Orginal Article

Influence of Inter-Pass Temperature on Residual Stress in Multi-Layer and Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes

  • Lei HU ,
  • Xue WANG ,
  • Xiaohui YIN ,
  • Hong LIU ,
  • Qunshuang MA
Expand
  • 1 School of Materials Science and Engineering, Anhui University of Technology, Ma'anshan, Anhui 243032, China
    2 School of Power and Mechanics, Wuhan University, Wuhan 430072, China
    3 Dong Fang Boiler Group Co., Ltd., Dong Fang Electric Corporation, Zigong 643001, China

Received date: 2018-02-02

  Online published: 2018-10-17

Supported by

Supported by National Natural Science Foundation of China (Nos.51374153 and 51574181) and Science and Technology Program of Sichuan Province (No.2018JY0668)

Abstract

9%Cr heat-resistant steels have been abundantly used in boilers of modern thermal plants. The 9%Cr steel components in thermal plant boilers are usually assembled by fusion welding. Many of the degradation mechanisms of welded joints can be aggravated by welding residual stress. Tensile residual stress in particular can exacerbate cold cracking tendency, fatigue crack development and the onset of creep damage in heat-resistant steels. It has been recognized that welding residual stress can be mitigated by low temperature martensitic transformation in 9%Cr heat-resistant steel. Nevertheless, the stress mitigation effect seems to be confined around the final weld pass in multi-layer and multi-pass 9%Cr steel welded pipes. The purpose of this work is to investigate the method to break through this confine. Influence of martensitic transformation on welding stress evolution in multi-layer and multi-pass butt-welded 9%Cr heat-resistant steel pipes for different inter-pass temperatures (IPT) was investigated through finite element method, and the influential mechanism of IPT on welding residual stress was revealed. The results showed that tensile residual stress in weld metal (WM) and heat affected zone (HAZ), especially the noteworthy tensile stress in WM at pipe central, was effectively mitigated with the increasing of IPT. The reasons lie in two aspects, firstly, there is more residual austenite in the case of higher IPT, as a result, lower tensile stress is accumulated during cooling due to the lower yield strength of austenite; secondly, the higher IPT suppresses the martensitic transformation during cooling of each weld pass, thus the tensile stress mitigation due to martensitic transformation was avoided to be eliminated by welding thermal cycles of subsequent weld passes and reaccumulating tensile residual stress. The influence of IPT on welding residual stress relies on the combined contribution of thermal contraction and martensitic transformation. When the IPT is lower than martensite transformation finishing temperature (Mf), thermal contraction plays the dominant role in the formation of welding residual stress, and tensile stress was formed in the majority of weld zone except the final weld pass. While, compressive stress was formed in almost whole weld zone due to martensitic transformation when the IPT is higher than martensite transformation starting temperature (Ms).

Cite this article

Lei HU , Xue WANG , Xiaohui YIN , Hong LIU , Qunshuang MA . Influence of Inter-Pass Temperature on Residual Stress in Multi-Layer and Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes[J]. Acta Metall Sin, 2018 , 54(12) : 1767 -1776 . DOI: 10.11900/0412.1961.2018.00051

