Fabrication and Mechanical Properties of Carbon Fiber-Reinforced Aluminum Matrix Compositeswith Cu Interphase
Received date: 2018-07-12
Revised date: 2018-10-20
Online published: 2018-11-05
Supported by
National Natural Science Foundation of China(U1630129)
Carbon fiber-reinforced aluminum matrix composite has been considering as an ideal structural material for aerospace and automotive industries due to its high specific strength, high specific modulus, high thermal and electric conductivity as well as low coefficient of thermal expansion. However, for the fabrication of carbon fiber-reinforced aluminum matrix composites, the critical issues are the poor wettability and chemical reaction between carbon fibers and aluminum matrix. In order to improve the wetting behavior and prevent the chemical reaction between carbon fibers and the aluminum matrix, the electroplating technology assisted with ultra-sonic vibration dispersion method was applied to fabricate the copper interphase on the carbon fibers. It was found that a smooth, continuous copper interphase with homogeneous thickness could be deposited on carbon fibers. The carbon fiber-reinforced aluminum matrix composite (Cf/Al) was fabricated by the melt-infiltration process under pressure and vacuum conditions. The microstructure observations found that the carbon fibers homogeneously dispersed in the aluminum matrix by the introduction of copper interphase. There was no obvious carbon fiber damage caused by the reaction between carbon fibers and Al matrix. When the volume fraction of carbon fibers was 8%, the density of Cf/Al was about 2.70 g/cm3. Compared with pure Al, the mean tensile stress of Cf/Al composite was increased from 59.1 MPa to 144.9 MPa, which increased by 143%. The observation of fracture surfaces revealed the occurrence of the sliding and pull out of carbon fibers under tensile stress. The sliding and pull-out of carbon fibers can refrain the crack initiation and propagation of micro-cracks in the Al matrix. Therefore, the tensile strength of Cf/Al composite was improved significantly.
Zhaozhao Lü , Yufei ZU , Jianjun SHA , Yuqiang XIAN , Wei ZHANG , Ding CUI , Conglin YAN . Fabrication and Mechanical Properties of Carbon Fiber-Reinforced Aluminum Matrix Compositeswith Cu Interphase[J]. Acta Metall Sin, 2019 , 55(3) : 317 -324 . DOI: 10.11900/0412.1961.2018.00323
| [1] | Sun D W, Zhang G Y, Zhang Q X, et al. Application of graphite fiber reinforced aluminum matrix composite to body tube structure in space remote sensor [J]. Optics Precis. Eng., 2009, 17: 368 |
| [1] | 孙德伟, 张广玉, 张其馨等. 石墨纤维增强铝基复合材料在空间遥感器镜筒结构中的应用 [J]. 光学精密工程, 2009, 17: 368 |
| [2] | Rawal S P. Metal-matrix composites for space applications [J]. JOM, 2001, 53(4): 14 |
| [3] | Kaczmar J W, Pietrzak K, W?osiński W. The production and application of metal matrix composite materials [J]. J. Mater. Process. Technol., 2000, 106: 58 |
| [4] | Prasad S V, Asthana R. Aluminum metal-matrix composites for automotive applications: Tribological considerations [J]. Tribol. Lett., 2004, 17: 445 |
| [5] | Deng C F, Zhang X X, Wang D Z. Chemical stability of carbon nanotubes in the 2024Al matrix [J]. Mater. Lett., 2007, 61: 904 |
| [6] | Shirvanimoghaddam K, Hamim S U, Karbalaei Akbari M, et al. Carbon fiber reinforced metal matrix composites: Fabrication processes and properties [J]. Composites, 2017, 92A: 70 |
| [7] | Wang X, Jiang D M, Wu G H, et al. Effect of Mg content on the mechanical properties and microstructure of Grf/Al composite [J]. Mater. Sci. Eng., 2008, A497: 31 |
