605 |
/
| 〈 |
|
〉 |