Research on Single SiC Fiber Reinforced TC17 CompositesUnder Transverse Tension
Received date: 2018-04-03
Online published: 2018-08-16
Transverse mechanical properties of titanium matrix composites (TMCs) play an important role during its engineering service. Although SiCf / TC17 composite is one of the most promising TMC candidates for aeroengine, as we know its transverse properties have not been reported yet until now. In this work, the transverse strength of single SiC fiber reinforced TC17 composite was evaluated using cruciform specimen. The surface and cross-section of fractured specimen were investigated by SEM to determine the failure position during tensile test. Finite element simulation method was also used to analyze the mechanism of interfacial failure and crack propagation. During the transverse tensile test of single fiber specimen, the initial non-linearity in the stress-strain curve occurred at the stress of (271±12) MPa, which indicated the beginning of fiber-matrix interface failure. SEM observation showed that the crack in the center of sample appeared at the interface of reaction layer and carbon coating with a 24°~68° angle to the applied loading direction and its length extended with the increase of the applied stress. The finite element simulation results based on bilinear cohesive element model showed that transverse fracture of composite interface was shear failure mode, which agreed well with the test results. Before the occurrence of non-linearity in the stress-strain curve, the crack initiated at the circular interface between reaction layer and carbon coating with a 40°~50° angle to the applied loading direction. Crack initiation locations in test samples were different with those in simulation samples, because the actual composite interface was rough and some micro-flaws formed in the interface, whereas it was assumed to be an ideal rigid interface for simulation. Then the crack propagated along both circumferential and axial directions because of the shear stress. With the crack growing, the interface close to 0°angle to the applied loading direction failed first caused by the radial tensile stress, whereas the interface near 90° failed later as a result of circumferential shear stress. After complete failure of the interface, stress redistribution occurred around the SiC fiber and the interface separation increased with the increasing of the applied load, which gave rise to the yielding and deforming of the matrix near fiber until the final fracture of the composite.
Jialin LIU , Yumin WANG , Guoxing ZHANG , Xu ZHANG , Lina YANG , Qing YANG , Rui YANG . Research on Single SiC Fiber Reinforced TC17 CompositesUnder Transverse Tension[J]. Acta Metall Sin, 2018 , 54(12) : 1809 -1817 . DOI: 10.11900/0412.1961.2018.00124
| [1] | Johnson A, Wright P.Application of advanced materials to aircraft gas turbine engines [A]. 26th Joint Propulsion Conference[C]. Orlando: American Institute of Aeronautics and Astronautics, 1990: 2281 |
| [2] | Wang Y M, Zhang G X, Zhang X, et al.Advances in SiC fiber reinforced titanium matrix composites[J]. Acta Metall. Sin., 2016, 52: 1153(王玉敏, 张国兴, 张旭等. 连续SiC纤维增强钛基复合材料研究进展[J]. 金属学报, 2016, 52: 1153) |
| [3] | Hyde T H, Punyong K, Becker A A.Elasto-plastic finite element analysis of titanium metal matrix composite shafts under torsional loading[J]. J. Strain Anal. Eng. Des., 2015, 50: 199 |
| [4] | Leyens C, Kocian F, Hausmann J, et al.Materials and design concepts for high performance compressor components[J]. Aerosp. Sci. Technol., 2003, 7: 201 |
| [5] | Carrere N, Feyel F, Kruch S.Multi-scale modelling of silicon carbide reinforced titanium MMCs: Application to advanced compressor design[J]. Aerosp. Sci. Technol., 2003, 7: 307 |
| [6] | Aghdam M M, Pavier M J, Smith D J.Micro-mechanics of off-axis loading of metal matrix composites using finite element analysis[J]. Int. J. Solids Struct., 2001, 38: 3905 |
| [7] | Ismar H, Schr?ter F, Streicher F.Effects of interfacial debonding on the transverse loading behaviour of continuous fibre-reinforced metal matrix composites[J]. Comput. Struct., 2001, 79: 1713 |
| [8] | Hu S F.The transverse failure of a single-fiber metal-matrix composite: Experiment and modeling[J]. Compos. Sci. Technol., 1996, 56: 667 |