References

[1] Abson D J, Rothwell J S.Review of type IV cracking of weldments in 9-12%Cr creep strength enhanced ferritic steels[J]. Int. Mater. Rev., 2013, 58: 437
[2] Wang X, Wang X, Li H J, et al.Laves phase precipitation behavior in the simulated fine-grained heat-affected zone of creep strength enhanced ferritic steel P92 and its role in creep void nucleation and growth[J]. Weld. World, 2017, 61: 231
[3] Liu W, Lu F G, Wei Y H, et al.Special zone in multi-layer and multi-pass welded metal and its role in the creep behavior of 9Cr-1Mo welded joint[J]. Mater. Des., 2016, 108: 195
[4] Paddea S, Francis J A, Paradowska A M, et al.Residual stress distributions in a P91 steel-pipe girth weld before and after post weld heat treatment[J]. Mater. Sci. Eng., 2012, A534: 663
[5] Francis J A, Bhadeshia H K D H, Withers P J. Welding residual stresses in ferritic power plant steels[J]. Mater. Sci. Technol., 2007, 23: 1009
[6] Ooi S W, Garnham J E, Ramjaun T I.Review: Low transformation temperature weld filler for tensile residual stress reduction[J]. Mater. Des., 2014, 56: 773
[7] Wang X, Li Y, Ren Y Y, et al.Effect of Laves phase precipitation on redistribution of alloying elements in P92 steel[J]. Acta Metall. Sin., 2014, 50: 1203(王学, 李勇, 任遥遥等. Laves相析出对P92钢合金元素再分布的影响[J]. 金属学报, 2014, 50: 1203)
[8] Yang J P, Guo J, Qiao Y X.Study on welding procedure of P92 steel using in ultra supercritical plants[J]. Proc. CSEE, 2007, 27(23): 55(杨建平, 郭军, 乔亚霞. 超超临界机组用P92钢焊接技术的研究[J]. 中国电机工程学报, 2007, 27(23): 55)
[9] Qiao Y X, Guo J.P92 steel (martensitic steel) welding used for power plant boilers[J]. Electr. Power Constr., 2007, 28(6): 87(乔亚霞, 郭军. 电站锅炉用马氏体耐热钢P92钢的焊接[J]. 电力建设, 2007, 28(6): 87)
[10] Richardot D, Vaillant J C, Arbab A, et al.The T92/P92 Book[M]. Boulogne: Vallourec & Mannesmann Tubes, 2000: 7
[11] Haarmann K, Vailant J C, Vandenberghe B, et al.The T91/P91 Book[M]. Boulogne: Vallourec & Mannesmann Tubes, 1999: 6
[12] Wang X, Hu L, Chen D X, et al.Effect of martensitic transformation on stress evolution in multi-pass butt-welded 9%Cr heat-resistant steel pipes[J]. Acta Metall. Sin., 2017, 53: 888(王学, 胡磊, 陈东旭等. 马氏体相变对9%Cr热强钢管道多道焊接头残余应力演化的影响[J]. 金属学报, 2017, 53: 888)
[13] Wang Z Y, Li S J, Hao X J, et al.Ultrasonic testing of interlayer cracks in P91 butt weld[J]. Nondestr. Test., 2011, 33(5): 54(王志永, 李树军, 郝晓军等. P91钢管对接焊缝层间裂纹的超声波检测[J]. 无损检测, 2011, 33(5): 54)
[14] Chen J P, Yang W F, Han T, et al.The ultrasonic testing of micro-crack in P91/92 steel pipe butt weld[J]. Nondestr. Test., 2016, 38(8): 44(陈君平, 杨文峰, 韩腾等. P91/P92钢管道对接焊缝微裂纹的超声波检测[J]. 无损检测, 2016, 38(8): 44)
[15] Javadi Y, Smith M C, Abburi Venkata K, et al.Residual stress measurement round robin on an electron beam welded joint between austenitic stainless steel 316L(N) and ferritic steel P91 [J]. Int. J. Press. Vessels Pip., 2017, 154: 41
[16] Pu X W, Zhang C H, Li S, et al.Simulating welding residual stress and deformation in a multi-pass butt-welded joint considering balance between computing time and prediction accuracy[J]. Int. J. Adv. Manuf. Technol., 2017, 93: 2215
[17] Deng D A, Ren S D, Li S, et al.Influence of multi-thermal cycle and constraint condition on residual stress in P92 steel weldment[J]. Acta Metall. Sin., 2017, 53: 1532(邓德安, 任森栋, 李索等. 多重热循环和约束条件对P92钢焊接残余应力的影响[J]. 金属学报, 2017, 53: 1532)
[18] Galler J P, Dupont J N, Siefert J A.Influence of alloy type, peak temperature and constraint on residual stress evolution in Satoh test[J]. Sci. Technol. Weld. Joining, 2016, 21: 106
[19] Thomas S H, Liu S.Analysis of low transformation temperature welding (LTTW) consumables-distortion control and evolution of stresses[J]. Sci. Technol. Weld. Joining, 2014, 19: 392
[20] Yaghi A H, Hyde T H, Becker A A, et al.Finite element simulation of welding and residual stresses in a P91 steel pipe incorporating solid-state phase transformation and post-weld heat treatment[J]. J. Strain Anal. Eng. Des., 2008, 43: 275
[21] Koistinen D P, Marburger R E.A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels[J]. Acta Metall., 1959, 7: 59
[22] Wang X, Pan Q G, Tao Y S, et al.Type IV creep rupture characteristics of P92 steel weldment[J]. Acta Metall. Sin., 2012, 48: 427(王学, 潘乾刚, 陶永顺等. P92钢焊接接头IV型蠕变断裂特性[J]. 金属学报, 2012, 48: 427)
[23] Yaghi A H, Hyde T H, Becker A A, et al.Finite element simulation of welded P91 steel pipe undergoing post-weld heat treatment[J]. Sci. Technol. Weld. Joining, 2011, 16: 232
[24] Deng D A, Zhang Y B, Li S, et al.Influence of solid-state phase transformation on residual stress in P92 steel welded joint[J]. Acta Metall. Sin., 2016, 52: 394(邓德安, 张彦斌, 李索等. 固态相变对P92钢焊接接头残余应力的影响[J]. 金属学报, 2016, 52: 394)
[25] Li S, Ren S D, Zhang Y B, et al.Numerical investigation of formation mechanism of welding residual stress in P92 steel multi-pass joints[J]. J. Mater. Process. Technol., 2017, 244: 240
[26] Radaj D.Heat Effects of Welding: Temperature Field, Residual Stress, Distortion[M]. Berlin: Springer-Verlag, 1992: 174
Outlines

/