Reconstruction of 3D Morphology of TiB2 in In Situ Fe Matrix Composites
Received date: 2018-07-01
Online published: 2018-10-17
Supported by
Supported by National Natural Science Foundation of China (Nos.51722402 and U1560204) and Fundamental Research Funds for the Central Universities (No.N170705001)
TiB2 strengthened Fe matrix composites (Fe-TiB2) are potential lightweight materials for lightweight structure materials as they possess high modulus, low density, high strength and good ductility. More importantly, Fe-TiB2 composite can be produced by eutectic solidification, which is suitable for massive production using thin slab casting and strip casting in the steel industry. The microstructure of Fe-TiB2 composite is composed of ferrite matrix, primary TiB2 and eutectic TiB2 reinforcements. Ceramic TiB2 is a hard brittle phase and it is easy to generate stress concentration when bearing load. The shape and size of TiB2 can affect the mechanical properties of Fe-TiB2 composite and the formability of sheet metal. The morphology and size of TiB2 reinforcements are commonly observed using optical or electron microscope, which can only provide two-dimensional (2D) cross-section of the reinforcements. Nevertheless, the TiB2 particles have various aspect ratios in three-dimensional (3D) space, which have not yet been well investigated. The present work proposes a new method combining deep etching and computer aided design (Creo Parametric) technology to reconstruct the 3D morphology of TiB2 reinforcements in the Fe-TiB2 composites. The OM, SEM were used to compare and analyze the 2D and 3D morphologies of the TiB2 reinforcements. The fracture mechanism of the Fe-TiB2 composite was reinterpreted by compression test. The results indicated that the primary TiB2 reinforcements have an octahedral prism structure, which is mostly composed of two or even more single crystal prisms, and are randomly distributed in the matrix without preferred orientations. The eutectic TiB2 reinforcements consist of lamelliform/fine columnar phase and dendrite phase. The lamelliform/fine columnar and dendrite eutectic phase in Fe-TiB2 composite are more prone to brittle fracture than the primary phase TiB2 during loading. Therefore, it is the main cause of fracture failure of the material during loading. The small TiB2 particles observed by 2D microstructure do not exist in real 3D space. It is proposed that small and spherical TiB2 particles are preferred and could be produced by controlling solidification process.
Baogang WANG , Hongliang YI , Guodong WANG , Zhichao LUO , Mingxin HUANG . Reconstruction of 3D Morphology of TiB2 in In Situ Fe Matrix Composites[J]. Acta Metall Sin, 2019 , 55(1) : 133 -140 . DOI: 10.11900/0412.1961.2018.00297
| [1] | Rana R.High modulus steels[J]. Can. Metall. Quart., 2014, 53: 241 |
| [2] | Bouaziz O, Zurob H, Huang M X.Driving force and logic of development of advanced high strength steels for automotive applications[J]. Steel Res. Int., 2013, 84: 937 |
| [3] | Bonnet F, Daeschler V, Petitgand G.High modulus steels: New requirement of automotive market. How to take up challenge[J]. Can. Metall. Quart., 2014, 53: 243 |
| [4] | Kulikowski Z, Godfrey T M T, Wisbey A, et al. Mechanical and microstructural behaviour of a particulate reinforced steel for structural applications[J]. Mater. Sci. Technol., 2000, 16: 1453 |
| [5] | Yi H L, Sun L, Xiong X C.Challenges in the formability of the next generation of automotive steel sheets[J]. Mater. Sci. Technol., 2018, 34: 1112 |
| [6] | Anal A, Bandyopadhyay T K, Das K.Synthesis and characterization of TiB2-reinforced iron-based composites[J]. J. Mater. Process. Technol., 2006, 172: 70 |
| [7] | Li B H, Liu Y, He L, et al.Fabrication of in situ TiB2 reinforced steel matrix composite by vacuum induction melting and its microstructure and tensile properties[J]. Int. J. Cast Met. Res., 2010, 23: 211 |
| [8] | Lü W J, Zhang X N, Zhang H, et al.Growth mechanism of reinforcement in in situ processed TiB/Ti composites[J]. Acta Metall. Sin., 2000, 36: 104(吕维洁, 张晓农, 张获等. 原位合成TiB/Ti基复合材料增强体的生长机制[J]. 金属学报, 2000, 36: 104) |
