Orginal Article

High-Temperature Oxidation Resistance of Mo-Si-B Alloys with Different B Contents

  • Bin LI ,
  • Xiaohui LIN ,
  • Rui LI ,
  • Guojun ZHANG ,
  • Laiping LI ,
  • Pingxiang ZHANG
Expand
  • 1 School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China
    2 Northwest Institute for Nonferrous Metal Research, Xi'an 710016, China

Received date: 2018-01-10

  Online published: 2018-09-12

Supported by

Supported by National Natural Science Foundation of China (Nos.51701162 and 51674196), China Postdoctoral Science Foundation (No.2016M602885), Excellent Doctoral Innovation Fund of Xi'an University of Technology (No.310-252071705) and Shaanxi Postdoctoral Scientific Research Project (No.2016-BSHEDZZ07)

Abstract

The oxidation behaviors of the Mo-Si-B alloy with B content in the range of 5% to 17% (atomic fraction) were experimentally investigated at temperatures ranging from 1000 ℃ to 1300 ℃. The microstructures and antioxidant mechanisms were also analyzed. Results showed that the oxidation behaviors were affected by both B content and oxidation temperature. The formation and growth process of oxidation film were mainly influenced by the B element which could improve the fluidity of surface glass phase and adjust the volume fraction and microstructure of α-Mo, Mo3Si and Mo5SiB2. The Mo-Si-B alloy with the B content increasing was favourable for quick forming and uniform covering by improving the mobility of the glass, but which decreased the oxidation resistance due to the sufficient liquidity of the oxidation film at high temperature. The oxidation resistance of the Mo-Si-B alloy is controlled by B content at low temperature and α-Mo content at high temperature, respectively. A large quantity of Mo5SiB2 phase and a small quantity of α-Mo phase existed in the high B content of Mo-12Si-17B alloy, which could promote the oxide layer to form rapidly but also cover uniformly under the temperature range of 1000~1300 ℃. The discussion illustrates that the fine-grained microstructure combining with the distributed intermetallics is a specific role to ensure the excellent oxidation resistance of Mo-Si-B alloy.

Cite this article

Bin LI , Xiaohui LIN , Rui LI , Guojun ZHANG , Laiping LI , Pingxiang ZHANG . High-Temperature Oxidation Resistance of Mo-Si-B Alloys with Different B Contents[J]. Acta Metall Sin, 2018 , 54(12) : 1792 -1800 . DOI: 10.11900/0412.1961.2018.00015

