Special Issue for the Solidification of Metallic Materials

Directional Solidification Under High Thermal Gradient and Its Application in Superalloys Processing

  • Lin LIU ,
  • Dejian SUN ,
  • Taiwen HUANG ,
  • Yanbin ZHANG ,
  • Yafeng LI ,
  • Jun ZHANG ,
  • Hengzhi FU
Expand
  • State Key Laborotory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China

Received date: 2018-02-28

  Online published: 2018-05-21

Supported by

Supported by National Natural Science Foundation of China (Nos.51331005, 51631008, 51690163 and 51771148), and National Key Research and Development Program (Nos.2016YFB0701400 and 2017YFB0702900)

Abstract

Industrial gas turbines (IGTs) are the key equipment to achieving energy strategy, such as energy conservation and clean power generation. When the large and complex IGT blades are fabricated by the conventional Bridgman directional solidification process, the thermal gradients at the solidification front are low and unstable, resulting in some disadvantages: the coarse dendrite structure with severe dendritic segregation, the increased occurrence of casting defects and the poor performance of mechanical properties. These disadvantages provide a good opportunity for rapid development of the directional solidification with high thermal gradient (HG), such as the liquid metal cooling (LMC). In the present work, the physical basis of HG process, the microstructure, mechanical properties, solution heat treatment, and casting defects of the superalloys processed by HG process, have been reviewed. The HG process increases the thermal gradient and the cooling rate, thus permitting microstructural improvements including a more homogeneous fine-dendrite structure with lower elemental segregation and shrinkage porosity, and refinement of carbide, γ′ phase and eutectic, reducing the volume fraction of eutectic and shrinkage porosity. During the solution heat treatment, the HG process increases the incipient melting temperature and reduces the residual segregation as well as the content of solution pore. The HG process could effectively inhibit the formation of freckle chains, increase the critical withdrawal rate of the stray grain formation, and decrease the degree of the misorientation of the <001> grain orientation from the casting axis. Moreover, the HG process could improve the mechanical properties including the stress rupture life, low-cycle fatigue (LCF), high-cycle fatigue properties and short-term strength, but the improvement might be reduced at higher temperature or under the oxidation condition.

Cite this article

Lin LIU , Dejian SUN , Taiwen HUANG , Yanbin ZHANG , Yafeng LI , Jun ZHANG , Hengzhi FU . Directional Solidification Under High Thermal Gradient and Its Application in Superalloys Processing[J]. Acta Metall Sin, 2018 , 54(5) : 615 -626 . DOI: 10.11900/0412.1961.2018.00075

