Orginal Article

Modification Mechanism of Cerium on the Inclusions in Drill Steel

  • Yu HUANG ,
  • Guoguang CHENG ,
  • You XIE
Expand
  • 1 State Key Laboratory of Advanced Metallurgy, University of Science and Technology Beijing, Beijing 100083, China
    2 Zenith Steel Group Co., Ltd., Changzhou 213011, China

Received date: 2018-03-05

  Online published: 2018-06-07

Supported by

Supported by National Natural Science Foundation of China (No.51674024)

Abstract

Fatigue fracture is the main failure forms of drill steel, and the hard oxide with large size is one of the main reasons for the fatigue fracture of drill steel. Therefore, the miniaturization and softening of inclusion can effectively improve the anti-fatigue performance of drill steel and prolong its service life. Rare earth elements have very good affinity with oxygen and sulfur in molten steel, and the hardness of resulting rare earth compounds is very low. In this work, the rare earth element cerium was added into drill steel to investigate the effect of Ce on the MgAl2O4 and sulfides. The composition, morphology, number, and size of inclusions in drill steel were analyzed by using SEM and EDS. The evolution process and modification mechanism of Ce on MgAl2O4 and sulfides were clarified by experimental results and calculated by thermodynamic software. The type of inclusions in drill steel without Ce addition is MgAl2O4 and (Ca, Mn)S. As the Ce content in drill steel reaches to 0.0078% (mass fraction), the type of inclusions changes to Ce-O and Ce-S. In addition, a few complex inclusions, mixture of Ce-O and MgO, were also found. The size of inclusions in drill steel decreases significantly as the oxides and sulfides were modified into Ce-O and Ce-S. The calculated results show that MgAl2O4 and (Ca, Mn)S in drill steel can be effectively modified into Ce-O and Ce-S as the Ce added into molten steel, and the modification sequence of Ce on the MgAl2O4 is as follows: MgAl2O4→CeAlO3+MgO→Ce2O3+MgO→Ce2O3. The content of Ce in drill steel has great influence on the type of inclusions. The modification mechanism of Ce on MgAl2O4 calculated by Factsage 6.3 agrees well with the experimental observations.

Cite this article

Yu HUANG , Guoguang CHENG , You XIE . Modification Mechanism of Cerium on the Inclusions in Drill Steel[J]. Acta Metall Sin, 2018 , 54(9) : 1253 -1261 . DOI: 10.11900/0412.1961.2018.00079