References

[1] Akinc M, Meyer M K, Kramer M J, et al.Boron-doped molybdenum silicides for structural applications[J]. Mater. Sci. Eng., 1999, A261: 16
[2] Kruzic J J, Schneibel J H, Ritchie R O.Fracture and fatigue resistance of Mo-Si-B alloys for ultra-high-temperature structural supplications[J]. Scr. Mater., 2004, 50: 459
[3] Yu J L, Li Z K, Zheng X, et al.Superplasticity of Mo-9Si-8B-3Hf multiphase refractory alloy prepared by mechanical alloying and hot pressing sintering[J]. Acta Metall. Sin., 2011, 47: 317(喻吉良, 李中奎, 郑欣等. 机械合金化热压烧结Mo-Si-B多相难熔合金的超塑性[J]. 金属学报, 2011, 47: 317)
[4] Alur A P, Chollacoop N, Kumar K S.High-temperature compression behavior of Mo-Si-B alloys[J]. Acta Mater., 2004, 52: 5571
[5] Pan K M, Zhang L Q, Wei S Z, et al.Study on the preparation process of T2 alloy in the Mo-Si-B system[J]. Acta Metall. Sin., 2015, 51: 1377(潘昆明, 张来启, 魏世忠等. Mo-Si-B三元系中T2相合金的制备工艺研究[J]. 金属学报, 2015, 51: 1377)
[6] Derkowitz-Mattuck J B, Dils R R. High-temperature oxidation II: Molybdenum silicides[J]. J. Electrochem. Soc., 1965, 112: 583
[7] Bartlett R W, McCamont J W, Gage P R. Structure and chemistry of oxide films thermally grown on molybdenum silicides[J]. J. Am. Ceram. Soc., 1965, 48: 551
[8] Meyer M K, Akinc M.Oxidation behavior of boron-modified Mo5Si3 at 800~1300 ℃[J]. J. Am. Ceram. Soc., 1996, 79: 938
[9] Meyer M, Kramer M, Akinc M.Boron-doped molybdenum silicides[J]. Adv. Mater., 1996, 8: 85
[10] Supatarawanich V, Johnson D R, Liu C T.Oxidation behavior of multiphase Mo-Si-B alloys[J]. Intermetallics, 2004, 12: 721
[11] Wang F, Shan A D, Dong X P, et al.Microstructure and Oxidation behavior of directionally solidified Mo-Mo5SiB2(T2)-Mo3Si alloys[J]. J. Alloys Compd., 2008, 462: 436
[12] Meyer M K, Thom A J, Akinc M.Oxide scale formation and isothermal oxidation behavior of Mo-Si-B intermetallics at 600~1000 ℃[J]. Intermetallics, 1999, 7: 153
[13] Mendiratta M G, Parthasarathy T A, Dimiduk D M.Oxidation behavior of a Mo-Mo3Si- Mo5SiB2(T2) three phase system[J]. Intermetallics, 2002, 10: 225
[14] Thom A J, Kramer M J, Mandal P, et al.Wet air and simulated combusion gas exposures of Mo-Si-B alloys[J]. Scr. Mater., 2005, 53: 915
[15] Perepezko J H, Sakidja R.Oxidation resistant coatings for ultrahigh temperature refractory Mo-base alloys[J]. Adv. Eng. Mater., 2009, 11: 892
[16] Majumdar S, D?nges B, Gorr B, et al.Mechanisms of oxide scale formation on yttrium-alloyed Mo-Si-B containing fine-grained microstructure[J]. Corros. Sci., 2015, 90: 76
[17] Burk S, Gorr B, Christ H J.High temperature oxidation of Mo-Si-B alloys: Effect of low and very low oxygen partial pressures[J]. Acta Mater., 2010, 58: 6154
[18] Nowotny H, Dimakopoulou E, Kudielka H.Untersuchungen in den dreistoffsystemen: Molybd?n-Silizium-Bor, Wolfram-Silizium-Bor und in dem system: VSi2-TaSi2[J]. Monatsh. Chem., 1957, 88: 180
[19] Vance E R, Hayward P J, Hamon R F. Volatile losses from sphene glass-ceramic and borosilicate glass melts [J]. J. Am. Ceram. Soc., 1988, 71: C-318
[20] Parthasarathy T A, Mendiratta M G, Dimikuk D M.Oxidation mechanisms in Mo-reinforced Mo5SiB2(T2)-Mo3Si alloys[J]. Acta Mater., 2002, 50: 1857
[21] Thom A J, Summers E, Akinc M.Oxidation behavior of extruded Mo3Si3BX-MoSi2-MoB intermetallics from 600-1600 ℃[J]. Intermetallics, 2002, 10: 555
[22] Rioult F A, Imhoff S D, Sakidja R, et al.Transient oxidation of Mo-Si-B alloys: Effect of the microstructure size scale[J]. Acta Mater., 2009, 57: 4600
[23] Zhang G J, Kou H, Dang Q, et al.Microstructure and oxidation resistance behavior of lanthanum oxide-doped Mo-12Si-8.5B alloys[J]. Int. J. Refract. Met. Hard Mater., 2012, 30: 6
[24] Doremus R H.Glass Science[M]. New York: Wiley>, 1973: 105
[25] Morin E I, Wu J S, Stebbins J F.Modifier cation (Ba, Ca, La, Y) field strength effects on aluminum and boron coordination in aluminoborosilicate glasses: The roles of fictive temperature and boron content[J]. Appl. Phys., 2014, 116A: 479
[26] Yoshimi K, Nakatani S, Suda T, et al.Oxidation behavior of Mo5SiB2-based alloy at elevated temperature[J]. Intermetallics, 2002, 10: 407
[27] Nomura N, Suzuki T, Yoshimi K, et al.Microstructure and oxidation resistance of a plasma sprayed Mo-Si-B multiphase alloy coating[J]. Intermetallics, 2003, 11: 735
[28] Wang J, Li B, Ren S, et al.Enhanced oxidation resistance of Mo-12Si-8.5B alloys with ZrB2 addition at 1300 ℃[J]. J. Mater. Sci. Technol., 2018, 34: 635
Outlines

/