Damping Capacities of (B4C+Ti) Hybrid Reinforced Mg and AZ91D Composites Processed by In Situ Reactive Infiltration Technique
Received date: 2018-03-21
Online published: 2018-10-09
Supported by
Supported by National Natural Science Foundation of China (No.51271051)
Mechanical vibration causes lots of damage in automotive industry, machinery manufacturing and aerospace field. Noise control also causes much damage to human health. So it is of great significance to seek materials with high damping capacity to alleviate or eliminate mechanical vibration and noise. Pure Mg has the highest damping capacity among all of the commercial metal materials, but its low mechanical property impose restrictions on its pervasive application. Therefore, magnesium matrix composites reinforced with high mechanical property reinforcement can exhibit excellent damping capacity and mechanical property simultaneously, and this kind of material has attracted great attention and interest from researchers in recent years. A variety of preparation methods has been utilized to prepare magnesium matrix composites reinforced with different reinforcements. In situ reactive infiltration is a relatively new processing method to prepare metal matrix composites, which combines the advantages of in situ reaction synthesis and pressureless infiltration, and it has received increasing attention because of its cost-effectiveness, simplicity and high-efficiency, and near-net shaping capability. And by tailoring the relative density of preform, magnesium matrix composites with a high volume fraction of ceramic reinforcement can be obtained. In view of the poor wettability of B4C/Mg system leading to low efficiency of composite, Ti particulates with high melting point and immiscible with magnesium was added. And (B4C+Ti)/Mg and (B4C+Ti)/AZ91D composites have been prepared successfully by in situ reactive infiltration method with high efficiency and low cost. Microstructure, phase composition and damping capacities of the as-fabricated composites were characterized and analyzed. Results showed that with increasing the preparation temperatures, the reaction between the starting materials is more complete, and the microstructure of (B4C+Ti)/AZ91D composites tends to be interpenetrating networks from particle reinforced structure. The strain-dependent and temperature-dependent damping capacities of (B4C+Ti)/Mg and (B4C+Ti)/AZ91D composites improve gradually with the increase of strain amplitude and temperature respectively, and the dominant damping mechanisms are dislocation damping and interface damping.
Yantao YAO , Liqing CHEN , Wenguang WANG . Damping Capacities of (B4C+Ti) Hybrid Reinforced Mg and AZ91D Composites Processed by In Situ Reactive Infiltration Technique[J]. Acta Metall Sin, 2019 , 55(1) : 141 -148 . DOI: 10.11900/0412.1961.2018.00108
| [1] | Carvalho O, Miranda G, Buciumeanu M, et al.High temperature damping behavior and dynamic Young's modulus of AlSi-CNT-SiCp hybrid composite[J]. Compos. Struct., 2016, 141: 155 |
| [2] | Jiang H J, Liu C Y, Zhang B, et al.Simultaneously improving mechanical properties and damping capacity of Al-Mg-Si alloy through friction stir processing[J]. Mater. Charact., 2017, 131: 425 |
| [3] | Li Q Y, Li J, He G.Compressive properties and damping capacities of magnesium reinforced with continuous steel wire[J]. Mater. Sci. Eng., 2017, A680: 92 |
| [4] | Deng K K, Li J C, Nie K B, et al.High temperature damping behavior of as-deformed Mg matrix influenced by micron and submicron SiCp[J]. Mater. Sci. Eng., 2015, A624: 62 |