| [9] | Kuang J C, Fu H G.Mechanical properties and wear resistance of In-situ synthesized (TiB2+Fe2B)/ferro-base composites[J]. Lubr. Eng., 2007, 32(8): 81(匡加才, 符寒光. 原位合成(TiB2+Fe2B)/铁基复合材料的力学性能和耐磨性[J]. 润滑与密封, 2007, 32(8): 81) |
| [10] | Zhang F, Li X D.Computer simulation of microstructure for metal matrix composites[J]. Chin. J. Nonferrous Met., 2014, 24: 97(张赋, 李旭东. 金属基复合材料微观组织结构的计算机模拟[J]. 中国有色金属学报, 2014, 24: 97) |
| [11] | Luo Z C, He B B, Li Y Z, et al.Growth mechanism of primary and eutectic TiB2 particles in a hypereutectic steel matrix composite[J]. Metall. Mater. Trans., 2017, 48A: 1981 |
| [12] | Akhtar F.Ceramic reinforced high modulus steel composites: Processing, microstructure and properties[J]. Can. Metall. Quart., 2014, 53: 253 |
| [13] | Feng Y J.Strengthening of steels by ceramic phases [D]. Westf?lischen: RWTH Aachen University, 2013 |
| [14] | Chen S, Seda P, Krugla M, et al.High-modulus steels reinforced with ceramic particles through ingot casting process[J]. Mater. Sci. Technol., 2016, 32: 992 |
| [15] | Springer H, Fernandez R A, Duarte M J, et al.Microstructure refinement for high modulus in-situ metal matrix composite steels via controlled solidification of the system Fe-TiB2[J]. Acta Mater., 2015, 96: 47 |
| [16] | Zhang H, Springer H, Aparicio-Fernández R, et al.Improving the mechanical properties of Fe-TiB2 high modulus steels through controlled solidification processes[J]. Acta Mater., 2016, 118: 187 |
| [17] | Aparicio-Fernández R, Springer H, Szczepaniak A, et al.In-situ metal matrix composite steels: Effect of alloying and annealing on morphology, structure and mechanical properties of TiB2 particle containing high modulus steels[J]. Acta Mater., 2016, 107: 38 |
| [18] | Tanaka K, Saito T.Phase equilibria in TiB2-reinforced high modulus steel[J]. J. Phase Equilib., 1999, 20: 207 |
| [19] | Wu R J.The present condition and prospects on metal matrix composites[J]. Acta Metall. Sin., 1997, 65: 78(吴人洁. 金属基复合材料的现状与展望[J]. 金属学报, 1997, 65: 78) |
| [20] | Ma Z Y, Bi J, Lü Y X, et al.On the in situ forming TiB2 reinforced Al composite[J]. Acta Metall. Sin., 1992, 28(9): 87(马宗义, 毕敬, 吕毓雄等. 原位生长TiB2增强Al复合材料的研究[J]. 金属学报, 1992, 28(9): 87) |
| [21] | Huang M X, He B B, Wang X, et al.Interfacial plasticity of a TiB2-reinforced steel matrix composite fabricated by eutectic solidification[J]. Scr. Mater., 2015, 99: 13 |
| [22] | Cha L M, Lartigue-Korinek S, Walls M, et al.Interface structure and chemistry in a novel steel-based composite Fe-TiB2 obtained by eutectic solidification[J]. Acta Mater., 2012, 60: 6382 |
| [23] | Yang N, Sinclair I.Fatigue crack growth in a particulate TiB2-reinforced powder metallurgy iron-based composite[J]. Metall. Mater. Trans., 2003, 34A: 2017 |
| [24] | Llorca J.An analysis of the influence of reinforcement fracture on the strength of discontinuously-reinforced metal-matrix composites[J]. Acta Metall. Mater., 1995, 43: 181 |
| [25] | Bacon D H, Edwards L, Moffatt J E, et al.Synchrotron X-ray diffraction measurements of internal stresses during loading of steel-based metal matrix composites reinforced with TiB2 particles[J]. Acta Mater., 2011, 59: 3373 |
| [26] | Li Y Z, Luo Z C, Yi H L, et al.Damage mechanisms of a TiB2-reinforced steel matrix composite for lightweight automotive application[J]. Metall. Mater. Trans., 2016, 3E: 203 |
| [27] | Hadjem-Hamouche Z H, Chevalier J P, Cui Y T, et al. Deformation behavior and damage evaluation in a new titanium diboride (TiB2) steel-based composite[J]. Steel Res. Int., 2012, 83: 538 |
| [28] | Dammak M, Ksaeir I, Brinza O, et al.Experimental analysis of damage of Fe-TiB2 metal matrix composites under complex loading [A]. 21ème Congrès Fran?ais de Mécanique[C]. Bordeaux: I-Revues, 2013: 1 |
| [29] | He L, Liu Y, Li J, et al.Effects of hot rolling and titanium content on the microstructure and mechanical properties of high boron Fe-B alloys[J]. Mater. Des., 2012, 36: 88 |
| [30] | Lartigue-Korinek S, Walls M, Haneche N, et al.Interfaces and defects in a successfully hot-rolled steel-based composite Fe-TiB2[J]. Acta Mater., 2015, 98: 297 |
| [31] | Springer H, Baron C, Szczepaniak A, et al.Stiff, light, strong and ductile: Nano-structured high modulus steel[J]. Sci. Rep., 2017, 7: 2757 |
/
| 〈 |
|
〉 |