Orginal Article

Protection Mechanism Study of Enamel-Based Composite Coatings Under the Simulated Combusting Gas Shock

  • Cean GUO ,
  • Minghui CHEN ,
  • Yimin LIAO ,
  • Bei SU ,
  • Dongbai XIE ,
  • Shenglong ZHU ,
  • Fuhui WANG
Expand
  • 1 Equipment Engineering School, Shenyang Ligong University, Shenyang 110159, China
    2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3 Chongqing Jianshe Industry (Group) LLC, Chongqing 400054, China
    4 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    5 Xinjiang Police College, Urumqi 830011, China

Received date: 2018-05-25

  Online published: 2018-07-06

Supported by

Supported by National Natural Science Foundation of China (No.51471177), Fundamental Research Funds for the Central Universities (No.N160205001) and National Science Foundation of Liaoning Province of China (No.201602643)

Abstract

High-temperature-resistant enamel coatings have been reported to be applied in non-critical hot end components of aero-engine and gas turbine recently. Although the enamel with a series of excellent properties can be as high-temperature-resistant coating material under appropriate condition, its lower soft point and inherent brittleness limit their use in broader application under severe service condition. Enamel-based composite coatings (an enamel matrix with the addition of ceramic particles and/or metal platelets) can remarkably increase the properties of the enamel coating and their protection mechanism under dynamic thermal shock needs further investigation. In this work, two kinds of enamel-based composite coatings, 70%enamel+25%Al2O3 and 70%enamel+20%Al2O3+10%NiCrAlY (mass fraction, %) abbreviated to E25A and E20A10M respectively, were designed and fired on K38G superalloy substrate, and their protection mechanism was comparatively studied at 900 ℃ under the simulated combusting gas shock. The thermal shock fire was produced by the mixture gas of C3H8+O2 and its ejecting pressure on the coating surface was 0.4 MPa. After the temperature has been stable at 900 ℃, samples were hold for 15 s and then cooling down in air for 120 s, constituting a thermal shock cycle. Results indicated that, after 150 cyc of thermal shock, both the coatings bond well with the alloy substrate, thus shows high resistance to spallation along interface. For the E25A coating, its microstructure had no obvious change after thermal shock and the surface is still intact. The addition of secondary phase Al2O3 increases the stability of enamel at high temperature. With regard to the E20A10M coating, holes and cracks form consecutively, and peeling off occurs at surface after thermal shock. Interfacial reaction between the NiCrAlY particles and enamel following Cr(NiCrAlY)+ZnO(enamel)→CrO(interface)+Zn↑ results in the formation of enamel swelling, which then, under the synergistic effect of combusting gas shear stress and interface thermal stress, leads to the peeling off of enamel and metal inclusions at surface.

Cite this article

Cean GUO , Minghui CHEN , Yimin LIAO , Bei SU , Dongbai XIE , Shenglong ZHU , Fuhui WANG . Protection Mechanism Study of Enamel-Based Composite Coatings Under the Simulated Combusting Gas Shock[J]. Acta Metall Sin, 2018 , 54(12) : 1825 -1832 . DOI: 10.11900/0412.1961.2018.00230