References

[1] Konter M, Thumann M.Materials and manufacturing of advanced industrial gas turbine components[J]. J. Mater. Proc. Technol., 2001, 117: 386
[2] Chang J X, Wang D, Zhang G, et al.Effect of Re and Ta on hot corrosion resistance of Nickel-base single crystal superalloys [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys[C]. Warrendale, PA: TMS, 2016: 177
[3] Link T, Zabler S, Epishin A, et al.Synchrotron tomography of porosity in single-crystal nickel-base superalloys[J]. Mater. Sci. Eng., 2006, A425: 47
[4] Sato A, Harada H, Yokokawa T, et al.The effects of ruthenium on the phase stability of fourth generation Ni-base single crystal superalloys[J]. Scr. Mater., 2006, 54: 1679
[5] Liu L.The progress of investment casting of nickel-based superalloys[J]. Foundry, 2012, 61: 1273(刘林. 高温合金精密铸造技术研究进展[J]. 铸造, 2012, 61: 1273)
[6] Carter P, Cox D C, Gandin C A, et al.Process modelling of grain selection during the solidification of single crystal superalloy castings[J]. Mater. Sci. Eng., 2000, A280: 233
[7] Bondarenko Y A, Kablov E N, Surova V A, et al.Effect of high-gradient directed crystallization on the structure and properties of rhenium-bearing single-crystal alloy[J]. Met. Sci. Heat Treat., 2006, 48: 360
[8] Gigliotti M F X, Huang S C, Klug F J, et al. GE casting project [R]. Niskayuna: General Electric Corporate, 2004
[9] Kermanpur A, Mehrara M, Varahram N, et al.Improvement of grain structure and mechanical properties of a land based gas turbine blade directionally solidified with liquid metal cooling process[J]. Mater. Sci. Technol., 2008, 24: 100
[10] Clemens M L, Price A, Bellows R S.Advanced solidification processing of an industrial gas turbine engine component[J]. JOM, 2003, 55(3): 27
[11] Ma D X.Development of single crystal solidification technology for production of superalloy turbine blades[J]. Acta Metall. Sin., 2015, 51: 1179(马德新. 高温合金叶片单晶凝固技术的新发展[J]. 金属学报, 2015, 51: 1179)
[12] Hofmeister M, Franke M M, Koerner C, et al.Single crystal casting with fluidized carbon bed cooling: A process innovation for quality improvement and cost reduction[J]. Metall. Mater. Trans., 2017, 48B: 3132
[13] Giamei A F, Tschinkel J G.Liquid metal cooling: A new solidification technique[J]. Metall. Trans., 1976, 7A: 1427
[14] Fitzgerald T J, Singer R F.An analytical model for optimal directional solidification using liquid metal cooling[J]. Metall. Mater. Trans., 1997, 28A: 1377
[15] Elliott A J, Pollock T M, Tin S, et al.Directional solidification of large superalloy castings with radiation and liquid-metal cooling: A comparative assessment[J]. Metall. Mater. Trans., 2004, 35A: 3221
[16] Wang F, Ma D X, Bogner S, et al.Comparative investigation of the downward and upward directionally solidified single-crystal blades of superalloy CMSX-4[J]. Metall. Mater. Trans., 2016, 47A: 2376
[17] Wang F, Ma D X, Zhang J, et al.Effect of local cooling rates on the microstructures of single crystal CMSX-6 superalloy: A comparative assessment of the Bridgman and the downward directional solidification processes[J]. J. Alloys Compd., 2014, 616: 102
[18] Wang F, Ma D X, Zhang J, et al.Microstructural evolution of aluminium-copper alloys during the downward directional solidification process[J]. Int. J. Mater. Res., 2014, 105: 168
[19] Liu L, Huang T W, Qu M, et al.High thermal gradient directional solidification and its application in the processing of nickel-based superalloys[J]. J. Mater. Proc. Technol., 2010, 210: 159
[20] Lohmuller A, Eber W, Grobmann J, et al.Improved quality and economics of investment castings by liquid metal cooling: The selection of cooling media [A]. Superalloys 2000[C]. Warrendale, PA: TMS, 2000: 181
[21] Huang T W, Liu L, Zhang W G, et al.A compound induction heating device in the directional solidification apparatus with the high thermal gradient [P]. Chin Pat, 200710017592.8, 2007(黄太文, 刘林, 张卫国等. 一种高温度梯度定向凝固的复合感应加热装置[P]. 中国专利, 200710017592.8, 2007)
