Sn-Induced Modification of the Precipitation Pathways upon High-Temperature Ageing in an Al-Mg-Si Alloy

  • Xuemei XIANG ,
  • Yuxiang LAI ,
  • Chunhui LIU ,
  • Jianghua CHEN
Expand
  • College of Materials Science and Engineering, Hunan University, Changsha 410082, China

Received date: 2018-04-04

  Online published: 2018-06-29

Supported by

Supported by National Key Research and Development Program of China (No.2016YFB0300801) and National Natural Science Foundation of China (Nos.11427806, 51471067 and 51671082)

Abstract

The 6xxx series aluminum alloys (Al-Mg-Si(-Cu) alloys) are widely used for the industrial applications in the lightweight construction, automotive and architecture because of their light weight, medium to high strength, excellent formability and good corrosion resistance. It has been reported that trace Sn addition can accelerate ageing kinetics and increase peak hardness of Al-Mg-Si alloys when ageing at high temperatures (>210 ℃). However, the mechanism about it has not been investigated comprehensively yet. For Mg-excess Al-Mg-Si alloys, when aged at 250 ℃, the alloys are hardened by the β'-precipitates. While after applying natural ageing prior to artificial ageing, the β"-precipitates will be formed, with the percentage of which increasing with natural ageing time, and eventually become the main hardening precipitates. In this work, the effect of Sn on natural ageing and subsequent artificial ageing at 250 ℃ in a Mg-rich Al-Mg-Si alloy was investigated by Vickers microhardness measurements and TEM. The results show that adding a small amount (0.2%, mass fraction) of Sn in the Mg-rich Al-Mg-Si alloy can modify the precipitation pathways upon 250 ℃-ageing: when the alloy is directly artificially aged, the β"-precipitates are dominant, whereas when the alloy is subjected to "natural ageing+artificial ageing" treatment, upon prolonged natural ageing time, the percentage of β"-precipitates would not increase but decrease and that of β'-precipitates would not decrease but increase, but ultimately the β"-precipitates are still dominant over the β'-precipitates. The Sn-induced modification of the precipitation pathways can significantly enhance the age-hardening potential of the alloy upon high-temperature artificial ageing. The addition of Sn increases the effective Si-concentration in the matrix, and consequently changes the precipitation pathways in the Sn-free alloy, which is different from the explanation proposed in literatures.

Cite this article

Xuemei XIANG , Yuxiang LAI , Chunhui LIU , Jianghua CHEN . Sn-Induced Modification of the Precipitation Pathways upon High-Temperature Ageing in an Al-Mg-Si Alloy[J]. Acta Metall Sin, 2018 , 54(9) : 1273 -1280 . DOI: 10.11900/0412.1961.2018.00125

