Phase Transformation and Texture Evolution During Cold Rolling and α'-M Reversion in High Manganese TRIP Steel
Received date: 2018-05-22
Online published: 2018-09-25
Supported by
Supported by National Natural Science Foundation of China (Nos.51771024 and 51571024)
To meet the requirement of environment, economy and safety, advanced high strength steels including dual phased (DP), complex phased (CP), transformation-induced plasticity (TRIP) and twinning-induced plasticity (TWIP) steels are widely used for automotive steel. Among them, high manganese TWIP and TRIP steels are particularly appealing due to their outstanding tensile strength and elongation. In contrast to high manganese TWIP steel, high manganese TRIP steel exhibits higher strength and work hardening rate due to strain induced martensitic transformation. The enhanced mechanical properties of high manganese TRIP steel are determined by both the stability of the retained austenite (γ ) and the initial microstructure. Strain induced martensitic transformation and subsequent reversion from deformed martensite to γ during annealing is often applied as one of the most effective methods for microstructure improvement. Microstructure and texture characteristics of high manganese TRIP steel during cold rolling together with the reversion of deformed bcc martensite (α'-M) at high temperature were investigated. It is shown that the γ was almost completely transformed into α'-M at medium cold rolling reduction. And a higher reduction after α'-M saturation resulted in dominantly the deformation of α'-M, hence thin laths paralleled to the rolling direction (RD) were obtained. The main components in α'-M were {113}<110>, {554}<225> and rotated cube ({001}<110>) textures at medium cold rolling reduction, which are the typical phase transformation textures. The {113}<110> texture rotated toward a more stable orientation {223}<110> and led to a strong cold rolling texture (<110>//RD) with increasing reduction. The reversion of martensite and recrystallization of γ proceeded at temperature ranging from 650 ℃ to 850 ℃. The reversion of α'-M proceeded in a diffusional mechanism, accompanying with the redistribution of Mn and Al between γ and α'-M. Deformed α'-M was merged by the adjacent γ , and columnar γ grains with a large amount of subgrains were obtained. The texture of reverted γ was approximately the same as that of the deformed γ , this phenomenon called texture inheritance was formed by the direct growth of γ . Subsequently, recrystallization of γ grains occurred by sub-grain coalescence and the columnar γ grains were instead by equiaxed γ grains.
Lina WANG , Ping YANG , Kai LI , Feng'e CUI , Weimin MAO . Phase Transformation and Texture Evolution During Cold Rolling and α'-M Reversion in High Manganese TRIP Steel[J]. Acta Metall Sin, 2018 , 54(12) : 1756 -1766 . DOI: 10.11900/0412.1961.2018.00222
| [1] | Frommeyer G, Brüx U, Neumann P.Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes[J]. ISIJ Int., 2003, 43: 438 |
| [2] | Gr?ssel O, Krüger L, Frommeyer G, et al.High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development-properties-application[J]. Int. J. Plast., 2000, 16: 1391 |
| [3] | Bouaziz O, Allain S, Scott C P, et al.High manganese austenitic twinning induced plasticity steels: A review of the microstructure properties relationships[J]. Curr. Opin. Solid State Mater. Sci., 2011, 15: 141 |
| [4] | Allain S, Chateau J P, Bouaziz O, et al. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys [J]. Mater. Sci. Eng., 2004, A387-389: 158 |
| [5] | Vercammen S, Blanpain B, De Cooman B C, et al. Cold rolling behaviour of an austenitic Fe-30Mn-3Si-3Al TWIP-steel: The importance of deformation twinning[J]. Acta Mater., 2004, 52: 2005 |
| [6] | Gr?ssel O, Frommeyer G.Effect of martensitic phase transformation and deformation twinning on mechanical properties of Fe-Mn-Si-Al steels[J]. Mater. Sci. Technol., 1998, 14: 1213 |
| [7] | Sato K, Ichinose M, Hirotsu Y, et al.Effects of deformation induced phase transformation and twinning on the mechanical properties of austenitic Fe-Mn-Al alloys[J]. ISIJ Int., 1989, 29: 868 |