[22] Zhang W G, Huang T W, Liu L, et al.A conical graphite induction heater in the directional solidification apparatus with the high thermal gradient [P]. Chin Pat, 200810017988.7, 2008(张卫国, 黄太文, 刘林等. 高温度梯度定向凝固锥形石墨感应加热器 [P]. 中国专利, 200810017988.7, 2008)
[23] Zhang J, Liu L, Fu H Z, et al.A zone intensified overheating by resistance heater in the directional solidification apparatus [P]. Chin Pat, 201010142263.8, 2010(张军, 刘林, 傅恒志等. 一种局部强化电阻加热高梯度定向凝固装置 [P]. 中国专利, 201010142263.8, 2010)
[24] Liu L, Ge B M, Zhang J, et al. A composite insulation baffle utilized in the directional solidification apparatus [P]. Chin Pat, 201110087122.5, 2011(刘林, 葛丙明, 张军等.一种定向凝固用复合隔热挡板 [P]. 中国专利, 201110087122.5, 2011)
[25] Hunt J D.Cellular and primary dendrite spacings [A]. International Conference on Solidification and Casting of Metals[C]. London: The Metal Society, 1979: 3
[26] Balsone S, Feng G F, Peterson L, et al.Microstructure and mechanical behavior of liquid metal cooled directionally solidified GTD-444 [A]. Solidification Processes and Microstructures—A Symposium in Honor of Wilfried Kurz[C]. Charlotte: TMS, 2004: 77
[27] Brundidge C L, Van Drasek D, Wang B, et al.Structure refinement by a liquid metal cooling solidification process for single-crystal nickel-base superalloys[J]. Metall. Mater. Trans., 2012, 43A: 965
[28] Brundidge C L, Miller J D, Pollock T M.Development of dendritic structure in the liquid-metal-cooled, directional-solidification process[J]. Metall. Mater. Trans., 2011, 42A: 2723
[29] Elliott A J, Karney G B, Gigliotti M F X, et al. Issues in processing by the liquid-Sn assisted directional solidification technique [A]. Superalloys 2004[C]. Warrendale, PA: TMS, 2004: 421
[30] Franke M M, Hilbinger R M, Lohmüller A, et al.The effect of liquid metal cooling on thermal gradients in directional solidification of superalloys: Thermal analysis[J]. J. Mater. Process. Technol., 2013, 213: 2081
[31] Lamm M, Singer R F.The effect of casting conditions on the high-cycle fatigue properties of the single-crystal nickel-base superalloy PWA 1483[J]. Metall. Mater. Trans., 2007, 38A: 1177
[32] Steuer S, Villechaise P, Pollock T M, et al.Benefits of high gradient solidification for creep and low cycle fatigue of AM1 single crystal superalloy[J]. Mater. Sci. Eng., 2015, A645: 109
[33] Bondarenko Y A, Kablov E N.Directional crystallization of high-temperature alloys with elevated temperature gradient[J]. Met. Sci. Heat Treat., 2002, 44: 288
[34] Bondarenko Y A, Kablov E N, Morozova G I.Effect of high-gradient directed crystallization on the structure and phase composition of a high-temperature alloy of the type RENE-N5[J]. Met. Sci. Heat Treat., 1999, 41: 61
[35] Liu L, Huang T W, Zhang J, et al.Microstructure and stress rupture properties of single crystal superalloy CMSX-2 under high thermal gradient directional solidification[J]. Mater. Lett., 2007, 61: 227
[36] Liu C, Li K W, Shen J, et al.Improved castability of directionally solidified, Ni-based superalloy by the liquid metal cooling process[J]. Metall. Mater. Trans., 2012, 43A: 405
[37] Fan Z D, Wang D, Liu C, et al.Low-cycle fatigue properties of nickel-based superalloys processed by high-gradient directional solidification[J]. Acta Metall. Sin.(Engl. Lett.), 2017, 30: 878
[38] Kuleshova E A, Cherkasova E R, Logunov A V.Dendritic segregation in heat-resistant nickel alloys[J]. Met. Sci. Heat Treat., 1981, 23: 392
[39] Zhao K, Ma Y H, Lou L H.Improvement of creep rupture strength of a liquid metal cooling directionally solidified nickel-base superalloy by carbides[J]. J. Alloys Compd., 2009, 475: 648
[40] Bondarenko Y A, Echin A B, Surova V A, et al.Special features of the structure of single-crystal refractory nickel alloy under directed crystallization[J]. Met. Sci. Heat Treat., 2017, 59: 39
[41] Zhang W G, Liu L, Huang T W, et al.Effect of cooling rate on γ' precipitate of DZ4125 alloy under high thermal gradient directional solidification[J]. Acta Metall. Sin., 2009, 45: 592(张卫国, 刘林, 黄太文等. 高温度梯度定向凝固冷却速率对DZ4125合金γ'相的影响[J]. 金属学报, 2009, 45: 592)