References

[1] Hu Z G.Research and development of drill steel and drill tools[J]. Rock Drill. Mach. Pneum. Tools, 2011, (4): 6(胡支国. 钎钢钎具产品的研制与开发[J]. 凿岩机械气动工具, 2011, (4): 6)
[2] Li B X.Failure analysis and fracture mechanism of whorl drill steel[J]. Rock Drill. Mach. Pneum. Tools, 1999, (2): 55(黎炳雄. 螺纹钎杆的失效分析和断裂机理[J]. 凿岩机械气动工具, 1999, (2): 55)
[3] Liang X J.Study on the substitution of domestic materials and manufacturing technology for rock drill[D]. Taiyuan: Taiyuan University of Science & Technology, 2014(梁晓捷. 凿岩钎具国产材料替代及制造工艺的研究[D]. 太原: 太原科技大学, 2014)
[4] Zhou F Y, Xu Z H.Failure analysis of the heavy drill rod made in China[J]. Mater. Mech. Eng., 1997, 21(3): 47(周凤云, 徐志宏. 国产重型凿岩钎杆的失效分析[J]. 机械工程材料, 1997, 21(3): 47)
[5] Zhu H W, Liu Y Z, Zhou L Y, et al.Failure analysis of 22Si2MnCrNi2MoA drilling rods[J]. J. Univ. Sci. Technol. Beijing, 2013, 35: 613(朱洪武, 刘雅政, 周乐育等. 22Si2MnCrNi2MoA钎杆断裂失效分析[J]. 北京科技大学学报, 2013, 35: 613)
[6] Yan Y M, Liu Y Z, Zhou L Y, et al.Influence of heat treatment process on microstructure and properties of 23CrNi3Mo steel[J]. Trans. Mater. Heat Treat., 2014, 35: 110(闫永明, 刘雅政, 周乐育等. 热处理工艺对23CrNi3Mo钎具钢组织及性能的影响[J]. 材料热处理学报, 2014, 35: 110)
[7] Hong D L, Gu T H, Xu S G, et al.Drill Steel and Drilling Tools [M]. Beijing: Metallurgical Industry Press, 2000: 24(洪达灵, 顾太和, 徐曙光等. 钎钢与钎具 [M]. 北京: 冶金工业出版社, 2000: 24)
[8] Tanaka K, Mura T.A theory of fatigue crack initiation at inclusions[J]. Metall. Trans., 1982, 13A: 117
[9] Wang Q Y, Bathias C, Kawagoishi N, et al.Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength[J]. Int. J. Fatigue, 2002, 24: 1269
[10] Gall K, Horstemeyer M F, Degner B W, et al.On the driving force for fatigue crack formation from inclusions and voids in a cast A356 aluminum alloy[J]. Int. J. Fract., 2001, 108: 207
[11] Melander A.A finite element study of short cracks with different inclusion types under rolling contact fatigue load[J]. Int. J. Fatigue, 1997, 19: 13
[12] Zhang J M, Li S X, Yang Z G, et al.Influence of inclusion size on fatigue behavior of high strength steels in the gigacycle fatigue regime[J]. Int. J. Fatigue, 2007, 29: 765
[13] Monnot J, Heritier B, Cogne J Y.Relationship of melting practice, inclusion type, and size with fatigue resistance of bearing steels [A]. Effect of Steel Manufacturing Processes on the Quality of Bearing Steels[C]. West Conshohocken: ASTM International, 1988: 149
[14] Wang L M, Lin Q, Ji J W, et al. New study concerning development of application of rare earth metals in steels [J]. J. Alloys Compd., 2006, 408-412: 384
[15] Waudby P E.Rare earth additions to steel[J]. Int. Met. Rev., 1978, 23: 74
[16] Yang X H, Wu P F, Cheng G G, et al.Behavior of rare earth on modifying inclusion in special steel[J]. J. Chin. Rare Earth Soc., 2010, 28: 612(杨晓红, 吴鹏飞, 成国光等. 特殊钢中稀土变质夹杂物行为研究[J]. 中国稀土学报, 2010, 28: 612)
[17] Wang L J, Liu Y Q, Wang Q, et al.Evolution mechanisms of MgO·Al2O3 inclusions by cerium in spring steel used in fasteners of high-speed railway[J]. ISIJ Int., 2015, 55: 970
[18] Hirata H, Isobe K.Steel having finely dispersed inclusions [P]. U.S. Pat, 20060157162A1, 2004
[19] Liu X, Yang J C, Yang L, et al.Effect of Ce on inclusions and impact property of 2Cr13 stainless steel[J]. J. Iron Steel Res. Int., 2010, 17: 59
[20] Wakoh M, Sawai T, Mizoguchi S.Effect of S content on the MnS precipitation in steel with oxide nuclei[J]. ISIJ Int., 1996, 36: 1014
[21] Verma N, Pistorius P C, Fruehan R J, et al.Calcium modification of spinel inclusions in aluminum-killed steel: Reaction steps[J]. Metall. Mater. Trans., 2012, 43B: 830
[22] Liu H L, Liu C J, Jiang M F.Effect of rare earths on impact toughness of a low-carbon steel[J]. Mater. Des., 2012, 33: 306
[23] Yan N, Yu S F, Chen Y.In situ observation of austenite grain growth and transformation temperature in coarse grain heat affected zone of Ce-alloyed weld metal[J]. J. Rare Earths, 2017, 35: 203
[24] Hao F F, Liao B, Li D, et al.Effects of rare earth oxide on hardfacing metal microstructure of medium carbon steel and its refinement mechanism[J]. J. Rare Earths, 2011, 29: 609
[25] Wang L M.Application of Rare Earth in Low Alloy and Alloy Steel [M]. Beijing: Metallurgical Industry Press, 2016: 16(王龙妹. 稀土在低合金及合金钢中的应用 [M]. 北京: 冶金工业出版社, 2016: 16)
[26] Li W C.Thermodynamics of the formation of rare-earth inclusions in steel[J]. Iron Steel, 1986, 21(3): 7(李文超. 钢中稀土夹杂物生成的热力学规律[J]. 钢铁, 1986, 21(3): 7)
[27] Adabavazeh Z, Hwang W S, Su Y H.Effect of adding cerium on microstructure and morphology of Ce-based inclusions formed in low-carbon steel[J]. Sci. Rep., 2017, 7: 46503
[28] Ma Q Q, Wu C C, Cheng G G, et al.Characteristic and formation mechanism of inclusions in 2205 duplex stainless steel containing rare earth elements[J]. Mater. Today, 2015, 2: S300
[29] Wilson W G, Kay D, Vahed A.The use of thermodynamics and phase equilibria to predict the behavior of the rare earth elements in steel[J]. JOM, 1974, 26(5): 14
Outlines

/