Distribution Characteristics of Twin-Boundaries in Three-Dimensional Grain Boundary Network of 316L Stainless Steel

  • Tingguang LIU ,
  • Shuang XIA ,
  • Qin BAI ,
  • Bangxin ZHOU ,
  • Yonghao LU
Expand
  • 1 National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China
    2 School of Materials Science and Engineering, Shanghai University, Shanghai 200072, China

Received date: 2018-02-12

  Online published: 2018-06-27

Supported by

Supported by National Natural Science Foundation of China (Nos.51701017 and 51671122), Fundamental Research Funds for the Central Universities (No.FRF-TP-16-041A1) and Beijing Natural Science Foundation (No.2182044)

Abstract

Grain boundaries are sources of failure and weakness due to their relatively excess free volume compared to the lattice of polycrystalline materials exposed to aggressive environment. The control of grain boundary degradation has become one of the key issues of materials science and engineering. It has been found that the coincidence site lattice (CSL) boundaries, especially Σ3 (the twin boundaries), have stronger resistance to intergranular degradation than random boundaries. Materials with a high proportion of CSL boundaries that could disrupt the connectivity of random boundaries have better performance to resist intergranular failures. However, the distribution characteristics of twin boundaries in grain boundary network are still unclear. In this work, three-dimensional electron backscatter diffraction (3D-EBSD) was used to map the 3D grain boundary network of a 316L stainless steel. The topological characteristics of triple junction and quadruple junction in the presence of twin boundaries were investigated. The distribution of twin boundaries around grains and grain boundaries was analyzed. The results show that the twin boundary number fraction in the 3D grain boundary network is lower than the measured twin boundary area fraction, indicating that the average area per twin boundary is larger than random boundary. Most of triple junctions in the 316L stainless steel have one twin boundary. The proportion of triple junctions with two twin boundaries is about 9.4%. A quadruple junction has three twin boundaries at most. Most of quadruple junctions have one or two twin boundaries. About 7.9% of quadruple junctions have three twin boundaries. The 3D-EBSD data of 316L includes 1840 grains, 7353 random boundaries and 1824 twin boundaries. On average, a 3D grain in the 3D microstructure has 11 faces (39.85 neighboring faces that includes all boundaries of the grain and all boundaries that connected with the grain by lines or points), in which the number of twin boundaries is 2.03 (8.02) on average. A 3D grain boundary has 9.35 neighboring boundaries, in which the number of twin boundaries is 1.99 on average.

Cite this article

Tingguang LIU , Shuang XIA , Qin BAI , Bangxin ZHOU , Yonghao LU . Distribution Characteristics of Twin-Boundaries in Three-Dimensional Grain Boundary Network of 316L Stainless Steel[J]. Acta Metall Sin, 2018 , 54(10) : 1377 -1386 . DOI: 10.11900/0412.1961.2018.00062

