Hydrogen embrittlement, the degradation of mechanical behaviors due to the existence of hydrogen, is an industrially and environmentally critical problem in metals and alloys. Yet the fundamental mechanism(s) of embrittlement are still controversial, and the molecular-level damage events shrouded in mystery. In hydrogen embrittlement phenomena, the molecular-level agents of damage are hypothesized to be hydrogen-vacancy complex (Va+nH→VaHn), hereupon called hydrogenated vacancy. Contrary to vacancy, hydrogen-vacancy complex has good thermal stability and low diffusivity. When metals undergo plastic deformation at low homologous temperature in the presence of hydrogen, the mechanically driven out-of-equilibrium dislocation processes produce extremely high concentrations of hydrogen-vacancy complexes. Under such high concentrations, these complexes prefer to grow by absorbing additional vacancies and act as the embryos for the formation of proto nano-voids. Our work provides the insight on the microscopic mechanism of hydrogen embrittlement. Moreover, this work also helps understanding some unique mechanical behaviors induced by hydrogen.
Jun SUN , Suzhi LI , Xiangdong DING , Ju LI . Hydrogenated Vacancy: Basic Properties and Its Influence on Mechanical Behaviors of Metals[J]. Acta Metall Sin, 2018 , 54(11) : 1683 -1692 . DOI: 10.11900/0412.1961.2018.00341
| [1] | Barnoush A, Horst V.Recent developments in the study of hydrogen embrittlement: Hydrogen effect on dislocation nucleation[J]. Acta Mater., 2010, 58: 5274 |
| [2] | Myers S M, Baskes M I, Birnbaum H K, et al.Hydrogen interactions with defects in crystalline solids[J]. Rev. Mod. Phys., 1992, 64: 559 |
| [3] | Gahr S, Grossbeck M L, Birnbaum H K.Hydrogen embrittlement of Nb I—Macroscopic behavior at low temperatures[J]. Acta Metall., 1977, 25: 125 |
| [4] | Gerberich W W, Oriani R A, Lii M J, et al.The necessity of both plasticity and brittleness in the fracture thresholds of iron[J]. Philos. Mag., 1991, 63A: 363 |
| [5] | Nakasato F, Bernstein I M.Crystallographic and fractographic studies of hydrogen-induced cracking in purified iron and iron-silicon alloys[J]. Metall. Trans., 1978, 9A: 1317 |
| [6] | Birnbaum H K, Sofronis P.Hydrogen-enhanced localized plasticity—A mechanism for hydrogen-related fracture[J]. Mater. Sci. Eng., 1994, A176: 191 |
| [7] | Robertson I M.The effect of hydrogen on dislocation dynamics[J]. Eng. Fract. Mech., 2001, 68: 671 |
| [8] | Nagumo M, Nakamura M, Takai K.Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels[J]. Metall. Mater. Trans., 2001, 32A: 339 |
| [9] | Sakaki K, Kawase T, Hirato M, et al.The effect of hydrogen on vacancy generation in iron by plastic deformation[J]. Scr. Mater., 2006, 55: 1031 |
| [10] | Takai K, Shoda H, Suzuki H, et al.Lattice defects dominating hydrogen-related failure of metals[J]. Acta Mater., 2008, 56: 5158 |
| [11] | Griffith A A.The phenomena of rupture and flow in solids[J]. Philos. Trans. Roy. Soc. London, 1921, 221A: 163 |
| [12] | Sarkar S, Li J, Cox W T, et al.Finding activation pathway of coupled displacive-diffusional defect processes in atomistics: Dislocation climb in fcc copper[J]. Phys. Rev., 2012, 86B: 014115 |
| [13] | Hayward E, Fu C C.Interplay between hydrogen and vacancies in α-Fe[J]. Phys. Rev., 2013, 87B: 174103 |
| [14] | Lu G, Kaxiras E.Hydrogen embrittlement of aluminum: The crucial role of vacancies[J]. Phys. Rev. Lett., 2005, 94: 155501 |