References

[1] Liu W, Li W Z, Yang J B, et al.Current research status of enamel coatings on titanium alloys[J]. Mater. Rev., 2013, 27(3): 45(刘伟, 李伟洲, 杨剑冰等. 钛合金搪瓷涂层研究现状[J]. 材料导报, 2013, 27(3): 45)
[2] Zhang C Y, Zhang Q G, Yang W K.Research on process improvement of the enamel coating for the 2nd stage guide vane of certain turbojet engine[J]. Aviat. Maint. Eng., 2015, (10): 99(张从艳, 张清贵, 杨武奎. 某型涡喷发动机II级导向器叶片搪瓷涂层工艺方法改进技术研究[J]. 航空维修与工程, 2015, (10): 99)
[3] Choi S Y, Ahn J M.Viscous sintering and mechanical properties of 3Y-TZP-reinforced LAS glass-ceramic composites[J]. J. Am. Ceram. Soc., 1997, 80: 2982
[4] Boccaccini A R, Pearce D H.Toughening of glass by a piezoelectric secondary phase[J]. J. Am. Ceram. Soc., 2003, 86: 180
[5] Rouxel T, Baron B, Verdier P, et al.SiC particle reinforced oxynitride glass: Stress relaxation, creep and strain-rate imposed experiments[J]. Acta Mater., 1998, 46: 6115
[6] Lange F F.Fracture energy and strength behavior of a sodium borosilicate glass-Al2O3 composite system[J]. J. Am. Ceram. Soc., 1971, 54: 614
[7] Bolelli G, Cannillo V, Lusvarghi L, et al.Glass-alumina composite coatings by plasma spraying. Part I: Microstructural and mechanical characterization[J]. Surf. Coat. Technol., 2006, 201: 458
[8] Ray A, Tiwari A N.Compaction and sintering behaviour of glass-alumina composites[J]. Mater. Chem. Phys., 2001, 67: 220
[9] Krstic V V, Nicholson P S, Hoagland R G.Toughening of glasses by metallic particles[J]. J. Am. Ceram. Soc., 1981, 64: 499
[10] Banuprakash G, Katyal V, Murthy V S R, et al. Mechanical behaviour of borosilicate glass-copper composites[J]. Composites, 1997, 28A: 861
[11] Cannillo V, Leonelli C, Manfredini T, et al.Mechanical performance and fracture behaviour of glass-matrix composites reinforced with molybdenum particles[J]. Compos. Sci. Technol., 2005, 65: 1276
[12] Dlouhy I, Reinisch M, Boccaccini A R, et al.Fracture characteristics of borosilicate glasses reinforced by metallic particles[J]. Fatigue Fract. Eng. Mater. Struct., 1997, 20: 1235
[13] Biswas D R.Strength and fracture toughness of indented glass-nickel compacts[J]. J. Mater. Sci., 1980, 15: 1696
[14] Nivas Y, Fulrath R M.Limitation of Griffith flaws in glass-matrix composites[J]. J. Am. Ceram. Soc., 1970, 53: 188
[15] Dlouhy I, Boccaccini A R.Preparation, microstructure and mechanical properties of metal-particulate/glass-matrix composites[J]. Compos. Sci. Technol., 1996, 56: 1415
[16] Pernot F, Rogier R.Mechanical properties of phosphate glass-ceramic-316L stainless steel composites[J]. J. Mater. Sci., 1993, 28: 6676
[17] Guo J T, Yuan C, Yang H C, et al.Creep-rupture behavior of a directionally solidified nickel-base superalloy[J]. Metall. Mater. Trans., 2001, 32A: 1103
[18] Wang J L, Chen M H, Cheng Y X, et al.Hot corrosion of arc ion plating NiCrAlY and sputtered nanocrystalline coatings on a nickel-based single-crystal superalloy[J]. Corros. Sci., 2017, 123: 27
[19] Guo C A, Wang W, Cheng Y Y, et al.Yttria partially stabilised zirconia as diffusion barrier between NiCrAlY and Ni-base single crystal René N5 superalloy[J]. Corros. Sci., 2015, 94: 122
[20] Chen M H, Shen M L, Wang X, et al.Oxidation and thermal shock behavior of a glass-alumina composite coating on K38G superalloy at 1000 ℃[J]. J. Mater. Sci. Technol., 2012, 28: 433
[21] Wu M Y.A study on microstructure regulation and protection mechanism against high temperature oxidation of enamel-based composite coatings [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2017(邬明玉. 搪瓷基复合涂层的组织结构调控及抗高温氧化机制研究 [D]. 沈阳: 中国科学院金属研究所, 2017)
[22] Chen M H, Zhu S L, Shen M L, et al.Effect of NiCrAlY platelets inclusion on the mechanical and thermal shock properties of glass matrix composites[J]. Mater. Sci. Eng., 2011, A528: 1360
[23] Chen M H, Zhu S L, Wang F H.High temperature oxidation of NiCrAlY, nanocrystalline and enamel-metal nano-composite coatings under thermal shock[J]. Corros. Sci., 2015, 100: 556
[24] Feng M, Chen M H, Yu Z D, et al.Comparative study of thermal shock behavior of the arc ion plating NiCrAlY and the enamel based composite coatings[J]. Acta Metall. Sin., 2017, 53: 1636(丰敏, 陈明辉, 余中狄等. 多弧离子镀NiCrAlY涂层与搪瓷基复合涂层的抗热震行为对比研究[J]. 金属学报, 2017, 53: 1636)
[25] Donald I W.Preparation, properties and chemistry of glass- and glass-ceramic-to-metal seals and coatings[J]. J. Mater. Sci., 1993, 28: 2841
[26] Donald I W, Metcalfe B L, Gerrard L A.Interfacial reactions in glass-ceramic-to-metal seals[J]. J. Am. Ceram. Soc., 2008, 91: 715
Outlines

/