[42] Liu G, Liu L, Zhao X B, et al.Microstructure and microsegregation in a Ni-based single crystal superalloy directionally solidified under high thermal gradient[J]. Acta Metall. Sin., 2010, 46: 77(刘刚, 刘林, 赵新宝等. 一种镍基单晶高温合金的高温度梯度定向凝固组织及枝晶偏析[J]. 金属学报, 2010, 46: 77)
[43] Zhao X B, Liu L, Yu Z, Zhang W H, et al.Influence of directional solidification variables on the microstructure and crystal orientation of AM3 under high thermal gradient[J]. J. Mater. Sci., 2010, 45: 6101
[44] Kurz W, Fisher D J.Fundamental of Solidification[M]. 4th Ed., Switzerland: Trans Tech Publications Ltd, 1998: 19
[45] Miller J D, Pollock T M.Stability of dendrite growth during directional solidification in the presence of a non-axial thermal field[J]. Acta Mater., 2014, 78: 23
[46] Pollock T M, Murphy W H.The breakdown of single-crystal solidification in high refractory nickel-base alloys[J]. Metall. Mater. Trans., 1996, 27A: 1081
[47] Schneider M C, Gu J P, Beckermann C, et al.Modeling of micro- and macrosegregation and freckle formation in single-crystal nickel-base superalloy directional solidification[J], Metall. Mater. Trans., 1997, 28A: 1517
[48] Meng X B, Li J G, Chen Z Q, et al.Effect of Platform dimension on the dendrite growth and stray grain formation in a Ni-base single-crystal superalloy[J]. Metall. Mater. Trans., 2013, 44A: 1955
[49] Ma D X, Bührig-Polaczek A.Application of a heat conductor technique in the production of single-crystal turbine blades[J]. Metall. Mater. Trans., 2009, 40B: 738
[50] Siredey N, Boufoussi M, Denis S, et al.Dendritic growth and crystalline quality of nickel-base single grains[J]. J. Cryst. Growth, 1993, 130: 132
[51] Bogdanowicz W, Albrecht R, Sieniawski J, et al.The subgrain structure in turbine blade roots of CMSX-4 superalloy[J]. J. Cryst. Growth, 2014, 401: 418
[52] Stanford N, Djakovic A, Shollock B A, et al.Seeding of single crystal superalloys-role of seed melt-back on casting defects[J]. Scr. Mater., 2004, 50: 159
[53] Li Y F, Liu L, Huang T W, et al.Simulation of stray grain formation in Ni-base single crystal turbine blades fabricated by HRS and LMC techniques[J]. China Foundry, 2017, 14(2): 75
[54] D'Souza N, Ardakani M G, mclean M, et al. Directional and single-crystal solidification of Ni-base superalloys: Part I. The role of curved isotherms on grain selection[J]. Metall. Mater. Trans., 2000, 31A: 2877
[55] Kermanpur A, Rappaz M, Varahram N, et al.Thermal and grain-structure simulation in a land-based turbine blade directionally solidified with the liquid metal cooling process[J]. Metall. Mater. Trans., 2000, 31B: 1293
[56] Price A R, Clemens M L.Improved casting process for large single crystal gas turbine components [A]. Advanced Materials and Processes for Gas Turbines[C]. Warrendale, PA: TMS, 2003: 119
[57] Liu C B, Shen J, Zhang J, et al.Effect of withdrawal rates on microstructure and creep strength of a single crystal superalloy processed by LMC[J]. J. Mater. Sci. Technol., 2010, 26: 306
[58] Zhang J, Lou L H.Directional solidification assisted by liquid metal cooling[J]. J. Mater. Sci. Technol., 2007, 23: 289
[59] McLean M. Investment casting-developments in microstructural control and mechanical performance[J]. Mater. Sci. Technol., 1988, 4: 205
[60] Quested P N, mclean M. Solidification morphologies in directionally solidified Superalloys[J]. Mater. Sci. Eng., 1984, A65: 171
[61] Zhang H, Pei Y, Li S, et al.Effect of process parameters on microstructures and properties of DZ125 superalloy solidified by LMC[J]. Mater. Res. Innov., 2014, 18(suppl.4): S4-385
[62] Khan T, Caron P.Effect of processing conditions and heat treatments on mechanical properties of single-crystal superalloy CMSX-2[J]. Mater. Sci. Technol., 1986, 2: 486
[63] Brundidge C L, Pollock T M.Processing to fatigue properties: Benefits of high gradient casting for single crystal airfoils [A]. Superalloys 2012: 12th International Symposium on Superalloys[C]. Warrendale, PA: TMS, 2012: 379
Outlines

/