| [9] | Dong M, Schmauder S.Transverse mechanical behaviour of fiber reinforced composites-FE modelling with embedded cell models[J]. Comput. Mater. Sci., 1996, 5: 53 |
| [10] | Li D S, Wisnom M R.Factors controlling the transverse tensile properties of unidirectional SiC/Ti-6AI-4V[J]. Compos. Eng., 1995, 5: 235 |
| [11] | Gundel D B, Miracle D B.The influence of interface structure and composition on the response of single-fiber SiC/Ti-6Al-4V composites to transverse tension[J]. Appl. Compos. Mater., 1998, 5: 95 |
| [12] | Gundel D B, Warrier S G, Miracle D B.The interface debond stress in single and multiple SiC fiber/Ti-6Al-4V composites under transverse tension[J]. Acta Mater., 1997, 45: 1275 |
| [13] | Warrier S G, Gundel D B, Majumdar B S, et al.Stress distribution in a transversely loaded cross-shaped single fiber SCS-6/Ti-6Al-4V composite[J]. Scr. Mater., 1996, 34: 293 |
| [14] | Akser E O, Choy K L.Finite element analysis of the stress distribution in a thermally and transversely loaded Ti-6Al-4V/SiC fibre composite[J]. Compos. Part. Appl. Sci. Manufactur., 2001, 32A: 243 |
| [15] | Warrier S G, Majumdar B S, Gundel D B, et al.Implications of tangential shear stress induced failure during transverse loading of SiCTi-6Al-4V composites[J]. Acta Mater., 1997, 45: 3469 |
| [16] | Gundel D B, Warrier S G, Miracle D B.The transverse tensile behavior of SiC-fiber/Ti-6Al-4V composites 2. Stress distribution and interface failure[J]. Compos. Sci. Technol., 1999, 59: 1087 |
| [17] | Gundel D B, Miracle D B.Transverse tensile behavior of SiC-fiber/Ti-6Al-4V composites—1. Experimental results[J]. Compos. Sci. Technol., 1998, 58: 1571 |
| [18] | Lou J H, Yang Y Q, Luo X, et al.Effects of fiber volume fraction on transverse tensile properties of SiC/Ti-6Al-4V composites[J]. Rare Met. Mater. Eng., 2011, 40: 575 |
| [19] | De Kok J M M, Meijer H E H. Deformation, yield and fracture of unidirectional composites in transverse loading: 1. Influence of fibre volume fraction and test-temperature[J]. Composites, 1999, 30A: 905 |
| [20] | Lou J H, Yang Y Q, Luo X, et al.The analysis on transverse tensile behavior of SiC/Ti-6Al-4V composites by finite element method[J]. Mater. Des., 2010, 31: 3949 |
| [21] | John R, Buchanan D J, Larsen J M.Prediction of transverse fatigue behavior of unidirectionally reinforced metal matrix composites[J]. Scr. Mater., 1998, 39: 1529 |
| [22] | Carrere N, Valle R, Bretheau T, et al.Multiscale analysis of the transverse properties of Ti-based matrix composites reinforced by SiC fibres: From the grain scale to the macroscopic scale[J]. Int. J. Plast., 2004, 20: 783 |
| [23] | Collings E W, Welsch G.Materials Properties Handbook: Titanium Alloys[M]. Materials Park, OH, USA: ASM International, 1994: 453 |
| [24] | Zhao C B, Wang Y M, Zhang G X, et al.Effect of heat treatment on the microstructure and properties of CVD SiC fiber[J]. J. Mater. Sci. Technol., 2017, 33: 1378 |
| [25] | Zhang X, Wang Y M, Lei J F, et al.The interfacial thermal stability and element diffusion mechanism of SiCf/TC17 composite[J]. Acta Metall. Sin., 2012, 48: 1306(张旭, 王玉敏, 雷家峰等. SiCf/TC17复合材料界面热稳定性及元素扩散机理[J]. 金属学报, 2012, 48: 1306) |
| [26] | Zhang X, Wang Y M, Yang Q, et al.Study on tensile behavior of SiCf/TC17 composites[J]. Acta Metall. Sin., 2015, 51: 1025(张旭, 王玉敏, 杨青等. SiCf/TC17复合材料拉伸行为研究[J]. 金属学报, 2015, 51: 1025) |
| [27] | Liu P F, Li X K.Explicit finite element analysis of failure behaviors of thermoplastic composites under transverse tension and shear[J]. Compos. Struct., 2018, 192: 131 |
| [28] | Chandra N, Li H, Shet C, et al.Some issues in the application of cohesive zone models for metal-ceramic interfaces[J]. Int. J. Solids Struct., 2002, 39: 2827 |
| [29] | Zhang X.Study on interface reaction, residual stress and mechanical properties of SiCf/TC17 composite [D]. Shenyang: Institute of Metal Research, 2013(张旭. SiCf/TC17复合材料界面反应、残余应力及力学性能研究 [D]. 沈阳: 中国科学院金属研究所, 2013) |
| [30] | Timoshenko S P, Goodier J N.Theory of Elasticity[M]. 3rd Ed., New York: McGraw-Hill Book Company, 1970: 18 |
| [31] | Li K J, Yang Y Q, Luo X, et al.Transverse mechanical properties of continuous SiC fiber reinforced titanium matrix composites[J]. Rare Met. Mater. Eng., 2009, 38: 426 |
/
| 〈 |
|
〉 |