| [8] | Zhang S F, Chen G Q, Pei R S, et al. Effect of Gd content on interfacial microstructures and mechanical properties of Cf/Mg composite [J]. Mater. Des., 2015, 65: 567 |
| [9] | Singh B B, Balasubramanian M. Processing and properties of copper-coated carbon fibre reinforced aluminium alloy composites [J]. J. Mater. Process. Technol., 2009, 209: 2104 |
| [10] | Zhang J J, Liu S C, Zhang Y X, et al. Fabrication of woven carbon fibers reinforced Al-Mg (95-5 wt%) matrix composites by an electromagnetic casting process [J]. J.Mater. Process. Technol., 2015, 226: 78 |
| [11] | Hajjari E, Divandari M, Mirhabibi A R. The effect of applied pressure on fracture surface and tensile properties of nickel coated continuous carbon fiber reinforced aluminum composites fabricated by squeeze casting [J]. Mater. Des., 2010, 31: 2381 |
| [12] | Tang Y P, Deng Y D, Zhang K, et al. Improvement of interface between Al and short carbon fibers by α-Al2O3 coatings deposited by sol-gel technology [J]. Ceram. Int., 2008, 34: 1787 |
| [13] | Ure?a A, Rams J, Escalera M D, et al. Characterization of interfacial mechanical properties in carbon fiber/aluminium matrix composites by the nanoindentation technique [J]. Compos. Sci. Technol., 2005, 65: 2025 |
| [14] | Suzuki T, Umehara H, Hayashi R, et al. Mechanical properties and metallography of aluminum matrix composites reinforced by the Cu- or Ni-plating carbon multifilament [J]. J. Mater. Res., 1993, 8: 2492 |
| [15] | Hua Z S, Liu Y H, Yao G C, et al. Preparation and characterization of nickel-coated carbon fibers by electroplating [J]. J. Mater. Eng. Perform., 2012, 21: 324 |
| [16] | Liu S J, Cui C X, Qi Y M, et al. Surface treating technology of carbon fibers [J]. Mater. Sci. Technol., 2008, 16: 840 |
| [16] | 刘双进, 崔春翔, 戚玉敏等. 碳纤维表面电镀铜工艺的研究 [J]. 材料科学与工艺, 2008, 16: 840 |
| [17] | Vijayaram T R, Sulaiman S, Hamouda A M S, et al. Fabrication of fiber reinforced metal matrix composites by squeeze casting technology [J]. J. Mater. Proc. Technol., 2006, 178: 34 |
| [18] | Alhashmy H A, Nganbe M. Laminate squeeze casting of carbon fiber reinforced aluminum matrix composites [J]. Mater. Des., 2015, 67: 154 |
| [19] | Shi Q Y, Cao X, Li J Y, et al. Improved mechanical properties in friction stir processed carbon fiber reinforced aluminum composites [J].J. Tsinghua Univ(Sci. Technol.), 2017, 57: 792 |
| [19] | 史清宇, 曹 雄, 李积元等. FSP制备碳纤维增强铝基复合材料的强韧化机理 [J]. 清华大学学报(自然科学版), 2017, 57: 792 |
| [20] | Tao Z H, He W, Wang S X, et al. Synergistic effect of different additives on microvia filling in an acidic copper plating solution [J].J. Electrochem. Soc., 2016, 163: D379 |
| [21] | Shi D L, Lian J, He P, et al. Plasma coating of carbon nanofibers for enhanced dispersion and interfacial bonding in polymer composites [J]. Appl. Phys. Lett., 2003, 83: 5301 |
| [22] | Jiang H G, Dai J Y, Tong H Y, et al. Interfacial reactions on annealing Cu/Al multilayer thin films [J]. J. Appl. Phys., 1993, 74: 6165 |
| [23] | Oh S I, Lim J Y, Kim Y C, et al. Fabrication of carbon nanofiber reinforced aluminum alloy nanocomposites by a liquid process [J]. J. Alloys Compd., 2012, 542: 111 |
| [24] | Silvain J F, Proult A, Lahaye M, et al. Microstructure and chemical analysis of C/Cu/Al interfacial zones [J]. Composites, 2003, 34A: 1143 |
| [25] | Tanaka Y, Kajihara M. Numerical analysis for migration of interface between liquid and solid phases during reactive diffusion in the binary Cu-Al system [J]. Mater. Sci. Eng., 2007, A459: 101 |
| [26] | Tanaka Y, Kajihara M, Watanabe Y. Growth behavior of compound layers during reactive diffusion between solid Cu and liquid Al [J]. Mater. Sci. Eng., 2007, A445-446: 355 |
/
| 〈 |
|
〉 |