| [8] | Sun X R, Wang H Z, Yang P, et al.Mechanical behaviors and micro-shear structures of metals with different structures by high-speed compression[J]. Acta Metall. Sin., 2014, 50: 387(孙秀荣, 王会珍, 杨平等. 不同结构金属高速压缩力学行为及微观剪切结构差异[J]. 金属学报, 2014, 50: 387) |
| [9] | Li J, Yang H Y, Yang P.Prolonged work hardening range in high manganese TRIP steel during adiabatic shear band formation[J]. Mater. Lett., 2014, 134: 180 |
| [10] | Murata Y, Ohashi S, Uematsu Y.Recent trends in the production and use of high strength stainless steels[J]. ISIJ Int., 1993, 33: 711 |
| [11] | Tomimura K, Takaki S, Tanimoto S, et al.Optimal chemical composition in Fe-Cr-Ni alloys for ultra grain refining by reversion from deformation induced martensite[J]. ISIJ Int., 1991, 31: 721 |
| [12] | Cayron C, Barcelo F, de Carlan Y. The mechanisms of the fcc-bcc martensitic transformation revealed by pole figures[J]. Acta Mater., 2010, 58: 1395 |
| [13] | Dash J, Otte H M.The martensite transformation in stainless steel[J]. Acta Metall., 1963, 11: 1169 |
| [14] | Nagy E, Mertinger V, Tranta F, et al.Deformation induced martensitic transformation in stainless steels[J]. Mater. Sci. Eng., 2004, A378: 308 |
| [15] | Ray R K, Jonas J J.Transformation textures in steels[J]. Int. Mater. Rev., 1990, 35: 1 |
| [16] | Tomota Y, Gong W, Harjo S, et al.Reverse austenite transformation behavior in a tempered martensite low-alloy steel studied using in situ neutron diffraction[J]. Scr. Mater., 2017, 133: 79 |
| [17] | Takaki S, Tomimur K, Ueda S.Effect of pre-cold-working on diffusional reversion of deformation induced martensite in metastable austenitic stainless steel[J]. ISIJ Int., 1994, 34: 522 |
| [18] | Ma Y Q, Jin J E, Lee Y K.A repetitive thermomechanical process to produce nano-crystalline in a metastable austenitic steel[J]. Scr. Mater., 2005, 52: 1311 |
| [19] | Hu B, Luo H W, Yang F, et al.Recent progress in medium-Mn steels made with new designing strategies, a review[J]. J. Mater. Sci. Technol., 2017, 33: 1457 |
| [20] | Zhang Y, Jing X T, Lou B Z, et al.Mechanism and reversible behavior of the α′→γ transformation in 1Cr18Ni9Ti stainless steel[J]. J. Mater. Sci., 1999, 34: 3291 |
| [21] | Tomimura K, Takaki S, Tokunaga Y.Reversion mechanism from deformation induced martensite to austenite in metastable austenitic stainless steels[J]. ISIJ Int., 1991, 31: 1431 |
| [22] | Johannsen D L, Kyr?l?inen A, Ferreira P J.Influence of annealing treatment on the formation of nano/submicron grain size AISI 301 austenitic stainless steels[J]. Metall. Mater. Trans., 2006, 37A: 2325 |
| [23] | Tomida T, Wakita M, Yasuyama M, et al.Memory effects of transformation textures in steel and its prediction by the double Kurdjumov-Sachs relation[J]. Acta Mater., 2013, 61: 2828 |
| [24] | Watanabe S, Kunitake T.The influence of reduction-ratio in the hot-rolling on the strength and toughness of quenched and tempered steel[J]. Tetsu Hagané, 1975, 61: 828(渡辺征一, 邦武立郎. 調質鋼の強度と靱性におよぼす熱間圧延時の圧下比の影響[J]. 鉄と鋼, 1975, 61: 828) |
| [25] | Kimmins S T, Gooch D J.Austenite memory effect in 1Cr-1Mo-0.75V(Ti, B) steel[J]. Met. Sci., 1983, 17: 519 |
| [26] | Matsuda S, Okamura Y.Reverse transformation of low-carbon low alloy steels[J]. Tetsu Hagané, 1974, 60: 226(松田昭一, 岡村義弘. 低炭素低合金鋼の逆変態[J]. 鉄と鋼, 1974, 60: 226) |
| [27] | Hara T, Maruyama N, Shinohara Y, et al.Abnormal α to γ transformation behavior of steels with a martensite and bainite microstructure at a slow reheating rate[J]. ISIJ Int., 2009, 49: 1792 |
| [28] | Zhang L W, Yang P, Wang J H, et al.Transformation of {100} texture induced by surface effect in ultra-low carbon electrical steel[J]. J. Mater. Sci., 2016, 51: 8087 |
| [29] | Zhang L W, Yang P, Mao W M.Opposite relationship between orientation selection and texture memory in the deformed electrical steel sheets during α→γ→α transformation[J]. J. Mater. Sci. Technol., 2017, 33: 1522 |
| [30] | Lu F Y, Yang P, Meng L, et al.Behavior of martensite reverse transformation in 18Mn TRIP steel during warm deformation[J]. Acta Metall. Sin., 2010, 46: 1153(鲁法云, 杨平, 孟利等. 18Mn TRIP钢温变形过程中马氏体逆相变行为[J]. 金属学报, 2010, 46: 1153) |
| [31] | Lü Y P, Hutchinson B, Molodov D A, et al.Effect of deformation and annealing on the formation and reversion of ε-martensite in an Fe-Mn-C alloy[J]. Acta Mater., 2010, 58: 3079 |
/
| 〈 |
|
〉 |