Calculation of Magnetostriction Coefficient for Laser-Scribed Grain-Oriented Silicon Steel Based onMagnetic Domain Interaction

  • Shuangjie CHU ,
  • Yongjie YANG ,
  • Zhenghua HE ,
  • Yuhui SHA ,
  • Liang ZUO
Expand
  • 1. Baoshan Iron & Steel Cooperation Limited, Shanghai 201900, China
    2. Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China
    3. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2018-06-04

  Revised date: 2018-07-06

  Online published: 2018-11-19

Supported by

National Key Research and Development Program of China(2016YFB0300305);National Natural Science Foundation of China(51671049);Baosteel Research Project(BGFZ18A09)

Abstract

Grain-oriented silicon steel is a key material used for iron cores of transformers because grain-oriented is most desirable for magnetic cores. With the rapid development of modern power industry, the requirement for grain-oriented silicon steel with lower magnetostriction and iron loss have exigent. Although the application of laser-scribed technology can effectively reduce iron loss by refining main magnetic domain in high permeability grain-oriented silicon steels, the influence of laser-scribing on the magnetostriction of grain-oriented silicon steel is still controversial due to the complex magnetic domain structure led by interaction among crystal orientation, surface tension and scribing parameters. In this work, a magnetostriction model for laser-scribed grain-oriented silicon steel is proposed based on the relationship between magnetostrictive coefficient and two kinds of 90° magnetic domain, stress closure domain and transverse domain, and the interaction effects of laser scribing parameters and orientation deviation angle (tilt angle of [001] easy axis out of sheet surface) are analyzed. The orientation deviation angle determines which 90° domain structure of either transverse domain or stress closure domain acts as the dominant factor for magnetostrictive behavior. The stress closure domain and stray magnetic field introduced by laser scribing can reduce the magnetostriction coefficient originated from orientation deviation angle. The theoretical calculation on the effects of laser-scribed energy density and laser-scribed spacing on magnetostriction coefficient is in agreement with the direct experimental measurement. The proposed model concerning the interaction between laser-scribing parameters and orientation deviation angle can provide the theoretical basis to reduce the noise of laser-scribed grain-oriented silicon steel.

Cite this article

Shuangjie CHU , Yongjie YANG , Zhenghua HE , Yuhui SHA , Liang ZUO . Calculation of Magnetostriction Coefficient for Laser-Scribed Grain-Oriented Silicon Steel Based onMagnetic Domain Interaction[J]. Acta Metall Sin, 2019 , 55(3) : 362 -368 . DOI: 10.11900/0412.1961.2018.00242