References

[1] Edwards G A, Stiller K, Dunlop G L, et al.The precipitation sequence in Al-Mg-Si alloys[J]. Acta Mater., 1998, 46: 3893
[2] Marioara C D, Andersen S J, Jansen J, et al.The influence of temperature and storage time at RT on nucleation of the β" phase in a 6082 Al-Mg-Si alloy[J]. Acta Mater., 2003, 51: 789
[3] Zhang H, Li L X, Yuan D, et al.Hot deformation behavior of the new Al-Mg-Si-Cu aluminum alloy during compression at elevated temperatures[J]. Mater. Charact., 2007, 58: 168
[4] Tian N, Zhao G, Zuo L, et al.Study on the strain hardening behavior of Al-Mg-Si-Cu alloy sheet for automotive body[J]. Acta Metall. Sin., 2010, 46: 613(田妮, 赵刚, 左良等. 汽车车身用Al-Mg-Si-Cu合金薄板应变强化行为的研究[J]. 金属学报, 2010, 46: 613)
[5] Li L X, Zhou J, Zhang H.Advanced extrusion technology and application of aluminium, magnesium alloy for vehicle body[J]. J. Mech. Eng., 2012, 48(18): 35(李落星, 周佳, 张辉. 车身用铝、镁合金先进挤压成形技术及应用[J]. 机械工程学报, 2012, 48(18): 35)
[6] Zandbergen H W, Andersen S J, Jansen J.Structure determination of Mg5Si6 particles in Al by dynamic electron diffraction studies[J]. Science, 1997, 277: 1221
[7] Chen J H, Costan E, van Huis M A, et al. Atomic pillar-based nanoprecipitates strengthen Al-Mg-Si alloys[J]. Science, 2006, 312: 416
[8] Vissers R, van Huis M A, Jansen J, et al. The crystal structure of the β' phase in Al-Mg-Si alloys[J]. Acta Mater., 2007, 55: 3815
[9] Ravi C, Wolverton C.First-principles study of crystal structure and stability of Al-Mg-Si-(Cu) precipitates[J]. Acta Mater., 2004, 52: 4213
[10] Wang B, Wang X J, Song H, et al.Strengthening effects of microstructure evolution during early ageing process in Al-Mg-Si alloy[J]. Acta Metall. Sin., 2014, 50: 685(汪波, 王晓姣, 宋辉等. Al-Mg-Si合金时效早期显微组织演变及其对强化的影响[J]. 金属学报, 2014, 50: 685)
[11] Lai Y X, Jiang B C, Liu C H, et al.Low-alloy-correlated reversal of the precipitation sequence in Al-Mg-Si alloys[J]. J. Alloys Compd., 2017, 701: 94
[12] Pogatscher S, Antrekowitsch H, Leitner H, et al.Mechanisms controlling the artificial aging of Al-Mg-Si Alloys[J]. Acta Mater., 2011, 59: 3352
[13] de Geuser F, Lefebvre W, Blavette D. 3D atom probe study of solute atoms clustering during natural ageing and pre-ageing of an Al-Mg-Si alloy[J]. Philos. Mag. Lett., 2006, 86: 227
[14] Tors?ter M, Hasting H S, Lefebvre W, et al.The influence of composition and natural aging on clustering during preaging in Al-Mg-Si alloys[J]. J. Appl. Phys., 2010, 108: 073527
[15] R?yset J, Stene T, S?ter J A, et al. The effect of intermediate storage temperature and time on the age hardening response of Al-Mg-Si Alloys [J]. Mater. Sci. Forum, 2006, 519-521: 239
[16] Banhart J, Chang C S T, Liang Z Q, et al. Natural aging in Al-Mg-Si alloys—A process of unexpected complexity[J]. Adv. Eng. Mater., 2010, 12: 559
[17] Yamada K, Sato T, Kamio A. Effects of quenching conditions on two-step aging behavior of Al-Mg-Si Alloys [J]. Mater. Sci. Forum, 2000, 331-337: 669
[18] Banhart J, Lay M D H, Chang C S T, et al. Kinetics of natural aging in Al-Mg-Si alloys studied by positron annihilation lifetime spectroscopy[J]. Phys. Rev., 2011, 83B: 014101
[19] Zurob H S, Seyedrezai H.A model for the growth of solute clusters based on vacancy trapping[J]. Scr. Mater., 2009, 61: 141
[20] Liu C H, Lai Y X, Chen J H, et al.Natural-aging-induced reversal of the precipitation pathways in an Al-Mg-Si alloy[J]. Scr. Mater., 2016, 115: 150
[21] Chang C S, Wieler I, Wanderka N, et al.Positive effect of natural pre-ageing on precipitation hardening in Al-0.44at% Mg-0.38at% Si alloy[J]. Ultramicroscopy, 2009, 109: 585
[22] Saga M, Kikuchi M.Effect of Sn Addition on the two-step aging behavior in Al-Mg-Si Alloys for automotive application [A]. Proceedings of the 9th International Conference on Aluminium Alloys[C]. Melbourne: Institute of Material Engineering Australasia Ltd, 2004: 520
[23] Pogatscher S, Antrekowitsch H, Werinos M, et al.Diffusion on demand to control precipitation aging: application to Al-Mg-Si alloys[J]. Phys. Rev. Lett., 2014, 112: 225701
[24] Werinos M, Antrekowitsch H, Fragner W, et al.Influence of temperature on natural aging kinetics of AA6061 modified with Sn[A]. Light Metals 2015 [M]. Cham: Springer International Publishing, 2015: 367
[25] Werinos M, Antrekowitsch H, Kozeschnik E, et al.Ultrafast artificial aging of Al-Mg-Si alloys[J]. Scr. Mater., 2016, 112: 148
[26] Shishido H, Takaki Y, Kozuka M, et al.Effects of Sn addition on clustering and age-hardening behavior in a pre-aged Al-Mg-Si alloy[J]. Mater. Sci. Forum, 2016, 877: 455
[27] Pogatscher S, Antrekowitsch H, Ebner T, et al.The role of co-clusters in the artificial aging of AA6061 and AA6060 [A]. Light Metals 2012[C]. New York: Springer, 2012: 415
[28] Murayama M, Hono K.Pre-precipitate clusters and precipitation processes in Al-Mg-Si-Cu alloys[J]. Acta Mater., 1999, 47: 1537
Outlines

/