| [5] | Wu Y W, Wu K, Deng K K, et al.Damping capacities and microstructures of magnesium matrix composites reinforced by graphite particles[J]. Mater. Des., 2010, 31: 4862 |
| [6] | Wang C J, Deng K K, Liang W.High temperature damping behavior controlled by submicron SiCp in bimodal size particle reinforced magnesium matrix composite[J]. Mater. Sci. Eng., 2016, A668: 55 |
| [7] | Habibi M K, Hamouda A M S, Gupta M. Enhancing tensile and compressive strength of magnesium using ball milled Al+CNT reinforcement[J]. Compos. Sci. Technol., 2012, 72: 290 |
| [8] | Kevorkijan V, ?kapin S D.Mg/B4C composites with a high volume fraction of fine ceramic reinforcement[J]. Mater. Manuf. Processes, 2009, 24: 1337 |
| [9] | Yao J P, Li W, Zhang L, et al.RETRACTED ARTICLE: Wear mechanism for in situ TiC particle reinforced AZ91 magnesium matrix composites[J]. Tribol. Lett., 2010, 38: 253 |
| [10] | Yao Y T, Chen L Q.Processing of B4C particulate-reinforced magnesium-matrix composites by metal-assisted melt infiltration technique[J]. J. Mater. Sci. Technol., 2014, 30: 661 |
| [11] | Chen L Q, Yao Y T.Processing, microstructures, and mechanical properties of magnesium matrix composites: A review[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 762 |
| [12] | Sahoo B N, Panigrahi S K.Synthesis, characterization and mechanical properties of in-situ (TiC-TiB2) reinforced magnesium matrix composite[J]. Mater. Des., 2016, 109: 300 |
| [13] | Chen L Q, Dong Q, Zhao M J, et al.Synthesis of TiC/Mg composites with interpenetrating networks by in situ reactive infiltration process[J]. Mater. Sci. Eng., 2005, A408: 125 |
| [14] | Schaller R.Metal matrix composites, a smart choice for high damping materials[J]. J. Alloys Compd., 2003, 335: 131 |
| [15] | Zhang X Q, Wang H W, Liao L H, et al.In situ synthesis method and damping characterization of magnesium matrix composites[J]. Compos. Sci. Technol., 2007, 67: 720 |
| [16] | Wu Y W, Wu K, Nie K B, et al.Damping capacities and tensile properties in Grp/AZ91 and SiCp/Grp/AZ91 magnesium matrix composites[J]. Mater. Sci. Eng., 2010, A527: 7873 |
| [17] | Anasori B, Barsoum M W.Energy damping in magnesium alloy composites reinforced with TiC or Ti2AlC particles[J]. Mater. Sci. Eng., 2016, A653: 53 |
| [18] | Zhang X Q, Liao L H, Ma N H, et al.Mechanical properties and damping capacity of magnesium matrix composites[J]. Composites, 2006, 37A: 2011 |
| [19] | Huang W Z, Luo H J, Mu Y L, et al.Low-frequency damping behavior of closed-cell Mg alloy foams reinforced with SiC particles[J]. Int. J. Min. Metall. Mater., 2017, 24: 701 |
| [20] | Gu J H, Zhang X N, Qiu Y F, et al.Damping behaviors of magnesium matrix composites reinforced with Cu-coated and uncoated SiC particulates[J]. Compos. Sci. Technol., 2005, 65: 1736 |
| [21] | Wang H Y, Jiang Q C, Zhao Y Q, et al.Fabrication of TiB2 and TiB2-TiC particulates reinforced magnesium matrix composites[J]. Mater. Sci. Eng., 2004, A372: 109 |
| [22] | Shen P, Zou B L, Jin S B, et al. Reaction mechanism in self-propagating high temperature synthesis of TiC-TiB2/Al composites from an Al-Ti-B4C system [J]. Mater. Sci. Eng., 2007, A454-455: 300 |
| [23] | Prasad D S, Shoba C.Experimental evaluation onto the damping behavior of Al/SiC/RHA hybrid composites[J]. J. Mater. Res. Technol., 2016, 5: 123 |
| [24] | Cao W, Zhang C F, Fan T X, et al.In situ synthesis and damping capacities of TiC reinforced magnesium matrix composites[J]. Mater. Sci. Eng., 2008, A496: 242 |
| [25] | Liu Y C, Li J F, Yang G C, et al.High damping functional materials prepared by spray deposition[J]. J. Mater. Process Technol., 2000, 106: 94 |
/
| 〈 |
|
〉 |