References

[1] Xia Z S, Kang Y L, Wang Q L. Developments in the production of grain-oriented electrical steel [J]. J. Magn. Magn. Mater., 2008, 320: 3229
[2] Moses A J. Energy efficient electrical steels: Magnetic performance prediction and optimization [J]. Scr. Mater., 2012, 67: 560
[3] He Z Z, Zhao Y, Luo H W. Electrical Steel [M]. Beijing: Metallurgical Industry Press, 2012: 360
[3] 何忠志, 赵 宇, 罗海文. 电工钢 [M]. 北京: 冶金工业出版社, 2012: 360
[4] He C X, Yang F Y, Yan G C, et al. Effect of normalizing on textures of thin-gauge grain-oriented silicon steel [J]. Acta Metall. Sin., 2016, 52: 1063
[4] 何承绪, 杨富尧, 严国春等. 常化处理对薄规格取向硅钢织构的影响 [J]. 金属学报, 2016, 52: 1063
[5] Ushigami Y, Mizokami M, Fujikura M, et al. Recent development of low-loss grain-oriented silicon steel [J]. Magn J. Magn. Mater., 2003, 254-255: 307
[6] Nozawa T, Mizogami M, Mogi H, et al. Magnetic properties and dynamic domain behavior in grain-oriented 3% Si-Fe [J]. IEEE Trans. Magn., 1996, 32: 572
[7] Suzuki H, Akita K, Misawa H, et al. Mechanism of magnetic domain refinement on grain-oriented silicon steel by laser irradiation [J]. Soc J. Mater. Sci. Jpn, 2002, 8: 207
[8] Zhu Y C, Wang L F, Qiao X L. Methods and mechanism of the domain refinement of grain oriented Silicon steel by surface treament [J]. Res. Iron Steel, 2006, 34(6): 50
[8] 朱业超, 王良芳, 乔学亮. 表面处理细化取向硅钢磁畴的方法与机理 [J]. 钢铁研究, 2006, 34(6): 50)
[9] Imafuku M, Suzuki H, Akita K, et al. Effects of laser irradiation on iron loss reduction for Fe-3%Si grain-oriented silicon steel [J]. Acta Mater., 2005, 53: 939
[10] Iwata K, Imafuku M, Suzuki T, et al. Internal stress distribution for generating closure domains in laser-irradiated Fe-3%Si(110) steels [J]. J. Appl. Phys., 2015, 117: 2410
[11] Allia P, Celasco M, Milone A F, et al. Effect of the spike closure domains on the remanence and the magnetization curve in grain-oriented Si-Fe sheets [J]. J. Magn. Magn. Mater., 1982, 26: 25
[12] Imamura M, Sasaki T. The status of domain theory for an investigation of magnetostriction and magnetization processes in grain-oriented Si-Fe sheets [J]. Phy. Scr., 1988, 24: 29
[13] Zhang Z D. Magnetic structures, magnetic domains and topological magnetic textures of magnetic materials [J]. Acta Phys. Sin., 2015, 64: 67503
[13] 张志东. 磁性材料的磁结构、磁畴结构和拓扑磁结构 [J]. 物理学报, 2015, 64: 67503
[14] Moses A J. Effects of stresses on magnetic properties of silicon-iron laminations [J]. J. Mater. Sci., 1974, 9: 217
[15] Masui H. Influence of stress condition on initiation of magnetostriction in grain oriented silicon steel [J]. IEEE Trans. Magn., 1995, 31: 930
[16] Anderson P I, Moses A J, Stanbury H J. Assessment of the stress sensitivity of magnetostriction in grain-oriented silicon steel [J]. IEEE Trans. Magn., 2007, 43: 3467
[17] Tabrizi S. Study of effective methods of characterisation of magnetostriction and its fundamental effect on transformer core noise [D]. Wales: Cardiff University, 2013
[18] Redikul'tsev A A, Korzunin G S, Lobanov M L, et al. Effect of annealing on magnetostrictive characteristics of a grain-oriented electrical steel with ordinary and refined domain structure [J]. Phys. Met. Metall., 2014, 115: 650
[19] Fujikura M, Arai S, Kubota T. Effect of laser irradiation on the magnetostriction of grain-oriented electrical steels [J]. J. Magn. Soc. Jpn, 2001, 25: 895
[20] Ishida M, Nakano K, Honda A, et al. Analysis of the domain-refining effect of grooved grain-oriented silicon steel [J]. J. Magn. Soc. Jpn, 1994, 18: 809
[21] Iwata K, Fujikura M, Arai S, et al. Prediction method of basic domain structure in Fe3%Si(110) single crystal with grooved surface [J]. J. Appl. Phys., 2014, 115: 17A341
[22] Arai S, Mizokami M, Yabumoto M. Magnetostriction of grain oriented Si-Fe and its domain model [J]. Prz. Elektrotechniczny, 2011, 87: 20
[23] Hubert A, Sch?fer R. Magnetic Domains. The Analysis of Magnetic Microstructures [M]. Berlin: Springer,1999: 275
[24] Iwata K, Arai S, Ishiyama K. Calculation of basic domain width considering lancet domains in (110) [001] Fe3%Si [J]. IEEE Trans. Magn., 2014, 50: 353
[25] Iwata K, Ishiyama K, Suzuki M, et al. Quantitative analysis of 90° closure domains occurring by compressive stress in Fe3%Si (110) steels [J]. IEEE Trans. Magn., 2014, 50: 2007004
[26] Imamura M, Sasaki T, Nishimura H. AC magnetostriction in Si-Fe single crystals close to [J]. IEEE Trans. Magn., 1983, 19: 20
[27] Li J D, Gu Y Q, Guo Z Y. Decreasing the core loss of grain-oriented silicon steel by laser processing [J]. J. Mater. Process. Technol., 1997, 69: 180
[28] Sarkar S, Gopinath M, Chakraborty S S, et al. Analysis of temperature and surface hardening of low carbon thin steel sheets using Yb-fiber laser [J]. Surf. Coat. Technol., 2016, 302: 344
[29] Patri S, Gurusamy R, Molian P A, et al. Magnetic domain refinement of silicon-steel laminations by laser scribing [J]. J. Mater. Sci., 1996, 31: 1693
Outlines

/