Effect of Na on Early Atmospheric Corrosion of Al

  • Xingchen CHEN ,
  • Jie WANG ,
  • Deren CHEN ,
  • Shuncong ZHONG ,
  • Xiangfeng WANG
Expand
  • State Key Laboratory of Photocatalysis on Energy and Environment, School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350002, China

Received date: 2018-06-27

  Revised date: 2018-08-03

  Online published: 2018-10-09

Supported by

National Natural Science Foundation of China(No.51675103);State Key Laboratory of Photocatalysis on Energy and Environment(No.SKLPEE-KF201719);Fuzhou Science and Technology Bureau(No.2018-G-35)

Abstract

Aluminum and aluminum alloy are widely used in every field of modern life. It is especially important to understand the detailed mechanisms of aluminum atmospheric corrosion. Traditional studies only consider the role of oxygen reduction and focus on anions such as Cl, SO42- in the environment, ignoring the effects of cations such as Na+ on the atmospheric corrosion. However, recent studies have shown that the effect of Na element on the corrosion of aluminum can not be ignored. In this work, single-shot laser-induced breakdown spectroscopy (LIBS) was used to measure the aluminum atomic lines after corrosion for 35 d in the atmospheric environment, and combined with a three-dimensional tomography measurement, to study the depth profiling of Na on the aluminum surface. The results show that the Na element on the surface of the aluminum originates from the atmospheric environment, and Na is involved in the formation of corrosion product NaAlCO3(OH)2. The content of NaAlCO3(OH)2 decreases as the depth increases following an exponential power function. The content decrease of NaAlCO3(OH)2 in different depths can be transformed into the change of cathode area. Combined with the measured polarization curve of aluminum, the atmospheric corrosion model of aluminum including the presence of oxygen reduction and the change of cathode area was established using COMSOL software. The calculated corrosion depth is 6.155 μm, which is consistent with the depth of Na element measured by LIBS experiments. By studying the distribution of Na cations and corrosion products, a simulation model was established to reveal the influence on corrosion mechanism, which is of great significance for the study of early atmospheric corrosion of aluminum.

Cite this article

Xingchen CHEN , Jie WANG , Deren CHEN , Shuncong ZHONG , Xiangfeng WANG . Effect of Na on Early Atmospheric Corrosion of Al[J]. Acta Metall Sin, 2019 , 55(4) : 529 -536 . DOI: 10.11900/0412.1961.2018.00280