References

[1] Cahn R W.The Coming of Materials Science[M]. Oxford: Pergamon, 2001: 213
[2] Meyers M A, Chawla K K.Mechanical Behavior of Materials [M]. 2nd Ed., Cambridge: Cambridge University Press, 2009: 346
[3] Bhandari Y, Sarkar S, Groeber M, et al.3D polycrystalline microstructure reconstruction from FIB generated serial sections for FE analysis[J]. Comput. Mater. Sci., 2007, 41: 222
[4] Liu T G, Xia S, Bai Q, et al.Morphological characteristics and size distributions of three-dimensional grains and grain boundaries in 316L stainless steel[J]. Acta Metall. Sin., 2018, 54: 868(刘廷光, 夏爽, 白琴等. 316L不锈钢的三维晶粒与晶界形貌特征及尺寸分布[J]. 金属学报, 2018, 54: 868)
[5] Ullah A, Liu G Q, Luan J H, et al.Three-dimensional visualization and quantitative characterization of grains in polycrystalline iron[J]. Mater. Charact., 2014, 91: 65
[6] Gottstein G, Shvindlerman L S.Grain boundary junction engineering[J]. Scr. Mater., 2006, 54: 1065
[7] Frary M, Schuh C A.Connectivity and percolation behaviour of grain boundary networks in three dimensions[J]. Philos. Mag., 2005, 85: 1123
[8] Gertsman V Y.Coincidence site lattice theory of multicrystalline ensembles[J]. Acta Crystallogr., 2001, 57A: 649
[9] Li S F, Mason J K, Lind J, et al.Quadruple nodes and grain boundary connectivity in three dimensions[J]. Acta Mater., 2014, 64: 220
[10] Reed B W, Minich R W, Rudd R E, et al.The structure of the cubic coincident site lattice rotation group[J]. Acta Crystallogr., 2004, 60A: 263
[11] Randle V.The Role of the Coincidence Site Lattice in Grain Boundary Engineering [M]. London: Cambridge University Press, 1996: 1
[12] Liu T G, Xia S, Bai Q, et al.Three-dimensional study of grain boundary engineering effects on intergranular stress corrosion cracking of 316 stainless steel in high temperature water[J]. J. Nucl. Mater., 2018, 498: 290
[13] Hu C L, Xia S, Li H, et al.Effect of grain boundary network on the intergranular stress corrosion cracking of 304 stainless steel[J]. Acta Metall. Sin., 2011, 47: 939(胡长亮, 夏爽, 李慧等. 晶界网络特征对304不锈钢晶间应力腐蚀开裂的影响[J]. 金属学报, 2011, 47: 939)
[14] Zhang Z L, Xia S, Cao W, et al.Effects of grain boundary character on intergranular stress corrosion cracking initiation in 316 stainless steel[J]. Acta Metall. Sin., 2016, 52: 313(张子龙, 夏爽, 曹伟等. 晶界特征对316不锈钢沿晶应力腐蚀开裂裂纹萌生的影响[J]. 金属学报, 2016, 52: 313)
[15] Gertsman V Y, Bruemmer S M.Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys[J]. Acta Mater., 2001, 49: 1589
[16] Shi F, Tian P C, Jia N, et al.Improving intergranular corrosion resistance in a nickel-free and manganese-bearing high-nitrogen austenitic stainless steel through grain boundary character distribution optimization[J]. Corros. Sci., 2016, 107: 49
[17] Hu C L, Xi S, Li H, et al.Improving the intergranular corrosion resistance of 304 stainless steel by grain boundary network control[J]. Corros. Sci., 2011, 53: 1880
[18] Kobayashi S, Kobayashi R, Watanabe T.Control of grain boundary connectivity based on fractal analysis for improvement of intergranular corrosion resistance in SUS316L austenitic stainless steel[J]. Acta Mater., 2016, 102: 397
[19] Jothi S, Merzlikin S V, Croft T N, et al.An investigation of micro-mechanisms in hydrogen induced cracking in nickel-based superalloy 718[J]. J. Alloys Compd., 2016, 664: 664
[20] Xia S, Li H, Liu T G, et al.Appling grain boundary engineering to Alloy 690 tube for enhancing intergranular corrosion resistance[J]. J. Nucl. Mater., 2011, 416: 303
[21] Deepak K, Mandal S, Athreya C N, et al.Implication of grain boundary engineering on high temperature hot corrosion of alloy 617[J]. Corros. Sci., 2016, 106: 293
[22] Li H, Xia S, Zhou B X, et al.The dependence of carbide morphology on grain boundary character in the highly twinned Alloy 690[J]. J. Nucl. Mater., 2010, 399: 108
[23] Watanabe T.An approach to grain boundary design for strong and ductile polycrystals[J]. Res. Mech., 1984, 11: 47
[24] Lin P, Palumbo G, Erb U, et al.Influence of grain boundary character distribution on sensitization and intergranular corrosion of alloy 600[J]. Scr. Metall. Mater., 1995, 33: 1387
[25] Lehockey E M, Limoges D, Palumbo G, et al.On improving the corrosion and growth resistance of positive Pb-acid battery grids by grain boundary engineering[J]. J. Power Sources, 1999, 78: 79
[26] Watanabe T.Grain boundary engineering: Historical perspective and future prospects[J]. J. Mater. Sci., 2011, 46: 4095
[27] Randle V.Grain boundary engineering: An overview after 25 years[J]. Mater. Sci. Technol., 2010, 26: 253
[28] Michiuchi M, Kokawa H, Wang Z J, et al.Twin-induced grain boundary engineering for 316 austenitic stainless steel[J]. Acta Mater., 2006, 54: 5179
[29] Randle V.Mechanism of twinning-induced grain boundary engineering in low stacking-fault energy materials[J]. Acta Mater., 1999, 47: 4187
[30] Randle V, Coleman M.A study of low-strain and medium-strain grain boundary engineering[J]. Acta Mater., 2009, 57: 3410
[31] Liu T G, Xia S, Li H, et al.Effect of the pre-existing carbides on the grain boundary network during grain boundary engineering in a nickel based alloy[J]. Mater. Charact., 2014, 91: 89
[32] Liu T G, Xia S, Shoji T, et al.The topology of three-dimensional grain boundary network and its influence on stress corrosion crack propagation characteristics in austenitic stainless steel in a simulated BWR environment[J]. Corros. Sci., 2017, 129: 161
[33] Groeber M A, Jackson M A.DREAM.3D: A digital representation environment for the analysis of microstructure in 3D[J]. Integr. Mater. Manuf. Innov., 2014, 3: 5
[34] Brandon D G.The structure of high-angle grain boundaries[J]. Acta Metall., 1966, 14: 1479
[35] Ankem S, Pande C S, Ovid'ko I, et al. Science and Technology of Interfaces[M]. Hoboken: John Wiley & Sons, Inc., 2002: 387
[36] Marrow T J, Babout L, Jivkov A P, et al.Three dimensional observations and modelling of intergranular stress corrosion cracking in austenitic stainless steel[J]. J. Nucl. Mater., 2006, 352: 62
Outlines

/