Orginal Article

Out-of-Plane Constraint Effect on the Fracture Toughness of Single Edge Notch Tension Specimens

  • Yizhe LI ,
  • Baoming GONG ,
  • Xiuguo LIU ,
  • Dongpo WANG ,
  • Caiyan DENG
Expand
  • Tianjin Key Laboratory of Advanced Joining Technology, School of Materials Science and Engineering, Tianjin University, Tianjin 300354, China

Received date: 2018-04-02

  Online published: 2018-07-05

Supported by

Supported by National Natural Science Foundation of China (No.51305295) and National Key Research and Development Program of China (No.2016YFC0802105)

Abstract

The crack-tip stress and strain fields of single edge notch tension (SENT) specimen are similar to those of the full-scale pipe containing surface cracks under longitudinal tension and/or internal pressure. It is well known that material's fracture toughness is not constant, and the specimen size has a significant influence on fracture toughness. It is thus essential to consider the transferability from fracture specimens in laboratory testing to practical structures, i.e., size effects or constraint effects. However, the specimen dimensions for SENT specimens recommended by current design procedures have not validated the out-of-plane constraint effect on the fracture toughness. In this work, the effect of specimen thickness on the crack tip opening displacement (CTOD) of SENT specimen was investigated using an API X90 grade steel. Full-field deformation measurement by digital image correlation (DIC) technique and stretching zone width (SZW) examination were performed to analyze the size effects on fracture toughness. The results show that the critical crack initiation toughness is highly sensitive to specimen thickness, and decreases significantly as specimen thickness increases until the thickness-to-width ratio (B/W) equals to 4, beyond which the effect of specimen thickness becomes relatively weak. As the specimen thickness increases, the maximum longitudinal strain and stretching zone width decrease sharply, and the location of high-strain zones changes significantly; when B/W≥3, strain is initiated from the area opposite the cracked side rather than from the crack tip, indicating a strong loss of plasticity for thicker specimens. A dimension size is recommended for the fracture toughness testing to take the out-of-plane constraint into account for SENT specimen.

Cite this article

Yizhe LI , Baoming GONG , Xiuguo LIU , Dongpo WANG , Caiyan DENG . Out-of-Plane Constraint Effect on the Fracture Toughness of Single Edge Notch Tension Specimens[J]. Acta Metall Sin, 2018 , 54(12) : 1785 -1791 . DOI: 10.11900/0412.1961.2018.00122

References

[1] British Standard Institution.Guide to methods for assessing the acceptability of flaws in metallic structures[S]. London: British Standard Institution, 2007
[2] Paredes M, Ruggieri C.Further results in J and CTOD estimation procedures for SE(T) fracture specimens- Part II: Weld centerline cracks[J]. Eng. Fract. Mech., 2012, 89: 24
[3] Chen Y, Lambert S.Analysis of ductile tearing of pipeline-steel in single edge notch tension specimens[J]. Int. J. Fract., 2003, 124: 179
[4] Tang H, Macia M, Minnaar K, et al.Development of the SENT test for strain-based design of welded pipelines [A]. The 8th International Pipeline Conference[C]. Calgary, Alberta, Canada: American Society of Mechanical Engineers, 2010: 303
[5] Pisarski H G.Determination of pipe girth weld fracture toughness using SENT specimens [A]. The 8th International Pipeline Conference[C]. Calgary, Alberta, Canada: American Society of Mechanical Engineers, 2010: 217
[6] API 579. Recommended practice 579, for fitness-for-service[S]. Washington, DC: American Petroleum Institute, 2000
[7] BSI 7910. Guide on methods for assessing the acceptability of flaws in metallic structuresSI 7910. Guide on methods for assessing the acceptability of flaws in metallic structures[S]. London: British Standards Institution, 1999
[8] Wallin K.The size effect in KIC results[J]. Eng. Fract. Mech., 1985, 22: 149
[9] Yang J, Wang G Z, Xuan F Z, et al.Unified characterisation of in-plane and out-of-plane constraint based on crack-tip equivalent plastic strain[J]. Fatigue Fract. Eng. Mater. Struct., 2013, 36: 504
[10] Hebel J, Hohe J, Friedmann V, et al.Experimental and numerical analysis of in-plane and out-of-plane crack tip constraint characterization by secondary fracture parameters[J]. Int. J. Fract., 2007, 146: 173
[11] Sarzosa D F B, Ruggieri C. A numerical investigation of constraint effects in circumferentially cracked pipes and fracture specimens including ductile tearing [J]. Int. J. Press. Vessels Pip., 2014, 120-121: 1
[12] DNV-OS-F101. Submarine pipeline systems text version[S]. Norway: Det Norske Veritas, 2010
[13] BSI 8571 Method of test for determination of fracture toughness in metallic materials using single edge notched tension (SENT) specimens[S]. London: British Standards Institution, 2014
[14] Lu K, Meshii T.Three-dimensional T-stresses for three-point-bend specimens with large thickness variation[J]. Eng. Fract. Mech., 2014, 116: 197
[15] Shlyannikov V N, Boychenko N V, Tumanov A V, et al.The elastic and plastic constraint parameters for three-dimensional problems[J]. Eng. Fract. Mech., 2014, 127: 83
[16] Meshii T, Lu K, Fujiwara Y.Extended investigation of the test specimen thickness (TST) effect on the fracture toughness (Jc) of a material in the ductile-to-brittle transition temperature region as a difference in the crack tip constraint—What is the loss of constraint in the TST effects on Jc ?[J]. Eng. Fract. Mech., 2015, 135: 286
[17] American Society for Testing and Materials. ASTM E1820-17 Standard test method for measurement of fracture toughness[S]. America: American Society for Testing and Materials, 2013
[18] Shen G W, Tyson W R, Gianetto J A, et al.Effect of side grooves on compliance, J-integral and constraint of a clamped SE(T) specimen [A]. ASME 2010 Pressure Vessels and Piping Division/K-PVP Conference[C]. Bellevue, Washington, USA: Pressure Vessels and Piping Division, 2010: 81
[19] Li Y Z, Gong B M, Corrado M, et al. Experimental investigation of out-of-plane constraint effect on fracture toughness of the SE(T) specimens [J]. Int. J. Mech. Sci., 2017, 128-129: 644
[20] Verstraete M A, Hertelé S, Denys R M, et al.Evaluation and interpretation of ductile crack extension in SENT specimens using unloading compliance technique[J]. Eng. Fract. Mech., 2014, 115: 190
[21] Verstraete M A, Denys R M, Van Minnebruggen K, et al.Determination of CTOD resistance curves in side-grooved single-edge notched tensile specimens using full field deformation measurements[J]. Eng. Fract. Mech., 2013, 110: 12
[22] Moore P L, Pisarski H G.Validation of methods to determine CTOD from SENT specimens [A]. The 22nd International Ocean and Polar Engineering Conference[C]. Rodos Palace Hotel, Rhodes, Greece: ISOPE, 2012: 577
[23] Zhu X K, Zelenak P, McGaughy T. Comparative study of CTOD-resistance curve test methods for SENT specimens[J]. Eng. Fract. Mech., 2017, 172: 17
[24] Meshii T, Lu K, Takamura R.A failure criterion to explain the test specimen thickness effect on fracture toughness in the transition temperature region[J]. Eng. Fract. Mech., 2013, 104: 184
[25] Bansal S, Nath S K, Ghosh P K, et al.Stretched zone width and blunting line equation for determination of initiation fracture toughness in low carbon highly ductile steels[J]. Int. J. Fract., 2009, 159: 43
Outlines

/