References

1 Hou B R, Li X G, Ma X M, et al. The cost of corrosion in China [J]. npj Mater. Degrad., 2017, 1: 4
2 An B G, Zhang X Y, Han E-H, et al. Research situation of atmospheric corrosion of aluminum and aluminum alloys [J]. Chin. J. Nonferrous Met., 2001, 11(增刊2): 11
2 安百刚, 张学元, 韩恩厚等. 铝和铝合金的大气腐蚀研究现状 [J]. 中国有色金属学报, 2001, 11(suppl.2): 11)
3 Nesic S, Nordsveen M, Maxwell N, et al. Probabilistic modelling of CO2, corrosion laboratory data using neural networks [J]. Corros. Sci., 2001, 43: 1373
4 Song Y R, Jiang G M, Chen Y, et al. Effects of chloride ions on corrosion of ductile iron and carbon steel in soil environments [J]. Sci. Rep., 2017, 7: 6865
5 Mccafferty E. Sequence of steps in the pitting of aluminum by chloride ions [J]. Corros. Sci., 2003, 45: 1421
6 Vera R, Delgado D, Rosales B M. Effect of atmospheric pollutants on the corrosion of high power electrical conductors: Part 1. Aluminium and AA6201 alloy [J]. Corros. Sci., 2006, 48: 2882
7 Schaller R F, Jove-Colon C F, Taylor J M, et al. The controlling role of sodium and carbonate on the atmospheric corrosion rate of aluminum [J]. npj Mater. Degrad., 2017, 1: 20
8 Ejaz A, Lu Z P, Chen J J, et al. The effects of hydrogen on anodic dissolution and passivation of iron in alkaline solutions [J]. Corros. Sci., 2015, 101: 165
9 Alcántara J, Chico B, Díaz I, et al. Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel [J]. Corros. Sci., 2015, 97: 74
10 Watanabe M, Hokazono A, Handa T, et al. Corrosion of copper and silver plates by volcanic gases [J]. Corros. Sci., 2006, 48: 3759
11 Blücher D B, Lindström R W, Svensson J E, et al. The effect of CO2 on the NaCl-induced atmospheric corrosion of aluminum [J]. J. Electrochem. Soc., 2001, 148: B127
12 Blücher D B, Svensson J E, Johansson L G. The NaCl-induced atmospheric corrosion of aluminum the influence of carbon dioxide and temperature [J]. J. Electrochem. Soc., 2001, 150: B93
13 Wen S B, Mao X L, Greif R, et al. Laser ablation induced vapor plume expansion into a background gas. II. Experimental analysis [J]. J. Appl. Phys., 2007, 101: 023115
14 Li T C, Yuan C S, Huang H C, et al. Inter-comparison of seasonal variation, chemical characteristics, and source identification of atmospheric fine particles on both sides of the Taiwan Strait [J]. Sci. Rep., 2016, 6: 22956
15 Xiao H W, Xiao H Y, Luo L, et al. Atmospheric aerosol compositions over the South China Sea: Temporal variability and source apportionment [J]. Atmos. Chem. Phys., 2017, 17: 3199
16 Zhao R J, Han B, Lu B, et al. Element composition and source apportionment of atmospheric aerosols over the China Sea [J]. Atmos. Pollut. Res., 2015, 6: 191
17 Chen Z Y, Cui F, Kelly R G. Calculations of the cathodic current delivery capacity and stability of crevice corrosion under atmospheric environments [J]. J. Electrochem. Soc., 2008, 155: C360
18 Galvele J. Transport processes in passivity breakdown—II. Full hydrolysis of the metal ions [J]. Corros. Sci., 1981, 21: 551
19 Gravano S M, Galvele J R. Transport processes in passivity breakdown—III. Full hydrolysis plus ion migration plus buffers [J]. Corros. Sci., 1984, 24: 517
20 Nguyen T H, Foley R T. The chemical nature of aluminum corrosion. Ш. The dissolution mechanism of aluminum oxide and aluminum powder in various electrolytes [J]. J. Electrochem. Soc., 1980, 127: 2563
21 Graedel T E. Corrosion mechanisms for aluminum exposed to the atmosphere [J]. J. Electrochem. Soc., 1989, 136: 204C
22 El Sherbini A M, El Sherbini T M, Hegazy H, et al. Evaluation of self-absorption coefficients of aluminum emission lines in laser-induced breakdown spectroscopy measurements [J]. Spectrochim. Acta, 2005, 60B: 1573
23 Lazic V, Barbini R, Colao F, et al. Self-absorption model in quantitative laser induced breakdown spectroscopy measurements on soils and sediments [J]. Spectrochim. Acta, 2001, 56B: 807
24 Rai A K, Yueh F Y, Singh J P. Laser-induced breakdown spectroscopy of molten aluminum alloy [J]. Appl. Opt., 2003, 42: 2078
25 Lutey A H A. An improved model for nanosecond pulsed laser ablation of metals [J]. J. Appl. Phys., 2013, 114: 083108
26 Aziz P M, Godard H P. Pitting corrosion characteristics of aluminum—Influence of magnesium and manganese [J]. Ind. Eng. Chem., 2002, 44: 1791
27 Mansfeld F, Kenkel J V. Galvanic corrosion of Al alloys—III. The effect of area ratio [J]. Corros. Sci., 1975, 15: 239
28 Melchers R E. Time dependent development of aluminium pitting corrosion [J]. Adv. Mater. Sci. Eng., 2015, 2015: 215712
29 Deshpande K B. Validated numerical modelling of galvanic corrosion for couples: Magnesium alloy (AE44)-mild steel and AE44-aluminium alloy (AA6063) in brine solution [J]. Corros. Sci., 2010, 52: 3514
30 Ge J, Isgor O B. Effects of Tafel slope, exchange current density and electrode potential on the corrosion of steel in concrete [J]. Mater. Corros., 2007, 58: 573
31 Mizuno D, Kelly R G. Galvanically Induced intergranular corrosion of AA5083-H131 under atmospheric exposure conditions: Part 2—Modeling of the damage distribution [J]. Corrosion, 2013, 69: 681
32 Millero F J, Huang F, Laferiere A L. Solubility of oxygen in the major sea salts as a function of concentration and temperature [J]. Mar. Chem., 2002, 78: 217
33 Verbrugge M. Galvanic corrosion over a semi-infinite, planar surface [J]. Corros. Sci., 2006, 48: 3489
34 Antonijevic M M, Alagic S C, Petrovi M B, et al. The influence of pH on electrochemical behavior of copper in presence of chloride ions [J]. Int. J. Electrochem. Sc., 2009, 4: 962
35 Lin J M. Effect of city on the atmosphere humidity distribution—Taking Fuzhou as an example [J]. Areal Res. Dev., 1991, 10(2): 51
35 林家蒙. 城市对大气湿度分布影响研究——以福州市为例 [J]. 地域研究与开发, 1991, 10(2): 51)
36 Mattsson E, Lindgren S. Hard-rolled aluminum alloys [A]. Metal Corrosion in the Atmosphere [C]. Philadelphia: American Society for Testing and Materials, 1968: 240