| [15] | Tateyama Y, Ohno T.Stability and clusterization of hydrogen-vacancy complexes in α-Fe: An ab initio study[J]. Phys. Rev., 2003, 67B: 174105 |
| [16] | Li S Z, Li Y G, Lo Y C, et al.The interaction of dislocations and hydrogen-vacancy complexes and its importance for deformation-induced proto nano-voids formation in α-Fe[J]. Int. J. Plast., 2015, 74: 175 |
| [17] | Henkelman G, Jonsson H.Improved tangent estimate in the nudged elastic band method for finding minimum energy paths and saddle points[J]. J. Chem. Phys., 2000, 113: 9978 |
| [18] | Hirth J P, Lothe J.Theory of Dislocations[M]. 2nd Ed., New York: Wiley, 1992: 1 |
| [19] | Militzer M, Sun W P, Jonas J J.Modelling the effect of deformation-induced vacancies on segregation and precipitation[J]. Acta Metall. Mater., 1994, 42: 133 |
| [20] | Mecking H, Estrin Y.The effect of vacancy generation on plastic deformation[J]. Scr. Mater., 1980, 14: 815 |
| [21] | Kraftmakher Y.Equilibrium vacancies and thermophysical properties of metals[J]. Phys. Rep., 1998, 299: 79 |
| [22] | Fischer F D, Svoboda J, Appel F, et al.Modeling of excess vacancy annihilation at different types of sinks[J]. Acta Mater., 2011, 59: 3463 |
| [23] | Brailsford A D, Bullough R.The rate theory of swelling due to void growth in irradiated metals[J]. J. Nucl. Mater., 1972, 44: 121 |
| [24] | Zehetbauer M.Cold work hardening in stages IV and V of F.C.C. metals—II. Model fits and physical results[J]. Acta Metall. Mater., 1993, 41: 589 |
| [25] | Valiev R Z, Ivanisenko Y V, Rauch E F, et al.Structure and deformaton behaviour of Armco iron subjected to severe plastic deformation[J]. Acta Mater., 1996, 44: 4705 |
| [26] | Bortz A B, Kalos M H, Lebowitz J L.A new algorithm for Monte Carlo simulation of Ising spin systems[J]. J. Comput. Phys., 1975, 17: 10 |
| [27] | Fichthorn K A, Weinberg W H.Theoretical foundations of dynamical monte carlo simulations[J]. J. Chem. Phys., 1991, 95: 1090 |
| [28] | Li Y G, Zhou W H, Ning R H, et al.A cluster dynamics model for accumulation of helium in tungsten under helium ions and neutron irradiation[J]. Commun. Comput. Phys., 2012, 11: 1547 |
| [29] | Golubov S I, Ovcharenko A M, Barashev A V, et al.Grouping method for the approximate solution of a kinetic equation describing the evolution of point-defect clusters[J]. Philos. Mag., 2001, 81A: 643 |
| [30] | Neeraj T, Srinivasan R, Li J.Hydrogen embrittlement of ferritic steels: Observations on deformation microstructure, nanoscale dimples and failure by nanovoiding[J]. Acta Mater., 2012, 60: 5160 |
| [31] | Hru?ka P, ?í?ek J, Knapp J, et al. Characterization of defects in titanium created by hydrogen charging[J]. Int. J. Hydrogen Energy, 2017, 42: 22557 |
| [32] | Doshida T, Suzuki H, Takai K, et al.Enhanced lattice defect formation associated with hydrogen and hydrogen embrittlement under elastic stress of a tempered martensitic steel[J]. ISIJ Int., 2012, 52: 198 |
| [33] | Rosenberg G, Sinaiova I.Evaluation of hydrogen induced damage of steels by different test methods[J]. Mater. Sci. Eng., 2017, A682: 410 |
| [34] | Xie D G, Li S Z, Li M, et al.Hydrogenated vacancies lock dislocations in aluminium[J]. Nat. Commun., 2016, 7: 13341 |
| [35] | Zhou X, Song J.Effects of alloying elements on vacancies and vacancy-hydrogen clusters at coherent twin boundaries in nickel alloys[J]. Acta Mater., 2018, 148: 9 |
| [36] | Li M, Xie D G, Ma E, et al.Effect of hydrogen on the integrity of aluminium-oxide interface at elevated temperatures[J]. Nat. Commun., 2017, 8: 14564 |
/
| 〈 |
|
〉 |